IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 741 documents. Displaying 25 entries per page.


Laboratory test to determine the effect on durability of combining biobased building materials with timber in construction
2017 - IRG/WP 17-20604
The use of Structural Insulated panels is a construction approach that is seeing more abundant use and is becoming a widely available method. Preformed units are usually a composite structure which often include a range of bio-based materials such as timber, wool or straw. Traditional laboratory based wood decay tests do not take into account this combination of biobased materials and it may be po...
S F Curling, G A Ormondroyd


Modelling of moisture content in timber bridge details
2017 - IRG/WP 17-20613
The design of details is an important aspect in durability design of timber bridges. Details are often considered the weakest points in bridges due to their tendency to trap and accumulate moisture and thus facilitate decay. When designing maintenance plans and inspection intervals, it is important to know how design choices will come to influence the service life. Moreover, service life and wood ...
J Niklewski, C Brischke, E Frühwald Hansson, L Meyer-Veltrup


Comparative Durability of Timber Bridges in the USA
2017 - IRG/WP 17-20615
As engineers begin to utilize life-cycle-cost design approaches for timber bridges, there is a necessity for more reliable data about their durability and expected service life. This paper summarizes a comprehensive effort to assess the current condition of more than one hundred timber highway bridge superstructures throughout the United States. This national study was jointly administered by the ...
J P Wacker, B K Brashaw


Overview of the treated wood quality control program in the United States with the recent challenges and advances
2017 - IRG/WP 17-20616
In the past two decades, there have been significant and rapid changes in wood protection technologies for residential applications which have moved away from long established heavy duty metal oxide based products such as chromated copper arsenate (CCA). The successor generation of wood protection systems usually contain copper as the primary biocide, in combination with carbon-based co-biocides s...
L Jin


Moisture content as a quality control parameter in thermally modified timber production
2017 - IRG/WP 17-20622
Quality assurance (QA) or factory production control (FPC) is necessary to ensure a proper production process. The requirements of QA/FPC can result from EN and national standards, quality assurance systems, or producer-specific rules. TMT producers must ensure that the process was correct, and to ensure traceability of products. In addition to the electronic records, the material should be che...
W Scheiding, H Turkulin, S Stein


An experimental study of mould growth and wood decay in timber frame walls
2017 - IRG/WP 17-20623
This paper deals with parameters related to the occurrence of mould growth and wood decay in timber frame walls. In a first part, the hygrothermal conditions inside a timber frame wall finished with brick veneer cladding are analysed to get an idea of possible moisture related problems. It is shown that, based on the VTT mould prediction model, there is a mould risk on the interface between the in...
M Vanpachtenbeke, J Van den Bulcke, I De Windt, J Langmans, S Roels, J Van Acker


Ensuring Quality of Treated Wood – Regulations, Certifications and Associative Background in the Field of Wood Protection in Europe
2017 - IRG/WP 17-20626
Beside legal requirements, buyers and end-users of wood preservatives and/or of treated wood and wood-based materials may require additional warranties regarding the quality and the performance of the products available on the market. These greatly enhance the confidence of end-users and the chance for a product of being marketed with a quality label. Additionally, quality control systems and trai...
M Kutnik, M Klamer, E Melcher


Activity of Two Strobilurin Fungicides Against Three Species of Decay Fungi in Agar Plate Tests
2017 - IRG/WP 17-30704
The objective of this study was to examine the toxicity of strobilurin fungicides against wood decay fungi in order to assess their potential to act as a co-biocide for copper-based wood protection. Two strobilurin fungicides, Heritage (50% azoxystrobin active ingredient) and Insignia (20% pyraclostrobin active ingredients), and copper sulfate pentahydrate were tested against one white rot fungus...
J D Tang, T Ciaramitaro, M Tomaso-Peterson, S V Diehl


Efficacy of Erythropleum suaveolens (potrodom) and Distemonanthus benthamianus (bonsamdua) water extractives on the durability of five Ghanaian less used timber species of varying perviousness and retentiveness
2017 - IRG/WP 17-30705
Conventional wood preservatives are not only toxic to target bio-deterioration organisms but also to humans, other organisms and the environment. In an effort to find preservatives that are less toxic or non-toxic to man, other organisms and the environment, efficacy of branch bark and heartwood water extracts (0.65 g/ml) of Erythropleum suaveolens (potrodom) and Distemonanthus benthamianus (bonsa...
A Asamoah, K Frimpong-Mensah, C Antwi-Boasiako


Liquefaction of woody waste: A novel approach in wood protection from CNSL based liquefied wood polyols
2017 - IRG/WP 17-30711
Liquefaction of lingo-cellulosic biomass is one of the thermo-chemical conversion processes for developing new materials, adhesives, preservatives and energy systems. The process also provides an opportunity to utilize waste wood such as saw-dust, woody wastes, branches and twigs for the development of value added products. Thus, this research paper deals with an investigation of antifungal and a...
A Kumar, G B.Nagarajappa, S Singh Chauhan


Bio-friendly wood protection systems - resistance to mould and blue-stain fungi
2017 - IRG/WP 17-30713
With stricter restrictions on the use of biocides and increasing environmental awareness there is a pronounced need for effective bio-friendly protection systems in the wood preservative and wood coating industry. One of the possible pathways is to exploit and utilize natural substances with active biological effects. Silanes, caffeine, natural oils and potassium carbonate were chosen as compounds...
L Ross Gobakken, W Perdoch, B Mazela, P Kwaśniewska-Sip, G Cofta


Weathering protection of European hardwoods through double modification
2017 - IRG/WP 17-30715
Beech and poplar were thermally modified, treated with melamine resin and both treatments were combined. The weathering performance (cracks and general appearance) of modified beech and poplar was assessed in natural weathering and correlated to material properties such as work in bending (WB) and Brinell hardness. In addition, the equilibrium moisture content after exposure of 12 months and subse...
G Behr, A Gellerich, S Bollmus, H Militz


Thermal stability of a wood protective biofinish and the influence of flame retardants on Aureobasidium cells
2017 - IRG/WP 17-30716
In general there is an increasing need for sustainable resources, including sustainable building materials. Wood is one of these sustainable resources and is more used as an outdoor building material. Since unprotected wood will usually be degraded during outdoor exposure, many different protection systems are available on the market. Protection systems containing biocides however might create obs...
S Rensink, E A M Klein Rot, M F Sailer


Prefacricated modular wooden bridges
2017 - IRG/WP 17-40785
The bridge consists of simple, identical pre-fabricated triangular wooden panels joined top and bottom to make up trusses. These trusses are in turn joined together side by side in pairs and are braced to one another to create a girder construction. The deck is carried on top of the trusses, an arrangement which has several advantages for such an uncomplicated structure. It is built up on site, af...
L Jayanetti


Solid Timber Bridges – Latest Developments
2017 - IRG/WP 17-40788
The technology of gluing in wood construction has evolved considerably in recent years. This has been shown especially in timber bridges that Glulam is now the main building material. A further development is the so-called block gluing, which provides a good basis for supporting structures. Numerous bridges, especially in central Europe, appeal by unique design and monolithic and solid construction. These structures base on two main developments: block lamination of glulam and the composite of timber and concrete to one structural system.
F Miebach


The potential and the challenges of acetylated wood in timber bridges - experiences from an ongoing project
2017 - IRG/WP 17-40792
Acetylated wood is known to be a durable and dimensional stable alternative for high performance materials, and has high potential for exterior timber structures. Research has shown that acetylated wood can be effectively bonded by various adhesive types. However, one of the most common used adhesives for timber constructions, Melamine Urea Formaldehyde (MUF), shows a high degree of delamination o...
A Treu, R Bredesen, F Bongers


A summary of history and use of timber bridges in New Zealand
2017 - IRG/WP 17-40801
Wooden bridges have been an important part of road and rail networks in New Zealand. While wooden structures have largely been replaced by concrete and steel on major arteries they still have a place where lightweight, easily assembled structures are needed. These timber bridges may also be a cheaper alternative to other materials in roads which carry relatively low traffic loads. In the last ten ...
D Page, T Singh


Surface Protection of Wood with Metal Acetylacetonates
2017 - IRG/WP 17-40802
Metal acetylacetonates are coordination complexes of metal ions and the acetylacetonate anion. They have diverse uses as catalysts, cross-linking and curing agents and adhesion promotors. Some metal acetylacetonates can photostabilise polymers whereas others are photocatalysts. We hypothesise that the ability of metal acetylacetonates to photostabilise wood will vary depending on the metal in the ...
Yuner Zhu, P D Evans


Durability of energy efficient wooden buildings: a building physical point of view
2017 - IRG/WP 17-40812
The drive for more energy efficient and sustainable buildings resulted in an increased popularity of wooden buildings, even in countries with a masonry tradition. Often guidelines and prescriptions then are copied from other countries. Different climatic boundary conditions and tradition of finishing, though, do require different moisture tolerance criteria. This is clearly the case for water vapo...
S Roels, J Langmans


Corrosion verification experiment of the screw driven into CLT
2017 - IRG/WP 17-40816
Japan has abundant forest resources, but we depend on import for 70 percent of the consumed timber. Japan has the vision which promotes the timber self-sufficiency rate 30% to 50% by 2020. Therefore CLT attracts attention as a new timber material. Japan has a climate with high temperature and humidity, and wooden buildings are often treated with chemicals as a measure against biological deteriorat...
N Wada, H Ishiyama, S Yamamoto


Influence of sea water on timber and metal joints
2017 - IRG/WP 17-40818
In the Great East Japan Earthquake that occurred in March 2011, many buildings suffered from seawater immersion caused by the tsunami. Saito's study revealed that corrosion progresses on metal plate that experienced seawater immersion 1). However, the detailed mechanism of corrosion progresses has not yet been clarified. Therefore, in this study, salinity which is one of causes of corrosion w...
T Nishimura, H Ishiyama, F Hirose, N Wada


Functional silicones used for wood protection: preliminary study
2017 - IRG/WP 17-30720
Due to worldwide regulation the wood preservation domain is constantly changing. Silicones are used for different industrial applications as hydrophobic agents. This property could enable to reduce water uptake of wood treated with these compounds. Treated wood could then be less prone to dimensional variation and fungal attack, those parameters being driven by variations in wood’s moisture cont...
C Reynaud, F Marchal, F Pochon, M Kutnik


UV-curable coatings developed for aesthetic and biological protection of wood outdoors
2017 - IRG/WP 17-40821
To avoid wood greying, dimensional variations, and degradation by biological agents wood is protected with preservation products and coatings when used outdoors. For some wood species used for cladding, a treatment with a preservation product is required, and is frequently additionally protected with a coating. In this study, Mäder Group developed a new UV-curable coating for outdoors application...
C Reynaud, A S Schuller, M Kutnik, L Podgorski


Biocontrol of wood decay insects and nematodes as an alternative to traditional chemical treatments
2018 - IRG/WP 18-10914
The protection of wood has been defined until relatively recently, as the application of a chemical to increase its durability. On the other hand, society is becoming more and more demanding in terms of the use of products which have the minimum ecological impact. This has led many countries to reduce the list of biocidal products that can be used (European Biocides Regulation), therefore it is ne...
L Robertson, J F Galván, F Llinares, R Viñambres, M T de Troya


Liquefied wood polyols: Ecofriendly bio-based preservative for sustainable protection of wood from Termite attack
2018 - IRG/WP 18-10916
The major problems encountered in both indoor and outdoor utilization of wood are biological decay due to termite. The modification of wood with liquefied wood polyols has been found to be effective against termite attack. The liquefaction of wood aims to utilize woody wastes which are being generated during primary and secondary processing of wood in wood based industry. One of promising approach...
A Kumar, A John, T S Mehra, A K Pandey, S Singh Chauhan


Previous Page | Next Page