IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 57 documents. Displaying 25 entries per page.


Surface morphology and short-term water uptake of charred and coated wood
2021 - IRG/WP 21-40916
Charring of the wood surface represents a traditional alternative surface treatment technique with the purpose of aesthetics and protection. By the treatment with flame the surface of wood becomes carbonized and a few millimetres thick charred layer is formed on the top of the wooden element. Further, the charred layer can be removed by brushing, which accentuates the structure of the surface. Add...
J Zigon


Effect of densification of Eucalyptus nitens and E. obliqua on moisture uptake, swelling, decay resistance, and fire performance
2022 - IRG/WP 22-40946
Some Australian Eucalyptus species that are abundantly available have low natural durability and poor resistance to fire. These same species are also extremely difficult to treat with preservatives or fire retardants using conventional pressure treatment methods due to a large proportion of refractory heartwood. The aim of this research was to understand whether thermo-mechanical densification had...
B Hassan, J J Morrell, F Wiesner, W Wu, B Belleville, K C Wood


Modification of Gmelina arborea wood for utilization in Nigeria
2023 - IRG/WP 23-40986
The level of protection achieved by any wood treatment process is dependent on achieving a sufficient uptake and penetration of the treatment chemicals. This phenomenon is also applicable when considering chemical modification of any wood species. The desired changes in physical, mechanical or durability enhancement of treated species can only be achieved beyond a superficial treatment. For this, ...
S O Olaniran, H Militz


Intra-species variability of moisture dynamics in wood
2024 - IRG/WP 24-11040
Moisture dynamics of wood and wood-based materials play a major role in wood durability against different decay organisms. Their impact becomes particularly evident when wood is exposed, but not permanently wet. To date, however, this has only been taken into account indirectly and therefore inadequately when testing the durability of wood. While test methods are available, for example to determin...
C Brischke, H Purps, L Emmerich


International joint field trial on the moisture performance of wood – Set up and first results
2024 - IRG/WP 24-40996
Wood durability to decay stems from its inherent resistance to fungi resistance to fungi. In this regard, wood's ability to withstand moisture uptake plays an important role as the lower threshold for wood decay is a moisture content of 25%. However, the aspect of moisture resistance is not yet sufficiently emphasized as a durability factor, both in the assessment of durability as a material prope...
C Brischke, et al. (33 co-authors)


Moisture uptake in CLT during the construction phase: real construction conditions versus specimens exposed to environment
2025 - IRG/WP 25-41019
The rapid growth in the use of Cross-Laminated Timber (CLT) in construction highlights the need to address durability concerns, particularly in regions with less experience in Mass Timber Construction and favourable climatic conditions for the biological degradation of wood, such as Mediterranean countries. A lack of awareness and deficient construction management can negatively impact the public ...
D Lima, S Duarte, J M Branco, L Nunes (†)


Experimental characterizing of liquid water uptake and release – key to understand moisture-induced decay risk analysis
2025 - IRG/WP 25-41020
Wood can absorb water vapour (sorption) or liquid water (capillarity). Moisture from liquid water (rain, spray water) is often a problem for the performance of wood products used in outdoor structures. Wood is prone to biodegradation when is it too moist for too long periods. Experimental studies that allow conclusions to be drawn about the practical use of wood water uptake are limited due to the...
M Nopens, J T Benthien, J Trautner, C Brischke