Screening of fungal strains for wood extractive degradation
1998 - IRG/WP 98-10254
Fungal strains were screened for their ability to degrade apolar extractives in wood from scots pine. The degradation of total wood extractives by 91 different strains was monitored in stationary batch assays incubated for 6 weeks. The results obtained show that the ability of wood-inhabiting fungi to utilize wood extractives varied greatly, even for different isolates of the same species. Fungal ...
J Dorado, M J Martinez-Inigo, T A van Beek, F W Claassen, J B P A Wijnberg, R Sierra-Alvarez


Biological resistance of furfuryl alcohol-treated wood
1992 - IRG/WP 92-3703
Biological resistance of FFA (furfuryl alcohol)-treated wood was investigated in relation to the rise of ASE (anti-swelling efficiency) resulting from the treatment. Sapwood blocks of Japanese red pine, cedar and beech were vacuum-impregnated with various concentrations of aqueous FFA solutions to get the target levels of% (w/w) RL (resin loading). Air-dried blocks were kept in an oven at 120°C f...
J Y Ryu, Y Imamura, M Takahashi


Copper based wood preservative - A new approach using fixation with resin acids of rosin
2000 - IRG/WP 00-30249
Copper soaps with carboxylic acid groups of resin acids of rosin were shown to be potential long-term wood preservatives. The principle involved is the attachment of copper to the network formed by the inorganic part of the preservative (rosin) through the -COOH groups. The mechanisms of fixation have been studied, and it has been shown that this association could be obtained : (1) by forming the ...
C Roussel, J P Haluk, A Pizzi, M-F Thévenon


Glue-line additives for protecting plywood. A review
1978 - IRG/WP 2102
The conclusions of this review are: 1) Insecticidal glue-line additives can be used satisfactorily to protect plywood against insect attack. 2) It is uncertain, in spite of some claims, wether fungicidal glue-line additives can be similarly used to protect plywood against fungi under damp conditiones. There is a need for further work to validate the mycological tests that may be used to investigat...
R Cockcroft


Degradation of resin constituents in various wood species by the white rot fungus Bjerkandera sp. strain BOS55
1999 - IRG/WP 99-10301
In previous studies, the white-rot fungus Bjerkandera sp. strain BOS55 was shown to cause extensive degradation of lipophilic extractives (resin) in Scots pine wood. Further research was carried out in order to investigate the ability of Bjerkandera sp. for reducing resinous constituents in various softwood (Douglas fir, larch and spruce) and hardwood species (birch, beech and poplar). The greates...
J Dorado, T A Van Beek, F W Claassen, R Sierra-Alvarez


Compatibility of deltamethrin with wood adhesives
1993 - IRG/WP 93-30031
This work presents the studies conducted on the compatibility of deltamethrin when mixed with wood adhesive to manufacture plywood in order to protect the wood against wood-borers insects and termites. The following types of adhesive were tested: PVA, Urea-formaldehyde, phenol-formaldehyde and a formulation based on tannin. The experiments were made in the adhesive manufacturers' laborato...
A M F Oliveira


Algal growth resistance of paints for coating of wood; a laboratory study
1997 - IRG/WP 97-10213
Twelve paints were tested for resistance against algae. In addition, one algicidal compound commercially used for remedial treatments of algal growth on paints was tested for its effectiveness for prevention of algal growth. An agar diffusion bioassay was employed in which paint films on filter paper discs were placed on mineral salt medium and sprayed with an algal suspension containing a mixture...
J Bjurman


A substantively bonded water repellent treatment based on chromium carboxylates
1985 - IRG/WP 3344
Chromium carboxylates soluble in toluene have been synthesised and applied to Scots pine (Pinus sylvestris) sapwood. Without any further treatment, the compounds may be readily leached from wood surfaces with toluene. After a period of heating however, they become fixed to the cell wall, substantial amounts being resistant to leaching even under reflux conditions for several hours. Treatment of wo...
J K Wright, W B Banks, W J Eilbeck


Melamine resins as preservatives results of biological testing
1996 - IRG/WP 96-40061
Based on previous work of the authors on resins, the upgrading of wood with a true solution of a methanol etherificated melamine resin in low aqueous concentration was performed. For the relative assessment of the biological resistance against brown and white-rot fungi were used not only untreated controls of pine sapwood (Pinus sylvestris L.), but also heartwood of European larch (Larix decidua M...
A O Rapp, R-D Peek


Risk of extension of Hylotrupes bajulus attack in glued laminated timber
1977 - IRG/WP 278
Although efficient work-methods and maintenance procedures, which prevent the wood from becoming damp and are therefore successful in considerably reducing and even in excluding the risks of decay, such methods are ineffective in eliminating the risks of infestation and destruction of timber by the House Longhorn Beetle, Hylotrupes bajulus, the chief enemy of softwood timber structures. The possib...
M-M Serment


The resistance of wood coated with different water-borne paints against colonisation by decay fungi
1996 - IRG/WP 96-10165
The susceptibility of wood painted with model paints of known composition to decay fungi was tested without previous weathering. Included in the study were five alkyd emulsion paints and five acrylic paints; one linseed oil paint and two solvent-borne alkyd paints. It was found that several components influenced the susceptibility of these paints. The results of the present study indicate that the...
J Bjurman


Changes in transverse wood permeability during the drying of rimu and radiata pine
1990 - IRG/WP 3636
When softwoods are dried and subsequently impregnated with waterborne preservatives two problems frequently occur, preservative screening of multi-salt preservatives and difficult re-drying. To study the causes, the permeability of rimu and radiata pine wood has been measured along the three principal directions. The radial and tangential permeabilities of the green sapwood of the two species were...
R E Booker


Assessment of the Envelope Effect of Three Hot Oil Treatments: Resistance to Decay by Coniophora puteana and Postia placenta
2006 - IRG/WP 06-40344
Timber of Corsican pine (Pinus nigra var. maritima) and Norway spruce (Picea abies) was treated in hot linseed oil, rapeseed oil and a proprietary resin derived from linseed oil. The samples were immersed in oil or resin under reduced pressure at temperatures of 180°C and 200°C. Very high uptakes of the oils or resin were recorded for pine, while spruce showed lower weight percent gains, below...
M J Spear, C A S Hill, S F Curling, D Jones, M D C Hale


Water repellency and dimensional stabilIty of wodd treated with waterborne resin acids/TOR
2007 - IRG/WP 07-40364
Wood used in above ground applications such as decking undergoes undesired dimensional changes leading to the lumber warping, cupping, splitting, etc. This is a major concern to consumers but it can be reduced by treating lumber with a water repellent. The ability of resin acids, hydrophobic compounds naturally present in southern yellow pines, was examined as a possible water repellent. A wate...
T P Schultz, D D Nicholas, J Shi


Leaching performance, decay and termite resistance of wood treated with boron compounds incorporated with phenol-formaldehyde resin
2009 - IRG/WP 09-30503
A resol-type phenol-formaldehyde (PF) resin was synthesized and designed to penetrate wood incorporated with boron compounds in order to immobilize boron in wood. The leaching performance, decay and termite resistance of treated wood was investigated. Three kinds of boron compounds, that is, boric acid (BA), borax (BX) and disodium octaborate tetrahydrate (DOT), were selected to mix with PF and tw...
Liping Yu, Jinzhen Cao


Properties of strand board bonded with ammonium pentaborate (APB) modified phenol formaldehyde resin
2009 - IRG/WP 09-40455
Ammonium pentaborate (APB) is combined with phenol formaldehyde (PF) resin in this study to develop a high-performance wood-based composite. The effect of APB and its combination with polyethylene glycol (PEG) on the physical, mechanical properties as well as formaldehyde emission of strand board were tested and compared with disodium octaborate tetrahydrateand (DOT) and zinc borate (ZB). The resu...
Wei Gao, Jinzhen Cao


Eco-Friendly Composites from Bagasse and Soy-based Resin
2009 - IRG/WP 09-40462
In this study, bagasse and soy-based resin were used for producing composite materials. The objective of this study was evaluation of some physical and mechanical properties of boards made of various ratios (100:0, 60:40, 40:60 and 0:100) of bagasse to wood fiber mixtures (wt: wt) with addition of Soy/PF resin at three levels (4, 8 and 10%) and 1.5% wax. All properties were tested according to AST...
G Rassam, B Jamnani


Effect of 4 Preservatives on Physical, Mechanical and Mold-Resistant Properties of Bamboo Oriented Strand Boards
2010 - IRG/WP 10-40483
This study investigated the effects of 4 preservative systems on physical, mechanical and mold-resistant properties of bamboo oriented strand board (OSB) panels bonded with urea formaldehyde resin. Preservative A (Zinc Borate), B (IPBC), C (AAC+Borate) and D (carbendazim + prochloraz) were incorporated with strands during blending at three loading levels. The results showed that the mechanical and...
Juwan Jin, Daochun Qin, Wanshu Wei, Kuan Fan


Comparison of colour change in wood clear-coating systems including inorganic and organic UV absorbers for exterior use
2010 - IRG/WP 10-40499
The aim of this work is to compare the performance of inorganic and organic UV absorbers used in a wood coating application against weathering. Our study has investigated the colour changes of selected UV absorbers; hombitec 402 RM from the Sachtleben Company as an inorganic UV absorber, tinuvin 477 DW from the Ciba Company as an organic UV absorber. The study was carried out on two wood species; ...
Ö Özgenç, B Forsthuber, A Teischinger, C Hansmann


Silicon compounds as additives improving alkyd-based wood coatings performance
2010 - IRG/WP 10-40531
The reactivity of cellulose with solvent-born alkyd-based wood coatings supplemented with organosilanes was analyzed. Structural analysis of cellulose subjected to the reaction with organosilanes and following extraction with water was performed using Fourier-transform infrared spectroscopy (FTIR). The analyzed IR spectra comprise bands 1250 cm-1 typical for the SiC group and 800 cm-1 typical for ...
B Mazela, I Ratajczak, K Wichłacz-Szentner, P Hochmańska


Effects of intumescent formulation of vinyl acetate-based coating on flame-retardancy of thin painted red lauan (Parashorea spp.) plywood
2011 - IRG/WP 10-40537
Using intumescent coatings on wood-based materials is an effective method for fire safety. The intumescent coatings consist of four major components: (1) binder resin (BR), (2) carbonizing substance (CS), (3) foam producing substance (FPS) and (4) dehydrating agent (DA). Previous studies have demonstrated that the formulation of the four components strongly influences the performance of coatings. ...
Chih-Shen Chuang, Kuang-Chung Tsai, Te-Hsin Yang, Ming-Kuang Wang, Chun-Han Ko


Effect of P/F ratio, PF concentration and treating method on boron leaching from wood treated with PF modified boron compounds
2011 - IRG/WP 11-30559
In order to immobilize boron in wood, three kinds of resol-type phenol-formaldehyde (PF) resin with different P/F ratios were synthesized in laboratory and incorporated with three types of boron compounds to treat wood. The used boron compounds included boric acid (BA), borax (BX) and disodium octaborate tetrahydrate (DOT). The leaching test of boron from wood blocks was performed according to the...
Liping Yu, Jinzhen Cao


Tannin resin-boron for outdoor wood protection and fire retardancy
2011 - IRG/WP 11-30567
Boron in the form of boric acid is well known for its efficacy against wood destroying organisms, as well as for its high leachability from treated wood when in outside exposure. Moreover, due to the European directive 2008/58/EC, boric acid is only authorized at low levels. In order to keep considering boric acid as an interesting active ingredient for wood protection, the issue is now to fix it ...
M-F Thévenon, G Tondi, N Leménager, S Wieland, A Pizzi


Use of X-Ray Micro-Computed Tomography to Visualize Copper in Preservative Treated Wood
2012 - IRG/WP 12-20488
This study tests the hypothesis that X-ray micro-computed tomography will be able to visualize the distribution of copper in wood treated with a micronized wood preservative containing copper carbonate. A small wood block measuring 12 x 12 x 19 mm was cut from a 2.4 m x 51 mm x 51 mm southern pine batten that had been treated with a micronized wood preservative. Tomograms of the wood block were ob...
P D Evans, A Limaye, H Averdunk, M Turner, T J Senden, M A Knackstedt


Tannin resin-boron associations: Leaching and biological resistance
2012 - IRG/WP 12-30587
The easy leaching of boron in wood preservation formulations has allowed to use this fungicide only for short term applications. The recently discovered adduct with flavonoids allows boron to resist longer periods of time within wood and consequently extend its life. Two different leaching treatments were compared and the fungal and termite decay was examined. The biological tests have shown extre...
G Tondi, S Wieland, N Lemenager, A Petutschnigg, A Pizzi, M-F Thevenon