Your search resulted in 837 documents. Displaying 25 entries per page.
Susceptibility testing protocol for powderpost beetles in Australia
2002 - IRG/WP 02-20242
Several species of lyctine (powderpost) beetle are able to attack a range of hardwood timbers in Australia. Powderpost beetles infest only the starch-containing sapwood of certain
hardwoods and do not infest softwoods. Attack by powderpost beetles on susceptible timber in Australia is almost inevitable and may continue until the food resource is completely utilised. Prevention of powderpost beetl...
B C Peters, J W Creffield, R H Eldridge
The Use of Insect Hormones as Non-Neurotoxic Insecticides in Wood Preservatives
2002 - IRG/WP 02-30277
The ecdyson and juvenile hormone analogues show a clear difference in their effect on the house borer, Hylotrupes bajulus. In the tested dosages, the ecdyson analogues have only a slight ovicidal effect but a very clear effect on old larvae. With a dosage of 1250 mg/m², Halofenozid achieved 100% mortality after 27 weeks and Tebufenozid after 40 weeks.
The two juvenile hormone analogues, Fenoxy...
E Graf, M Barkhoff, R Hamberg, H Büttner, M Pallaske
A new technique for testing decay resistance of framing lumber
2002 - IRG/WP 02-20247
Model house frame units (two studs, top and bottom plates and a central “dwang”) were constructed using short (500-600 mm) lengths of framing timber. Constructed frames were impregnated with water using a mild pressure schedule to raise the initial moisture content to 35-40 % mc. The back face of each unit was then covered with black polyethylene. Two locations at the stud/dwang and stud/botto...
M E Hedley, D Page, B E Patterson
Natural durability of 4 different Larix species tested in soil contact
2002 - IRG/WP 02-10434
Importers of Siberian Larch claimed to have a material which can replace pressure treated wood in soil contact. This gave reason to investigate the durability of 4 different Larix species (L. decidua, L. sibirica, L. decidua x sibirica, L. gmelini var ologenis) coming from 7 different origins in comparison with sapwood of Pinus sylvestris untreated as well as pressure impregnated with retentions o...
A O Rapp, H Viitanen, T Nilsson
L-joint trials: Part 1: Observations on the process of colonisation and decay
2002 - IRG/WP 02-20250
The first trials using the small L-joint, later adopted for use in BS EN 330 and AWPA Standard E9-97 were exposed at BRE in 1975 but all were assessed destructively during the early stages of exposure. The longest running trial which included replicates for long-term exposure will have been exposed for 20 years in July 2002. This paper provides an overview of the results of testing during that p...
J K Carey
Advances in understanding the mode of action of methylene bisthiocyanate against Sphaeropsis sapinea
2002 - IRG/WP 02-30284
The importance of arresting sapstain pre-infection in radiata pine in New Zealand, to prevent downstream sapstain in both logs and sawn timbers has been clearly demonstrated. Efforts are being made to improve the efficacy of diffusible antisapstain agents through improved understanding wood/fungicide/fungus interactions. The mechanism of action of methylene bisthiocyanate (MBT) was investigated u...
T Singh, R N Wakeling, B Kreber, A Stewart
Mechanisms of Protection by NHA Against Fungal Decay
2002 - IRG/WP 02-10429
Treating wood with the water-borne sodium salt of N'-N-naphthaloylhydroxylamine (Na-NHA) protects wood against decay and termite damage. Initial testing indicated little or no inhibition of sapstain fungi, molds, or soft-rot fungi by Na-NHA, suggesting that the
mechanism by which this compound protected wood was complex and not that of a broad-spectrum biocide. Previously, we (Green et...
F Green III, W Henry, T Schultz
Use of mixed populations of microflora to control sapstain on radiata pine
2002 - IRG/WP 02-10427
Most methods of biological control in the wood products field have focused on the use of single species of fungi or bacteria to control sapstain or decay. The approach taken in this study involved applying soil microorganisms, in combination with nutrients and various adjuvants that collectively form the biological control system.
Radiata pine branch discs, autoclaved or fresh, were dipped in ...
C Chittenden, R Wakeling, B Kreber
Field Trials with mini-stakes
2002 - IRG/WP 02-20244
In 1995 an extensive field test program with wood mini-stakes, 8 x 20 x 200 mm, was started. In these trials a large number of parameters are being evaluated, including several new wood preservatives, differently chemically modified woods and natural durability of various wood species. The test sites are three fields in Sweden for in-ground and “close to ground” testing, one subterranean termi...
M Westin, A O Rapp, Y S Hadi, T Nilsson
The Effect on Biological and Moisture Resistance of Epichlorohydrin Chemically Modified Wood
2002 - IRG/WP 02-40224
Southern pine solid wood and fiber were chemically modified with epichlorohydrin to help in understanding the role of moisture in the mechanism of biological effectiveness of chemically modified wood. The solid wood had weight gains from 11% to 34%, while the fiber had weight gains from 9% to 75%. After modification, part of the specimens were water leached
for 2 weeks or extracted for 2 hours ...
R E Ibach, B-G Lee
Creosote losses due to ageing methods prior to laboratory efficacy testing
2002 - IRG/WP 02-20256
Laboratory efficacy testing of creosote is affected by the impact of volatile components on the fungal growth. European test methods for assessing efficacy against Basidiomycetes and soft rot fungi is based on two standard methods, EN 113 and ENV 807 respectively. Combined with both fungal tests two pre-treatment methods are commonly used, namely EN 84 (leaching) and EN 73 (evaporation). Within th...
J Van Acker, K Ghekiere, M Stevens
Artificial weathering exposure as an alternative for standard ageing according to EN 84 (leaching) and EN 73 (evaporation)
2002 - IRG/WP 02-20254
In order to verify potential weaknesses of wood preservatives fungal tests are carried out after ageing of wood preservative treated test blocks. The European standard EN 599 as a framework for efficacy assessment of wood preservatives includes the use of two ageing methods prior to fungal testing, namely a leaching method (EN 84) and an evaporation method (EN 73). The European research project "F...
J Van Acker, M Grinda, D J Dickinson
The Bacterial Biotransformation of IPBC
2002 - IRG/WP 02-10437
The bacterial biotransformation of the biocide IPBC, widely used as an antisapstain wood preservative, was investigated in bacteria isolated from failed wood, soil experiencing IPBC wash-off, and John Innes No. 2 compost. Nine strains of bacteria were isolated, belonging to the genera Alcaligenes, Enterobacter, Microbacterium and Pseudomonas. The sole organic degradation product in an enteric bact...
S R Cook, J Sullivan, D J Dickinson
Evaluation of wood preservatives for Nordic wood preservation class AB
2002 - IRG/WP 02-30297
In the Nordic countries there are restrictions in the use of wood preservatives based on chromium and arsenic. For above ground use, class AB according to the Nordic system, only
copper based preservatives are allowed in Sweden. Thus several new preservatives, copper based or metal free are now used. They have been approved by the Nordic Wood Preservation Council after passing laboratory tests ag...
M-L Edlund, J Jermer
Ecotox Testing of Leachates as an Alternative Approach for Environmental Impact Assessment of Wood Preservatives
2002 - IRG/WP 02-50185
Driven by the implementation of the EU Biocidal Product Directive (BPD) in the environmental assessment of treated wood different methodologies and test strategies are at present under discussion within industry, regulatory authorities and standardizing comittees.
Test procedures for the analytical determination of emissions to different environmental compartments according to exposure scenario...
H-W Wegen
Test methods for modifies wood: The EU-Thematic network approach
2002 - IRG/WP 02-20255
The last decade wood modification systems have become new wood treatment methods in Europe. Alongside several industrial initiatives for heat treatments also scaling up and pilot plant projects for chemical wood modification have recently been carried out. In 2000 an initiative to create a network related to these new developments was supported by the European Commission. Within the work proposed ...
J Van Acker, D Jones
Bethoguard; A new wood protecting fungicide for use in metal free ground contact wood preservatives
2002 - IRG/WP 02-30301
Research has identified the limitations in both the spectrum of activity and permanence of organic biocides placed in wood in high hazard environments, particularly in the absence of heavy metals such as copper. More specifically, the control of soft rot decay in wood in soil contact has proven to be most problematic.
The new organic biocide, Bethoguard; an oxathiazine, has demonstrated excellen...
S C Forster, G R Williams, M Van Der Flaas, M Bacon, J Gors
The use of zirconium as an inert fixative for borates in preservation
2001 - IRG/WP 01-30256
Stand-alone borates have been used in internal protected situations as wood preservatives for about 60 years. They have not been deemed acceptable for external situations because of their leaching characteristics. Work carried out to reduce the leachability of borates has been reviewed briefly here, and a specific fixation agent based on zirconium has been tested in standard leaching and decay tes...
J D Lloyd, J L Fogel, A Vizel
Weather testing of timber - discoloration
2001 - IRG/WP 01-20221
The brightness and color saturation of the timber were reduced over time. The perception of an increasingly dark color in the timber over time is due to the gradual reduction in brightness. The period from May to September was characterized by the greatest discoloration of all three periods of the year. Because this period has the largest number of sunlight hours, and the timber is subjected to a ...
T Toyoda, M Azuma, Y Hikita
The Biocidal Products Directive ( 98/8/EC ) - its consequences for the wood preservation industry
2001 - IRG/WP 01-50166-04
1. The Current Position
This European Union Directive is one of the most technically complex pieces of legislation that has been developed by the European Commission (EC). Although the Directive was to have been implemented in the legislation of individual Member States of the EU by May 2000 progress has been slow. A number of Member States have yet to declare the Competent Authority who will han...
D Aston
Data requirements for wood preservatives in the EU Biocides Directive
2001 - IRG/WP 01-50166-08
Directive 98/8/EC of the European Parliament and of the Council concerning the placing of biocidal products (the Biocidal Products Directive, BPD) lays down the requirements on data needed for authorisation of a biocidal product and approval of its active substance(s). The dossier must contain data needed for the proper risk assessment of the biocidal product. A detailed technical guidance documen...
H Braunschweiler
Fungus cellar testing as an evaluation method for performance of treated timber in ground contact
2001 - IRG/WP 01-20227
A fungus cellar method for the accelerated evaluation of performance of treated wood in ground contact is described. The test soil comprised of sandy loam, vermiculite and Japanese horticulture soil "Kanumatsuchi" in a ratio of 6:2:2 by volume. The soil was inoculated with the dominant test fungus isolated with selective medium from decayed wood samples. Pairs of treated and untreated wood specime...
Y Nagano
The effect of hemicellulose degradation on the mechanical properties of wood during brown rot decay
2001 - IRG/WP 01-20219
Incipient decay of wood by brown rot fungi causes measurable strength losses in wood before measurable weight loss occurs. Previous studies have shown that the high levels of strength loss that occur during incipient brown rot decay may be related to loss in hemicellulose. This paper investigates the effect of decay on hemicellulose composition and the relationship to the mechanical properties of ...
S F Curling, C A Clausen, J E Winandy
The efficacy of Sentry® as a treatment for the control of sapstain in pre-infected radiata pine
2001 - IRG/WP 01-30260
Experiments were conducted to determine the efficacy of Sentry® when used to control sapstain fungi on radiata pine branch billets stored under high fungal hazard conditions. Prior to antisapstain treatment, the billets were pre-infected with a mixed inoculum of staining fungi and held from zero to 10 days at 25°C and 75% relative humidity. This was done to produce billets with different degrees...
C Chittenden, J G van der Waals, B Kreber, R N Wakeling
Wood-based composites exposed to fungal degradation: Laboratory results
2001 - IRG/WP 01-40215
Oriented strandboard (OSB) and laminated veneer lumber (LVL) are widely used as residential construction materials. The durability of OSB and LVL against biological degradation has not been studied comprehensively. The objective of this research was to investigate the durability of OSB and LVL when exposed to wood decay fungi. Fourteen brown-rot and eight white-rot wood decay fungi were screened f...
V W Yang, B Illman, L A Ferge, R J Ross