IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 954 documents. Displaying 25 entries per page.


Status of Work on OECD Test Guidelines for Emissions of Wood Preservatives to the Environment
2005 - IRG/WP 05-50224-3
In April, 2003, OECD published an ESD on wood preservatives that provides guidance on how to estimate emissions: 1) during the wood preservative application processes and storage of treated wood prior to shipment; and 2) from treated wood-in-service. The ad hoc Expert Group that developed the wood preservatives ESD identified the need to develop Test Guidelines to estimate the amount of biocides ...
W Jakob


Five years leaching of Boron
1999 - IRG/WP 99-30195
The diffusibility of Boron in wood and thus its leaching behaviour in water contact is known since long. Nevertheless quantitative data on the long-term leaching behaviour are rare. Consequently, field exposure tests were started with beam-segments treated with pure boric acid and with poles treated with CCB. Detailed data of more than five years of field exposure are now available. Pure boron tre...
A Peylo, H Willeitner


Experiences with the OECD guideline proposals for the estimation of emissions from preservative-treated wood in the environment
2004 - IRG/WP 04-50209
The practicability of 2 CEN proposals for OECD guidelines on the estimation of emissions from preservative treated wood by laboratory methods for either wood held in storage after treatment and for wooden commodities that are not covered, and are not in contact with ground (guideline 1) or wooden commodities that are not covered and are in contact with ground, fresh water or seawater (guideline 2...
U Schoknecht, R Wegner, E Melcher


Laboratory Evaluation and Field Trial of Chlorothalonil and Copper-based Preservatives and Leaching Performance of Copper in Copper Treated Wood
2002 - IRG/WP 02-30279
Soil block test and field trial of some Chinese plantation wood species pine and poplar treated with chlorothalonil formulations and copper-based preservatives such as ACQ-B and copper citrate (CC) were conducted. The results of soil block test indicated that chlorothalonil formulations and ACQ-B as well as CC are very effective for controlling the 2 fungi species Corious versicolor and Poria plac...
Mingliang Jiang, Ping Wang, Chungen Piao, Zhaobang Li, Quan Lu, Lei Liu


Leaching of Boron - more than 3 years of field exposure
1997 - IRG/WP 97-30143
The diffusibility of Boron in wood and thus the ability of its leaching is known since long. Nevertheless quantitative data on this process are only rarely available. To overcome this lack of information field exposure tests were started with beam-segments treated with pure boric acid and poles treated with CCB. In addition some of the beam-segments were surface-treated with a varnish to investiga...
A Peylo, H Willeitner


Chromated copper arsenate preservative treatment of hardwoods. Part 2: leaching performance of seven North American hardwoods
1997 - IRG/WP 97-30132
Seven North American hardwood species were treated with 2% CCA-C solution and fixed at temperatures of 21°C and 50°C and conditions of high relative humidity (95%) as described in Part 1 of this presentation. Red pine (Pinus resinosa) was included as a softwood for comparison. Adequately fixed wood blocks (99.9% chromium fixation) were exposed to leaching tests according to AWPA E11-87 test. Par...
T Stevanovic-Janezic, P A Cooper, Y T Ung


Development of a mini-block test method for the rapid evaluation of preservative performance against Basidiomycte fungi
1991 - IRG/WP 2379
Screening procedures for new biocides used as wood preservatives can be a time consuming process using conventional Basidiomycete assay procedures. This is due mainly to the long exposure periods required to achieve adequate levels of decay (weight loss) in the test blocks. A number of alternative methods have been developed but most utilise artificial substrates such as filter paper or agar in wh...
J Brown, S Caswell, G R Williams


Leaching from field test stakes. Part 2: The distribution in and leaching from different parts of test stakes
1994 - IRG/WP 94-50026
Field test stakes treated with Boliden K33 (copper, chromium and arsenic) and Cuprinol Tryck (CT86) (copper and N-alkylbenzyldimethylammoniumchloride) respectively were exposed in ground contact at two different test fields in Sweden and rejected due to decay after 2 to 28 years. Stakes treated with the same preservatives were also exposed during 7 years above ground. The test stakes have been ana...
F G Evans, B Nossen, M-L Edlund


Methods for the assessment of wood preservative movement in soil
1995 - IRG/WP 95-50040-08
This paper presents preliminary results from a series of experiments constructed to provide laboratory data for the evaluation of the leaching of wood preservatives into and through soil. The experiments included: i) measurement of the adsorption of preservatives by soil; ii) determination of the concentration gradient of preservatives in soil following percolation of preservative solution through...
G E Holland, R J Orsler


Leaching of copper-chrome-arsenic treated timber: Simulated rainfall testing
1996 - IRG/WP 96-50074
Six kiln dried radiata pine sapwood packs of timber were preservative treated with copper-chrome-arsenic preservative using a modified Bethell treatment schedule. The packs were then subjected to simulated rain leaching at specified periods after treatment. Higher chromium leachate was obtained when higher volumes of simulated rainfall were applied. Lower chromium leachate was obtained for timber ...
S Walley, P R S Cobham, P Vinden


Comparison of laboratory tests and field experiments for the estimation of emissions from treated wood
2005 - IRG/WP 05-50224-6
The authorisation procedure for biocidal products according to the European Biocides Direc¬tive in¬cludes the assessment of possible environmental risks by the emission of ac¬tive ingre¬dients. This needs an input of data on the expected emissions of biocides into environmental com¬part¬ments. The procedures for the estimation of these emissions should be harmonised. La¬boratory test proceÂ...
U Schoknecht


Depletion of preservatives from treated wood: Results from laboratory, fungus cellar and field test
1993 - IRG/WP 93-50001-07
This paper compares results of preservative component losses using a range of test procedures with several different water-borne preservatives. The data shows that laboratory leaching tests are in some cases comparable to, but in other cases significantly underestimate preservative component losses when compared with field or fungus cellar depletion tests. The results also suggest that preservativ...
L Jin, A F Preston


Leaching of components from CCF treated timber in ground contact
1998 - IRG/WP 98-50108
In order to investigate the depletion of different CCF-salts during service small stakes (10*10*450mm³) were treated with five water-borne wood preservatives and after fixation brought into ground contact for several years. After failing some of the broken down stakes were used to determine the remaining concentration of relevant ions and their distribution in different segments of the stakes. A...
E Melcher


Leaching from field test stakes. Results from two different methods of analysis
1993 - IRG/WP 93-50013
Field test stakes treated with Boliden K33 containing copper, chromium and arsenic exposed at three different fields in Sweden and rejected due to decay, have in two studies been analysed regarding leaching and remaining preservatives. The stakes have been exposed during 20 to 43 years. The density of the stakes and content of copper, chromium and arsenic have been determined in the top part of th...
F G Evans, M-L Edlund


The influence of UV and IR radiation on leaching of copper and chromium from preservative-treated pine and spruce
1992 - IRG/WP 92-3687
The influence of artifical UV- and IR-radiation on the leaching of copper and chromium components of a CCB-preservative from freshly treated pine and spruce was evaluated. On small pinewood samples it could be shown, that the leaching of copper and chromium can considerabely be reduced by UV-radiation. A Philips HPA lamp type reduced the leaching most effective. IR-radiation lead to higher leachin...
H Militz


A comparison of shower test results from CCF, CCZF, CCB and Cu-quat treated timber
1995 - IRG/WP 95-50054
The shower test quantifies the amount of specific preservative components which leach from treated timber under simulated open storage conditions. The test method measures leaching from both organic and inorganic salt treated timber. Shower tests of CCF, CCZF, CCB and Cu-quat treated timber which have been performed over the last 5 years by TNO are reviewed and compared. Leached components are qua...
M J Boonstra, A J Pendlebury, P Esser


Above and Below-Ground Depletion of Copper, Chromium and Arsenic from Pinus radiata and Fagus sylvatica at Thirteen Test Sites in New Zealand and Australia
2006 - IRG/WP 06-30402
The objective was to determine the significance of site and wood species on preservative depletion for a copper chrome arsenate preservative (CCA) from 20 x 20 x 500 mm field test stakes after 5.5 and 4.5 years for pine and beech respectively. At least 5 sacrificial stakes were used to produce site means. Site and wood species had a major effect on copper, chromium and arsenic loss from CCA treate...
R Wakeling


Laboratory Leaching Tests to Study the Effects of Post-Treatment Storage Periods on CCA Leachability and Fixation in Treated Permeable and Refractory Malaysian Hardwoods
2006 - IRG/WP 06-50240
The biological resistance and environmental safety of CCA-treated wood relies on the extent of post-treatment storage fixation of CCA in wood prior to being utilized. A study on the comparative leachability (fixation) of CCA-treated refractory and permeable heartwoods of 3 Malaysian hardwoods subjected to different post-treatment storage (fixation) periods of up to 4 weeks, at 2 laboratory leachin...
A H H Wong, H C Lai, N P T Lim


Comparative Laboratory Leaching Test Methods to Study Post-Treatment Storage Period Impacts on CCA Leachability and Fixation in Treated Kempas (Koompassia malaccensis) Heartwood
2007 - IRG/WP 07-20376
Three laboratory leaching test methods were compared to determine the effects of different post-treatment storage fixation periods on leachability/fixation of CCA components from treated kempas (Koompassia malaccensis) permeable heartwood. End-sealed test wood blocks of permeable were treated with CCA to target retention of 5.6 kg/m3, immediately stored to fix at ambient conditions for 0 and 48 ho...
A H H Wong, H C Lai


Resistance to decay fungi of ammonium borate oleate treated wood
2009 - IRG/WP 09-30505
Ammonium borate oleate molecule (ABO) produced from reaction between boric acid, ammonia and oleic acid was tested as wood preservative treatment against brown and white rot fungi according to European standards. This compound was prepared according to a previous study which has proved existence of synthesis reaction and effectiveness against termites (Lyon et al. 2007b). Four solutions of ABO in ...
F Lyon, M-F Thevenon, A Pizzi, J Gril


Component leaching from CCA, ACQ and a micronized copper quat (MCQ) system as affected by leaching protocol
2009 - IRG/WP 09-50261
Leaching results for Cu, Cr and As (CCA) and Cu (ACQ and MCQ) from southern pine are compared for laboratory tests (AWPA E11, and draft OECD methods I and II) and natural weathering of horizontally and vertically oriented lumber samples over two seasons. This paper expands on results and comparison of results presented at the IRG regional meeting in Costa Rica in Dec 2008 (Cooper and Ung 2008) a...
P A Cooper, Y T Ung


Termite Resistant Properties of Wood and Natural Fiber Plastic Composites - AWPA E1 Test Data
2009 - IRG/WP 09-40466
This paper deals with resistance properties of wood plastic composites against Formosan Subterranean Termites (FSTs) based on the AWPA E1 test standard. Sixteen laboratory WPC formulations, four WPC commercial materials, and southern pine (Pinus sp.) wood control were tested for termite mortality, sample weight loss, and sample damage rating. The results show that FSTs did attack WPC products in ...
Q Wu, T Shupe, J Curole, K Ragon, M Voitier, M Freeman, D Ring


Comparison of laboratory and semi-field tests for the estimation of leaching rates from treated wood
2010 - IRG/WP 10-50274
The authorization of wood preservative formulations in the European Union according to the Biocidal Products Directive (BPD) includes the assessment of environmental risks by the emission of active ingredients. This risk assessment includes scenarios for preserved wood (e.g. house scenario, noise barrier), in which the predicted environmental concentration (PEC) for soil and water is calculated, u...
N Morsing, M Klamer, B Seidel, J Wittenzellner, M Maier, J Habicht


Determination of the natural durability of solid wood against wood-destroying fungi - a European round-robin test
2013 - IRG/WP 13-20511
In Europe the durability of wood against wood-destroying basidiomycetes is tested according to CEN/TS 15083-1 (2005). Hitherto existing experience with this standard is quite heterogeneous and results from previous round-robin tests have stayed unreported or have been reported incompletely. In particular the need for natural pre-weathering of the test specimens to allow potential detoxification of...
C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar, K Plaschkies, W Scheiding, G Alfredsen, J Van Acker, I De Windt


Post-layup protection of mass timber elements in above ground protected exposures: 2-year results
2022 - IRG/WP 22-30766
Mass timber has seen increased use as a building material for low and mid-rise construction in recent decades. The durability of mass timber elements has not been fully examined and the effects of wood destroying organisms on this these materials merits attention. The effectiveness of currently labeled soil termiticides and passively applied biocides at post-construction or as remedial agents need...
M E Mankowski, T G Shelton, G T Kirker, J J Morrell


Previous Page | Next Page