A light and electron microscopic study of decayed CCA-treated radiata pine (Pinus radiata) wood from a cooling tower
1994 - IRG/WP 94-10056
An inspection of an industrial cooling tower in New Zealand showed surface decay of 12 year old Pinus radiata wood panels treated with CCA preservative to a retention of around 15 kg/m³ of salt. Wood decay micromorphology typical of that caused by soft rot fungi, white rot fungi, 'stripy' and 'v-shaped' erosion bacteria and cavitation bacteria were all commonly...
A P Singh, R N Wakeling, D R Page
Determination of the water sorption properties and preliminary results from field tests above ground of thermally modified material from industrial scale processes
2004 - IRG/WP 04-40279
In this study the differences in moisture behavior and durability above ground of heat treated wood originating from different European industrial heat treatment plants by means of the water sorption properties as well as field tests were examined. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood (Premium wood)/ Finland and Menz Holz/ Germany,
where Oil-...
C R Welzbacher; A O Rapp
Soft rot decay in acetylated wood. Chemical and anatomical changes in decayed wood
2002 - IRG/WP 02-40231
Acetylated Beech (Fagus sylvatica) and Scots Pine (Pinus sylvestris) wood were studied in soil beds under laboratory conditions for longer periods. High mass losses and dynamic MOE losses were measured in non-acetylated wood and at lower weight percent gains (WPG). Rapid losses of lignin, holocellulose and ?-cellulose occurred in non-acetylated beech wood and no losses were detected at the highest...
B Mohebby, H Militz
Microscopic characteristics of microbial attacks of CCA-treated radiata pine wood
1993 - IRG/WP 93-10011
Light and electron microscopic observations were made of CCA-treated radiata timbers, which had been placed in service in a vineyard soil as supporting poles and as part of a house pile, to determine the cause of their deterioration. The house pile had failed in service after between 9 and 13 years and was of particular interest because decay was more severe in deeper regions than at the surface a...
A P Singh, R N Wakeling
Description of a trial with wood preservatives against marine wood boring organisms
1975 - IRG/WP 412
Wood situated in sea water along the Atlantic coasts of the Nordic countries is attacked by marine wood boring organisms. Timber constructions in these waters therefore must be preservative treated. In order to evaluate the effect of various preservatives against marine wood borers, the Nordic Wood Preservation Council (NWPC) organized a rather extensive trial in 1972. In the absence of and while ...
E Norman, B Henningsson
Unsuitability of the limiting dose as a criterion for assessing the toxicity of preservatives to wood-destroying fungi
1974 - IRG/WP 243
In the majority of methods for investigating preservatives for wood-destroying fungi their toxicity is assessed by determining what is called the "limiting dose". This normally denotes a range of preservative solution concentrations or retentions of dry preservative in the timber, the lower value serving to indicate the amount of preservative at which is observed the expected effect, e.g. the grow...
D A Belenkov
Marine trials with ammoniacal wood preservatives
1980 - IRG/WP 423
Ammoniacal wood preservatives have been known for many years and are considered among the best water-borne systems for protecting wood in ground contact. In recent years attention has been increasingly focussed on these preservatives because of their ability to penetrate difficult-to-treat species better than most other fixed water-borne preservatives. This is particularly important for example, i...
M A Hulme, D P Ostaff
Screening results of fungicides for sapstain control on Pinus radiata
1983 - IRG/WP 3236
Thirty-two compounds were tested to determine their ability to contain the growth of stain, mould and rot organisms on fresh Pinus radiata D Don. A screening technique was employed using 35 to 50 mm diameter biscuits of Pinus radiata stemwood 10 mm thick. No compound was found to be cost effective when compared against the standard treatments of NaPCP (0.5% a.i.) plus borax (1.5%) and Captafol (0....
P J Hayward, J Duff, W Rae
Accelerated decay tests on DNBP-treated Pinus patula and Eucalyptus grandis
1987 - IRG/WP 3441
Blocks (10 x 10 x 5 mm³) of Pinus patula and Eucalyptus grandis were impregnated to 0, 1.5, 3.0 and 4.5 kg/m³ 2-sec-butyl, 4, 6 dinitrophenol (DNBP). They were monitored microscopically and for weight losses over 16 weeks against monocultures of Coriolus versicolor and Coniophora puteana. Treated ministakes (10 x 10 x 100 mm³) and blocks in soil contact were similarly monitored to determine wei...
L D Abraham, A A W Baecker
Hardwood field experiment - 10 year report
1989 - IRG/WP 3560
The international hardwood field experiment was planned in 1976 and set up in some 34 different sites around the world. The test stakes include 4 reference species common to each site and in most cases at least 2 species of local importance (supplementary species). It was hoped that a picture of performance of a range of economically important timber species would be built up and at the same time ...
D J Dickinson, S M Gray
Laboratory screening to determine the preventive effectiveness against blue stain fungi and moulds
1991 - IRG/WP 3677
This paper reports results of preservative treatment and leaching experiments, using borax, polybor and boracol 20, on small wood blocks of English oak and American pitch pine heartwood. Earlier experiments on the performance of various biocides as possible additives to bilgewater to prevent fungal decay of shipping timbers had suggested that some formulations of boron might be associated with phy...
M T De Troya, A M Navarrete
A marine borer test with water-borne preservatives
1980 - IRG/WP 452
The use of preservative treated timber in sea-water where marine borers are active is of great economic importance, since untreated wood immediately will be damaged. Vacuum/pressure treated timber has been tested in several marine exposure trials on the Swedish west coast since the 1930s (Hager 1941, Hultman 1949, Sandstrom 1951, Nylinder-Norman et al. 1974). Since new interesting materials or pre...
B Henningsson, E Norman
How predictive are laboratory experiments for assessing the effects of chitin synthesis inhibitors (CSI) on field colonies of terrnites? - A comparison of laboratory and field data from Australian mound-building species of termit
1996 - IRG/WP 96-10143
A singular advantage of using mound building species of termite is their directly accessible nest. This allows evaluation of control methods by accurate assessment of the effects at the colony level. The mound building species Coptotermes acinaciformis (Froggatt) and Nasutitermes exitiosus (Hill) were used to test the CSI, hexaflumuron, in laboratory and field trials. Laboratory results showed tha...
M Lenz, P V Gleeson, L R Miller, H M Abbey
Options for termite management using the insect pathogenic fungus Metarhizium anisopliae
1996 - IRG/WP 96-10142
The insect pathogenic hyphomycete fungus Metarhizium anisopliae (Metschnikoff) Sorokin is promising as a biological insecticide for many species of subterranean termites. In Australia, a survey of termite mounds and feeding sites using a selective medium showed that this fungus is widespread but rarely causes mortality of termites under natural conditions. One isolate, codenamed FI610, has been se...
R J Milner, J A Staples, M Lenz
Biodegradation of wood in wet environments: A review
1997 - IRG/WP 97-10217
Wood in wet environments is attacked and degraded by soft rot fungi and erosion and tunnelling bacteria, which are more tolerant to high moisture and reduced oxygen conditions than basidiomycetes, such as white and brown rot fungi. Since basidiomycetes are normally more aggressive and can degrade wood faster than soft rot fungi and bacteria wood in wet environments can survive longer. In fact, arc...
A P Singh, Yoon Soo Kim
Assessment of wood decay in small-scale unsterile soil-bed tests
1997 - IRG/WP 97-20111
This study is concerned with the investigation of wood decay in small-scale unsterile soil-bed tests. Tests were performed with untreated heartwood samples from five hardwood species of different natural durability classes ranging from highly perishable to very resistant. Our results confirmed the critical role of soil moisture content on wood decay. The highest decay rates were observed at moistu...
L Machek, A M Derksen, R Sierra-Alvarez
Protection of wood blocks treated with Trichoderma isolates selected on the basis of preliminary agar screening studies
1996 - IRG/WP 96-10154
Previously reported results of agar interaction screening studies for biocontrol agents of wood decay basidiomycetes showed two Trichoderma viride isolates, killed 16 of 19 target fungi (Tucker and Bruce, 1995). Testing of these isolates in wood was required to assess their performance at preventing decay of wood blocks. Standard testing of chemical wood preservatives is used to determine the toxi...
E J B Tucker, A Bruce, H J Staines
Remedial ground-line treatment of CCA poles in service. Results of chemical and microbiological analyses 6 months after treatment
1986 - IRG/WP 3388
CCA-treated poles in service with incipient internal soft rot were remedially treated by inserting borate rods, brushing with a boron/glycol solution and injecting boric acid paste, copper/creosote paste or a commercial product (DFCK paste). The spread of active chemicals in the treated zone as well as the change in microflora have been studied with time. After six months chemicals had spread to m...
B Henningsson, H Friis-Hansen, A Käärik, M-L Edlund
Termite Field Tests of Various Timber Species Treated with permethrin using supercritical carbon dioxide
2005 - IRG/WP 05-10560
Termite field tests were conducted on permethrin-treated Eucalyptus obliqua heartwood, Pinus radiata sapwood and P. radiata LVL. The permethrin was impregnated using either supercritical carbon dioxide (scCO2) or light organic solvent preservative (LOSP) systems. Comparative permethrin retentions were most accurately achieved in P. radiata sapwood, where no difference between impregnation systems ...
A Qader, L J Cookson, J W Creffield, D Scown
Variance in feeding on equivalent wood blocks by the Formosan subterranean termite (Coptotermes formosanus Shiraki)
1987 - IRG/WP 1325
We tested whether laboratory groups of Coptotermes formosanus Shiraki forage randomly when they are given 4 equivalent wood blocks, and whether group size affects variance of feeding on equivalent blocks. In all cases, foraging was not random, but, rather, the termites concentrated on a few preferred blocks. Group size did not affect this pattern of non-randomness. These data are useful for design...
J P La Fage, K S Delaplane
Localized induction of hemlock brownstain by Ophiostoma piceae
1995 - IRG/WP 95-10106
Hemlock brownstain, a coloration disfiguring western hemlock and amabilis fir, causes economic loss in the high-value Canadian export lumber market. Recent work by the author has suggested that wood-sapstaining fungi can induce the formation of brownstain. Ophiostoma piceae, the most frequent staining fungus on western hemlock lumber in B.C., was chosen as a model to investigate fungal participati...
B Kreber
Effect of microfibril orientation of bamboo cell wall on soft rot penetration hyphae
1994 - IRG/WP 94-10087
The effect of microfibrillar orientation of bamboo (Phyllostachys virideglaucescence) cell wall on the development of soft rot (Chaetomium globosum) penetration hyphae was investigated. It was found that the soft rot penetration hyphae normally followed the microfibril angle of the cell wall. Bamboo cell walls have alternating broad and narrow lamellae with different microfibrillar angles. The mic...
O Sulaiman, R J Murphy
Marine trial progress report
1980 - IRG/WP 453
In May 1977 and May 1978, tests of new chemical formulations for the protection of timber in the sea were installed in Mt. Maunganui Harbour. Investigation into new preservatives for such usage was urgently required since it had been found that there was progressive leaching of copper from copper-chrome-arsenate treated marine piles which could lead to a reduction in their service life. Hochmann (...
A F Preston, C M Chittenden
Report on the co-operative leaching tests
1975 - IRG/WP 246
The Work reported here was undertaken at the request of CEN to see (1) whether the standard beaker leaching method under discussion at CEN, and based on the German DIN could be made less labour intensive; and (2) whether the leaching parameters could be expressed in more general terms so that alternative procedures could be used. A co-operative experiment was set up in which the amount of leaching...
J W W Morgan
Some Experiences with Stake Tests at BAM Test Fields and in the BAM Fungus Cellar
Part 2: Comparison of Static and Dynamic Moduli of Elasticity (MOE)
2005 - IRG/WP 05-20320
In routine in-ground stake tests of wood preservatives at the BAM test field Horstwalde and in the BAM fungus cellar periodical determinations of both static moduli of elasticity (MOE) on the basis of bending tests and dynamic MOE on the basis of the vibration method were performed as a possible method for the assessment of fungal attack. As expected from other publications, the absolute values of...
M Grinda, S Göller