Comparison of performance of wood preservatives in laboratory and field tests of treated commodities
1993 - IRG/WP 93-20010
The purpose of laboratory tests for evaluating efficacy of wood preservatives is usually to establish toxic values against standard strains of wood decay fungi. Exposure conditions are usually chosen as optimal for fungal growth. Toxic values so determined serve as a guide as to expected performance of the preservative in field stake tests or in above ground exposure tests. Test material is select...
M E Hedley


Fundamentals on steam fixation of chromated wood preservatives
1988 - IRG/WP 3483
Weathering of treated wood directly after impregnation leaches up to 2% of copper-chromate-containing wood preservatives. Almost total fixation of Cr+6 is achieved by steaming the treated wood at 100°C to 120°C, preferably 110°C. To initiate such spontaneous fixation 85°C to 90°C inside the wood are essential, which requires heating times ranging from 20 to 80 min, depending on timber species...
R-D Peek, H Willeitner


Interactions between water-borne preservatives and emulsion additives that influence the water repellency of wood
1991 - IRG/WP 2374
Incorporation of non-polar additives into water-borne treatments through of emulsion technology can greatly improve the physical characteristics of wood in service. Of specific interest with these emulsions is their effectiveness in reducing the rate of wood swelling. We have observed that the presence or absence of preservatives can often significantly influence the resultant effectiveness of the...
A R Zahora


Research on wood protection at the Princes Risborough Laboratory 1975 & 1976
1977 - IRG/WP 3109
This paper is the latest of a 2-yearly series presenting a summarised account of the Laboratory's work in wood preservatives and related fields. The topics dealt with include: environmental studies on the usage of copper-chrome-arsenic and organic solvent preservatives; development of National and International Standards; recent developments in the preservation of external doors and windo...
J M Baker, R A Laidlaw, E R Miller, J G Savory


The evaluation of the effectiveness of wood preservatives by means of IUFRO's method for field tests with wooden stakes
1985 - IRG/WP 3348
Pinus elliottii and Eucalyptus saligna stakes treated with CCA-A, CCA-C, CCB, Cashew Nut Shell Oil and Benzotar solutions were exposed in seven test sites in Sao Paulo State, Brazil. After five years of exposure, between oil-borne preservatives Benzotar show better performance than CNSL (cashew nut shell liquid), and within waterborne preservatives the performance of CCB is not so good as that of ...
G A C Lopez, A M F Oliveira, E S Lepage


International collaborative laboratory comparison of two wood preservatives against subterranean termites: Second update
1995 - IRG/WP 95-10117
As was agreed by members at the termite workshop at the 24th annual meeting of IRG in Orlando, USA, in May 1993 to initiate an international subterranean termite laboratory bioassay to compare the various preferred termite protocols used by IRG termitologists was initiated. The author was nominated to co-ordinate this comparative laboratory evaluation of two wood preservatives (CCA and Cu-naphthen...
J R J French


Biological Safety Evaluation of Animal Contact of Preservative-Treated Wood
2003 - IRG/WP 03-50196
Biological safety of preservative-treated woods that could be contacted to human and animal was evaluated for rat and rabbit exposed to CCA-, ACQ- and CCFZ-treated woods. The accumulation of preservatives ingredient in the rat’s plasma and viscera, and the transforming function of replacing preservatives were examined in this study. The result indicated that preservative-treated wood did not bri...
Dong-heub Lee, Dong-won Son, Myung Jae Lee, Chang Ho Kang, Cheon Ho Kim, Eui-Bai Jeung


Effectiveness of wood preservatives by IUFRO's method
1984 - IRG/WP 3305
Pinus elliottii and Eucalyptus saligna stakes treated with 4.9; 6.9; 9.6 and 13.5 kg/m³ of CCA-A, CCA-C and CCB and with 30-50; 60-80; 90-110 and 120-140 kg/m³ of Benzotar and CNSL (cashew-nut shell liquid) were exposed in seven test sites in Sao Paulo State, Brazil. After 4 years it was concluded that the mean useful life of untreated Pinus elliottii stakes was 8 months and of untreated Eucalyp...
G A C Lopez, E S Lepage, O B Neto


Rapid fixation of Chromated Copper Arsenate (CCA) wood preservatives by microwave treatment
2000 - IRG/WP 00-40184
Rapid microwave heating of freshly chromated copper arsenate (CCA) treated timber indicates that rapid preservative fixation is possible within approximately 40 seconds. The leaching of CCA was evaluated using simulated rainfall. Cost analyses indicates that microwave fixation using an on-line conveyor belt fixation process with an output of 4m3/hour using a microwave power supply of 230 kW costs ...
G Torgovnikov, P Vinden, E Mapanda, P R S Cobham


Diffusion and interaction of components of water-borne preservatives in the wood cell wall
1988 - IRG/WP 3474
This study investigates the rates of diffusion and ultimate distributions of copper and arsenate components of wood preservatives in wood cell walls following vacuum treatment. Adsorption studies of copper on red pine (Pinus resinosa) and trembling aspen (Populus tremuloides) wood confirm the importance of cation exchange reactions on the ultimate distribution of copper in the wood substance and i...
P A Cooper


EPA’s Current Views on Heavy-Duty Wood Preservative Regulation
2003 - IRG/WP 03-50206
This paper describes the current EPA system for regulating pesticides and wood preservatives. In particular it focuses on the voluntary phase-out of CCA for residential uses after December 30, 2003, which was agreed between the CCA manufacturers and EPA. Even though the EPA reached an agreement with industry to phase out CCA for residential uses, EPA is continuing the most rigorous risk assessmen...
F T Sanders


Biosorption of metals for wood waste effluent clean up
1997 - IRG/WP 97-50090
The common filamentous fungi can sorb metal ions from aqueous solutions. The biosorption of metal ions like copper Cu2+, chromium Cr6+ and arsenic As5+ by dead fungal mycelia was investigated. Two industrial fermentation byproducts are tested: Mucor miehei and Aspergillus oryzae. The adsorption of metal ions depends on parameters such as chemical treatment of fungi before biosorption (acid or basi...
S Legay, G Labat


Comparison of Temporal Changes in Metal Leaching and Aquatic Toxicity from Wood Treated with CCA and Alternative Preservatives
2005 - IRG/WP 05-50236
This study compares the temporal variation of chemical leaching and aquatic toxicity of wood treated with chromated copper arsenate (CCA) and other copper-based wood preservatives (alkaline copper quaternary (ACQ), copper boron azole (CBA), copper citrate (CC) and copper dimethyldithiocarbamate (CDDC)). Treated wood blocks were leached for 21 days and the leachate collected was analyzed for prese...
B Dubey, T G Townsend, G Bitton, H M Solo-Gabriele


Development of software to automate the quantification of checking occurring in preservative treated wood exposed to weathering
2001 - IRG/WP 01-20228
Surface checking often disfigures the appearance of wood treated with water-borne preservatives and treatments designed to reduce such checking have been receiving increasing attention. Progress in this area has however been slowed by the lack of a method of rapidly and accurately quantifying checking at treated wood surfaces. A software package has therefore been developed which identifies, measu...
A G Christy, P D Evans


Evaluating the performance of wood preservatives against fungi
1974 - IRG/WP 247
A compilation is made of results published by various workers for agar/block laboratory tests of the effectiveness of wood preservatives against 11 species of wood destroying Basidiomycetes and one species of soft rot fungus. Preservatives include creosote, boron, metal/arsenic mixtures, metallic naphthenates, chlorinated naphthalene, chlorinated phenols and tri-n-butyl tin oxide. The results are ...
R Cockcroft


Determination of fungitoxic value of preservatives in laboratory wood-block tests. Part 2: Statistical estimation
1989 - IRG/WP 2327
Laboratory modified agar-block tests were made to determine the fungitoxic value of the wood preservative CCA against the test fungus Serpula lacrymans using statistical methods. With the aid of statistical computer programmes based on the least square method. the regression equation was found for the dependence between sample mass loss and preservative retention both in terms of percentage and fo...
J Wazny, J D Thornton, K J Krajewski


Determination of fungitoxic value of preservatives in laboratory wood-block tests. Part 1: Standard procedures
1989 - IRG/WP 2326
By applying a modified agar-block method, a comparative analysis was made on the toxic value of the wood preservative CCA against the test fungus Serpula lacrymans. The procedure applied to determine the results accounted for different standards: EN (Toxic limit), ASTM (threshold retention), GOST (threshold retention and protection probability), PN (toxic doses) and JIS (value of efficiency). Desp...
J Wazny, J D Thornton


Protection and efficient utilization of plantation grown lesser-known timbers of arid region in India - Acacia tortilis, Prosopis juliflora and Prosopis cineraria
2005 - IRG/WP 05-40321
The plantation-grown timbers are highly susceptible to insects/pests, borers and wood rot fungus. Wood preservatives copper chrome arsenic (CCA) 2% and chloropyriphos 2% solution treated under pressure on three plantation grown timber species viz. Acacia tortilis, Prosopis juliflora and Prosopis cineraria have shown encouraging results in enhancement of shelf life by protection of wood against woo...
S H Jain, H Kumar, R Arya, R L Srivastava


Inorganic preservative levels in soil under treated wood decks after 8 years natural exposure in Borås, Sweden
2005 - IRG/WP 05-50233
Inorganic preservative components (Cu, Cr and As) were measured to a depth of 150 mm under deck structures made with Scots pine lumber treated with several different wood preservatives and installed in Borås Sweden 8 years ago. Higher contaminant levels were observed mainly under the drip lines and in the top 50 mm of soil. Under CCA treated decks, soil arsenic concentrations increased from ba...
P A Cooper, Y T Ung, M-L Edlund, J Jermer


Inter-laboratory comparison of assessment methods for wood preservatives against subterranean termites: Determination of protection threshold limits for CCA
1999 - IRG/WP 99-10317
In 1996, several institutes conducted laboratory bioassays on the efficacy of unleached Pinus radiata specimens treated with copper-chromium-arsenic (CCA) and copper naphthenate (Cu Naph) at retentions of 0.5, 1.0, 2.0 and 4.0 kg/m3 (total salt for CCA; elemental copper for Cu Naph) against a range of species of subterranean termites (IRG/WP/96-10174). Each participant employed the standard test m...
J W Creffield, M Lenz


Field test of wood preservatives with Nasutitermes rippertii RAMBUR in Cuba
1996 - IRG/WP 96-10181
A field test of wood preservatives was carried out with Nasutitermes rippertii RAMBUR in the vicinity of the Material Testing Centre „Alexander von Humboldt" in Santiago de las Vegas/ Havana (Cuba) for 12 and 24 months. Test specimens of Pinus sylvestris L., Picea abies (L.) Karst. and Fagus sylvatica L. with dimensions of 25 x 25 x 490 mm³ were arranged vertically or horizontally in a circle o...
W Unger


Technologies for the Management of Wood Waste Containing Metals-Based Preservatives
2005 - IRG/WP 05-50224-16
Disposal of the metals from preservative treated wood can occur through two general strategies: “removal and confinement” or “dilution”. The acceptability of each of these two choices is typically dictated through the disposal regulations of a particular region. A considerable amount of research has been conducted to develop new and innovative “removal and confinement” technologies...
H M Solo-Gabriele, T G Townsend


Determination of toxicity data for preservatives against Basidiomycetes by measuring the reduction in compression strength of wood
1988 - IRG/WP 2297
Blocks of Pinus radiata D. Don were treated to 12 retention levels with CCA and NaPCP. These were exposed for 12 weeks in agar jars to the dry rot (brown rot) Serpula lacrymans (Schum. ex Fr.) S.F. Gray. After mass loss determination, the same blocks were tested for reduction in compression strength parallel to the grain. Using both these parameters, together with interpolated 6 week strength loss...
J Wazny, J D Thornton


The resistance of timbers to impregnation with wood preservatives
1979 - IRG/WP 3137
It is anatomical structure which determines liquid flow rate within different timber species. This cannot be deduced from properties such as density or rate of growth, and can only be found by experiment. A standard test has been in use at the Princes Risborough Laboratory for many years, employing a pressure-impregnation treatment, and a large number of timbers have been studied. The test consist...
Anonymous


Less pollution due to technical approaches on accelerated steam fixation of chromated wood preservatives
1988 - IRG/WP 3487
Steaming of freshly treated wood at 100°C to 120°C initiates a spontaneous fixation of copper-chromate-containing wood preservatives. For the performance, a suitable anticorrosive equipment is necessary. Good results can be achieved using a separate steaming equipment which allows a rapid heating of the wood. While warming-up, in the wood some preservative solution extends and can be partly extr...
H Willeitner, R-D Peek