Corrosion of fasteners in treated wood
1971 - IRG/WP 303
Surveying tests for determining the corrosion rates of some metals and alloys in wood untreated as well as treated have been made. It is shown that ordinary steel corrodes faster than other common fastener metals such as copper, brass, aluminium and stainless steel do. Zinc coatings, however, will prevent the steel corrosion effectively provided that the coatings are thick sufficiently. Catalytic ...
T Wallin


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 6: The length of the primary precipitation period
1975 - IRG/WP 359
The end of the primary precipitation fixation period of CCA preservatives coincides with the first peak in pH versus time. This offers a simple way of estimating the duration of the period. The duration is determined by a number of factors and their interactions, the most important of which are: wood species (anatomy, natural pH, accessibility of reducing agents), preservative type, preservative c...
S-E Dahlgren


Solidification - A viable option for the safe disposal of CCA treatment plant wastes
1993 - IRG/WP 93-50001-21
Treatment plant operations generate small quantities of waste materials contaminated with wood preservatives - for example, sludges, contaminated sawdust, yard dirt. A practical system involving the immobilisation of such wastes has been established to assist the operators to safely dispose to landfill sites. The results of cold water and hot dilute acid leaching regimes are described, which simul...
M R Gayles, D Aston


Environmental fate of copper-based wood preservatives in different soil substrates - Part 1: Screening of the metal adsorption potential
1998 - IRG/WP 98-50101-21 a
In treatment plants, spillage of wood preservatives onto soil may be of environmental concern. This potential soil contamination served as an objective for a screening study. Three different mineral soils, a mineral substrate and two horticultural substrates are examined for their sorptive potential of copper through mixing with wood preservative solutions. Depending on the soil/substrate charact...
G M F Van Eetvelde, J M Mwangi, F Tack, R Hartmann, M Stevens


Environmental situations on wood preservation industries in Japan
1995 - IRG/WP 95-50040-21
Because of environmental civil oppinions, Ministry of Agriculture, Forestry and Fisheries in Japan, reviesed "the standards for sawn lumber" in 1994. For the possibilities of the use of preservatives out of CCA, by the using of the hazard levels, new products like ACQ, DDAC and emulsified zinc-naphthenate can be used in the standards. Since 1994, the permitable limit of the arsenic in the waste wa...
K Suzuki


Investigation of temperature effect on fixation of Celcure preservative (ACC) in Hornbeam (Carpinus betulus I)
2003 - IRG/WP 03-30304
In this research, the fixation speed of Celcure 2 % (ACC) preservative salt, under temperature of 30 ºC, 40 ºC and 50 ºC on intact wood specimens of hornbeam was investigated. For this purpose, blocks of wood with 2Í 2 Í2 cm dimensions of hornbeam were prepared and saturated with 2% ACC concentration by full-cell process. The specimens were put in three incubators at the above-mentioned temperatures. For measuring the percentage of fixation through time, the specimens were extracted by using hydraulic pressure equipment, under 70 Mpa pressure. The PH of extraction was measured with the method of Diphenyl Carbazid and by using spectrophotometer. This measurement was done continuously and the amount of 6-valence chromium concentration present in the extract was compared with the amount of chromium concentration in the primary solution and then the percentage of fixation was calculated. The results showed that the decrease in 6-valence chromium is accompanied with increase of PH, this due to absorption of positive hydrogen ion by 6-valence chromium for reduction to 3-valence chromium and also ion –exchange of active components with wood during the primary phase of fixation. Also, the time necessary for reaching complete fixation in intact wood in the fixation temperature conditions of 30, 40, 50 ºC were 98, 52, 24 hours, respectively. In general, the results showed that temperature has effective role accelerating of fixation process.
R Imani, R E Majdar, A Karimi


Experiences with environmental risk assessment within the Biocidal Products Directive
2005 - IRG/WP 05-50224-21
The Biocidal Products Directive (98/8/EC, the BPD) aims to authorize biocidal products based on risk assessment for both man and the environment. Active substances for wood preservation products and rodenticides were selected for the first list under the review program (Regulations EC 1896/2000 and EC 2032/2003) because several member states had experience with the evaluation and authorization of ...
P Blancquaert


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 4: Conversion reactions during storage
1974 - IRG/WP 332
Precipitates simulating those produced in wood by preservative fixation reactions were prepared by the reduction of Boliden K 33 and Celcure AP solutions with hydrogen peroxide and hydrazine. The pH changes on aging at 20 and 50°C were studied and related to the chemistry of fixation previously described. Hydrolysis of copper arsenates may render arsenic acid temporarily water soluble pending pre...
S-E Dahlgren


Performance of resin-treated solid wood and laminated veneer lumber (LVL) under marine conditions
2021 - IRG/WP 21-10973
Wood is a traditional building material in the marine environment, where it is exposed to extremely harsh conditions. Most of the indigenous softwood and hardwood species in Europe are not durable against attack by marine organisms. Recently, wood modification has been considered as an alternative to protect non-durable wood species under use class (UC) 5 (EN 335, 2013) conditions. The present stu...
L Emmerich, C Brischke, S Bicke, H Militz


Assessing the risk of marine borer attack of the timber trestles and decay of timber above the intertidal zone of the Barmouth Viaduct
2021 - IRG/WP 21-10974
The Barmouth Viaduct is a Grade II* listed structure which carries the single track of the Dovey Junction to Pwllheli line and footway over the Mawddach estuary. It is in a marine environment where timber below the high tide mark is at most risk in Use Class 5 and all timber above in Use Class 3.2, permanently exposed to the risk of wetting. The structure consists of a timber trestle viaduct of ...
J R Williams


Validating a short-term laboratory method to assess the resistance of timber to biodegradation by marine wood-borers
2021 - IRG/WP 21-10975
Novel approaches to protecting wood in coastal and marine environments are needed as the use of traditional broad-spectrum biocides are now restricted. Wood is widely utilised in marine environments where it can be rapidly degraded by wood-boring organisms, causing billions of dollars of damage per annum. Biocidal compounds such as CCA and creosote have been popular treatments for timber products ...
L S Martin, J R Shipway, G P Malyon, S M Cragg


Experience Experience from over 20 years of field trials of resin treated wood – Marine borer resistance of MMF and DMDHEU modified wood
2021 - IRG/WP 21-10976
In 1999 a field test of Scots pine treated with MMF (Methylated Melamine Formaldehyde) resin and acetylated Scots pine post treated with MMF resin was started. Six years later a commissioned full NWPC test for BASF of Belmadur® (DMDHEU resin treated wood) was started at the same site. The testing, according to European Standard EN 275, was done in a bay by Kristineberg Marine Research Station o...
M Westin, P Larsson Brelid, A O Rapp, J Habicht


Plasma treatment of wood - a review of 15 years of research in Göttingen
2021 - IRG/WP 21-40913
Wood is an important renewable resource and can be found omnipresent in everyday life. Its natural properties offer numerous advantages regarding physical, mechanical but also aesthetic aspects, but also challenges that one has to address with various modification methods. Driven by the desire to promote the use of promising new technologies using plasmas, there has been a close research network ...
P Sauerbier, R Köhler, G Avramidis, W Viöl, H Militz


Influence of weathering on surface roughness of thermally modified wood
2021 - IRG/WP 21-40915
Thermally modified wood is exposed to weathering similarly as other wood-based building materials. It has been reported that if thermally modified wood is exposed to weathering, its moisture performance might decrease fairly fast. The aim of this study was to determine whether this phenomenon is associated with crack formations or roughness. Norway spruce, thermally modified spruce, wax-treated th...
E Kerzic, B Lesar, M Humar


Surface morphology and short-term water uptake of charred and coated wood
2021 - IRG/WP 21-40916
Charring of the wood surface represents a traditional alternative surface treatment technique with the purpose of aesthetics and protection. By the treatment with flame the surface of wood becomes carbonized and a few millimetres thick charred layer is formed on the top of the wooden element. Further, the charred layer can be removed by brushing, which accentuates the structure of the surface. Add...
J Zigon


Effect of MVOC exposure on mycelial growth of wood rotting fungi
2021 - IRG/WP 21-10977
It is well known that wood rotting fungi produce microbial volatile organic compounds (MVOCs) as metabolites. In our previous studies, we have found that some MVOCs produced by wood rotting fungi are common to fungal species tested in the studies, while others are specific to each species. Furthermore, it has been also shown that each wood rotting fungi do not always produce the same type of MVOCs...
S Horikawa, R Konuma, M Yoshida


Decomposition and metabolism of gaseous COS by wood rotting fungi
2021 - IRG/WP 21-10978
Previous studies on physiology of wood rotting fungi have mostly focused on the metabolisms of carbon and nitrogen sources. On the other hand, despite of the biological importance of minerals such as sulfur, our knowledge of their metabolic systems is limited. The sulfur source for wood-rotting fungi has been thought to be water-soluble sulfur compounds such as sulfate esters and cysteine, which a...
R Iizuka, O Iwao, Y Katayama, M Yoshida


The iron reduction by chemical components of wood blocks decayed by wood rotting fungi
2021 - IRG/WP 21-10979
Brown-rot fungi, a group of wood rotting fungi, is well known to be one of major microorganisms that cause the deterioration of wooden buildings in Japan and have been considered to use chelator-mediated Fenton (CMF) reaction in concert with hydrolytic and redox enzymes for degradation of wood cell wall. CMF can be described as a non-enzymatic degradation system that utilizes hydroxyl radicals pro...
R R Kondo, Y Horikawa, K Ando, B Goodell, M Yoshida


Occurrence of synanthropic beetles (Coleoptera Ptinidae) and checkered beetles (Coleoptera Cleridae) in relation to climatic factors in historical buildings from North-Eastern Germany
2021 - IRG/WP 21-10980
Predatory checkered beetles occur in many historical buildings. Thus, it is essential to learn more about the ecology of these beetles, specifically for their further use as suitable beneficial organisms in biological control of wood-destroying insects. In this study, indoor climatic conditions were examined as a major factor influencing their occurrence and that of their prey Anobium punctatum an...
C Baar, C von Laar, M Willert, H Bombeck


Comparison of AE-apparatus for detection of activity of Old house borer larvae, including reality check
2021 - IRG/WP 21-10981
As part of the German funded project ‘InsectDetect’ comparative measurements were done with three different Acoustic-Emission-(AE)-apparatus on 14 pine beams in order to assess presence of active attack by the Old house borer (Hylotrupes bajulus (L.)). In all beams active attack was measured, though in varying intensity. This was corroborated by completely dissecting 10 of the beams. All thre...
J Creemers, B Plinke, U Noldt


Genetic relationships of local infestations by Anobium punctatum, Xestobium rufovillosum and their associated predator Korynetes caeruleus from buildings in North-Eastern Germany
2021 - IRG/WP 21-10982
Wood-destroying pests such as Anobium punctatum and Xestobium rufovillosum cause damage to art and cultural objects as well as to buildings. Monitoring population dynamics of pest species as well as of their naturally occurring counterparts are an essential part in the development of biological control measures as alternatives to conventional wood protection. Therefore, both the dispersal and homo...
C von Laar, C Baar, R Plarre, D P McMahon


Marine borer resistance of various wood materials in Japan
2021 - IRG/WP 21-10983
Wood resistance against marine borer was intensively studied in the 1940s in Japan, but the research activities on the subject diminished afterward, as the use of wooden marine structures and ships decreased. Today, however, use of wood as a construction material is officially promoted for its environmental benefits. The author started to immerse some wood materials in the seawater pool at PARI ...
M Yamada


Studies on the material resistance and moisture dynamics of Douglas fir and Sitka spruce from Slovenia
2021 - IRG/WP 21-20677
Wood in outdoor applications is subject to various decomposition factors. Wood degradation can be prevented by construction details, biocide protection of wood, wood modification, or selection of naturally durable wood species. Unfortunately, the majority of timber species in Europe do not have naturally durable wood. Imported tree species represent a new pool from which we can draw wood species w...
M Humar, B Lesar, D Krzisnik, E Kerzic, R Brus


Development of software to automate the quantification of the extent of penetration of treated wood
2021 - IRG/WP 21-20678
In Japan, Japanese Agricultural Standard (JAS) by the Ministry of Agriculture, Forestry and Fisheries and Approved Quality (AQ) by the Japan Housing and Wood Technology Center have established the penetration standard for treated wood. In our company, we measure the degree of penetration by either visual assessment or image processing. In the visual assessment, the degree of penetration is determi...
Y Susa, D Watanabe, T Shigeyama, Y Sugai


Development of Wooden Fireproof Structures for Mid- and High-rise Buildings in Japan
2021 - IRG/WP 21-30757
When constructing a mid-to-high-rise building more than 4 stories in general in Japan, it is necessary to have a fireproof structure stipulated by the Building Standard Law. The performance required as a fireproof structure in Japan is generally stricter than in other countries, and it is required to be structurally sound after a fire even without fire extinguishing activities. In order to satisfy...
D Kamikawa, M Harada, H Matsunaga, R Takase, N Hattori, Keisuke Ando, M Miyabayashi