Fungicidal and termiticidal effectiveness of alkylammonium compounds
1983 - IRG/WP 3232
This paper is related to effectiveness of several AAC's against wood decay fungi and termites by Japanese standardized test methods....
K Tsunoda, K Nishimoto


An interim report on trials with 'Boliden K33' and 'Celcure A' in water of different salinities in the Baltic Sea and in the UK
1974 - IRG/WP 406
It was felt necessary to undertake field trials using large test samples exposed in natural water of different salinity in order to determine preservative leaching and to assess the degree of biological attack....
R A Eaton, D J Dickinson


Copper based water-borne preservatives: The use of a thin section technique to compare the protection of wood by copper based preservatives against soft-rot and bacterial decay
1987 - IRG/WP 2286
This paper describes the techniques developed and gives examples of results obtained for the performance of copper based wood preservatives against both the bacterial and fungal hazards....
A M Wyles, D J Dickinson


Corrosion of fasteners in treated wood
1971 - IRG/WP 303
Surveying tests for determining the corrosion rates of some metals and alloys in wood untreated as well as treated have been made. It is shown that ordinary steel corrodes faster than other common fastener metals such as copper, brass, aluminium and stainless steel do. Zinc coatings, however, will prevent the steel corrosion effectively provided that the coatings are thick sufficiently. Catalytic ...
T Wallin


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 6: The length of the primary precipitation period
1975 - IRG/WP 359
The end of the primary precipitation fixation period of CCA preservatives coincides with the first peak in pH versus time. This offers a simple way of estimating the duration of the period. The duration is determined by a number of factors and their interactions, the most important of which are: wood species (anatomy, natural pH, accessibility of reducing agents), preservative type, preservative c...
S-E Dahlgren


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 4: Conversion reactions during storage
1974 - IRG/WP 332
Precipitates simulating those produced in wood by preservative fixation reactions were prepared by the reduction of Boliden K 33 and Celcure AP solutions with hydrogen peroxide and hydrazine. The pH changes on aging at 20 and 50°C were studied and related to the chemistry of fixation previously described. Hydrolysis of copper arsenates may render arsenic acid temporarily water soluble pending pre...
S-E Dahlgren


Soft rot in CCA-treated utility poles in Sweden
1989 - IRG/WP 1398
Soft rot investigations of CCA-treated utility poles (Pinus sylvestris L.) have been conducted throughout large parts of Sweden during 1974-1985. The investigation included 179 utility poles of the State Power Board which had been used for 10-18 years in the different administrative regions from northern to southern Sweden. In addition, 193 telephone poles from the Östersund area and 218 from the...
H Friis-Hansen, H Lundström


An investigation of the effects of pre-steaming on the treatment of sawn spruce timber with Celcure A, a copper-chrome-arsenic preservative
1981 - IRG/WP 3150
Difficulties in the treatment of spruce using standard vacuum/pressure techniques with both water-borne and organic solvent preservatives are well known. We have evaluated the influence of steaming on treatability with a waterborne CCA preservative....
C R Coggins


The leaching of copper, chrome and arsenate from CCA-impregnated poles stored for ten years in running water
1978 - IRG/WP 3122
There is no evidence to indicate that the chromium and copper components are leached from the outermost 5 mm of sapwood in poles impregnated with Boliden K33 and Tanalith C and stored in running water for ten years. The arsenic component, however, seems to be leached out during the first few months to an extent of about 20% of the initial amount. The leaching time is dependent on the preservative ...
F G Evans


Resistance to soft rot of hardwood plywood treated with CCA salt
1983 - IRG/WP 3258
Plywood made from indigenous hardwoods was treated at an average loading of 34 kg Celcure A per m³ and was installed in a field test. After 20 years the samples were only slightly attacked by soft rot and the glue bonds were still intact....
R S Johnstone


A short note on fungal decay in K33-treated poles
1982 - IRG/WP 1169
Soft rot cavities and erosion of the lumen have been found in K33-treated Pinus sylvestris poles from the years 1956-66 by microscopic studies. Poor treatment quality has been proved for some of these poles. The microscopy showed an unusual pattern of attack, and pre-treatment decay is suspected but not yet proved. Sounding the poles and using the Pilodyn indicated decay, but poking did not. Quant...
H Friis-Hansen


Draft of a mongraphic card for Serpula himantioides (Fr.) Karst. according to the 'Model Questionnaire for preparation of monographic cards for wood-destroying fungi'
1978 - IRG/WP 174
L Harmsen


Soft rot decay of 23 CCA-treated hardwoods from Sabah, Malaysia, in ground contact in Australia
1986 - IRG/WP 1280
The performance against soft rot decay of 23 CCA-treated hardwoods from Sabah, Malaysia, was examined after 20 months in ground contact at Pennant Hills, Australia. The results indicate that between these species soft rot decay is excluded by different levels of CCA salt suggesting that the threshold level for exclusion of soft rot in these hardwoods is a function of anatomical structure/ultrastru...
R S Johnstone


Performance of CCA treated Eucalyptus round ties
1985 - IRG/WP 3342
After 5.5 years of field exposure in the south of Brazil round Eucalyptus ties treated with CCA type A Oxide (OSMOSE K-33-A) preservative with retentions from 12 to 14 kg/m³ (0.75 to 0.873 PCF) (active ingredient basis) are performing very well. No decay or insect attack was observed in the 100 ties in test in real conditions of use; 10% of ties show incipient checking (what is a natural trend of...
V J Carlos, F R Niederauer, J P P Wehr


The variation in electrical resistance in the CCA-treated wood during the fixation
1989 - IRG/WP 3554
The curve commonly used in Scandinavia for describing the fixation period at different temperatures for CCA-impregnated wood is based on investigation by Dahlgren on the pH-variations in a mixture of sawdust and preservative solution. As far as we know there is no such investigation on solid wood. We have therefore measured the electrical resistance in CCA-treated solid wood to see if this will di...
F G Evans, B Nossen


Performance of chromated copper arsenate-treated aspen fence posts installed in Forintek's Eastern test plot from 1951 to 1963
1984 - IRG/WP 3272
Aspen poplar fence posts were pressure treated by the full cell process using three formulations of copper chrome arsenate wood preservative. A total of one hundred and fifty nine of the posts were installed in service in Forintek's Chalk River post plot from 1951 to 1962. During the 1982 general inspection of the post plot all 159 posts were still in service. A groundline inspection was ...
C D Ralph


The effect of ACC (Celcure) on durability of blue beech
1999 - IRG/WP 99-30209
Durability of the sapwood and heartwood of blue beech (Carpinus betulus) against white rot fungus (Coriolus versicolor) was studied. As treatment three concentrations of preservative (control or 0%, 3%, and 5% of ACC) were applied. The measuring 1.5x2.5x5cm3 as dimension of wood samples (sap and heartwood) was used. During 16 weeks exposure, untreated wood blocks were completely deteriorated by th...
S M Kazemi


Preservación de maderas en Bolivia
1986 - IRG/WP 3360
Este documento ofrece datos generales concerníentes a los recursos forestales de Bolivia, las facilidades existentes para preservación de maderas, la investigación y educación en esa materia. Se proporciona información sobre instituciones vinculadas a la actividad y las perspectivas del tratamiento de maderas en el país....
A S Viscarra


Assessment of the toxicity of some copper-, zinc- and boron-based wood preservatives to the cellar fungus Coniophora cerebella Schröet
1974 - IRG/WP 242
This article reports the use of a method based on the determination of the probability of the protection of timber against destruction by fungi. By converting the probability values to probit values and plotting them as a function of the amount of preservative retained in the timber, curves of the toxic effect are obtained, enabling any timber protection probability to be assessed....
V N Sozonova, D A Belenkov


Investigation of temperature effect on fixation of Celcure preservative (ACC) in beech (Fagus orientalis)
2001 - IRG/WP 01-40200
In this research, the fixation speed of Celcure 2% (ACC) preservative salt, under temperature of 17°C, 27°C and 50°C, on intact and stained wood specimens of beech was investigated. For this purpose, blocks of wood with 5x5x7 cm dimensions were prepared and saturated with 2% ACC concentration by full-cell process. The specimens were put in three incubators at the above-mentioned temperatures. F...
A Karimi, M Ghorbani


An investigation of the effects of pre-steaming on the treatment of sawn spruce timber with Celcure A, a copper/chrome/arsenic preservative
1981 - IRG/WP 3180
Difficulties in the treatment of spruce using standard vacuum/pressure techniques with both water-borne and organic solvent preservatives are well known. The growth characteristics of spruces (Picea spp) make them attractive candidates for forestry schemes. In 1975 the UK Forestry Commission had about 400 000 hectares, about 20% of total UK forest area, planted with Sitka spruce (Picea sitchensis)...
C R Coggins


Treatability of waterstored poles of Norway spruce by sap-displacement and pressure treatment with Boliden K33 and creosote
1973 - IRG/WP 328
Poles of windthrown Norway spruce were stored in bark under water sprinklers for 11-20 months or fully submerged in a lake for 3 years (tab. 1 and 2). Water content after storage is shown in fig. 1 and 8. Treatment with Boliden K33 by sap-displacement (open tank suction) gave a poor result. The Danish requirements of delivery claim a penetration of 20 mm and a net retention of 12 kg/m³ in outer 2...
P Moltesen, E Borsholt, B Bang


Discoloration of pressure impregnated wood caused by Amorphotheca resinae
1990 - IRG/WP 1438
Amorphotheca resinae Parbery with the anamorph Cladosporium resinae (Lindau) von Arx & de Vries is a cosmopolitan fungus known from aviation kerosene, hydrocarbon contaminated soil and creosoted timbers. In Denmark it causes heavy discoloration on wood treated with waterborne chromate-containing preservatives e.g. CCA-oxide type. The teleomorph produces small spherical fruitbodies widespread o...
F Rune, A P Koch


A laboratory technique to measure the performance of preservative treated hardwoods in ground contact
1982 - IRG/WP 2172
A laboratory technique to measure the performance of preservative treated timber in ground contact is described. It uses partially sealed blocks of timber which are treated, leached and sawn into small stakelets for soil exposure in a fungal cellar. Performance is monitored by the loss of static bending strength with time, and a simple apparatus for measuring the deflection of a stakelet under a l...
E F Baines


Inadequacies in preservative retention and formulation as contributory causes of premature failure of CCA-treated vineyard posts
1984 - IRG/WP 3280
Analyses of severely decayed or failed vineyard posts and examination of stake test data on effectiveness of copper-chrome-arsenate (CCA) preservatives have suggested two contributory causes of premature failure of vineyard posts: 1. Preservative retentions in posts are such that after 15 years' exposure some decay is inevitable. 2. The high arsenic, low chrome formulations with which the...
M E Hedley