Collaborative experiments in testing the toxicity of wood preservatives to soft rot fungi
1970 - IRG/WP 25
Eight Institutes from seven countries, Austria, England, France, Germany, Holland, Sweden and Switzerland have collaborated in an attempt to assess the suitability of various laboratory test procedures for acceptance as standard methods of determining the toxicity of wood preservatives to the cellulose-attacking micro-fungi which cause 'soft rot' of wood. Pure culture methods wit...
J G Savory, A F Bravery


What can DNA fingerprinting, aggression tests and morphometry contribute to the identification of colonies of the Formosan subterranean termite
2000 - IRG/WP 00-10371
Multilocus DNA fingerprinting, aggression tests and morphometry were compared to evaluate their potential for the identification of colonies of the Formosan subterranean termite, Coptotermes formosanus (Isoptera: Rhinotermitidae) in Hawaii. DNA fingerprinting separates the termites from all studied collection sites. Since the genetic similarity between termites from different collection sites lies...
C Husseneder, J K Grace


Contribution to the testing of wood based board material
1982 - IRG/WP 2176
R G Lea


Procedure for a collaborative study of leaching from CCA-treated timber in the sea
1988 - IRG/WP 4143
As a follow-up to the collaborative IRG/COIPM marine trial of CCA and CCB preservatives, a further trial is proposed with the objective of measuring the degree of leaching of CCA components from three timber species at marine sites in Malaysia and the U.K.. Details of the planned procedure are given....
S M Cragg, J E Barnacle, J D Bultman, R A Eaton, B R Johnson, L E Leightley, K D Singh


How best to specify retentions of preservative treatments: kg/m3 or % (m/m)
1998 - IRG/WP 98-20151
When specifying treatments according to the European Standard EN 351-1, retentions in the analytical zone are based on the amount of product found to be effective in biological tests; this is expressed in terms of the retention of the product per unit volume (kg/m3) for penetrating treatments and per unit area (g/m2) for superficial treatments. However, to check whether the retentions have been ac...
J K Carey


Diffusion of fused borate rods in top ends of poles
1989 - IRG/WP 3518
Diffusion tests of fused borate rods were carried out on extremities of sapwood poles in service. Rods were set in drills under the cone with or without addition of liquid Boracol 40. After one year of weathering, a good diffusion in the slice under the cone and even below the slice and in the cone itself was observed in Scots pine and spruce poles. The rods were still intacts and constitute, in f...
D Dirol, J P Guder


Efficacy of some extractives from Pinus heartwood for protection of Pinus radiata sapwood against biodeterioration. Part 1: Fungal decay
1995 - IRG/WP 95-30072
Chemical compounds thought to contribute to the natural durability of heartwood of Pinus spp. were either chemically synthesised in the laboratory or extracted from the heartwood of Pinus elliottii or Pinus caribaea. These compounds included the stilbenes, pinosylvin and its mono- and di-methyl ethers, and the flavonoids, pinobanksin and pinocembrin. Small blocks of Pinus radiata sapwood were impr...
M J Kennedy, J A Drysdale, J Brown


Accelerated wood decay in a soil bed test under greenhouse conditions compared with a stake test under field condition
1991 - IRG/WP 2384
The rate of decay of oak, beech, Douglas fir, pine and spruce stakes in an outside test field were compared with the decay rate of the same species in a greenhouse soil-bed test. Strength loss after four and six months respectively was measured by determining the compression strength parallel to the grain. The results show that all species, strength loss in the greenhouse was 2 to 4 times higher t...
J E Polman, S G Michon, H Militz


A new ground-contact wide-spectrum organic wood preservative: DNBP
1986 - IRG/WP 3358
A new organic wood preservative, which 25 years field tests have proved to be of efficiency and effectiveness comparable to CCA wood preservatives for ground-contact applications, is presented. Physical and chemical tests, supporting the long term field test results as well as indicating the characteristics of this preservative, are also presented....
W E Conradie, A Pizzi


Rapport sur l'activité du CEN/TC 38
1983 - IRG/WP 2204
M Pottevin


Development of marine borers research in Sao Paulo State, Brazil
1985 - IRG/WP 4117
This paper describes some field tests which have been carried on marine sites in Sao Paulo State mainly to investigate the natural resistance of Brazilian woods and the occurrence of marine borers. Some laboratory breeding tests which are being developed are also describe...
G A C Lopez


IRG Working Group II. Co-operative leaching test (letter to collaborators)
1974 - IRG/WP 234
J W W Morgan


Fungus cellar and stake tests with tall oil derivatives. Progress Report after 5 years' testing
1987 - IRG/WP 3442
Two derivatives of tall oils have been tested for five years in fungus cellar and stake tests. The samples were relatively quickly attacked on the surface by decay fungi, mainly soft rot, but the decay has progressed very slowly. The performance of the stakes in the tests has so far been equivalent or even better than some CCA preservatives and creosote....
J Jermer, Ö Bergman, T Nilsson


Report of field test results for dichloro-n-octyl-isothiazolone: A potential new wood preservative
1988 - IRG/WP 3495
In a previous report (IRG/WP/3306) we presented preliminary laboratory test results on 4,5-dichloro-2-n-octyl-4-isothiazolone (RH 287). Laboratory data indicated toxic threshold values for RH 287 ranging from 0.37 to 0.50 kg/m³. In this report we present field test results on an IRG L-joint test and an in-ground stake test for RH 287, pentachlorophenol and biocide free test units. (a) L-joint tes...
D E Greenley, B M Hegarty


Potentialities of protein borates as low-toxic, long-term wood preservatives - Preliminary trials
1999 - IRG/WP 99-30212
Boron compounds are efficient wood preservatives, as well as safe for the mammals and environmentally acceptable. Their natural solubility allows them to treat almost any wood species, but is also the cause of their high depletion from treated timber in outside exposure. In order to reduce this leachability, potentialities of proteinic polymer networks retaining boron within the wood have been inv...
M-F Thévenon, A Pizzi, J P Haluk


The performance of wood preservatives in soil-bed soft rot tests
1993 - IRG/WP 93-20007
Testing the efficacy of wood preservatives in soil is recognised as a fundamental part of the assessment of long-term wood protection in ground contact. Laboratory based tests can provide a hazardous environment in which a preservative can be challenged by a range of micro-organisms. This paper presents the results of tests carried out to investigate the performance of wood preservatives in a wet ...
G R Williams, S Caswell


Report on marine borer attack on some timbers treated with CCA wood preservative and exposed for three months in sea-water
1985 - IRG/WP 4112
Destruction of timbers by marine borers has long been a problem for the coastal population of Thailand. The use of heavy durable timbers with frequent maintenance, or total replacement, is the only solution for fishermen with their fishing craft or marine installations, meanwhile wharves or other large scale constructions are usually made by using concrete pilings or concrete casings. In recogniti...
A Rananand, W Yoosukh, U Sittiphuprasert


A critical review of the AWPA standard method (M12-72) for laboratory evaluation to determine resistance to subterranean termites
1986 - IRG/WP 1298
The American Wood Preservers' Association standard (M12-72) for evaluation of candidate wood preservatives against subterranean termites is reviewed and suggestions for revision are made. The most serious flaws in the current test procedure involve a failure to recognize inter- and intraspecific variation and a lack of quantification of test results....
J P La Fage, M Jones


A collaborative test to determine the efficacy of polyurethane coatings on wood samples exposed in the marine environment
1984 - IRG/WP 4113
Aims are: a) to determine the effectiveness of elastomeric polyurethane as a protective coating against marine wood boring animals in a range of tropical and tempreate sites; b) to compare the adhesion of polyurthane coatings on different wood species exposed in seawater; c) to record the severity of attack in failed samples and to identify the causal marine organisms....
R A Eaton


Evaluation of polystyrene as a protective of wood in sea-water
1986 - IRG/WP 4129
A test is described on the biological protection of wood by treatment with polystyrene. The results, obtained in marine trials, after 18 months, show that the treatment with polystyrene is not all that effective in preventing the attack of marine borers....
A Gambetta


Above ground testing of wood preservatives - some experiences from Sweden
1995 - IRG/WP 95-20079
Field stake tests for the evaluation of wood preservatives have been used for more than 50 years in Sweden. In the Nordic countries a system for approval of wood preservatives, which includes field test, has also been in operation for more than 25 years. This system has been described in an IRG Document by Henningson & Jermer (1988). The Nordic system is now in a process of harmonization with ...
B Henningsson, Ö Bergman


Treatment of Douglas fir heartwood with disodium octaborate tetrahydrate (Tim-BorÒ ) to prevent attack by the Formosan subterranean termite
1991 - IRG/WP 1487
Toxicity of disodium octaborate tetrahydrate (Tim-BorÒ) to Coptotermes formosanus Shiraki (Isoptera: Rhinotermitidae), and termite feeding on treated Douglas-fir heartwood were evaluated in laboratory and field tests. Feeding on filter papers impregnated with Tim-BorÒ solutions reduced but did not eliminate termite gut protozoan populations. In a forced-feeding laboratory assay, Douglas-fir hear...
M Tamashiro, R T Yamamoto, J K Grace


On the use of % weight loss as a measure for expressing results of laboratory decay experiments
1992 - IRG/WP 92-2394
It is suggested that careful consideration should be given for the presentation of data from laboratory decay experiments, especially when comparisons are being made from experiments involving wood blocks of varying densities. Percent weight loss can be used for comparisons of durability even if wood blocks vary in density. It is suggested that the absolute weight loss for a given volume (g/cm³) ...
T Nilsson, G F Daniel


Collaborative soft rot tests: Summary of comments on 'Proposals for a standardized soil burial test'
1971 - IRG/WP 202
J G Savory


Collaborative soft rot tests: 2nd interim report
1975 - IRG/WP 258
J G Savory, J K Carey