IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1058 documents. Displaying 25 entries per page.


Electron microscopic detection and chemical analysis of three-lamellar structures in wood-destroying fungi
1984 - IRG/WP 1240
In the course of transmission electron microscopical investigations of pine wood decay by various brown- and white-rot fungi extracellular three-lamellar structures (TLS) formed by the fungi were found in specimens stained with ruthenium red. These structures occured in the lumen of the wood cell surrounding the hypha at the outermost layer of the fungal cell wall. In the course of the investigati...
R Foisner, K Messner, H Stachelberger, M Röhr


Rapport sur l'activité du CEN/TC 38
1983 - IRG/WP 2204
M Pottevin


Questionnaire pour la préparation de fiches monographiques pour les champignons lignivores
1972 - IRG/WP 103 F
C Jacquiot


Detection of defects in standing poles by X-ray techniques
1980 - IRG/WP 2132
The application of X-ray techniques to wood pole inspection procedures has been evaluated. Internal defects were accurately identified using X-ray inspection methods. These methods and their possible influence on the safety and economic aspects of wood pale utilization are discussed....
W D Gardner, R S Johnstone, W Pitt


Long-term effectiveness of fumigants in controlling decay in Douglas fir waterfront timbers
1986 - IRG/WP 3364
The persistence, movement, and effectiveness of chloropicrin and Vapam (sodium N-methyl dithiocarbamate) in large, horizontal Douglas fir timbers were evaluated 7 years after fumigation. Chloropicrin prevented reestablishment of decay fungi; reinvasion occurred in some Vapam-treated timbers. Residual fungistatic effect was detected up to 1.2 m from the fumigation site in chloropicrintreated timber...
T L Highley


An in-ground natural durability field test of Australian timbers and exotic reference species. Part 2: Progress report after approximately 13 years' exposure
1983 - IRG/WP 1189
The condition of heartwood specimens of Australian and exotic timber species after approximately 13 years' in-ground exposure is given. Four of the 5 test sites have a termite hazard in addition to the hazard from a range of decay fungi. Values for specimen life are given only where all replicates of a timber species have become unserviceable. Results give evidence leading to doubt about ...
J D Thornton, G C Johnson, I W Saunders


Changes in the degree of decay of lignocellulosic substrate used in a screening test of fungicidal wood preservatives
1977 - IRG/WP 287
This report contains results of investigations aimed at: a) determination of the effect of the kind of substrate and species of test fungus on quantitative changes in used samples prepared from spruce cardboard, and b) comparison of the threshold fungicidal values of come fungicides determined with accelerated method, with values obtained by block method. During performed investigations, the metho...
K Lutomski


Some observations on causes of failure of preservative treated natural round transmission poles in Nigeria
1977 - IRG/WP 291
Treated natural round transmission poles in Nigeria have been discovered to be attacked underground as early as two years after planting. Termites and rot fungi attack the inner tissues and leave a pattern characteristic for the species of the pole. Tectona grandis, Nauclea diderrichii and Wide Pore pine, the major species for transmission poles in Nigeria show these attacks. A form of termite shi...
M A Odeyinde


Some physiological characteristics of a non-degradative strain of Postia (=Poria) placenta
1988 - IRG/WP 1341
The decay capacity of 14 strains of the brown-rot fungus Postia (= Poria) placenta was determined using soil-wood block tests. One isolate was identified as being unable to degrade wood and was determined to be monokaryotic. It retained the ability to produce extracellular carbohydrate-degrading enzymes, although regulation of certain enzymes was atypical under certain cultural conditions. It prod...
J A Micales, T L Highley


A technique for the quantitative isolation of Actinomycetes from decayed wood
1980 - IRG/WP 1116
A technique combining comminution and high-speed homogenisation has been developed for the preparation of suspensions of micro-organisms in colonised wood. When standard inocula of Streptomyces spores were applied to wood, constant proportions of the inocula were recovered. This method was used in conjunction with selective culture media to isolate actinomycetes from wood which had been buried in ...
A A W Baecker, B King


Forest products laboratory methodology for monitoring decay in wood exposed above ground
1995 - IRG/WP 95-20074
Research at the Forest Products Laboratory on the durability of wood in service has included a full complement of laboratory and field tests. In this report, we present a review of past and current methods used to evaluate the condition of preservative-treated wood exposed above ground. Current protocols are described for tests on wood packaging, roofing, and dimension lumber....
R C De Groot, T L Highley


Some thoughts on the future strategy for eradicating Serpula lacrymans from a building
1989 - IRG/WP 1405
We now have a clear view of the mechanism of translocation of nutrients in the mycelium of Serpula lacrymans which is one of the physiological processes underlying the remarkable capacity of this fungus to spread through a building. Here the elements of the mechanism of translocation are dissected out to suggest avenues which might be followed in the search for new ways for eradicating the fungus ...
D H Jennings


The effect of sapwood on the rate of deterioration of fence posts
1986 - IRG/WP 1277
In order to evaluate the effect of the presence of sapwood on the rate of deterioration of fence posts, 30 specimens with and without sapwood of Eucalyptus citriodora, Eucalyptus paniculata, Eucalyptus saligna and Eucalyptus tereticornis were exposed in three test sites in the State of São Paulo, Brazil. The results of the inspection carried out in 1985, after 5 years of exposure, are reported in...
M S Cavalcante, G A C Lopez, E S F Mucci, R G Montagna


Collaborative soft rot tests
1981 - IRG/WP 2151
There appears to be need for reconsideration of attitudes towards Standardisation of laboratory tests for determining the toxicity of preservatives to soft rot fungi. The original approach was that a limited number of test methods were available and that collaborative effort would determine the suitability of the methods for Standardisation. It has been established so far that pure culture testing...
J G Savory


Proposal for further work on pretreatment decay
1988 - IRG/WP 1374
Pretreatment decay is a world wide problem sometimes ignored by pole producers. Words like "poles are not worse now than they were 50 years ago" or "we have always handled poles in this way without trouble" are weak defences. All other industries try to make their products better, so why not the impregnation industry? Or is the pole industry right? What do we know about the long term effect of pre...
M-L Edlund


Decay patterns observed in butylene oxide modified ponderosa pine attacked by Fomitopsis pinicola
1983 - IRG/WP 1183
Small blocks of ponderosa pine chemically modified by butylene oxide to three different weight percent gains (WPG) were decayed for 2 months with the brown rot fungus Fomitopsis pinicola. Wood substance loss and the type of decay pattern recognised were fairly similar both for control and blocks treated to 8 and 15 WPG. No difference in attack was observed between radial or tangential walls in lat...
T Nilsson, R M Rowell


Extracellular layers of wood decay fungi and copper tolerance
1983 - IRG/WP 1180
Extracellular layers around the hyphae of brown, white and soft rot fungi have been examined using electron microscopy. These layers were isolated for identification. Particular interest was directed towards the extracellular layers of copper-tolerant soft rot fungi....
D M Francis, L E Leightley


Fungus cellar and stake tests with tall oil derivatives. Progress Report after 5 years' testing
1987 - IRG/WP 3442
Two derivatives of tall oils have been tested for five years in fungus cellar and stake tests. The samples were relatively quickly attacked on the surface by decay fungi, mainly soft rot, but the decay has progressed very slowly. The performance of the stakes in the tests has so far been equivalent or even better than some CCA preservatives and creosote....
J Jermer, Ö Bergman, T Nilsson


Detection of brown rot decay in wood by ion mobility spectrometry
1991 - IRG/WP 2377
A test method for the detection of brown rot decay in wood is described and involves a two-step procedure: thermal release of vapours from wood samples followed by analysis using Ion Mobility Spectrometry (IMS), with results being obtained in 5-10 seconds. The advantages, limitations as well as the detection limit of the technique are presented....
A H Lawrence, T Nilsson


Short term preconditioning of preservative-treated wood in soil contact in relation to performance in field trials
2000 - IRG/WP 00-20185
The effect of pre-exposure to primary colonising micro-organisms on preservative-treated wood, prior to a basidiomycete decay test, was determined by preconditioning in two soil types. Scots pine EN 113 blocks treated with 3 model systems (a triazole, a copper quaternary compound and a copper boron triazole) were leached according to EN 84 and subjected to 6 weeks and 8 weeks burial in either John...
S Molnar, D J Dickinson


Efficacy of some extractives from Pinus heartwood for protection of Pinus radiata sapwood against biodeterioration. Part 1: Fungal decay
1995 - IRG/WP 95-30072
Chemical compounds thought to contribute to the natural durability of heartwood of Pinus spp. were either chemically synthesised in the laboratory or extracted from the heartwood of Pinus elliottii or Pinus caribaea. These compounds included the stilbenes, pinosylvin and its mono- and di-methyl ethers, and the flavonoids, pinobanksin and pinocembrin. Small blocks of Pinus radiata sapwood were impr...
M J Kennedy, J A Drysdale, J Brown


Prevention of brown-rot decay by chelators
1992 - IRG/WP 92-1540
In this work the brown-rot decay was shown to be prevented by chelating the endogenous metals existing in wood by using organic or inorganic chelators or iron-binding siderophores. The fungal growth and decaying ability were significantly decreased by the chelating treatments of the solid wood-based culture medium and pine wood pieces, respectively. The transition metals existing in native wood ar...
L Viikari, A-C Ritschkoff


Description of the damage produced by xilophagus Curculionides in Spain
1989 - IRG/WP 1408
Cossoninae are a reduced subfamily of Curculionidae. These xilophagus insects produce significant damage in Spain, mainly affecting old buildings. Their activity is a real problem for the preservation of the country's historical-artistic heritage. The three Cossoninae species most widespread in Spain are described for the first time as well as the conditions under which they develop. The ...
E L Rodríguez Trobajo


The effect of storage or simulated internal use on the durability of wood based panels to decay fungi
1997 - IRG/WP 97-20106
Wood based panels such as particleboard and medium density fibreboard are experiencing a steady increase in use, in areas from structural to decorative applications. Understanding the "natural" durability of these panel products against basidiomycete fungal decay is therefore of great importance. Various methods have been proposed or are under development to test the durability/susceptibility of v...
S F Curling, R J Murphy, J K Carey


Preventive action against fungal decay: A comparative experiment on the effects of natural and artificial infection of wood by Basidiomycetes
1981 - IRG/WP 2160
M Fougerousse


Previous Page | Next Page