Laboratory culturing and decay testing with Physisporinus vitreus and Donkioporia expansa orginating from identical cooling tower environments show major differences
1996 - IRG/WP 96-10184
Both Basidiomycete fungi Physisporinus vitreus (Pers.:Fr.) P. Karst. and Donkioporia expansa (Desm.) Kotl. & Pouz. were isolated from identical cooling tower environments. Azobé heartwood (Lophira alata), a very durable tropical wood species was totally deteriorated in cooling towers in a similar way by both fungi. First attempts to culture Physisporinus vitreus in laboratory circumstances sh...
J Van Acker, M Stevens


Scientific development for prolonging the service life of timbers by impregnating with creosote or organic solvent type preservatives in which additive has been incorporated
1977 - IRG/WP 382
Chemically impregnated wood has played a prominent part in the Telephone and Electricity Distribution Industry during the past century and there is no doubt that it will play an equally prominent part in the future. The reasons why wood poles and wooden, structures predominate, are that when adequately chemically impregnated with a recognised timber preservative to ensure the expected service life...
P R B D De Bruin


Efficacy of anhydrides as wood protection chemicals - II. Performance against soft rot fungi
1998 - IRG/WP 98-30174
Pine sapwood modified with various anhydrides and with butyl isocyanate was tested for its resistance to soft rot decay. Small stakes were exposed for 20 months in unsterile soil in a fungal cellar test. Wood modified with butyl isocyanate performed better than any of the anhydrides tested, with a threshold level of protection (less than 3% weight loss) at 12% weight percent gain (WPG). Stakes ac...
S C Forster, M D C Hale, G R Williams


Detection of defects in standing poles by X-ray techniques
1980 - IRG/WP 2132
The application of X-ray techniques to wood pole inspection procedures has been evaluated. Internal defects were accurately identified using X-ray inspection methods. These methods and their possible influence on the safety and economic aspects of wood pale utilization are discussed....
W D Gardner, R S Johnstone, W Pitt


Long-term effectiveness of fumigants in controlling decay in Douglas fir waterfront timbers
1986 - IRG/WP 3364
The persistence, movement, and effectiveness of chloropicrin and Vapam (sodium N-methyl dithiocarbamate) in large, horizontal Douglas fir timbers were evaluated 7 years after fumigation. Chloropicrin prevented reestablishment of decay fungi; reinvasion occurred in some Vapam-treated timbers. Residual fungistatic effect was detected up to 1.2 m from the fumigation site in chloropicrintreated timber...
T L Highley


Forest products laboratory methodology for monitoring decay in wood exposed above ground
1995 - IRG/WP 95-20074
Research at the Forest Products Laboratory on the durability of wood in service has included a full complement of laboratory and field tests. In this report, we present a review of past and current methods used to evaluate the condition of preservative-treated wood exposed above ground. Current protocols are described for tests on wood packaging, roofing, and dimension lumber....
R C De Groot, T L Highley


Some thoughts on the future strategy for eradicating Serpula lacrymans from a building
1989 - IRG/WP 1405
We now have a clear view of the mechanism of translocation of nutrients in the mycelium of Serpula lacrymans which is one of the physiological processes underlying the remarkable capacity of this fungus to spread through a building. Here the elements of the mechanism of translocation are dissected out to suggest avenues which might be followed in the search for new ways for eradicating the fungus ...
D H Jennings


Electron microscopic detection and chemical analysis of three-lamellar structures in wood-destroying fungi
1984 - IRG/WP 1240
In the course of transmission electron microscopical investigations of pine wood decay by various brown- and white-rot fungi extracellular three-lamellar structures (TLS) formed by the fungi were found in specimens stained with ruthenium red. These structures occured in the lumen of the wood cell surrounding the hypha at the outermost layer of the fungal cell wall. In the course of the investigati...
R Foisner, K Messner, H Stachelberger, M Röhr


An in-ground natural durability field test of Australian timbers and exotic reference species. Part 2: Progress report after approximately 13 years' exposure
1983 - IRG/WP 1189
The condition of heartwood specimens of Australian and exotic timber species after approximately 13 years' in-ground exposure is given. Four of the 5 test sites have a termite hazard in addition to the hazard from a range of decay fungi. Values for specimen life are given only where all replicates of a timber species have become unserviceable. Results give evidence leading to doubt about ...
J D Thornton, G C Johnson, I W Saunders


Changes in the degree of decay of lignocellulosic substrate used in a screening test of fungicidal wood preservatives
1977 - IRG/WP 287
This report contains results of investigations aimed at: a) determination of the effect of the kind of substrate and species of test fungus on quantitative changes in used samples prepared from spruce cardboard, and b) comparison of the threshold fungicidal values of come fungicides determined with accelerated method, with values obtained by block method. During performed investigations, the metho...
K Lutomski


Some observations on causes of failure of preservative treated natural round transmission poles in Nigeria
1977 - IRG/WP 291
Treated natural round transmission poles in Nigeria have been discovered to be attacked underground as early as two years after planting. Termites and rot fungi attack the inner tissues and leave a pattern characteristic for the species of the pole. Tectona grandis, Nauclea diderrichii and Wide Pore pine, the major species for transmission poles in Nigeria show these attacks. A form of termite shi...
M A Odeyinde


Some physiological characteristics of a non-degradative strain of Postia (=Poria) placenta
1988 - IRG/WP 1341
The decay capacity of 14 strains of the brown-rot fungus Postia (= Poria) placenta was determined using soil-wood block tests. One isolate was identified as being unable to degrade wood and was determined to be monokaryotic. It retained the ability to produce extracellular carbohydrate-degrading enzymes, although regulation of certain enzymes was atypical under certain cultural conditions. It prod...
J A Micales, T L Highley


The effect of sapwood on the rate of deterioration of fence posts
1986 - IRG/WP 1277
In order to evaluate the effect of the presence of sapwood on the rate of deterioration of fence posts, 30 specimens with and without sapwood of Eucalyptus citriodora, Eucalyptus paniculata, Eucalyptus saligna and Eucalyptus tereticornis were exposed in three test sites in the State of São Paulo, Brazil. The results of the inspection carried out in 1985, after 5 years of exposure, are reported in...
M S Cavalcante, G A C Lopez, E S F Mucci, R G Montagna


Extracellular layers of wood decay fungi and copper tolerance
1983 - IRG/WP 1180
Extracellular layers around the hyphae of brown, white and soft rot fungi have been examined using electron microscopy. These layers were isolated for identification. Particular interest was directed towards the extracellular layers of copper-tolerant soft rot fungi....
D M Francis, L E Leightley


Fungus cellar and stake tests with tall oil derivatives. Progress Report after 5 years' testing
1987 - IRG/WP 3442
Two derivatives of tall oils have been tested for five years in fungus cellar and stake tests. The samples were relatively quickly attacked on the surface by decay fungi, mainly soft rot, but the decay has progressed very slowly. The performance of the stakes in the tests has so far been equivalent or even better than some CCA preservatives and creosote....
J Jermer, Ö Bergman, T Nilsson


Collaborative soft rot tests
1981 - IRG/WP 2151
There appears to be need for reconsideration of attitudes towards Standardisation of laboratory tests for determining the toxicity of preservatives to soft rot fungi. The original approach was that a limited number of test methods were available and that collaborative effort would determine the suitability of the methods for Standardisation. It has been established so far that pure culture testing...
J G Savory


A technique for the quantitative isolation of Actinomycetes from decayed wood
1980 - IRG/WP 1116
A technique combining comminution and high-speed homogenisation has been developed for the preparation of suspensions of micro-organisms in colonised wood. When standard inocula of Streptomyces spores were applied to wood, constant proportions of the inocula were recovered. This method was used in conjunction with selective culture media to isolate actinomycetes from wood which had been buried in ...
A A W Baecker, B King


Proposal for further work on pretreatment decay
1988 - IRG/WP 1374
Pretreatment decay is a world wide problem sometimes ignored by pole producers. Words like "poles are not worse now than they were 50 years ago" or "we have always handled poles in this way without trouble" are weak defences. All other industries try to make their products better, so why not the impregnation industry? Or is the pole industry right? What do we know about the long term effect of pre...
M-L Edlund


Detection of brown rot decay in wood by ion mobility spectrometry
1991 - IRG/WP 2377
A test method for the detection of brown rot decay in wood is described and involves a two-step procedure: thermal release of vapours from wood samples followed by analysis using Ion Mobility Spectrometry (IMS), with results being obtained in 5-10 seconds. The advantages, limitations as well as the detection limit of the technique are presented....
A H Lawrence, T Nilsson


Preventive action against fungal decay: A comparative experiment on the effects of natural and artificial infection of wood by Basidiomycetes
1981 - IRG/WP 2160
M Fougerousse


Decay in external joinery in the United Kingdom
1978 - IRG/WP 3116
no abstract available...
J G Savory, J K Carey


A short note on fungal decay in K33-treated poles
1982 - IRG/WP 1169
Soft rot cavities and erosion of the lumen have been found in K33-treated Pinus sylvestris poles from the years 1956-66 by microscopic studies. Poor treatment quality has been proved for some of these poles. The microscopy showed an unusual pattern of attack, and pre-treatment decay is suspected but not yet proved. Sounding the poles and using the Pilodyn indicated decay, but poking did not. Quant...
H Friis-Hansen


Decay patterns observed in butylene oxide modified ponderosa pine attacked by Fomitopsis pinicola
1983 - IRG/WP 1183
Small blocks of ponderosa pine chemically modified by butylene oxide to three different weight percent gains (WPG) were decayed for 2 months with the brown rot fungus Fomitopsis pinicola. Wood substance loss and the type of decay pattern recognised were fairly similar both for control and blocks treated to 8 and 15 WPG. No difference in attack was observed between radial or tangential walls in lat...
T Nilsson, R M Rowell


Short term preconditioning of preservative-treated wood in soil contact in relation to performance in field trials
2000 - IRG/WP 00-20185
The effect of pre-exposure to primary colonising micro-organisms on preservative-treated wood, prior to a basidiomycete decay test, was determined by preconditioning in two soil types. Scots pine EN 113 blocks treated with 3 model systems (a triazole, a copper quaternary compound and a copper boron triazole) were leached according to EN 84 and subjected to 6 weeks and 8 weeks burial in either John...
S Molnar, D J Dickinson


Long-term performance of a "wax" type additive for use with water-borne pressure preservative treatments
2000 - IRG/WP 00-40159
Field performance results are updated for matched CCA treated decking boards with and without an emulsion water repellent additive incorporated with the initial pressure treatment. Decks have been exposured for over 9 years in Harrisburg, NC. Boards were evaluated for in-service and laboratory performance for water repellent efficacy, as well as additive loadings in the boards after this exposure....
A R Zahora