Your search resulted in 90 documents. Displaying 25 entries per page.
CCFZ, a new type of water-borne wood preservative for vacuum pressure impregnation
1991 - IRG/WP 3643
By combination of CCF-Salt types with zinchexafluorosilicate a remarkable improvement of efficacy is achieved. In the same time the ecotoxicoligical data become more save. As well as the efficacy against wood-destroying organisms (Basidiomycetes, Soft rot and Long horn beetle) the basic data to evaluate the ecotoxicological behaviour of a CCFZ-Salt are described and compared with the properties of...
W Metzner, D Seepe, H-W Wegen
A new type of biocide suitable for use in different fields of wood preservation
1993 - IRG/WP 93-30014
A new type of polymeric biocides was developed containing quaternary ammonium and boron ester groups as active structure elements, to overcome the disadvantages of AAC's in wood preservation use and to utilise their good performance due to a broad efficacy against fungi on the other hand. The new biocides called polymeric betains have been tested in laboratory and field tests and especial...
V Barth, H Härtner
Survey of conditioning treatment practices in the Philippines
1975 - IRG/WP 349
The wood preservation industry in the Philippines is at present beset by many problems. An association of the industry similar to those existing in other countries has only been initiated last year by FORPRIDECOM. It is hoped that the formal organisation of this association will bring into focus the importance of this particular industry in the economic and industrial development of the country. L...
R F Casin
Tilting and vacuum treatment - two methods to obtain a non-dripping freshly treated timber
1989 - IRG/WP 3535
Modern impregnation plants are designed to prevent spread of impregnation solutions from the plant through leakage, etc. It is also important that freshly treated timber does not spread solutions through dripping on the storage area. To prevent this, the impregnation procedure is terminated with a vacuum period. In many plants in Sweden this period is minimized or even excluded to gain time. Inste...
I Johansson, M-L Edlund
A new preservative - A double-edged sword
1990 - IRG/WP 3573
Increasing environmental pressures on the use of pesticides throughout the world will impact more on the use of all wood preservatives. In particular the use of traditional wood preservatives and methods of application are under close scrutiny. The industry is responding to the challenge of developing alternative products and systems but faces great problems due to the excellent performance and sa...
M Connell, J A Cornfield, G R Williams
A new vacuum/pressure plant system
1988 - IRG/WP 3479
In the subtropical regions, the problem of wood supplying becomes more and more difficult to be solved. In that context, the Centre Technique Forestier Tropical had paid a particular attention to the valorization of products issued from plantations in dry zones of Africa. In these plantations, the products of clearings can be used as fencing, stakes or for traditional construction. However in thes...
C Dalois, R Schwartz, G R Y Déon
Characteristics of thermally modified wood in vacuum
2004 - IRG/WP 04-40287
In commercial thermal wood modification processes nitrogen, steam or oil has been used for the reduction of oxygen content in the reactor atmosphere. In present study no special heating medium, but an initial vacuuming step has been used for this purpose. Mass loss, resistance to fungal decay, dimensional stability, bending strength and modulus of elasticity of heat treated wood were evaluated and...
G Rep, F Pohleven, B Bucar
Preservation of coppice wood for the fabrication of glued beams or panels
1987 - IRG/WP 3427
In this survey we will examine the specific problems concerning the conservation and the preservation of timber (issued from trunks of small diameter corresponding to products of clearings or coppices) destined for the fabrication of solid reconstituted elements. Thus for six metropolitan species of wood, we first characterized the biological deteriorations which occur after felling and their kine...
G R Y Déon, R Schwartz
Effectiveness of wood preservatives and treatments against marine borers in Philippine waters
1976 - IRG/WP 416
A 5-year exposure test was conducted on the effectiveness of wood preservatives and treatments against marine borers in Philippine waters. Air-dried heartwood samples of apitong (Dipterocarpus grandiflorus) 76.2 x 88.9 x 609.6 mm³ (3 x 3.5 x 24 in³) in size were pressure treated with coal tar creosote and two types of CCA (copper/chrome/arsenic) and CuCZA (copperized chromated zinc arsenate) wat...
F R Siriban, M G Laxamana, P G Mata
Moisture content and other tested values in. Double layer tests of different size in Lithuania and Germany
2004 - IRG/WP 04-20299
The paper presents measurement results of moisture content and the analysis of durability trial of double layer wood in variants of varying size, conducted in Girionys, Kaunas distr., Lithuania and in Hamburg, Germany. In this trial 3 sample sets of varying size, containing 25, 50 and 100 specimens, are used. The aim of this trial is to ascertain an optimal number of test specimens. The dynamics o...
J Saladis, A O Rapp
Application of paint primers after light organic solvent preservative treatment
1986 - IRG/WP 3381
The application of three alternative paint primers is investigated, including a slow-drying oil-based primer, a fast-drying oil-based primer, and a fast-drying water-based primer. The treatment schedules employed, in particular the evacuation period after treatment, have a marked effect on subsequent paintability. Priming can potentially be carried out immediately after treatment with approved Tim...
P Vinden
Fixation of chromated wood preservatives through technical drying
1990 - IRG/WP 3623
Twin samples of sawn timber of Pinus sylvestris and Picea sp. were treated with copper-chromate-containing wood preservatives and subsequently kiln resp. air dried. After drying, the distribution of preservative and rate of fixation were determined. Drying of freshly treated wood in a condenser type kiln at temperatures of 60°C and 80°C and in a vacuum type kiln at 55°C with a pressure of about...
R-D Peek, H Klipp
The natural durability of wood in different use classes - PART II
2006 - IRG/WP 06-10598
The natural durability of important European wood species has been tested on 3970 speci¬mens in field trials. The wood was exposed at five test sites in Germany with different climates, at each site in European use class 4 and 3 (with and without soil contact). Within European use class 3 three different expositions were tested: vertical with sheltered end grain, vertical unsheltered and horizont...
A O Rapp, U Augusta, K Brandt
Comparison of permeability at different levels of moisture content in Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) impregnated under vacuum/pressure through full-cell method by using CCA and CCB of different concentrations
2007 - IRG/WP 07-40366
In this study, a comparison has been made in terms of the combined, longitudinal, tangential, and radial permeability of the species of Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) with moisture contents of 50 % and 15 %, which were impregnated under vacuum/pressure through full-cell method by using water-borne wood preservatives (impregnation materials)...
I Usta
Effect of juglone from Juglans mandshurica bark activity of wood decay fungi
2009 - IRG/WP 09-30502
Juglone was extracted from Juglans mandshurica bark via vacuum-assisted steam stripping. The extract was characterized by Fourier Transform Infrared Spectroscopy (FTIR), 1H Nuclear Magnetic Resonance (NMR) and Gas chromatography/mass spectrometry (GC-MS). The extraction process was easy to perform and produced excellent yields (0.22 g juglone/100 g of bark) of a high purity extract (96.42% juglone...
Dongmei Yang, Shuangyue Li, Shujun Li, Wenqiang Su, Yan Jin, Molong Sun
Service life prediction of wooden components – Part 1: Determination of dose-response functions for above ground decay
2010 - IRG/WP 10-20439
Scots pine sapwood (Pinus sylvestris L.) and Douglas fir heartwood (Pseudotsuga menziesii Franco) specimens were exposed in double layer field trials at 24 different European test sites under different exposure conditions (in total 28 test sets). The material climate in terms of wood moisture content (MC) and wood temperature was automatically recorded over a period of up to eight years and compar...
C Brischke, A O Rapp
Vacuum drying of European oakwood: Color, chemistry and anti-oxidant potency of wood. Improving appearance in forest value added products
2008 - IRG/WP 08-40432
In hardwoods used for decorative and appearance purposes, wood colour is one of the most important factors of wood quality; in addition colour is related with durability and biological decay of wood. Wood discolouration during drying is mainly affected by heat, light, physiological reactions, combinations of reactions, biochemical and chemical reactions, and micro-organisms attack. In freshly fell...
S Sandoval, W Jomaa, F Marc, J-R Puiggali
Impact of climate change on wood deterioration - Challenges and solutions for cultural heritage
2010 - IRG/WP 10-20441
Deterioration of wood in cultural assets follows the same physiological mechanisms as in modern structures. Therefore rules and data for prediction of service life derived from old wooden structures can be used to model the service life of recent wooden structures and vice versa. The latter is done in this paper: From experimental test set ups in the field spread over Europe, climatic data, wood t...
C Brischke, A O Rapp, M Hasan, R Despot
Theoretic discussion on the way and driving forces of moisture migration in wood during vacuum drying
2011 - IRG/WP 10-40538
Most of parameters in conventional drying cannot explain a lot of phenomena appeared in vacuum condition, so it is necessary to further explore the moisture migration way and driving forces in wood under vacuum condition. For the water movement channel in wood is very narrow, the characteristic of heat and mass transfer in wood is similar to that in microscale. This article applies theory of liqui...
Zhengbin He, Xueli Yao, Liqiong Chen, Songlin Yi
Natural durability of wood tested in different environments in Northern Europe
2011 - IRG/WP 11-10747
Moisture is often recognised as a key factor regarding the long time performance of wooden products, and one of the main challenges for timber products is to predict accurate service life in use class 3 (not covered above ground) and use class 4 (in soil or fresh water contact). A range of durability classification studies have been performed both in field and laboratory. But for several wood spec...
P O Flæte, G Alfredsen, F G Evans
The potential of silicone-based formulations to enhance wood properties through industrial treatment for outdoor use
2011 - IRG/WP 11-30578
High hygroscopicity is one of the main weaknesses of wood as far as its susceptibility to biodegradation, and specifically to fungal decay. New wood preservation technologies are constantly entering the wood protection market, competing with traditional, biocide-based preservation. Silicones are commercially used as hydrophobic agents on stones and concrete. They belong to the restricted number of...
F Simon, F Marchal, F Pochon, M Kutnik, I Le Bayon
Limited variability in biological durability of thermally modified timber using vacuum based technology
2011 - IRG/WP 11-40567
The SmartHeat® thermal timber treatment is a new technology based on the process parameters being steered very precisely mainly due to the vacuum applied and heating system involved. Timber treated with this technology shows a potential for less variability of biological durability in one batch. Several batch treatments were sampled and assessed on statistical variability of decay resistance agai...
J Van Acker, S Michon, J Van den Bulcke, I De Windt, B Van Swaay, M Stevens
Moisture performance based wood durability testing
2012 - IRG/WP 12-20495
In the frame of a scientific cooperation within the Swedish research program ‘WoodBuild’ comparative field and laboratory durability studies have been carried out by the Technical Research Institute of Sweden SP and Leibniz University Hannover. One objective was to improve test methods as well as evaluation systems in order to facilitate the use of (field) testing for service life prediction. ...
L Meyer, C Brischke, A Pilgård
Durability of Furfurylated Wood – Results from Laboratory and Field Tests in the Ecobinders project
2012 - IRG/WP 12-40602
Within the EU project Ecobinders, laboratory tests were performed with furfurylated wood produced in semi-industrial scale in the factory of Kebony ASA. Field trials in Horizontal double layer decks and in-ground of transmission poles were also started. Four wood species, Southern yellow pine (SYP), maple, beech and aspen were treated to two treatment levels by using two impregnating liquids with ...
M Westin
A critical view on early indicators for above ground field performance of wood
2013 - IRG/WP 13-20509
Above ground field tests are quite often a balancing act between the provision of realistic test conditions, reliable statistics, and acceptable long test durations. Within this study we therefore reviewed 543 data sets from above ground field tests performed at 36 different test sites in 8 countries in Australia and Europe. The main objective was to investigate possible correlations between early...
C Brischke, L Meyer, G Alfredsen, P-O Flæte, L Francis, M Hansson, P Larsson Brelid, J Jermer