Interaction of Boultonizing and through-boring of Douglas fir sapwood
2018 - IRG/WP 18-40833
The interaction of combining through-boring and Boultonizing treatment effects on strength properties was investigated. Small, clear Douglas fir beams were through-bored and/or Boultonized in full factorial design and evaluated for toughness, MOE and MOR. The simulated through-boring treatment lowered the mechanical properties but the Boultonizing process did not. There was also no evidence for a ...
F Gasteiger, J Lloyd, A Taylor


Boron dual-treatments for Douglas-fir utility poles: Tracking boron migration over time
2019 - IRG/WP 19-30739
The potential for using boron pressure-treatment prior to over-treatment with conventional, heavy-duty wood preservatives to limit internal decay in-service was investigated in two field tests on Douglas-fir utility poles. Pole sections were pressure-treated with disodium octaborate tetrahydrate (DOT) and then over-treated with either pentachlorophenol or copper naphthenate in oil. Alternatively, ...
J Cappellazzi, M J Konkler, J J Morrell


Effect of damage to polyurea coatings on metal losses from ammoniacal copper zinc arsenate treated Douglas-fir pile sections
2019 - IRG/WP 19-40867
Metal-based preservatives remain the most widely used treatments for protecting wood in soil or water contact. While these treatments are highly effective, one drawback is a tendency for small amounts of metal to migrate into the surrounding environment. The greatest risk in this regard is copper because many organisms are highly sensitive to this metal. While post treatment practices can reduce ...
M J Konkler, J J Morrell


Sterilization of Large Timbers during Preservative Treatment: How Quickly We Forget
2020 - IRG/WP 20-40902
Air seasoning is a common method of moisture management in utility poles and is done de facto during pole storage prior to treatment. However, extended air drying prior to treatment encourages fungal attack and can facilitate establishment of decay fungi in poles before a protective preservative barrier is applied. This problem can be mitigated by proper air-seasoning methods coupled with heat ste...
G Presley, J Cappellazzi, M Konkler, K Maguire, R Nelson, J J Morrell


Studies on the material resistance and moisture dynamics of Douglas fir and Sitka spruce from Slovenia
2021 - IRG/WP 21-20677
Wood in outdoor applications is subject to various decomposition factors. Wood degradation can be prevented by construction details, biocide protection of wood, wood modification, or selection of naturally durable wood species. Unfortunately, the majority of timber species in Europe do not have naturally durable wood. Imported tree species represent a new pool from which we can draw wood species w...
M Humar, B Lesar, D Krzisnik, E Kerzic, R Brus


Durability of fast- and slow-grown Douglas fir in above ground exposures in Australia
2023 - IRG/WP 23-11009
Natural durability is a key property for untreated timber used outdoors and exposed to the weather. The natural durability of fast- and slow-grown Douglas fir heartwood was compared in an above-ground L-joint field test near Brisbane, Queensland, Australia. The L-joint test provides conditions that are favourable to decay. Fast-grown (regrowth) Douglas fir had ≤ 10 growth rings per 50 mm, while ...
L P Francis


Gloeophyllum trabeum and Gloeophyllum abietinum, the most frequent brown rot fungi in fir wood joinery
1999 - IRG/WP 99-10319
In Croatia the primary raw material for joinery production is silver fir wood (Abies alba Mill). L-joints made of home-grown fir sapwood and prepared according to EN 330: 1993 were used to establish the infection and colonisation of micro-organisms, particularly wood decay fungi, to compare the performance of untreated and 1% TnBTO treated L-joints. The L-joints were coated with two types of coat,...
R Despot, M Glavas


A behaviour of CCA penetration of fir (Abies bornmulleriana Mattf.) at different ramp times and constant vacuum/pressure applications
2006 - IRG/WP 06-40346
A behaviour of CCA penetration of Bornmulleriana fir (Abies bornmulleriana Mattf.) at different ramp times and constant vacuum/pressure applications was illustrated for the main flow directions by the experimental pictures....
I Usta, R Despot, M Hasan


Above ground performance of CCA-treated fingerjointed lumbe
1993 - IRG/WP 93-40003
Studs made from short lengths by finger jointing are becoming more commonly used in North America. Recently Forintek has received enquiries about the performance of such material in a treated form. Treated and untreated nominal 2x4 inch² spruce-pine-fir (SPF) studs exposed above ground for 12 years in southwestern British Columbia were evaluated for evidence of decay. Despite shallow preservative...
P I Morris, G E Troughton


Evaluation of Barrier Wrap Systems after 71 Months of Exposure
2013 - IRG/WP 13-40631
A 71 month study of the performance of booted samples in ground contact was conducted in AWPA hazard zone 4. Data indicated that excellent performance of wrapped systems, even over untreated wood, could be obtained. Instances of decay colonization or termite attack could all be attributed to some breaking of the integrity of the barrier system. Good performance for treatment below ground contact...
H M Barnes, M G Sanders, G B Lindsey, C McIntyre


A Soil Bed Test of the Effect of CCA Penetration on the Performance of Hem-fir Plywood
2004 - IRG/WP 04-30332
An accelerated decay test was set up to compare the performance of CCA-treated Western hemlock/amabilis fir plywood treated to meet the preserved wood foundation (PWF) retention standard with various patterns of preservative penetration. Short lengths of treated plywood and comparable untreated material were installed in a soil bed. After eleven years of exposure, the CCA treatments were all sou...
P I Morris, J K Ingram


Long-term protection of stored lumber against mould, stain, and specifically decay: A comparative field test of fungicidal formulations
1984 - IRG/WP 3281
The problem of decay in packaged, unseasoned lumber stored for many months has become of major importance in recent years. Large financial claims have resulted from decay in Canadian lumber stored at length in seaports and storage yards of distributors. For decades acceptable protection from moulds and sapstain was readily achieved with chlorinated phenols applied at appropriate treating levels. H...
A J Cserjesi, A Byrne, E L Johnson


Performance of non-incised CCA-treated hem-fir decking
1993 - IRG/WP 93-40004
The question of what preservative penetration will provide an acceptable service life for treated wood in residential above-ground applications is topical in North American standards committees. Non-incised CCA-treated nominal 2 x 4 inch² hem-fir decking with penetrations close to the proposed CSA O80 2 decking standard of 80% over 5 mm, has remained without decay after 10 years exposure in south...
P I Morris, J N R Ruddick


Comparative studies on the species effects of wood preservatives
1989 - IRG/WP 3521
For the examination of the resistance against fungal attack, wood blocks of 3 softwood species were treated with CCA (type 3), CFK, AAC and IF-1000 independently. The wood blocks were exposed to the fungal decay with Tyromyces palustris. The degradation of the wood blocks treated with these preservatives was quite widely different among wood species examined in this study. Hem-fir treated with CCA...
K Yamamoto, S Matsuoka


The comparative resistance to fungi of the wood munika (Pinus heldreichii Christ.), fir (Abies alba Mill.) and spruce (Picea excelsa Poir.) compared with Pinus sylvestris L. and some physical and mechanical characteristics of munika
1981 - IRG/WP 1129
The munika (Pinus heldreichii Christ.) is situated primarily in the Balkans, and partially in the south of the Apenine peninsula. As an endemic species, with a very little annual increment, it has not been used enough as a timber for mechanical conversion up till now, although the oldest trees can grow to 27 m in height, with a diameter at breast height of about 60 cm. According to data of many Ba...
M Petrovic, M Miric


Investigation of the suitability of silver fir (Abies alba Mill.) for thermal modification
2004 - IRG/WP 04-40275
In this study the suitability of silver fir (Abies alba Mill.) was examined for thermal modification. Comparative experimental investigations were performed with silver fir and Norway spruce (Picea abies Karst.) after thermal treatments. Besides properties, which characterize the quality of heat treatments, like dimensional stability and resistance against fungal attack, strength properties of the...
C Brischke, A O Rapp


The effect of rate of pressure application on preservative uptake along and across the grain of fir (Abies bornmulleriana Mattf.) at different ramp and constant pressure times
2004 - IRG/WP 04-20292
This study was particularly design to determine the preservative uptake at different ramp (rate of increase in pressure) and constant pressure times on longitudinal, tangential and radial penetrations of fir (Abies bornmulleriana Mattf.) which grown indigeneously in Turkey. The samples of 2 cm cubes of kiln-dried wood (nominated to 12% moisture content) were treated at different ramp times varied ...
I Usta


Sawn timber of fir (Abies alba Mill.) - Treatability and usability for the Hazard Classes 3 and 4
1999 - IRG/WP 99-40147
Within a national research project, tests on the treatability on sawn timber of fir (Abies alba Mill.) in oscillation pressure, vacuum pressure and double-vacuum processes have been worked out with 95 trunks taken from 3 different altitude levels (up to a height of 590 metres, 600 to 990 metres and over 1000 metres) and from 4 different regions of Switzerland. As the treatability of round wood can...
E Graf, T Bör


The performance in the sea of seven experimental piles after sixteen years at Port Douglas, North Queensland
1989 - IRG/WP 4151
After 16 years at Port Douglas, two double-treated Pinus radiata piles were in excellent condition, a CCA-treated Pinus elliottii pile was in good condition other than for a confined streak of teredinid attack, while two CCA-treated and two untreated turpentine piles were moderately to severely attacked by Sphaeroma in the tidal zone. The marine borers collected were Sphaeroma terebrans, Martesia ...
L J Cookson, J E Barnacle, C N McEvoy


A study of fungal biodeterioration in unseasoned, packaged hem-fir lumber
1978 - IRG/WP 2116
This study was undertaken to determine the extent of biodeterioration that could occur within British Columbia (BC) prior to the export of packaged Canadian Lumber Standard Hem-Fir (Tsuga heterophylla, Abies amabilis and small amounts of Abies grandis). By examining the anti-stain treatments received by the lumber and identifying and characterizing the organisms responsible for the biodeterioratio...
P W Perrin, A J Cserjesi


Specifying preservative-treated resistant timber: Conforming to European Standards
2001 - IRG/WP 01-20235
The most common construction timbers used in the UK are of low natural durability and, generally, resistant to preservative treatment. These include species of spruce, hemlock and fir. However, their characteristically limited and non-uniform uptake of preservatives may still confer sufficient protection to give satisfactory durability performance in terms of biological resistance. This paper desc...
E D Suttie, A F Bravery, T B Dearling


"Refractory" is a relative term. Incised alpine fir is treatable
1991 - IRG/WP 3670
While certain wood species carry a reputation for being 'treatable' this normally refers to the sapwood. For most Canadian species, heartwood penetration is the major determinant of whether treatment meets Canadian, USA and Japanese standards and in this respect alpine fir turns out to be a treatable species. Alpine fir is the fir component of the Western Canadian spruce-pine-fir...
P I Morris


Long term marine performance of ACZA treated Hem fir in Krishnapatnam harbour, east coast of India
2006 - IRG/WP 06-30409
The performance of Hem fir (Tsuga heterophylla) and Southern pine (Pinus sp.) treated with ammoniacal copper zinc arsenate (ACZA) and copper dimethyldithio carbamate (CDDC) at two retention levels of each preservative was assessed in tropical marine waters at Krishnapatnam harbour on the east coast of India. Panels treated with ACZA of lower loadings (23.1 Kg/m3) had failed in 38 months while the ...
B Tarakanadha, K S Rao, J J Morrell


Copper fixation in ACQ-D treated Chinese fir at various temperature and relative humidity conditions
2007 - IRG/WP 07-30436
In this study, the effect of different conditions of temperature, relative humidity, and duration of post-treatments on accelerating copper fixation in ACQ-D treated Chinese fir wood blocks was investigated. The conditions include the combination of three temperatures (21, 50, and 70?) and two relative humidity levels (20% and 80%), also include four temperatures (50, 70, 90, and 110?) without con...
Jinzhen Cao, Lili Yu


Accelerated fixation of ACQ-D treated Chinese fir with different post-treatments
2008 - IRG/WP 08-40400
With the enhanced focus on the environmental impact of the preservative-treated wood in recent years, it is necessary to perform some post treatments to prevent contamination of soil and ground water and reduce copper losses from ACQ treated wood in service. In this study, the potential of hot air, hot water, steaming and microwave post treatments to accelerate the fixation of copper in ACQ-D trea...
Lili Yu, Jinzhen Cao, P A Cooper


Previous Page | Next Page