Penetration as Key Factor for Determining the Performance of Wood Preservatives
2004 - IRG/WP 04-20293
Stakes of Scots pine sapwood with a dimension of 4 x 4 x 75 cm³ were impregnated with preservatives containing 2 % of propiconazole which had passed the EN 113 test criteria without any problems. The penetration of the colourless preservative was determined successfully by a fungal screening test described by Sutter (1978). The test revealed the insufficient penetration behaviour within the gi...
H Leithoff, I Stephan, R-D Peek


Variations in the virulence of test strains of Coniophora puteana (Schum ex Fr) Karst
1982 - IRG/WP 2185
In laboratory experiments using petri-dishes and small wood blocks (30 x 10 x 5 mm³) 6 different isolates of Coniophora puteana strain BAM 15 were compared with strain FPRL 11E for growth rate and decay capability. Only the recently received strain from EMPA was suitably active giving 24% weight loss after 6 weeks compared with 38.1% for 11E. Collation of data from standard test records revealed ...
A F Bravery, J K Carey, W Worley


A possible role of unique TCA cycles in wood-rotting basidiomycetes
2003 - IRG/WP 03-10461
The copper tolerant brown-rot fungus, Fomitopsis palustris, acquires metabolic energy by use of the constitutively-occurring Kornberg’s glyoxylate cycle coordinating with oxalate biosynthesis and glucose oxidation (Erman Munir et al. Proc. Natl. Acad. Sci. USA, (2001) 98, 11126-11130). Furthermore, this fungus does not have the normal TCA cycle, lacking 2-oxoglutarate dehydrogenase which is a ke...
E Munir, T Hattori, M Shimada


Mobility of zinc borate wood composite preservative
1997 - IRG/WP 97-30153
Zinc borate (ZB) is being used as an antifungal and insecticidal wood preservative for flake/strand-based composites. Data is reported on the laboratory and field leaching behavior of ZB when contained in apen flake composites. In general, the performance results correlate with leaching hazard. Although the boron in ZB is more resistant to depletion than in sodium borates, the ZB boron will deplet...
P E Laks, M J Manning


In-house accelerated method for testing decay resistance of treated wood
2004 - IRG/WP 04-20286
Fungicidal compounds often change their effectiveness when they are incorporated into candidate formulations. For this reason fungistatic effectiveness needs to be re-evaluated as many times as the formula has been modified for better performance. To avoid multiple expenses, in-house fungistatic tests are essential. Our goal was to develop in-house usable, simple but reliable and reproductive proc...
N Vidovic


Evaluation of the natural durability and ultrasonic method for decay detection of some european hardwood and softwood species
2004 - IRG/WP 04-10537
This paper presents the first part of an investigation on the natural durability of mixed plywood made of durable and non durable plies from the following selected timbers : Cedrus atlantica, Cupressus sempervirens, Castanea sativa, Populus sp. I 214 and Fagus sylvatica. In order to carry out this study, the natural durability of the massive wood used to manufacture the plywood panels was asses...
F Faraji, M-F Thévenon, B Thibaut


Residual resistance in eucalypt poles according to the degree of sanity
1984 - IRG/WP 2225
A lot of 50 eucalypt poles presenting external deterioration by fungus was taken from service and tested. These poles were classified into five degrees of sanity according to evaluation criteria adopted by the IPT Wood Division. After being classified, they were tested with respect to their bending resistance, in order to gather information about their critical degree of sanity which may define th...
F C Geraldo, S Milano, S G De Sequeira


The use of selective media for studying the colonization of wood in ground contact by microorganisms
1978 - IRG/WP 186
In October1976 a field trial was set up in order to monitor the progressive colonisation of wood in ground contact using orientated small stakes of Scots pine (Pinus sylvestris) and birch (Betula sp.) (30 x 45 x 250 mm³). Half the number of each species were treated with a 1% solution of CCA by a vacuum impregnation process. All the stakes were coated on three sides with an epoxy-resin sealant to...
C P Clubbe


Evaluation of the effectiveness of defence anti-stain in the control of sapstain in laboratory and field tests
1990 - IRG/WP 3593
The anti-sapstain product Defence Anti-stain (DAS) has been evaluated internationally in laboratory and field tests during the years 1988 and 1989. Results of tests carried out by institutes and by own companies in countries like Indonesia, Ivory Coast, Japan, Portugal, Belgium, The Netherlands and Spain will be presented. In the several tests Defence Anti-stain showed a high fungicidal activity t...
G Rustenburg, C J Klaver


Application of DNA fingerprinting methods to identify biocontrol strains of fungi imperfecti
1994 - IRG/WP 94-10068
We have analyzed a number of biocontrol strains of Trichoderma harzianum and other Trichoderma strains with the methods DNA fingerprinting and PCR fingerprinting to differentiate and identify these strain which is not possible with morphological or biochemical methods. We could differentiate even gamma-ray induced mutants from each other as well as different strains form the same and different spe...
A Schlick, K Kuhls, W Meyer, E Lieckfeld, T Börner, K Messner


Use of compression strength loss for measuring decay in the soil block test
1996 - IRG/WP 96-20083
The possibility of using radial direction compression strength of wood, rather than mass loss, was evaluated for both a brown-rot fungus (Gloeophyllum trabeum) and white-rot fungus (Trametes versicolor). With untreated pine wafers (5 x 19 x 19 mm³ - l x r x t) exposed to Gloeophyllum trabeum in a soil block test for five days, the compression strength loss was nearly 50% compared to a 5% mass los...
D D Nicholas, Zhongwei Jin


Redox regulation of enzyme activity during wood decay
1996 - IRG/WP 96-10172
A potential strategy in the search for alternative wood preservatives against fungal decay is to target the extracellular wood-decay process itself, rather than the decay organisms. This presents novel targets for selective disruption and possibly without the broad-spectrum toxicity associated with conventional wood preservatives. The enzymes of white rot decay are mechanistically diverse (e.g. hy...
P J Kersten, B Kurek, J W Whittaker


Heat inactivation of mould fungi on wood
1993 - IRG/WP 93-40012
Heat treatments have been successfully used for eradication of dry rot. The effect of heat treatments at 40, 50 and 60°C for various time intervals on the inactivation of Penicillium brevicompactum was determined. The effect of heat on ungerminated spores and spores "pregerminated" for 24 hours was evaluated by plating on malt-extract agar. Although most ungerminated spores were inactivated after...
J Bjurman


Characteristics of the pigments produced by sap-staining fungi
1997 - IRG/WP 97-10223
The present study was conducted to characterize the pigments produced by sap-staining fungi, Aureobasidium pullulans (de Bary) Arnaud and Ceratocystis piceae (Münch) H. and P. Sydow. The pigments isolated from tested fungi were identified as melanins by spectroscopic methods (UV and infrared spectra). The UV and the infrared spectra of the fungal pigments were similar to those of the synthetic me...
M Mori, M Takahashi


The relationship between blue-stain and bark beetles
1971 - IRG/WP 19
The attack of bark beetles on standing or in newly-felled stems provides special growth conditions to wood-inhabiting fungi. In the wood attacked by bark beetles, a specific and rich fungus flora is found, and from these fungi the economically important group of blueing fungi has been more thoroughly investigated. These fungi live on nutritive substances present in the cells, especially in the med...
A Käärik


Computerized axial tomography. A non-destructive method for three-dimensional wood density/moisture content measurement
1987 - IRG/WP 2285
Computerized Axial Tomography (CAT-scanning) - used for medical investigations of the brain - has been evaluated as a nondestructive method of three-dimensional wood density/moisture content measurements. Density can be measured with an accuracy of ±3 kg/m³, and the accuracy in average moisture content is ±1% below and above fibre saturation point. It is theoretically possible that measurements...
L O Lindgren


Fungicidal effectiveness of amended alkylammonium compound
1987 - IRG/WP 3421
Amendment of didecyldimethylammonium chloride was attempted to improve its fungicidal effectiveness and properties of treating solutions. Addition of copper definitely increased effectiveness in controlling wood decay fungi, although metal corrosiveness and stability of treating solutions was unsatisfactory. Further amendment with stabilizer(s), anticorrosive agent(s) and sequestering agent(s) res...
K Tsunoda, K Nishimoto


Preservative treatment of wood-based composites with a mixture formulation of IPBC-silafluofen using supercritical carbon dioxide as a carrier gas
2003 - IRG/WP 03-40251
Wood-based composites treated with a mixture formulation of a fungicide, 3-iodo-2-propynyl butylcarbamate (IPBC) and a termiticide, silafluofen using supercritical carbon dioxide (SC-CO2) as a carrier solvent were tested for their resistance to decay and termite attack in the laboratory. The treatment solution was prepared by mixing both biocides (IPBC 10 + silafluofen 1) with a co-solvent, ethano...
K Tsunoda, M Muin


The effect of initial moisture content on wood decay at different levels of gaseous oxygen concentration
1999 - IRG/WP 99-10316
The influence of initial moisture content on wood decay at different levels of atmospheric oxygen concentration was studied. Three fungi, Coriolus versicolor a white rot, Coniophora puteana a brown rot, and Chaetomium globosum a soft rot, were chosen. The mycelia of the fungi were inoculated on mini blocks of Fagus sylvatica (beech) and Pinus sylvestris (Scots pine). Incubations were under four le...
S M Kazemi, D J Dickinson, R J Murphy


Domestic wood preservation - Remedial treatments in Australia
1978 - IRG/WP 3128
Domestic construction in Australia relies heavily upon timber. Because of availability, local conditions and building practices, the timbers and other materials employed vary considerably between the States. In recent years, the timber floor has given way to 'raft construction' (concrete slab-on-ground). Not surprisingly, there is a tendency in each State to use local timbers for...
J Beesley, H Greaves


NMR T1 relaxation time as a non-destructive method for the study of decay in wood
1992 - IRG/WP 92-2406
The NMR spectroscopic technique of measuring the T1 spin-lattice relaxation times has been investigated for its potential in the detection of microbial decay in wood. The T1 NMR analyses were carried out on samples of Scots pine and European beech that had been exposed to decay and non-decay fungi representing each of the important groups colonising wood. Decay in the test material was also assess...
P W McCormack, A E G Cass, R J Murphy


Repairs of dry rot damages. A follow-up survey
1989 - IRG/WP 1400
The success of repairs of dry rot (Serpula lacrymans) damage in small houses was studied by means of a questionnaire, interviews and inspections. The research material consisted of 92 buildings in the first follow-up survey and of 71 of those 92 buildings in the second survey 6 years later. In 55 buildings the damages had been repaired once and at that time the harmfulness of dry rot fungus was kn...
L Paajanen


Suitability of propiconazole (R 49362) as a new-generation fungicide
1989 - IRG/WP 3529
Propiconazole (R 49362), an anti-fungal triazole-compound of Janssen Pharmaceutica, has been extensively tested to determine its potential use as a wood preserving fungicide. Various tests in both private laboratories and official institutes indicate a good activity against Basidiomycetes (brown and white rot) and Ascomycetes (blue stain-in-service). The active ingredient seems very resistant to w...
A R Valcke


Detection of dry rot by air analysis
1992 - IRG/WP 92-2399
Detection of dry rot (Serpula lacrymans) at an early stage appears to be very difficult in practice. Also control inspections in buildings, after remedial treatment of dry rot, have a limited accuracy. The use of trained dogs in Denmark initiated the idea for this research on the possible use of air analysis as a detection method. The Centre for Timber Research-TNO (TNO-CHT) and the Institute for ...
P Esser, A C Tas


Sterilization to limit pretreatment decay: Internal temperature during kiln drying of Douglas-fir poles
2001 - IRG/WP 01-40206
Sterilization to limit pretreatment decay: Internal temperature during kiln drying of Douglas-fir poles. Fungal colonization of poles following peeling has been the subject of considerable concern among electric utilities. While the presence of fungi does not, in itself constitute a risk, the survival of these fungi through the conventional treating processes could allow them to continue to degrad...
J J Morrell, P G Forsyth, K L Levien