Evaluation of the pulsed-current resistance meter (Shigometer®) for determination of the internal condition of utility poles
1979 - IRG/WP 2128
A number of Telecom poles, which had been removed from service to be replaced by a radio link, were inspected using an electrical resistance meter (Shigometer®). These poles were creosoted, non-durable Victorian species in service in New South Wales. Six of these poles, chosen to represent various internal conditions typical of the range of the population tested, are discussed here. Data, from tr...
J D Thornton, W G Seaman, M McKiterick


Leaching characteristics, decay and termite resistance of treated wood with boron compounds, N'-N-(1,8-Naphthalyl) hydroxylamine (NHA-Na), and hydroxynaphthalimide (NHA-H)
2003 - IRG/WP 03-30307
Despite many advantages of boron wood preservatives, boron itself does not adequately protect wood in ground contact and exterior applications because its natural diffusibility and susceptibility to leaching. As a result of previous studies to limit or decrease boron leaching, several fixation systems have been developed. In this study, we evaluated the effects of N'-N-(1, 8-Naphthalyl) h...
S N Kartal, Y Imamura


Decay and termite durabilities of heat-treated wood
2004 - IRG/WP 04-40272
Decay and termite resistances of Plato-treated timbers were evaluated using a modified JIS decay test method, feeding test in a laboratory scale and a field exposure against Reticulitermes speratus (Kolbe) or Coptotermes formosanus Shiraki. The results showed that no significant decay durability of the treated timbers although mass loss from decay slightly decreased in case of treated timbers. ...
S Doi, K Hanataa, E Kamonji, Yuuji Miyazaki


Preservation of robinia wood (Robinia pseudoacacia L.) stakes by vintners
1982 - IRG/WP 3194
This work discusses decay resistance of robinia wood to fungi Trametes versicolor (L.ex Fr.) Pil. and Coniophora puteana (Schum. ex Fr.) Karst., and also the possibility of influencing its resistance by means of chemical protection. The results showed that natural resistance of robinia wood to these two different agents of wood decay is not the same. It is much less resistant to the fungus Conioph...
R Benko


Resistance of various wood species against decay by Coniophora cerebella (Pers) Duby and Lenzites trabea (Pers) Bres
1976 - IRG/WP 142
Both fungi, Coniophora cerebella and Lenzites trabea, are important destroyers of timber. Coniophora often occurs inside buildings and Lenzites trabea has been observed on southern facades of buildings, on balconies and window frames. In most instances that we investigated coniferous timber had been decayed. But both species are known to attack also various hardwoods. For this reason tests similar...
O Wälchli


Resistance of wood inorganic material composites against decay fungi and subterranean termites
1996 - IRG/WP 96-40062
Double diffusion process was applied to the treatment of small sound sapwood specimens [20(T) x 20(R) x 10(L) mm³] of Cryptomeria japonica D. Don. The specimens were consecutively dipped in the two kinds of acqueous solutions to form water insoluble deposits within the wood after an expected reaction between the solutes. Following the comparison of deposits formed and treating conditions (tempera...
K Tsunoda, T Yoshimura, M Takahashi, S Hirao, H Usui


Efficacy of anhydrides as wood protection chemicals
1997 - IRG/WP 97-30162
Wood samples treated with anhydrides of various compositions have been examined for their decay resistance and moisture behaviour. For this purpose two brown rot fungi (Coniophora puteana and Gloeophyllum trabeum) and two white rot fungi (Trametes versicolor and Pycnoporus sanguineus) were used in conventional and modified soil block tests. The modified soil block tests conformed to the method as ...
S C Forster, M D C Hale, G R Williams


Decay resistance of densified ammonia-plasticized stems of oil palm (Elaeis guineensis)
1991 - IRG/WP 3673
When wafers of oil palm stems (Elaeis guineensis) were plasticized with 28% aqueous ammonia and immediately compressed mechanically, the treated material, gained 73% in basic density (average basic density, 0.695 g/cm³), and was highly resistant to decay by wood rot basidiomycetes. Compared with the control specimens (density, 0.403 g/cm³), resistance to decay of the densified specimens by Corio...
A H H Wong, M P Koh


NIR spectroscopy for rapid estimation of decay resistance
2004 - IRG/WP 04-20294
In Scandinavia Scots pine (Pinus sylvestris L.) is an important commercial tree species. Its heartwood has traditionally been used in constructions exposed to risk of decay. In a laboratory experiment Scots pine wood specimens sampled from inner heartwood, outer heartwood and sapwood were exposed to the brown rot fungus Poria placenta. In general outer heartwood was more resistant than inner heart...
P O Flæte, E Ystrøm Haartveit


Decay resistance of Platanus acerifolia wood against White Rot Fungi (Coriolus versicolor)
2002 - IRG/WP 02-10431
Degradation of the lignocellulose complex in wood varies on the microorganism causing decay and chemical composition of wood. The weight loss of Platanus acerifolia wood after decay by white rot fungus (Coriolus versicolor) for period 16 weeks were evaluated according to European standard EN 113 and beech wood as a control. The samples were collected in October 2000 from Nantes, France. The aim of...
M Irmouli, O Duchelier, N Ayadi, B Charrier


Is laboratory testing of decay resistance questionable as a single criterion for natural durability?
1996 - IRG/WP 96-20096
In a laboratory test set up over 20 hardwood species were evaluated according to the European Standard EN 350-1 including Basidiomycete and soft rot testing. Half of the species used were of a known natural durability. The Basidiomycete testing was carried out using Coriolus versicolor, Gloeophyllum trabeum and Coniophora puteana in a malt agar test similar to EN 113. From this test it was not pos...
J Van Acker, M Stevens, T Van Cauwenberghe, T Seynaeve


The Protection of Wood with Oxy-aluminium Compounds
2002 - IRG/WP 02-30286
Wood inorganic composites (WICs) containing aluminium compounds were developed and tested in relation to some essential requirements of preservative treated wood. Four different oxy-aluminium treatments were developed and identified according to the final insoluble compounds formed (sodium aluminate, aluminium hydroxide, magnesium aluminate and aluminium borate) in wood. Vacuum impregnation or dou...
F A Ximenes, P D Evans


Soil-bed decay resistance evaluation of strandboards treated with preservative at different points of the manufacture process after 18 months exposure
2002 - IRG/WP 02-40230
Strandboards were treated with a copper-boron water-based preservative at different points of manufacture process namely, green strand diffusion, vacuum, spray application in the resin blender and post manufacture heat and cold quench. Preservative was applied to achieve five different retentions (0, 1.5, 3, 6, 12 kg m-3). The modulus of rupture and modulus of elasticity were assessed before expo...
G J Goroyias, M D C Hale


Evaluating the resistance of wood-based panel products to fungal attack
1995 - IRG/WP 95-20071
At present there is considerable disagreement among national research institutes within Europe and panel product manufacturers on the most appropriate method of testing and indeed the need for specific biological durability testing. This paper seeks to place before a broader international audience, the issues related to development of a European standard for evaluating the resistance to fungal dec...
R G Lea, R W Berry


On the resistance of consolidated ancient wood against Serpula lacrymans (Wulfen: Fr.) Schroeter
2000 - IRG/WP 00-10348
Structural timbers and other wood objects of cultural value in historical buildings and museums are often attacked by wood-destroying fungi. The aim of conservators is to preserve such damaged timbers and prevent further biodeterioration by impregnation with consolidants. There is little knowledge of the resistance of consolidated timber and art objects to a new attack by wood-destroying fungi. Br...
W Unger, A Unger, U Schiessl


Difference of CCA efficacy among coniferous wood species
1990 - IRG/WP 3601
Wood blocks of Cryptomeria japonica, Tsuga heterophylla, and Pinus radiata successively extracted with n-hexane, ether, and methanol were treated with various concentrations of CCA type 3, which were subjected to the decay by Tyromyces palustris. The weight loss were different among species and kinds of extraction. Cryptomeria japonica treated with CCA had higher fungal resistance than Tsuga heter...
K Yamamoto, M Inoue


Resistance to decay of particle boards: Presentation of a test method
1986 - IRG/WP 2260
The experimentations were undertaken on particle boards 35 and 50 mm thick. The rot resistance tests were carried out on specimens whose dimensions were 600 x 75 x 35 mm³ for particle boards 35 mm thick and 800 x 75 x 50 mm³ for particle boards 50 mm thick according to a method derived from the one described in the documents IRG/WP/2214 and IRG/WP/2243. Two exposure periods were used: 12 and 16 ...
G R Y Déon, N Trong


Properties-enhanced albizzia particleboards by incorporating fungicide and insecticide in the glue
1994 - IRG/WP 94-30060
Preservative-treated particleboards were prepared by using tropical fast-growing albizzia and adding fungicides and insecticides to the adhesive-glue. the physical and biological properties of these boards were evaluated. No significant reduction in bending or internal-bond strength due to incorporation of the chemicals was detected. Treated particleboards effectively resisted attack by Coptoterme...
B Subiyanto, S Yusuf, Y Imamura, S Fushiki, T Saito, T Katuzawa


The improvement of wood durability by retification process
1993 - IRG/WP 93-40015
A material with new properties is obtained by retification process. It consists of a light pyrolysis of wood which becomes more stable and especially more resistant to fungal attack with few decrease of mechanical properties. Tests were carried out on three susceptible wood species (Poplar, Spruce, Fir) that are used in construction and are difficult to treat with wood preservatives. Retified wood...
D Dirol, R Guyonnet


Relative merits of laboratory and field tests for assessing wood decay resistance
1993 - IRG/WP 93-20009
Laboratory and field trials have long been employed for assessing natural durability of a variety of wood species, but there is a continuing debate concerning the relative merits of approach. While laboratory tests provide carefully controlled conditions for decay, they are often criticized for being too artificial to produce meaningful results. Conversely, field trials often vary widely between t...
T C Scheffer, J J Morrell


Resistance of acetylated wood to biological degradation. Evaluation of field test
1997 - IRG/WP 97-30139
Acetylated wood samples were tested in ground contact (stake test) at two test fields, one in Simlångsdalen, Sweden, and one in Viikki, Finland, according to European standard EN 252. The test samples were inspected annually and their condition was compared with that of untreated controls and of samples treated with two reference CCA preservatives. The use of untreated controls and preservative t...
P Larsson Brelid, R Simonson, Ö Bergman


The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...
A A H Wong, A P Singh


Window test. Direct testing of wood resistance to decay: A study of its fitness, its reliability and its accelerating factor
1984 - IRG/WP 2219
This is the results of an experiment using the window-test specimens, exposing the specimens to three different types of testing procedure: 1. Natural infestation in the open air; 2. Artificial infestation and exposure in the open air; 3. Artificial infestation in a green-house. The results show good similiraties of the three parallel tests in term of decay, and assess the reliability of the windo...
G R Y Déon, L N Trong


Dimensional stabilization and decay resistance of wood treated with brown-rotted lignin and copper sulfate
1990 - IRG/WP 3608
The objective of this study was to evaluate the potential usefulness of brown-rotted lignin (BRL) as a dimensional stabilization and copper complexing agent for wood treatment. For dimensional stabilization, aqueous solutions of the lignin extract were combined with either copper sulfate, glyoxal or other additives. Anti-shrink efficiency (ASE) values as high as 42% were obtained with wood treated...
L Jin, D D Nicholas, T Schultz


Decay and termite resistance of wood treated with boron-containing quaternary ammonia compound, didecyl dimethyl ammonium tetrafluoroborate (DBF) incorporated with acryl-silicon type resin
2004 - IRG/WP 04-30334
This study evaluates the decay and termite resistance of surface-treated wood with didecyl dimethyl ammonium tetrafluoroborate (DBF) incorporated with acryl-silicon type resin emulsion. DBF is a quaternary ammonia compound and contains boric tetrafluoride (BF4-) as a counter ion in its chemical structure. In the study, DBF was incorporated with an acryl-silicon type resin to increase water-resista...
S N Kartal, W J Hwang, K Shinoda, Y Imamura