Your search resulted in 928 documents. Displaying 25 entries per page.
Antagonistic effect of Trichoderma spp. against Serpula lacrymans in the soil treatment test
1991 - IRG/WP 1473
Soil treatment tests for preventing growth of Serpula lacrymans were conducted using Trichoderma spp. as antagonists. Soil specimens tested were Kanuma-soil without organic matter and the horticultural soil which was collected from the test site of the stake test. Perfect efficacy of treatment with Trichoderma spp. was shown when the horticultural soil without sterilization was used as a soil spec...
S Doi, A Yamada
36 years of wood preservative tests in Tanzania
1992 - IRG/WP 92-3731
The performanee of major wood presevatives which are used widely commereially are given. These include creosote, CCA's and 5% Pentachlorophenol dissolved in heavy industrial diesel. Tests are conducted at three ecologically different using pine stakes. Results show that the striking performance of creosote and CCA's is noticeable at above 128 kg/m³ and 16 kg/m³ respectively....
K K Murira, P F Nangawe
Field trials on preserved timber out of ground contact
1978 - IRG/WP 3154
This report describes two different field trials studying the performance of preservative treatments on timber exposed to the weather, but above the ground. Results are presented on the protection afforded against decay, and on the efficiency of water-repellent preservative treatments in controlling the uptake of moisture by the timber. Proposals for a standard field test system are briefly discus...
D F Purslow, N A Williams
Evaluation of the leach resistance and preservative efficacy of novel biocides as surface treatments applied by brush to spruce (Picea abies)
1998 - IRG/WP 98-30170
The comparative leach resistance and preservative efficacy of a number of alternative organic preservatives (available from Zeneca Specialties) and selected commercially available biocides as surface coatings to wood in Hazard Class 3 have been assessed. Two concentrations of test preservatives were applied by brush to Spruce (Picea abies), including formulation and untreated controls. A leaching ...
I M Tierney, A Bruce, D C R Sinclair, T Yeates
Protection of Ochroma pyramidale from fungal decay with N,N-napthaloylhyroxylamine
1998 - IRG/WP 98-30182
Fungal decay of wood in service results in billions of dollars (U.S.) in losses annually. Recent environmental restrictions, both U.S. and international, are limiting and eliminating the use of broad-spectrum, heavy metal biocides for wood preservation. Restrictions result primarily from problems with disposal. New wood preservatives need to be developed and tested which specifically target key el...
F Green III, T L Highley
Thirty-four year test of on-site preservative treatments to control decay in wood above ground
1993 - IRG/WP 93-30015
This research was initiated in 1958 to investigate efficacy of various preservatives and treating methods for new lumber going into exterior structures of buildings. Post-rail units (2x4 inches) constructed of Southern Pine sapwood, Douglas-fir heartwood, and mill run western hemlock were dip- or brush-treated before or after assembly. Units were trested with pentachlorophenol in various petroleum...
T L Highley, T C Scheffer
A method of predicting the average life of field tests on preservative-treated stakes
1977 - IRG/WP 297
The paper presents an analysis of the results of completed field stake tests on untreated and preserved timber, and develops a method of predicting the average life of incomplete stake tests on wood preservatives from the failures that have occurred so far....
D F Purslow
Biological control of blue stain on wood with Pseudomonas cepacia 6253. Laboratory and field test
1989 - IRG/WP 1380
Pseudomonas cepacia strain 6253 was tested as a biological control agent on wood samples under laboratory conditions, as well as in the field. In the laboratory this bacterium controlled blue stain on Pinus radiata, but field test were not totally satisfactory. However, after 2 months of field test, the test samples were 1/3 to 1/2 less stained then the control samples....
R Benko
Results of field tests on the natural durability of timber (1932-1975)
1976 - IRG/WP 3105
This paper describes a continuing field stake trial to determine the natural resistance of different species of timber to decay. Data are presented for about 180 timbers, covering over 6000 stakes, and the results are discussed in terms of a natural durability classification....
D W Purslow
Isolation and identification of the fungal flora in treated wood
1976 - IRG/WP 144
J F Levy
Termite field test results of preservative treated and modified woods in Kumamoto, Japan
2001 - IRG/WP 01-30275
Various preservative treated or modified wood stakes other than CCA, were buried in the soil, maximum for six years in Kumamoto, south west side of Japan. In this area, two main termite species, Coptotermes formosanus and Reticulitermes speratus, are distributed. After two years in field, untreated sapwood of sugi (Cryptomeria japonica) were observed severe attacks by termites, but the preservativ...
K Suzuki
A field test with anti-sapstain chemicals on sawn pine timber in Finland
1986 - IRG/WP 3368
Fourteen formulations, each in two concentrations, were tested for effectiveness against sapstain, mould and decay on Scots pine (Pinus sylvestris L.) in a field test in South-Finland. The trial was commenced in June 1985 and finished in October 1985. During the test the boards were infected mainly by mould fungi. In kiln dried boards the protective effects of nine and in green boards of four trea...
L Paajanen
Biological effectiveness of ground-contact wood preservatives as determined by field exposure stake tests
1984 - IRG/WP 3297
Field exposure tests conducted on stakes treated with different creosotes, mixtures of creosote and waxy oil as well as different CCA wood preservatives over a period of 25 years, gave the following results: The CCA preservatives provided excellent biological protection to treated stakes, especially against fungal attack. The CCA Type I, currently approved for use under South African conditions is...
W E Conradie, A Pizzi
Field Test Results after Nine Years for CCA and ACQ Preservative-treated Wood Fixed in Different Climates
2003 - IRG/WP 03-30303
During assessment of the ground contact stakes in the Norwegian test field, we have frequently found that the first visual rot attack is in the zone of the stakes, where the stakes have been in contact with each other during the fixation. These parts are usually light green, caused by the lack of light during fixation, compared to the rest of the stake surface, which has a darker colour.
To inves...
F G Evans
Programme Section 2 Test methodology and assessment
1999 - IRG/WP 99-20180
IRG Secretariat
Final proposals for collaborative work on laboratory soft rot testing
1987 - IRG/WP 2292
In this paper proposals are made to scope, timbers, preservatives, leaching, drying, soil type, moisture content, soil burial (blocks and stakes), incubation and dry weight determination and the expression of results....
D J Dickinson, S M Gray
Quelques observations biologiques sur la conduite des essais de protection des bois immerges en milieu marin
1976 - IRG/WP 421
P Deschamps
Measurement of VOC emissions from curative treated wood: A new emission test chamber
2001 - IRG/WP 01-50166-13
A poor indoor air quality (IAQ) is now recognized as a potential factor affecting occupants health. There are three basic strategies to improve IAQ: source control, improvement of the ventilation and use of air cleaners. Usually, the most efficient way to improve IAQ is to eliminate the different pollutant sources or to reduce their emissions. In order to precisely measure emissions from building ...
F Maupetit, O Ramalho, C Yrieix
Climate indices at work: Above ground decay L-joint tests (EN 330 and AWPA E9) at two sites 12000 km apart and with Scheffer climate indices of 60-65 and 300-330
1996 - IRG/WP 96-20095
Matched sets of Scots pine sapwood (Pinus sylvestris) L-joints were exposed above ground at two field sites for approximately five years. One site, at Garston, Watford, UK has a climate index between 60 and 65 while the other, close to Hilo, HI, USA has an index between 300 and 330. The joints were treated with a range of organic solvent treatments applied either by three minute dip immersion or b...
A F Preston, K J Archer, D M Roberts, J K Carey, A F Bravery
Co-operative field experiment. Performance of preservative-treated hardwoods with particular reference to soft rot: Report of condition of specimens installed in Victoria, Australia
1978 - IRG/WP 3118
J Beesley
Preservación de maderas en Bolivia
1986 - IRG/WP 3360
Este documento ofrece datos generales concerníentes a los recursos forestales de Bolivia, las facilidades existentes para preservación de maderas, la investigación y educación en esa materia. Se proporciona información sobre instituciones vinculadas a la actividad y las perspectivas del tratamiento de maderas en el país....
A S Viscarra
Questionnaire concerning assessment of test data from laboratory and field tests
1992 - IRG/WP 92-2418
During the WG II session in Harrogate, UK it was announced, that possibly a working-session on the assessment of test data and correlation between laboratory and field tests might be organised during next year's meeting in Orlando. For that pupose a questionnaire was prepared. The valuable comments and input of Prof. Thomas Nilsson from Sweden is hereby greatly acknowledged....
A R Valcke
Environmental risk assessment of preservative treated wood
1998 - IRG/WP 98-50101-19
This paper reviews the status of the environmental risk assessment of preservative treated wood and confirms the distinction between the risks presented by wood preservatives and preservative treated wood. The paper proposes a tiered approach to risk assessment and discusses the rationale. Flowcharts are presented which summarise the tiered approach to risk assessment, show the tests required, and...
E F Baines, S J Davis
How to determine what is a realistic emission from treated wood - basic reflections
1998 - IRG/WP 98-50105
Emissions from treated wood occur by evaporation and by leaching. Up to date by far more experience exists on leaching tests than on evaporation test. The methods applied will be of interest to give answers to the questions about the quantity of possible emissions. Standardisation on leaching started very early. One of the first attempts to quantify the effect of leaching on the remaining efficacy...
H Willeitner, R-D Peek
Performance of treated spruce in Canadian field test sites
1989 - IRG/WP 3506
Spruce material under test in Canadian field test sites is performing better than anticipated. From the comparison of the performance of spruce treated with various preservatives, it appears that penetration may be far more important on durability performance than the preservative itself or the retention of preservatives in the wood. However, there is still insufficient data on the influence of pe...
J P Hösli, E E Doyle