IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 29 documents. Displaying 25 entries per page.


Examen chimique du traitement de poteaux effectué à St-Michel s/Meurthe
1974 - IRG/WP 337
J Guillemain-Thévenot, C Jacquiot


The internal-external diffusion process: Table salt treated poles
2005 - IRG/WP 05-50224-25
This new technique of preservation of wooden poles consists of keeping preservative in stock, in a reservoir drilled inside the pole, in its whole length. This permits the use of non toxic, common products such as table salt, grease, etc, in the preservation of utility poles, building columns, or the like. Some major obstacles to a good implementation of a good preservation with the classical pr...
L Nitunga


Detoxification of preservatives: Tri-n-butyltin oxide as a biocide
1982 - IRG/WP 1156
T E Dudley-Brendell, D J Dickinson


Decay in external joinery in the United Kingdom
1978 - IRG/WP 3116
no abstract available...
J G Savory, J K Carey


An approach to testing the preventive effectiveness of preservative treatments for wooden joinery
1981 - IRG/WP 2156
The ecological sequence established in field trial samples exposed out of ground contact has shown the need for outdoor exposure in testing potential joinery preservative pretreatments. A system of exposure of L-joint units is proposed. Data obtained by examining samples destructively show promise as the basis for predicting service life after relatively short exposure periods (within 2 years)....
J K Carey, A F Bravery, J G Savory


Exterior wood stains
1980 - IRG/WP 3135
Experience has shown that conventional paints cannot now be relied upon to provide a complete seal against water entry, that in practice water can often circumvent the film and that the paint, far from serving to keep water out will seal it in. Moreover present-day paints are often subject to localised and premature failure out of doors and consequently entail high maintenance costs. Problems of w...
E R Miller


The use of bifluorides-diffusion in remedial treatments
1983 - IRG/WP 3256
A description is given about the experience to date of a 14 years' development to bring bifluorides-diffusion from laboratory evaluation to commercial service application. The described treatment is an adjunct to good design and not a replacement for it. The process is also used with an injection method for the remedial treatment of premature decayed external joinery....
H F M Nijman


The window joinery test hut
1975 - IRG/WP 257
D F Purslow


Remedial treatment of joinery. Comparison of distribution of organic solvent preservative and ammonium bifluoride
1978 - IRG/WP 3115
It is some years since it was recognised in the United Kingdom that there was a problem of premature decay in untreated external joinery. Consequently, recommendations for preservative treatment were made by the Building Research Establishment, Princes Risborough Laboratory. In addition, the National House-Building Council has also included the preservative treatment of external joinery in its req...
J M Taylor


Fluoride woodpill
1987 - IRG/WP 3431
Decay problems of spruce joinery in the Netherlands in the 1960's and 1970's led to the introduction of preservative treatment. Because of the known penetration difficulties with Spruce, the results of the treatments were not always successful. The fact that the decay was found only in the joints led to development of the philosophy of "local preservation" of the joints in remedi...
J W P T Van der Drift, K J M Bonsen


Xenon simulation of natural weathering of external joinery preserving - Finishing systems
1992 - IRG/WP 92-2412
Semitransparent wood stains ('lazures') for external joinery have developed by means of product combination towards complete wood finishing systems that are easy to applicate, have a good weathering resistance and low maintenance cost. The search for enhanced formulations and the possibilities to standardize these products or treatment systems are always facing long periods of we...
J Van Acker, M Stevens, M Nys


Interim report on the use of borate rods for the in-situ treatment of joinery
1980 - IRG/WP 3159
In the U.K. in recent years, it has been recognised that there is a major need for in-situ treatment of joinery at risk from or showing the early signs of decay. Several techniques have been developed to provide such a treatment, one of which is based on the insertion of anhydrous borate glass rods. The tests in hand are long term and this report is confined to the mycological isolation data from ...
D J Dickinson


Raising of the grain and deformation of Scots pine (Pinus sylvestris) treated with water-borne preservatives
1987 - IRG/WP 3456
In Sweden partial impregnation to 10 mm depth of the pine sapwood (class B in the Nordic preservation standard) of joineries was introduced during the seventies. To avoid product quality problems, organic solvent-based systems have been used. However, the Swedish industry today has problems with organic solvents, mainly for environmental reasons. We have studied raising of the grain and deformatio...
G Hägglund, T Sebring


New perspectives on the biology of the tropical powderpost beetle, Minthea rugicollis (Walk.)
1994 - IRG/WP 94-10085
Minthea rugicollis (Walk.) is one of the most important pests of seasoned hardwoods in the tropics. The species owes its ubiquity largely to its insidious development within a nutrient-filled environment and also to a strong coevolutionary specialization with its natural habitat, wood. Such an environment provides a buffer to extrinsic fluctuations and accounts for a wider range of tolerance by im...
F Abood, R J Murphy, R W Berry


Decay in window joinery in Sweden
1977 - IRG/WP 390
Systematic investigations of decay in window joinery in Sweden have not been undertaken until very recently. One might guess that one of the reasons for the minor interest is that this type of joinery did not rot strikingly faster than people expected. In the last 10-15 years, however, house owners, tenantowners, building societies and others have repeatedly argued that windows do rot more than in...
B Henningsson


Färbeverfahren zur Unterscheidung von Holzzonen mit unterschiedlichem Absorptionsvermögen, insbesondere bei Fichtenholz (Picea abies Karst.). [Staining method for distinguishing zones of wood with different absorption behaviour, particularly in spruce (Picea abies Karst.)]
1980 - IRG/WP 3163
A simple regressive staining method for crosscut wood surfaces is described. Phloroglucinol-hydrochloric acid serves as stain; flowing water and a solution of sodium carbonate are used for development and fixation of a picture showing the differences of absorption. Hydrophobic zones and, contrary to this, zones with a high water content can also be shown. Comparing green spruce wood before and dur...
S Cymorek


Chemical and biological investigations of double-vacuum treated windows after 5 years in service
1983 - IRG/WP 3219
In 1980 The Swedish Wood Preservation Institute initiated an investigation to study the degradation of TBTO and possible fungal attack in double-vacuum treated window joinery in service during 5 years. A hospital in Gothenburg was chosen that was built during 1969 to 1976. Both untreated and double-vacuum treated windows of Pinus sylvestris were used. A brown alkyl oil type paint (Nordsjö system ...
J Jermer, M-L Edlund, B Henningsson, W Hintze, S V Ohlsson


Wood preservation requirements in Queensland, Australia
1983 - IRG/WP 3227
In Queensland the preservative treatment and utilization of timber must comply with the Timber Users' Protection Act. Preservative retention levels and penetration patterns must be complied with. Analytical zones are specified for removing samples for chemical analysis of preservative retention. The required retention levels have been expressed as percent weight of oven dry wood weight. T...
L E Leightley, M J Kennedy


Studies and experiences of occurrence and development of soft rot in salt-treated poles of pine (Pinus sylvestris) installed in Swedish transmission lines in the years 1940-1945
1977 - IRG/WP 277
The present work describes the result of microscopic examinations of some 2,000 borings extracted from 20 to 23-year-old salt-treated poles (Scots pine) from the southern and central parts of Sweden. The purpose was to map out the occurrence of soft rot in Sweden and its influence on the mechanical strength of the poles as well as to contribute to the development of new and more satisfactory metho...
H Friis-Hansen


Chemical and biological investigations of double-vacuum treated windows after 7½ years in service
1985 - IRG/WP 3339
Earlier investigations of double-vacuum treated windows after five years in service have shown that tributyltin oxide (TBTO) degrades to di- and monobutyltin compounds and that the resistance of the wood against decay decreases. An investigation 2.5 years later of the same windows shows that the degradation of TBTO proceeds fast. After 7.5 years in service only 15-35% of the remaining organotin co...
M-L Edlund, J Jermer, B Henningsson, W Hintze


Testing blue stain fungicides for joinery timber in combination with natural weathering
1976 - IRG/WP 268
Joinery timber in outside use becomes affected by blue-stain after a short time of exposure. This is especially the case with pine sapwood treated with unpigmented lacquer, but also with other timber species as well as different types of surface treatment. According to the basic investigations of BUTIN this is due to special types of blue-stain fungi, called "Lack-bläue" (lacquer blue-stain), in ...
H Willeitner


A technique for determining the efficacy of water diffusible preservative plugs for implanting in joinery in service
1987 - IRG/WP 2291
A technique is described for determining the efficacy of soluble, diffusible preservative plugs for eradicating decay in joinery. It uses blocks of Scots pine sapwood or heartwood adjusted to known moisture contents prior to the establishment of the test fungus Coniophora puteana, from a single longitudinal dowel and the subsequent introduction of the preservative plugs. Prevention of decay, eradi...
J K Carey, A F Bravery


Comparative study of blue stain resistance of various types of wood stains after artificial and natural weathering
1992 - IRG/WP 92-2411
For the determination of the protective effectiveness of a preservative treatment against blue stain in service, artificial weathering has been proposed as an alternative for the natural weathering period of 6 months in the European standard EN 152. Research on a range of products and on complete finishing systems for external joinery was conducted during 1986-1990. It revealed that the decisions ...
J Van Acker, M Stevens, M Nys


Whitewood - An external joinery timber?
1975 - IRG/WP 253
The timber used traditionally for softwood joinery in the UK is redwood (Pinus sylvestris). In the past its ready availability in the desired sizes and quality and its durability in service encouraged little competition. However, the past decade has seen some erosion of this position, particularly through the increased proportion of sapwood in redwood supplies. Since the sapwood is less durable th...
J W W Morgan


Qualitative - Quantitative Analysis of Wood-Inhabiting Fungi in External Wooden Structures of the Latvian Cultural Heritage
2010 - IRG/WP 10-10728
The frequency and diversity of wood inhabiting fungi in the exterior wood were established in the Araishi lake fortress, the Lielvarde wooden castle, the Latvian Ethnographic Open-Air Museum, Riga, and twelve wooden heritage objects in the Eastern part of Latvia (Latgale). The inspected wooden structures of the external woodwork included windows, stairs, walls, floorings, roofs, fences, and benche...
I Irbe, M Karadelev, B Andersons


Next Page