Accelerated decay tests on DNBP-treated Pinus patula and Eucalyptus grandis
1987 - IRG/WP 3441
Blocks (10 x 10 x 5 mm³) of Pinus patula and Eucalyptus grandis were impregnated to 0, 1.5, 3.0 and 4.5 kg/m³ 2-sec-butyl, 4, 6 dinitrophenol (DNBP). They were monitored microscopically and for weight losses over 16 weeks against monocultures of Coriolus versicolor and Coniophora puteana. Treated ministakes (10 x 10 x 100 mm³) and blocks in soil contact were similarly monitored to determine wei...
L D Abraham, A A W Baecker


An Australian test of wood preservatives. Part 1: Preservatives, principles and practices
1978 - IRG/WP 2123
Between November, 1963, and July, 1964, a graveyard test of some 6000 preservative-treated stakes was installed at 8 sites equally distributed between Papua New Guinea in the tropics, through Queensland and New South Wales to Victoria. More than 40 different preservatives and preservative mixtures, mostly at several different levels of retention, were used to impregnate sawn specimens of Pinus rad...
J Beesley


A laboratory technique to measure the performance of preservative treated hardwoods in ground contact
1982 - IRG/WP 2172
A laboratory technique to measure the performance of preservative treated timber in ground contact is described. It uses partially sealed blocks of timber which are treated, leached and sawn into small stakelets for soil exposure in a fungal cellar. Performance is monitored by the loss of static bending strength with time, and a simple apparatus for measuring the deflection of a stakelet under a l...
E F Baines


A comparison of effectiveness of three waterborne preservatives against decay fungi in underground mines- An appraisal
2005 - IRG/WP 05-30366
To understand the effectiveness of waterborne preservatives and to explore the behaviour of roof supporting poles after pressure treatment, an experiment was conducted and thorough investigation was carried out during the last decade in the underground mines. Prior to commencement of the experiment, a survey was conducted at different depths in underground mines and collected decayed wood samples ...
P Narayanappa


Biostatic film as a primary treatment against pole failure in soil
1995 - IRG/WP 95-40053
Field liners of low density polyethylene (LDPE) film applied as primary treatment of soil-contact surfaces of creosote-treated poles prevented their detoxification and premature failure by establishing hurdles against microbiological colonisation. These hurdles include low water activity, low oxygen tension and nutrient limitations. Moreover, under conditions of high soil moisture, field trials sh...
A A W Baecker, M Behr


Estimation of oral toxicity of boron as a bait toxicant and the trophallactic effects between individual members of termite colonies.
2003 - IRG/WP 03-10495
In recent years, because of the favourable environmental characteristics of boron, researchers in the wood preservation industries have refocussed on the use of boron as a major wood preservative against wood-destroying insects. Currently the greatest use of boron compounds is in remedial treatments. Boron has been found to have slow-acting toxicity against subterranean termites. Because of thi...
B M Ahmed


A field method for determining the above-ground resistance of wood and wood products to attack by subterranean termite
1994 - IRG/WP 94-20035
A method for determining the above-ground resistance of wood and wood products to subterranean termites in the field is described. Termites are aggregated in 20-litre steel drums, each containing a highly susceptible timber substrate. At the centre of each drum, specimens of the test material under evaluation are sandwiched, using circular sections of wire mesh, between two layers of the substrate...
J W Creffield


A study on the pressure impregnation of Eucalyptus globulus fence-posts with CCA preservatives. Part 2
1989 - IRG/WP 3514
This paper describes the second part of a study on pressure impregnation of Eucalyptus globulus fence-posts with CCA preservatives presented at the IRG 19th Meeting. Fence-posts of three diameter classes, were treated, considering only one treatment schedule. The results show possibility of vacuum-pressure impregnation of blue gum fence-posts, with diameter less than 9 cm, though mainly by longitu...
L Nunes, D De Sousa Castro Reimão


Eucalyptus globulus. Impregnability in relation with plantation and crop
1992 - IRG/WP 92-2402
Eucalyptus globulus Lasill is currently classified in Pr EN 350 on the basis of the characteristics of the first log. In practice, there are usually several following crops of branches developped on each stump in plantations. Up to a diameter of 8 cm, round wood of 2nd crop and further crops present a maximum of sapwood and characteristics which differ significantly from the basic classification a...
D Dirol


Quantification of wood decay effects by HPLC analysis
1992 - IRG/WP 92-1576
The present work quantified the effects of the white rot basidiomycetes Coriolus versicolor and Phanaerochaete chrysosporium, and also those of the brown rot fungi Coniophora puteana and Lentinus lepideus, on Pinus patula and Eucalyptus grandis. Wood colonisation was quantified by Kjeldahl nitrogen determinations converted to biomass assays, and degradation was quantified by weight losses produced...
V Singh, M Tarin, G D Shelver, A A W Baecker


The colonisation pattern of anaerobic fungi in wood
1989 - IRG/WP 1403
Timber foundations may be degraded in service in anaerobic conditions. The present work was conducted to investigate whether anaerobic fungi could colonise wood, using rumen fungi as test microorganisms. Strictly anaerobic fungi were isolated and purified from cow dung and goat and sheep rumen fluids respectively. Colonisation of Eucalyptus grandis and Pinus patula by these fungi and Neocallimasti...
A H Wiederhold, M Morrison, A A W Baecker


Field Liners™ prevent creosote migration from transmission poles to soil during service
1996 - IRG/WP 96-40067
A full scale trial utilised 150 12m Eucalyptus grandis transmission poles treated with standard retentions of creosote according to SABS Method 457. One hundred poles had Field Liners™ applied while 50 did not. The 150 poles were used to complete an electricity transmission line in Southern KwaZulu-Natal. After 18 months service, incremental cores were taken from 15 cm below the ground lines of ...
M R Behr, G D Shelver, A A W Baecker


A novel solvent penetration assessment technique for wood preservativation treatments using waterborne systems
1990 - IRG/WP 2346
Solvent and hence solute (a.i.) penetration during any wood preservation treatment cycle and the flow pathways taken by the solvent in the wood are crucial elements in determining the adequacy of any treatment. Inadequate solvent penetration into specimens or an inappropriate tissue throughflow pattern during impregnation will markedly affect the distribution pattern achieved by many non-diffusibl...
A J Pendlebury, J Coetzee, E Sorfa, A Botha


Performance trials of treated hardwood fences
2002 - IRG/WP 02-30281
This paper examines the performance of the traditional hardwood paling fence used in Australia, after preservative treatment. Unseasoned rails, palings and plinths of the low natural durability species Eucalyptus regnans (mountain ash) and E. obliqua (messmate) were treated with PEC (pigment emulsified creosote) or PROCCA (an oil emulsion of CCA). Treated posts of these species were also compared ...
L J Cookson D Scown, B Iskra


Soluble nutrient influences on toxicity and permanence of CCA preservatives in wood
1980 - IRG/WP 3144
The influence of soluble carbohydrate and nitrogenous components concentrated at evaporative surfaces of wood on the toxicity and permanence of CCA preservatives has been examined using soil-burial techniques. Nutrient concentrations in lime (Tilia vulgaris Hayne) have been shown to be associated with reduction of toxic limits of preservatives to an extent in which a 100% increase in preservative ...
B King, G M Smith, A Bruce


Treatment of refractory timbers
1993 - IRG/WP 93-40001
Worldover crisis of wood is being felt due to the global environmental problems. Wood preservation technology plays a good role in curtailing the demands of wood for replacement by prolonging the service life of the timber and thus indirectly helps in saving the environment. Some species of timbers which could not be treated to the desired level by virtue of their refractory nature by any of the c...
I Dev, S Kumar


The performance of metal-chromium-arsenic formulations after 32 to 38 years' in-ground exposure in Australia
2000 - IRG/WP 00-30240
Two trials of metal-chromium-arsenic preservatives were exposed in-ground in Australia. In Trial 1, Pinus radiata stakes treated with Boliden K.33, Boliden S.25, Celcure A, Tanalith C and Tanalith CA were installed at Sydney and Narrandera in 1961/1962. In Trial 2, P. radiata and Eucalyptus regnans sapwood were treated with Celcure A, Celcure A21-N, Celcure A 21-O and Tanalith CA (new) and install...
G C Johnson, J D Thornton, J Beesley


Performance of different treatments and finishes on wood out of ground contact. Preliminary results
1984 - IRG/WP 2221
Pinus and Eucalyptus L-joints treated with CCA, a water dispersable PCP and untreated ones were painted according to seven different finish's schedules and exposed at two sites in State of Sao Paulo. After ten months of exposure, it was possible to verify that preservative treatment improve the performance of both wood and finish. It was also possible to observe that wood substrate, prese...
S Milano


Adequate preservative treatment of kiln dried Eucalyptus camaldulensis and Acacia mangium for tropical and subtropical wood poles
1996 - IRG/WP 96-40075
The Eucalyptus camaldulensis and Acacia mangium round timbers kiln-dried at EMC and full cell pressure treated with CCA-C ensured requisite penetration and adequate dry retention (30 kg/m³ or 4% w/w). The sufficient inherent strength, seasoning property, treatability of sapwood and heartwood equivalent to 44% of radius, natural durability of heartwood, and field investigation on service performan...
A K Lahiry


The evaluation of the effectiveness of wood preservatives by means of IUFRO's method for field tests with wooden stakes
1985 - IRG/WP 3348
Pinus elliottii and Eucalyptus saligna stakes treated with CCA-A, CCA-C, CCB, Cashew Nut Shell Oil and Benzotar solutions were exposed in seven test sites in Sao Paulo State, Brazil. After five years of exposure, between oil-borne preservatives Benzotar show better performance than CNSL (cashew nut shell liquid), and within waterborne preservatives the performance of CCB is not so good as that of ...
G A C Lopez, A M F Oliveira, E S Lepage


Clean creosote - its development, and comparison with conventional high temperature creosote
1983 - IRG/WP 3235
Pigment emulsified creosote (PEC) is presently being tested and shows considerable stability in terms of water content, pigment level, pH, viscosity, rheological behaviour and microscopy. Timber samples from several eucalypt species have been treated with PEC and side matched samples treated with conventional high temperature creosote (HTC). The PEC treated specimens showed higher weight retention...
C W Chin, J B Watkins, H Greaves


A comparative study of some anti-splitting devices, using Eucalyptus saligna and hybrids of Eucalyptus saligna X Eucalyptus spp poles
1983 - IRG/WP 3251
It is commom for some Brazilian wood pole users to require devices such as banding steel, to avoid or reduce splits at the end of Eucalyptus treated poles. On other hand users and manufacturers do not have data to confirm the effectiveness of the banding steel types normally used such as galvanized "Steel-Belt" and galvanized "Wire-Belt". For this reason a comparative study was carried out includi...
F C Geraldo, J A C Sodré


Nasutitermes exitiosus and wood-rotting fungi in Eucalyptus regnans, E. acmenioides, E. wandoo, and E. marginata: force-feeding, laboratory study
1985 - IRG/WP 1231
Under a force-feeding regime, the termitid Nasutitermes exitiosus was fed on four eucalypt timbers infested with several fungal species to investigate the influence of such fungus-infested timbers on mass of wood lost, termite biomass, fat content and water content. The results showed that wood mass losses were markedly affected by species of fungi and timber. The interaction of fungi and timbers ...
D B A Ruyooka


Field fencepost test of several species treated with water-borne preservatives by rural methods
1986 - IRG/WP 3385
Fencepost field results in ground-contact treated by rural methods: immersion-diffusion and sap displacement by evaporation are analyzed. Copper-chrome-arsenic and copper-fluor-chrome preservatives were used in two concentrations. The wooden species studied were: Pinus pinaster, Eucalyptus globulus and Quercus rubra. For each of the test units decay index evolution was analyzed after five years ex...
M V Baonza Merino


Assessment of untreated Papua New Guinea timbers against subterranean termites. Progress report 2
1993 - IRG/WP 93-10040
Eight species of Papua New Guinea wood including Kwila (Intsia palembanica), Taun (Pometia pinnata), Malas (Homalium foetidum), PNG Walnut (Dracontomelon dao), Calophyllum (Calophyllum sp.), Kamarere (Eucalyptus deglupta), PNG Beech (Nothofagus spp.) and White Cheesewood (Alstonia scholaris) were exposed groun contact for their natural durability against subterranean termites. Inspection after 42 ...
M Rokova, H C Konabe