Soft rot
1978 - IRG/WP 179
Soft rot decay of treated wood is examined with special reference to hardwoods treated with CCA. Factors which adversely affect the chances of protection of hardwoods against soft rot are discussed. The ratio of the volume of the fibre cell wall to the volume of the fibre lumen is presented as a major factor influencing final preservative concentration in the fibre cell wall, the major strength co...
C R Levy


Field trials of Sinesto B at some sawmills in Portugal
1989 - IRG/WP 3512
The efficacy of SINESTO B as antistain chemical for use in Portugal has been studied. The studies were done during the years 1987-1988 at several Portuguese sawmills in co-operation with the Instituto dos Produtos Florestais and the APCIM (Associacao Portuguesa de Comercio e Industria de Madeiras). SINESTO B was used in 5% and 8% concentrations. The storage time varied from 10 weeks to 6 months. I...
I A Linderborg


Studies on the permeability of Norway spruce (Picea abies)
1987 - IRG/WP 2295
It is well known that the bordered pits play a dominating role for liquid transport in softwoods. The mechanism behind pit aspiration during drying or heartwood formation seems to be well understood. The reason why the fixation of the membrane (torus) to the pit opening remains almost irreversible is, however, still unclear. A technique has been developed combining so-called "solvent exchange dryi...
I Johansson, K Nordman-Edberg


Evaluating the resistance of wood-based panel products to fungal attack
1995 - IRG/WP 95-20071
At present there is considerable disagreement among national research institutes within Europe and panel product manufacturers on the most appropriate method of testing and indeed the need for specific biological durability testing. This paper seeks to place before a broader international audience, the issues related to development of a European standard for evaluating the resistance to fungal dec...
R G Lea, R W Berry


Preservative treatment of Gollah cane (Daemonorops jenkinsiana) by soaking method
2001 - IRG/WP 01-40197
The feasibility of preservative treatment of gollah cane (Daemonorops jenkinsiana (Griff.) Mart.) by soaking method was tested in the present study. Cane samples of 1m, 2m and 3m long were soaked with 10% borax and boric acid solution. The study revealed that adequate dry salt retention (DSR) in the above samples could be obtained in 3 days, 4 days and 5 days of soaking, respectively. Within these...
M Younus-uzzaman, K Akhter, M H Chowdhury


Resistance to decay of particle boards: Presentation of a test method
1986 - IRG/WP 2260
The experimentations were undertaken on particle boards 35 and 50 mm thick. The rot resistance tests were carried out on specimens whose dimensions were 600 x 75 x 35 mm³ for particle boards 35 mm thick and 800 x 75 x 50 mm³ for particle boards 50 mm thick according to a method derived from the one described in the documents IRG/WP/2214 and IRG/WP/2243. Two exposure periods were used: 12 and 16 ...
G R Y Déon, N Trong


European standardization for wood preservation. Progress report 91-92
1992 - IRG/WP 92-2398
Since the IRG 22 conference in Kyoto, CEN/TC 38 Plenary met twice in relation with several working group meetings. 5 upon 6 of the interpretative documents have been prepared by adhoc groups of the Standing Committee for Construction within the scope of the 89/106/EEC directive on Construction Products. The expected requirements attached to wood preservation are both requirements 1) and 3): 1) mec...
R Hüe


The development of soft rot decay in bamboo fibres
1992 - IRG/WP 92-1572
The development of decay by soft rot fungus Chaetomium globosum was investigated in young and mature culms of bamboo Phyllostachys virideglaucescens. Soft rot decay was influenced both quantitatively and qualitatively by the differing levels of lignification in the material. Weight loss was significantly greater in the younger culm compared with the older, more heavily lignified culm. The distribu...
O Sulaiman, R J Murphy


Study on leaching of a magnesium fluorosilicate product (SF salt) from wood-boards by rain in the open and by artificial shower
1976 - IRG/WP 264
The test was performed in 1961 to obtain information about (1) the comparative leaching effect of natural rain and of artificial shower in the laboratory; (2) the comparative leaching effect on the active ingredient in proportion to the dye-stuff of the product. The results show that a continuos light rainfall with low precipitation has a much stronger leaching effect than short heavy showers with...
S Cymorek


Gelatin encapsulated fumigants for wood fumigations: Current research status
1985 - IRG/WP 3336
The fumigants chloropicrin (trichloronitromethane) and methylisothiocyanate (MIT) were encapsulated in gelatin as an alternative to liquid fumigant treatments for control of decay fungi in wooden utility poles. Gelatin-encapsulated MIT was stored for over 2 years under dry conditions without significant fumigant leakage. Gelatin encapsulated MIT and chloropicrin were released from capsules when pl...
A R Zahora, M E Corden, J J Morrell


Moisture correction for ultrasonic MOE measurements above fibre saturation point in Scots pine sapwood
2006 - IRG/WP 06-20333
There is a high correlation between methods for dynamic modulus of elasticity (MOEdyn) and static modulus of elasticity (MOEstat). MOEdyn methods have been found sensitive to detect early stages of decay and may be seen as an option for non-destructive wood durability testing. As the MOEstat measurements do not change after reaching the fibre saturation point, the uncorrected MOEdyn data from ultr...
E Larnøy, G Alfredsen, H Militz


COST Action E37. Sustainability Through New Technologies For Enhanced Wood Durability -
2008 - IRG/WP 08-40417
The main overall objective of the Action was to concentrate on the contribution of wood durability to sustainability through the development of systems for quality assurance and performance classification of modified wood and wood products as alternatives to wood treated with traditional preservatives. By this means it seeked to improve and consequently to increase the cost-effective use of compon...
R-D Peek, J Van Acker


SEM-EDXA of CCA-treated Rubberwood (Hevea brasiliensis)
2009 - IRG/WP 09-20399
The microdistribution of chromated copper arsenate (CCA) preservative in rubberwood was studied using scanning electron microscope in conjunction with energy dispersive X-ray analyzer (SEM-EDXA). Bulk X-ray analysis showed that there was a high accumulation of chromium, copper, and arsenic in the vessels and lower concentration of the three preservative elements in fibres. Chromium appeared to rec...
I Jusoh, D P Kamdem


Leaching of the copper component from full scale decking boards during one summer season
2009 - IRG/WP 09-50260
The leaching of copper has been tested in laboratory and in outside exposure for freshly treated pine sapwood samples with three different copper preservatives, Cu HDO, copper quat and copper triazoles. We found in the laboratory leaching test that a fixation with warming to 60 °C (140 °F) for 48 hours without drying and then drying in the laboratory in room temperature gave the lowest leaching of copper. We also found that surface treatments with wood oils reduced the leaching, and that washing of the surface before testing had no effect. Full scale decking board samples (0.25 m2) were then exposed outdoors for rain. The rain water was collected and analysed for copper. After one summer season (about 600 mm rain) we found that the leaching differ for the three preservatives. All samples with a water borne surface treatment had the lowest leaching, about half the amount of untreated.
F G Evans


Barefoot-heat-impact of oil-heat-treated wood: An important thermal property of decking boards
2009 - IRG/WP 09-40458
In this study the phenomenon of sensual heat impression was examined, when walking with bare feet on sun exposed wood based decking boards. A suitable method for measuring the heat flux from decking boards into an artificial foot was developed. The method and measuring device is described as well as results from measuring three different decking board materials: Oil-heat-treated spruce (OHT), untr...
A O Rapp, C R Welzbacher, C Brischke


Effect of 4 Preservatives on Physical, Mechanical and Mold-Resistant Properties of Bamboo Oriented Strand Boards
2010 - IRG/WP 10-40483
This study investigated the effects of 4 preservative systems on physical, mechanical and mold-resistant properties of bamboo oriented strand board (OSB) panels bonded with urea formaldehyde resin. Preservative A (Zinc Borate), B (IPBC), C (AAC+Borate) and D (carbendazim + prochloraz) were incorporated with strands during blending at three loading levels. The results showed that the mechanical and...
Juwan Jin, Daochun Qin, Wanshu Wei, Kuan Fan


Copper distribution in soil leached from full scale decking boards during one year
2010 - IRG/WP 10-50265
The distribution of copper in the soil under exposed decking boards after one year has been analysed. The decking boards were impregnated with copper HDO, copper quat and copper triazoles. The decking boards were pine sapwood and pressure treated in a full cell process, fixed by heating and then dried. The samples were not surface treated. Each decking sample of five boards (0.25 m2) was placed on...
F G Evans


Correlation of %Acetyl and Fiber Saturation in Acetylated Southern Pine Boards
2012 - IRG/WP 12-40598
Wood acetylation represents a chemical modification that increases the hydrophobicity of wood. The level of acetylation in the wood structure determines the extent of hydrophocity with higher levels providing reduced moisture affinity. Due to the reduced hygroscopic nature of acetylated wood, performance features such as dimensional stability, resistance to termites, and resistance to rot and de...
J Dickerson, E Cwirko, J Allen


Study of weathering Characteristics in Profiled and Treated Deck Boards
2014 - IRG/WP 14-40680
Wood exposed outdoors to repeated wetting and drying develops surface checks. Excessive checking of wooden deck boards has been a major source of dissatisfaction to consumers. In this study, Southern pine (Pinus sp.) deck boards were machined to flat (control) and ribbed surface profiles. The specimens were treated with aqueous formulations of 4,5-dichloro-2-N-octyl-4-isothiazolin-3-one (EL2) and ...
M Akhtari, D Nicholas, L Sites


Biological durability of natural fibre reinforced composites
2014 - IRG/WP 14-40681
Composite materials reinforced with wood or non-wood natural fibres have the potential to be a lighter and lower-cost alternative construction material. Until better availability and properties and a lower cost price of degradable polymers makes their use more prevalent, the application of natural fibre reinforcements in synthetic polymers is an intermediate step towards products that are complete...
N Defoirdt, I De Windt, J Van den Bulcke, J Van Acker


The resistance of composite boards protected with azole and inorganic nanoparticles to basidiomycetes and moulds
2015 - IRG/WP 15-40688
This paper presents a study on the resistance of wood composite boards, glued with silicone adhesive and obtained from chips of Scots pine Pinus silvestris L. and willow Salix viminalis L., to basidiomycetes and mould. The boards were protected in the production processes with fungicides based on metal nanoparticles, as well as on derivatives of 1,2,4-triazole, benzimidazole, and thiazole. The bio...
J Zabielska-Matejuk, I Frąckowiak, A Stangierska


Moisture behaviour and biological durability of high performance flax fibre reinforced composites
2017 - IRG/WP 17-40803
For natural fibre composites in structural and load bearing applications long reinforcing fibres are required. Therefore, much research is performed on flax fibre reinforced composites to optimize them for high performance use. In most cases such research focuses on the mechanical properties, yet the assessment of moisture behaviour, dimensional stability and biological durability is an important ...
N Defoirdt, J Van den Bulcke, F Bensadoun, J Ivens, I Verpoest, J Van Acker


Markers of quality in self-bonded beech boards
2017 - IRG/WP 17-40820
A self-bonding phenomenon takes place when five layers of beech (Fagus Sylvatica L.) veneers are pressed at temperatures higher than 200ºC. If the pressing temperature between veneer surfaces reaches at least 225ºC during pressing and if the pressure applied is optimal, water-resistant bonds are formed between veneers. This study investigates the relation of thickness reduction (marker of compre...
C Cristescu, D Sandberg, O Karlsson


Potential of totora and derivatives as sustainable lignocellulosic material
2019 - IRG/WP 19-40859
Totora (Schoenoplectus californicus C.A. Mey. Soják) is a macrophyte from the Cyperaceae family that grows in the Americas from California to Chile. This plant has long been used by several cultures such as the Ohlone in California, the Moche in Peru, or the Incas in Los Andes. Some communities have maintained its traditional use until the present, such as the communities living nearby Lake San P...
J F Hidalgo-Cordero, D Casado, J García, L Robertson, M T Troya


Long-term field exposure of wood-plastic composites processed on a commercial-size extruder
2020 - IRG/WP 20-40894
Wood-plastic composites (WPC) contain wood fiber (or flour), thermoplastics and additives and are exposed to UV light, moisture, and biological deterioration in outdoor installations. Accelerated laboratory tests can help to predict the durability of WPCs, but long term evaluations are needed to validate these results. Field exposed above-ground WPC deck boards (30.5 x 139.7 x 609.6 mm) and in-gro...
R E Ibach, C M Clemmons, N M Stark