Your search resulted in 3325 documents. Displaying 25 entries per page.
Laboratory determination of the natural decay resistance of some lesser-utilized timbers from Tanzania against wood decay fungi
2004 - IRG/WP 04-10517
Four lesser known/utilized timber species (sap and heartwoods) from Tanzania, namely Albizia lebbeck, Zanthoxylum gilletii, Faurea saligna and Parinari curatellifolia were exposed to the brown rot fungi (Gloeophyllum trabeum and Coniophora puteana) and the white rot fungus (Coriolus versicolor) to determine their natural decay resistance according to the EN 113 standard procedure. The timbers were...
P R Gillah, R C Ishengoma, E Julias, S A Amartey, D H Kitojo
Comparisons of differences in electrical conductivity and corrosivity between CCA-oxide and CCA-salt treated wood
1981 - IRG/WP 3178
CCA preservatives have served well in many applications throughout the world. In developed areas it is the preservative in demand for clean dry paintable surfaces with long durability. In developing areas it is widely used for economic and logistical reasons. With the current emphasis on energy resources, the CCA preservatives are gaining greater acceptance as a substitute for hydrocarbon-related ...
J A Taylor
Blue stain resistance of exterior wood coatings as a function of their typology
1998 - IRG/WP 98-20145
Paints and wood stains were evaluated on their blue stain resistance using both EN 152 method and the reverse method. The typology of these exterior coatings was varied including standard and high solid solvent-borne coatings as well as different types of waterborne coatings. For the water-borne acrylic, alkyd based and hybrid coatings both applied as opaque primer paints and as decorative wood st...
J Van Acker, M Stevens, C Brauwers, V Rijckaert, E Mol
The chemical analysis and biological evaluation of wood extractives as potential timber preservatives
1995 - IRG/WP 95-30090
Work involved the biological performance of water and organic solvent soluble extractives of four naturally durable wood species, namely; Matumi, Tamboti, Sneezewood and the Turpentine tree. These timber species are known to be naturally durable against termites and fungi (±25 to 35 years). The extractives were evaluated against termites and fungi using impregnated pine pencil stakes in field tes...
P Turner, D Conradie
Vapour boron treatment of wood based panels: Mechanism for effect upon impact resistance
1994 - IRG/WP 94-40036
Samples of medium density fibreboard, chipboard and oriented strandboard (OSB) were treated to two retentions of boric acid by a vapour phase treatment. The results of a range of mechanical tests were reported by Hashim et al. (1992, 1993) in which a small reduction in impact resistance was observed. Several investigations were carried out to study how and where this loss in impact resistance occu...
R Hashim, R J Murphy, D J Dickinson, J Dinwoodie
Evaluation of the fire retardant efficacy and leach resistance of an amino resin fire retardant - Preliminary report
1983 - IRG/WP 3260
The Early Fire Hazard Indices of untreated Pinus radiata were determined by testing to Australian Standard 1530, Part 3 - 1976. Differences in the performance of heartwood and sapwood were noted, with heartwood samples giving higher Ignitability, Heat Evolved and Spread of Flame indices. The treatability of Pinus radiata with Pyrogard H was assessed, and backsawn sapwood treated more effectively t...
W D Gardner, P N Alexiou, P Lind, D Butler
Natural durability of Iranian saxual wood (Haloxylon persicum) against the fungal decay
1991 - IRG/WP 1515
Haloxylon persicum is vidly planted in the deserfic region of Iran. At the present time, in the age of 30, these small trees are ready for cutting for the different uses, specially for rural buildings. But there's any knowledge about its durability. In this study the laboratory tests were carried out in accordance to European Standard. 5 fungi were used as: Trametes versicolor, Coniophora...
D Parsapajouh, F H Schweingruber, K Richter
Leachability And Decay Resistance of Copper-Treated Wood
2004 - IRG/WP 04-30337
Samples of scots pine sapwood (Pinus sylvestris L.) were treated with solutions of (Copper II sulfat-5 hydro + fluoroboric acid) and (Copper II sulfat-5 hydro + fluoroboric acid + boric acid) in order to determining to leachability and decay resistance against brown rot fungus (Postia placenta) and white rot fungus (Coriolus versicolor).
Results indicated that the copper in treated wood is less s...
A Temiz, T Nilsson, I Deemirtas, Ü C Yildiz
Decrease of the antidecay resistance of beech wood treated with organotin fungicides after its natural ageing
1998 - IRG/WP 98-30185
The antidecay resistance of beech-wood samples (120 x 8.5 x 8.5 (MM)) treated with tributyltin fungicides gradually decreased due to prolongation of their natural ageing:
tributyltin fungicides (TBTO, TBTS, TBTCA, TBT-DEDTK were applied by pressure impregnation technique in ethanole solutions (c = 0. 1%, 0.33% or 1%);
treated beech-wood samples were naturally aged without their contact with grou...
L Reinprecht
Resistance of Teak, Balau, keruing and Chengal Wood species against marine borers attack
2004 - IRG/WP 04-10513
Wood samples of Teak (Tectona grandis) , Keruing (Dipterocarpus alatus),Yellow Balau (Shorea laevis) and Chengal (Balanocarpus heimii) were treated by Creosote, using Ruping method. The dimension of samples were 200 x 75 x 20 mm and the retention were 188, 186, 331, 40 kg /m3 respectively. Both treated and untreated samples were installed in sea water (Mahshar in Persian gulf and Bandar Torkman an...
A Rezanejad
Durability of surface preserved wood particle boards submitted to atmospherical influence
1995 - IRG/WP 95-40039
The worldwide problem of the continuously growing deficit of high quality natural wood material has caused the attempts of many research workers to find effective composites such as wood particle boards (WPBs) for replacing the massive wood for constructive purposes, depending on where the boards are exploited - in the open or under a shed, they are submitted to various climatic factors such as he...
L Valcheva
Resistance of painted wood to mould fungi. Part 2. The effect of wood substrate and acrylate paint systems on mould growth
1997 - IRG/WP 97-10234
Resistance of acrylate paint systems on different types of pine and spruce sapwood to mould fungi was studied. Dipping into the preservative prior to painting, a primer with and without a fungicide (propiconazole + IPBC 0.50 + 0.2%) and a topcoat with and without a fungicide (propiconazole + IPBC 0.25 + 0.12%) were combinations of the treatments studied. The efficacy of the treatment systems varie...
H Viitanen, P Ahola
Practical consequences of the clarification of the chemical mechanism of CCA fixation to wood
1983 - IRG/WP 3220
Practical consequences derived from the chemical investigation of the mechanism of fixation of CCA to the wood constituents are discussed. Among these, formulas for the calculation of the time of hexavalent chrome fixation are presented. Furthermore, three parameters are shown to be important to the long-term effectiveness of CCA-treated timber: (i) the temperature of treatment, (ii) the initial p...
A Pizzi
International comparison of three field methods for assessing the in-ground termite resistance of materials - highlights after two years
1999 - IRG/WP 99-20157
First-year results of a comparative study, evaluating the in-ground termite resistance of a range of materials, including CCA and ACQ-treated timbers, using the below-ground exposure, ground contact and graveyard methods against diverse termite faunas were provided in IRG/WP/98-20132. Further annual inspections have confirmed early trends and identified notable differences between sites and method...
M Lenz, J W Creffield, A F Preston, B M Kard, C Vongkaluang, Y Sornnuwat
Evaluating the natural durability of native and tropical wood species against Reticulitermes flavip
2004 - IRG/WP 04-10539
Environmental pressures to eliminate arsenate from wood preservatives has resulted in voluntary removal of CCA for residential applications in the United States. A new generation of copper organic preservatives has been formulated to replace CCA for decking and in-ground applications but there is no guarantee that these preservatives represent a permanent solution to all related problems. There...
R A Arango, F Green III, K Hintz, R B Miller
Improvement of some technological and biological properties of poplar wood by impregnation with aqueous macromolecular compounds
1992 - IRG/WP 92-3721
Poplars (Populus spp) belong to the most important tree species in afforestation programs of the Netherlands. Due to their rapid growth, the wood quality is usually low. Therefore, studies were performed to elucidate whether some technological properties and the resistance against fungal attack could be improved by impregnation with water-soluble resins. The results showed that swelling and shrink...
R D Peek, H Militz, J J Kettenis
Improvement of wood decay resistance by tannin impregnation
1991 - IRG/WP 2380
The fungical effect of tannins is appraised after exposure of treated woods samples to wood rotting fungi. A screening-test is carried out with several solutions containing extracts of two kinds of tannins; a condensed tannin derived from Quebracho heartwood (Schinopsis sp.) and a hydrolyzable one extracted from chestnut heartwood (Castanea sativa Mill). If a fungicidal action was indeed found it ...
D Dirol, A Scalbert
Decrease in the mechanical resistance of blue stained and "orange stained" Pinus radiata wood
1999 - IRG/WP 99-10313
It is recognised that sapwood attacked by Ceratocystis pilifera increases its permeability to pressure preservative treatments. Since hiphae not only utilise pits, but also the cell wall for crossing from one cell to another, the mechanical resistance of the stained wood might be affected. The orange colour very commonly present in Pinus radiata logs heartwood under water sprinklers, has not recei...
M C Rose, L Reyes, J Alvarez, A Andaur, C Beltran, D Rivera
Properties of hot oil treated wood and the possible chemical reactions between wood and soybean oil during heat treatment
2005 - IRG/WP 05-40304
Thermal treatment with hot oil as the heating media based on the original idea from oil-heat treatment in Germany was investigated. The treatment was mainly carried out at 200ºC and 220ºC for 2 hours and 4 hours, and the wood species were mainly spruce and fir. This paper focuses on the difference between soybean oil and palm oil and the possible chemical reactions between wood and soybean oil. ...
Jieying Wang, P A Cooper
Biological resistance of aldehyde-treated wood
1994 - IRG/WP 94-40018
Biological resistance of wood treated with aldehyde cross-linking agents such as glyoxal, glutaraldehyde and dimethylol dihydroxy ethyleneurea (DMDHEU) were investigated. Sapwood blocks of Japanese cedar and Japanese beech, measuring 20 x 20 x 10 mm³ (T x R x L), were vacuum-impregnated at room temperature with 5-25% of aldehyde solutions. Blocks were kept in the solution for 1 week to gain the o...
S Yusuf, Y Imamura, M Takahashi, K Minato
Effect of Scytalidium lignicola on decay resistance and strength of wood
1994 - IRG/WP 94-10061
We reported previously that in laboratory tests, pretreatment of Douglas-fir and Southern Pine blocks with Scytalidium lignicola prevented decay. In the present work, we determined 1) the ability of Scytalidium lignicola to colonize and survive in wood exposed in the field, 2) the decay resistance of blocks removed from previously treated Scytalidium lignicola wood and 3) the effect of Scytalidium...
T L Highley
Preliminary results of the treatment of wood with chlorosilanes
1981 - IRG/WP 3172
It is clear from the initial data reported here that the treatment of pine sapwood with chlorosilanes under the reaction conditions employed did not significantly reduce the decay by both white rot and brown rot fungi. Only the dichlorosilane compounds showed to possess some protective action against fungal attack. Before drawing conclusions on the application of organosilicon compounds as potenti...
M Stevens
Termite resistance of Malaysian and exotic woods with plantation potential: Laboratory evaluation
1998 - IRG/WP 98-10280
The resistance of selected Malaysian woods to attack by the representative aggressive subterranean termite Coptotermes formosanus Shiraki (Isoptera: Rhinotermitidae) was evaluated in four-week, no-choice laboratory tests. This is part of an ongoing effort between the Forest Research Institute Malaysia and the University of Hawaii to document the termite resistance of Malaysian timber species of po...
J K Grace, A A H Wong, C H M Tome
Decay resistance of Siberian larch wood against brown rot fungi - Part 2. The effect of genetic variation
1998 - IRG/WP 98-10287
Wood natural decay resistance is mainly restricted in the heartwood part of tree and based on wood microstructure and chemical composition. However, the variation of decay resistant in different wood species is vide and the effect of genotype on decay resistance of Siberian larch wood grown in Finland is not known. The aim of this work was to find out the variation on decay resistance of Siberian ...
H Viitanen, L Paajanen, T Nikkanen, P Velling
Leaching characteristics, decay and termite resistance of treated wood with boron compounds, N'-N-(1,8-Naphthalyl) hydroxylamine (NHA-Na), and hydroxynaphthalimide (NHA-H)
2003 - IRG/WP 03-30307
Despite many advantages of boron wood preservatives, boron itself does not adequately protect wood in ground contact and exterior applications because its natural diffusibility and susceptibility to leaching. As a result of previous studies to limit or decrease boron leaching, several fixation systems have been developed. In this study, we evaluated the effects of N'-N-(1, 8-Naphthalyl) h...
S N Kartal, Y Imamura