IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 133 documents. Displaying 25 entries per page.


Ultrastructure of degraded, CCA-treated Pinus radiata wood from a marine pile
1990 - IRG/WP 1461
During an inspection of marine piles, 12 years after installation, severe degradation was noted on one of them in the vicinity of a corroded eye-bolt. The wood was dark brown in colour and tended to crumble easily. Wood fragments were examined by light microscopy and scanning and transmission electron microscopy and were also analysed for carbohydrates and lignin. Light microscopy showed numerous ...
A P Singh, M E Hedley


Effect of treatment process on performance of copper-chrome-arsenate. Part 2: Field stake tests
1995 - IRG/WP 95-40046
Pinus radiata sapwood stakes 20 x 20 x 400 mm³ were treated with CCA Type C using a range of concentrations and three treatment processes; Bethell, Lowry and Rueping. Preservative retention was determined by chemical analysis of treated material. Following fixation stakes were installed in a randomised plot in the Whaka graveyard located on the FRI campus. Stakes were inspected at yearly interval...
M E Hedley, J Anderson, J B Foster, B E Patterson


Degradation of the gelatinous-layer in aspen and rubber wood by the blue stain fungus Lasiodiplodia theobromae
1996 - IRG/WP 96-10168
Studies on the degradative ability of the blue stain fungus Lasiodiplodia theobromae Pat. have shown several strains to cause significant weight losses (i.e. ca 20%) in the temperate and tropical wood species, aspen (Populus tremula) and rubber wood (Hevea brasiliensis). In addition to the consumption of soluble carbohydrates and extractives, major changes in the ultrastructure of fibre cell walls...
O Encinas, G F Daniel


EELS (Electron Energy Loss Spectroscopy) - a technique for quantification of nitrogen and other light elements in the cell wall
1999 - IRG/WP 99-20163
A literature survey was performed to find progress in techniques for monitoring penetration of synthetic resins in wood cell walls. Electron energy loss spectroscopy (EELS) in combination with transmission electron microscopy (TEM) was successfully applied for the high resolution examination of the distribution of a partly methylated hydroxymethyl melamine resin in Norway spruce (Picea abies Karst...
A O Rapp, H Bestgen, W Adam, R-D Peek


Microwave conditioning of Pinus radiata D. Don for preservative treatment
2000 - IRG/WP 00-40182
This paper reviews the effect of pressure steam conditioning on the permeability and treatability of green radiata pine heartwood and the potential for substituting microwave conditioning for steaming. The penetration of liquids into radiata pine occurs mainly in the radial tissue. The permeability of green radiata pine improves following steam conditioning by blowing out the soft radial tissue. T...
P Vinden, G Torgovnikov, J Romero


An in-ground natural durability field test of Australian timbers and exotic reference species. Part 5: Extensive data from a site where both decay and termites are active. Results from a full-replicated set of heartwood specimens from each of ten myrtaceous hardwoods after 18, 19 and 20 years' exposure - A discussion paper
1988 - IRG/WP 2324
Extensive data are presented on the decay situation, the termite situation and the decay-termite associations; all gathered from a fully-replicated set of heartwood specimens of 10 hardwood timbers after 18, 19 and 20 years' exposure in the ground at a single test site, i.e. a semi-arid steppe site. Sixteen tables are presented in addition to the one table providing the rating data; the l...
J D Thornton, G C Johnson, J W Creffield


UV-microspectrophotometry of lignin and accessory compounds in wood cell walls of conifers
1999 - IRG/WP 99-20171
The distribution of lignin in the cell wall of conifer tracheids was determined by UV-VIS microspectro-photometer. Wood sections of one micron thickness were measured between the wavelength 240 and 700 nm. Spectral analyses revealed that the conifer lignin associated with the tracheid secondary wall and middle lamella is composed of guiacylpropane units which exhibit a characteristic UV absorption...
G Kleist, G Koch, J Bauch


Evidence for wood cell wall degradation by the blue stain fungus Botryodiplodia theobromae Pat
1994 - IRG/WP 94-10077
Botryodiplodia theobromae Pat., a world wide ubiquitous polyfagus sapstain fungus, was found able to destroy the cell walls of birch fibres (Betula verrucosa Ehrh.) but not Caribbean (Pinus caribaea var. hondurensis Barr. and Golf.) and Scots pine (Pinus sylvestris L.) tracheids. The fungus caused characteristic erosion of fibre cell walls similar to soft rot type 2; destruction of the S1 - S2 int...
O Encinas, G F Daniel


Service life of pressure treated deckings of spruce in direct contact with the ground
1988 - IRG/WP 3463
For decking outdoors in Sweden, pressure treated Scots pine (Pinus sylvestris L.) is used, on account of its treatability. The feasibility of using instead the refractory Norway spruce (Picea abies Karst.) is tested in a field trial. The spruce decks were treated together with pine decks with an ordinary Bethell process. As yet, after more than four years of exposure, neither in the battens nor in...
J B Boutelje, T Sebring


Étude in vitro de la colonisation et de la dégradation structurale du bois d'aubier de Pin sylvestre par la Mérule: Serpula lacrymans Schum. ex Fr. S. F. Gray
1979 - IRG/WP 198
The degradation of Scots pine sapwood cell walls by Serpula lacrymans, a brown rot fungus, is observed after various periods of exposure from two weeks to twelve weeks. The observation by microscopy shows that the hyphae of Serpula rapidly invade the wood tissues as cell wall degradation starts. That deterioration is not gradual, it is observed to be very irregular as well within the whole of the ...
D Dirol


Formation of soft rot cavities in relation to concentric layers in wood fibre walls
1983 - IRG/WP 1185
A large number of timber species attacked by soft rot have been examined using light microscopy. The S2 layers in a large number of the timbers exhibited special structural features in the form of thin concentric layers. Several observations indicate that these layers may be characterised as "weak" zones by being more easily degradable than the surrounding wall layers. The chemical structure of th...
T Nilsson, G F Daniel


The multi-phase pressure (MPP) process. One stage CCA treatment and accelerated fixation process - Concepts proved by repetitive pilot plant treatments
1997 - IRG/WP 97-40079
Twenty-four charges of radiate pine roundwood or sawn timber were treated using the MPP Process and hot CCA solution. Treated timber met the CCA retention and penetration requirements of the NZ Timber Preservation Council for Hazard Classes H3 to H5. The objectives of the trials were: (1) To "stress" CCA solution by repetitive heating, treating and cooling to determine its stability in the process...
A J Pendlebury, J A Drysdale, K Nasheri, H Pearson, M E Hedley


Internal pressure monitoring during the treatment of Pinus radiata (D. Don)
1995 - IRG/WP 95-40049
The use of micro-transducers to monitor the internal pressure of wood during treatment is investigated. The rates of pressure transfer in radiata pine sapwood and heartwood are compared during Bethell treatment with copper chrome and arsenic preservative. The effect of pre-conditioning treatments are also evaluated using micro-transducer monitoring. It is anticipated that knowledge of the changes ...
P R S Cobham, P Vinden


Molecular analysis of the basidiomycete Coniophora puteana
1992 - IRG/WP 92-1534
Sodium dodecylsulphate polyacrylamide gel electrophoresis and Western Blotting, using a polyclonal antiserum produced against a whole cell extract of Coniophora puteana, were used to analyse the major proteins and antigens of the wet rot organism Coniophora puteana. The macromolecule profiles of this organism were different from other members of the Coniophora genus and from a set of unrelated org...
H E McDowell, D Button, J W Palfreyman


Changes in pore structure and cell wall volume in wood decayed by brown- and white-rot fungi
1991 - IRG/WP 1501
Sweetgum (Liquidambar styraciflua L.) wood blocks were decayed by Postia (=Poria) placenta or Phanerochaete chrysosporium in soil-block cultures. Decay was terminated at various weight losses, and the pore volumes available to probes of various molecular weight and diameter were determined by the solute exclusion technique (Stone, J.E. and A.M. Scallan. 1968. Cellulose Chem. Technol. 2, 343-358.)....
D S Flournoy


Soft rot decay of Belian (Eusideroxylon zwageri) wood
1995 - IRG/WP 95-10119
The heartwood of Belian (Eusideroxylon zwageri), an East Malaysian timber species, is naturally durable due to its certain unique anatomical features and high content of extractives. The timber can tolerate years of exposure to hazardous conditions in ground contact and other situations without any significant loss in its strength. A few Belian transmission poles sampled from one locality in Saraw...
A H H Wong, A P Singh


Microbial decay of an archaeological wood
1994 - IRG/WP 94-10053
A light and transmission electron microscopic investigation of an archaeological wood was undertaken to determine the cause of its deterioration. The wood came from a bulwark constructed in early 1100 in the lake Tingstäde Träsk on the island Gotland in Sweden. The samples of the wood, which was identified as Pinus sylvestris, were taken from a depth of 0.85 m below the bottom level. The wood wa...
A P Singh, T Nilsson, G F Daniel


The full guideline for the “double layer test method” - A field test method for determining the durability of wood out of ground
2004 - IRG/WP 04-20290
This guideline describes a test method for wood to be exposed to the weather out of ground contact. The main objective of the method is to evaluate the durability of wood in above ground exposure as shifted overlaid stakes, which form the so called double layer. The method is applicable to the testing of untreated, treated and modified wood. Initially it was developed and found to be most useful ...
A O Rapp, U Augusta


Effect of microfibril orientation of bamboo cell wall on soft rot penetration hyphae
1994 - IRG/WP 94-10087
The effect of microfibrillar orientation of bamboo (Phyllostachys virideglaucescence) cell wall on the development of soft rot (Chaetomium globosum) penetration hyphae was investigated. It was found that the soft rot penetration hyphae normally followed the microfibril angle of the cell wall. Bamboo cell walls have alternating broad and narrow lamellae with different microfibrillar angles. The mic...
O Sulaiman, R J Murphy


Degradation features of waterlogged archaeological compression wood
1998 - IRG/WP 98-10258
The degradation characteristics of waterlogged archaeological compression wood excavated in South Korea were examined by transmission electron microscopy (TEM) and confocal laser scanning microscopy (CLSM). Degradation of Pinus compression wood occurred mainly in the inner part of S2 layer. In contrast, the outer part of S2 layer remained relatively intact. CLSM and TEM showed the erosion type of ...
Yoon Soo Kim, A P Singh


Soft rot
1978 - IRG/WP 179
Soft rot decay of treated wood is examined with special reference to hardwoods treated with CCA. Factors which adversely affect the chances of protection of hardwoods against soft rot are discussed. The ratio of the volume of the fibre cell wall to the volume of the fibre lumen is presented as a major factor influencing final preservative concentration in the fibre cell wall, the major strength co...
C R Levy


Diffuse cavity formation in soft rot of pine
1992 - IRG/WP 92-1541
A new type of soft rot of southern pine longitudinal tracheids is described. In this type, soft rot cavities form by diffuse degradation of the S2 cell wall layer by hyphae growing within the cell wall. Erosion is diffuse and irregular as opposed to the restricted, periodic erosion typical of type 1 soft rot cavity formation. Proboscis hyphae remain small (diameter 0.6 to 0.8 µm) and rapidly auto...
S E Anagnost, J J Worrall, C J K Wang


Studies of the ray parenchyma cell ends on the radial flow of Sitka spruce (Picea sitchensis)
2000 - IRG/WP 00-40164
It is widely accepted that either ray tracheids or ray parenchyma cells offer the major flow pathways radially for the impregnation of softwood with preservative chemicals. It is now generally recognised that, if radial flow does occur through ray parenchyma cells, the cross-field pits play a dominating role for the liquid movement in the radial direction. In this case, the radial flow of fluid is...
I Usta


Treatment application method and CCA efficacy in Corsican pine - Assessment by serial exposure and soil burial tests
1993 - IRG/WP 93-40006
A previous report on this research (Newman and Murphy, 1992) identified possible variation in the efficacy of a CCA preservative applied to Corsican pine (Pinus nigra var. maritima) dependant upon the treatment application method (Bethel, Lowry or Steam/Bethel). This paper presents further data from biological testing of CCA treated Corsican pine using serial exposure and unsterile soil techniques...
P R Newman, R J Murphy


Immuno-electron microscopic localization of extracellular metabolites in spruce wood decayed by brown-rot fungus Postia placenta
1990 - IRG/WP 1441
Degradation by Postia placenta in spruce and birch wood was shown to occur not only in the wood cell wall but also in the middle lamellae region. Middle lamellae was often found to be degraded along the centerline so that cells could separate along this line. Extracellular membrane structures were found surrounding the hyphae and this matrix labelled positively with antisera produced to Postia pla...
Y S Kim, B Goodell, J Jellison


Previous Page | Next Page