IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 124 documents. Displaying 25 entries per page.


Laboratory tests on the natural durability of timber methods and problems
1984 - IRG/WP 2217
In literature a large variety of test methods is mentioned to examine the natural resistance of timber against fungal attack. This concerns the kind of sampling as well as the test procedure, the test fungi, the duration of test, and the classification of the resistance according to the test results. These variations, however, are of great influence on the test result. Long term exposure will lead...
H Willeitner


Influence of different resin treatments on the dimension stability of wood
1997 - IRG/WP 97-40090
The dimension stability of wood is considered to be an important contribution to its durability and its performance in practice. A number of different treatments have been developed to improve the dimension stability of wood. One applied method is the treatment of wood with monomers or resins. The application of appropriate impregnation conditions seemed to be essential to enhance the efficiency o...
M Sailer, A O Rapp


Extracellular substance from the white rot basidiomycete Irpex lacteus involved in wood degradation
1992 - IRG/WP 92-1571
Cellulases, phenol oxidase, and a substance that both produced and reduced H2O2 were isolated from cultures containing wood or glucose on which the white-rot fungus Irpex lacteus was growing. The rate of wood degradation by the fungus with different amounts of glucose in the medium was measured. More of the substance that produced and reduced H2O2 was found extracellularly in cultures containing w...
H Tanaka, T Hirano, G Fuse, A Enoki


Cytoplasmic and extracellular localization of manganese II dependent peroxidase(s) in white rot fungi during degradation of woody materials
1989 - IRG/WP 1416
The manner by which lignin is degraded in-situ in natural substrates by white rot fungi still remains a controversial issue particularly the distribution and role(s) played by lignin degrading enzymes (i.e. manganese II peroxidase and lignin peroxidase). In the present study, use was made of anti-manganese II peroxidase and immunolabelling techniques in conjunction with transmission electron micro...
G F Daniel, B Pettersson, T Nilsson, J Volc


Window test. Direct testing of wood resistance to decay: A study of its fitness, its reliability and its accelerating factor
1984 - IRG/WP 2219
This is the results of an experiment using the window-test specimens, exposing the specimens to three different types of testing procedure: 1. Natural infestation in the open air; 2. Artificial infestation and exposure in the open air; 3. Artificial infestation in a green-house. The results show good similiraties of the three parallel tests in term of decay, and assess the reliability of the windo...
G R Y Déon, L N Trong


Wood decay of Pinus sylvestris L. and Fagus sylvatica L. by marine fungi. Part 2
1991 - IRG/WP 1471
The water-logged wood conservation requires a good knowledge of the wood decay organims which produce the degradation. Previous conducted studies (ESCORIAL, TROYA, GARCIA DE LOS RIOS, 1990) have shown that the incubation times normally used for in vitro laboratory tests are not sufficients for a significant wood degradation. This has been the reason why the aim of this work was the study of such d...
M T De Troya, A M Navarrete, M C Escorial


The use of natural and synthetical tannins to improve the dimensional stability and durability of beechwood (Fagus sylvatica)
1993 - IRG/WP 93-30016
Synthetical tannins and natural extractives of oak, spruce and chestnut have been combined with different fungicides to make the wood more dimensionally stable and more durable. The anti-shrink-efficiency and the improvement of the durability of different synthetical and natural tannins have been evaluated. The results make clear, that an application of the mentioned agents for common use cannot b...
H Militz, W J Homan


Investigation of extracellular mucilaginous material in some wood decay fungi
1996 - IRG/WP 96-10188
The external morphology of the extracellular mucilagenous material (ECM) produced by Coriolus versicolor and Coniophora puteana during colonization of Scots pine and beech was studies using SEM. Specimens were examined in the frozen hydrated, freeze-dried and critical point dried state. All technics produced artefacts but the ECM was best preserved when examined the frozen hydated state. Critical ...
A R Abu, D J Dickinson, R J Murphy


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 5: Interim report
1980 - IRG/WP 454
Wood samples (15 x 2 x 2 cm³) were treated with one copper/chrome/arsenic (CCA) and one copper/chrome/boron (CCB) preservative using the following concentrations - O, 3, 6, 10%. Treated samples of three reference wood species - Alstonia scholaris, Fagus sylvatica, Pinus sylvestris were supplied to all participants. Additional local species were chosen by participants and included in the test at t...
R A Eaton


Design of a laboratory method for evaluating the effectiveness of soft rot preservatives
1988 - IRG/WP 2312
This purpose of this work was to design a method which makes it possible to evaluate the effectiveness of products which present protect wood against soft rot, using new products·of a different nature, on wood of·Pinus sylvestris L. and Fagus sylvatica L., and which, suitably applied, avoid big economic losses deriving from lack of knowledge of the active principles suitable to present protect w...
M T De Troya, A M Navarrete


Improvement in dimensional stability against water of the main Spanish timbers impregnated with water repellent organic protectors
1988 - IRG/WP 3468
The study reported the increase of dimensional stability against water of the main Spanish timbers, both broadleaved and coniferous, after impregnation in the autoclave with organic protector, with contains 33.3% water repellent waxes and resins. The proposed Spanish standard, U.N.E. n° 56541 is used, where dimensional stability of the impregnated wood is expressed as a% of that of the non-impreg...
J A Rodríguez Barreal


NMR T1 relaxation time as a non-destructive method for the study of decay in wood
1992 - IRG/WP 92-2406
The NMR spectroscopic technique of measuring the T1 spin-lattice relaxation times has been investigated for its potential in the detection of microbial decay in wood. The T1 NMR analyses were carried out on samples of Scots pine and European beech that had been exposed to decay and non-decay fungi representing each of the important groups colonising wood. Decay in the test material was also assess...
P W McCormack, A E G Cass, R J Murphy


Main problems of Turkish wooden boat manufacturers
1982 - IRG/WP 485
The best transportation system to the eastern Black Sea region of Turkey has been since the earliest history sea transportation. As is well known the historical 'silk road' from Europe to the Far East and China was over the Black Sea and via Trabzon. During the last five years also this same connecting route has become very important for the transportation of food and industrial ...
R Ilhan


Co-operative tests concerning influence of solvent and drying method on the toxic limit of wood preservatives against Basidiomycetes. Preliminary report
1971 - IRG/WP 204
In the Working Group II of the Organization for Economic Co-operation and Development working group on wood preservation (now International Research Group on wood preservation) it was agreed that more knowledge was necessary concerning the influence of the solvent on the toxic limit of organic solvent types of wood preservatives against Basidiomycetes. A test program was drawn up and after discuss...
T Hof


Preliminary results from the field experiment to determine the performance of preservative treated hardwoods with particular reference to soft rot. The four reference timber
1980 - IRG/WP 3164
The results given in the Tables 1-4 each refer to one of the four reference species treated with four solution concentrations of CCA as recorded from each test site. The species are: Alstonia scholaris, Betula pendula, Fagus sylvatica, Pinus sylvestris. The treatments were: Untreated, 0.66% CCA, 1.53% CCA, 3.01% CCA, 5.60% CCA. Each figure is an average of the ratings recorded for each replicate o...
J F Levy, D J Dickinson


Hardwood Field Experiment: Progress Report 1977-1986
1986 - IRG/WP 3391
The international hardwood field experiment was planned in l976 and set up in same 30 different sites around the world. The test stakes include 4 reference species common to each site and in most cases at least 2 species of local importance. It was hoped that a picture of performance of a range of economically important species would be built up and at the same time provide vital background inform...
D J Dickinson, S M Gray


Copper based water-borne preservatives: Copper adsorption in relation to performance against soft rot
1987 - IRG/WP 3452
As part of a fundamental study concerned with the performance of copper based water-borne preservatives the adsorption of copper from aqueous solutions by 4 hardwood and 1 softwood species has been studied. Experiments were conducted to determine the influence of solution pH, solution concentration and solution temperature. The results obtained were consistent with an acid form ion-exchange mechan...
P M S Rennie, S M Gray, D J Dickinson


Effect of test site location on in-ground preservative performance after 6 years
2001 - IRG/WP 01-20231
Pinus radiata test stakes were treated with 4.1 kg/m3 of CCA and Fagus sylvatica with 6.1 kg/m3 of CCA. Both wood species were also treated with a copper plus triazole preservative (3 kg/m3 of copper) and chlorothalonil plus chlorpyriphos in oil (4.8 kg/m3 chlorothalonil). Furthermore, P. radiata was treated with ammoniacal copper plus a quaternary ammonium compound (2.6 kg/m3 copper) and a 60/40 ...
R N Wakeling


The influence of carrier fluid type on the efficacy of a wood preservative against cavity forming soft rot
2000 - IRG/WP 00-30244
Propiconazole was applied to Scots pine sapwood (Pinus sylvestris) and beech (Fagus sylvatica) using three different carrier systems selected on their varying ability to swell timber. The effects of microdistribution on the activity of cavity forming soft rot fungi were examined to determine the practical benefits of using swelling and non-swelling carriers with this active ingredient. Efficacy of...
P A Hodges


Biological resistance of electrolessly plated wood (1). Preliminary report
1994 - IRG/WP 94-40024
Surface metal coating is considered to improve biological resistance of wood as some metal ions are fungitoxic. Six wood species (three softwoods: Cryptomeria japonica, Tsuga heterophylla and Larix spp; three hardwoods: Fagus crenata, Acer mono and Betula platyphylla) were electrolessly plated with nickel or copper, and those were served for laboratory evaluation of their resistance against decay ...
M Hasegawa, K Tsunoda, T Yoshimura


Information from the COIPM Wood Group
1988 - IRG/WP 4146
Abstract from the COIPM minutes: Wood in marine environment: Mrs Gambetta stated that the main item discussed by the Group was the collaborative work to test the durability of heat shrinkable polyolephin sheating materials for the protection of wood against marine organisms. The work began last year when wood samples were sent out to the participants. Three samples of Pinus sylvestris wrapped in ...
A Gambetta


Japanese standardized method for evaluating effectiveness of anti-sapstain and anti-mould chemicals
1988 - IRG/WP 2299
Japan Wood Preserving Association established a method for testing effectiveness of chemicals against sapstain and mold fungi on wood in 1979. The method is concerned with a laboratory technique using small timber specimens (20 x 50 x 3 mm³), petri dish and 5 test fungi. Effectiveness of each candidate chemical is evaluated on the basis of the relative resistance to sapstain and mold fungi which ...
K Tsunoda, K Nishimoto


Evaluation of a laboratory soft rot test on basis of weight loss and residual strength
1989 - IRG/WP 2336
Based on the principles of different previously reported experimental procedures dealing with laboratory soft rot testing, a study was conducted on treated poplar and beech. Preservatives used were CCA, CCF, AAC, Azaconazole and TCMTB. Treated samples were exposed for three months in a vermiculite substrate to Chaetomium globosum. Evaluation was based on absolute mass loss, percentage weight loss ...
W Verbeke, J Van Acker, M Stevens


Influence of the content of organic matter of soil on the degradation of wood by soft rot fungi
1970 - IRG/WP 27
The degradation of wood specimen burried in the soil by soft rot fungi is influenced by a number of factors. These are in particular the water holding capacity, water content, content of organic matter, pH, content of mineral nutritive substances etc. The results of the interlaboratory tests, carried out within the IRG/WP let presume that the intensity of wood degradation occurs proportionally inv...
O Wälchli


Degradation of woods by obligately anaerobic fungi
1990 - IRG/WP 1452
Little is known about the processes occurring during the degradation of wood by obligately anaerobic fungi. When woods from a range of hardwood species were incubated for 11 days with a strain of the Chytrid Neocallimastix frontalis many of the woods were measurably fermented; Fagus sylvatica (23%) was the most highly degraded. Microscopic examination of Populus tremuloides wood after incubation w...
K N Joblin, G E Naylor


Previous Page | Next Page