Methods to determine the efficacy of three water repellent additives in waterborne preservatives
1997 - IRG/WP 97-30142
The paper describes the methods used to determine the efficacy of three different water repellent additives in waterborne preservatives. The wooden samples used are pine (Pinus sylvestris) and spruce (Picea abies) that are treated with 9 different waterborne preservatives in retention for hazard class 3 (above ground commodities). There are two sample sizes exposed, cladding boards (19 x 148 mm) w...
F G Evans, B Nossen, K M Jenssen, L R Wilhelmsen, G Fuglum


A simple field apparatus for measuring relative gaff penetration and assessing the effect of additives for improving pole climbability
2000 - IRG/WP 00-20187
A simple apparatus for measuring and comparing the relative "hardness" of utility poles is described. This "slide-hammer" gaff penetration apparatus was designed as a field testing unit to measure the depth of gaff penetration into test poles after application of a uniform and reproducible force to the gaff. The apparatus is simple to use in both the laboratory and field. Data is provided for resu...
A R Zahora


Stability of bifenthrin in a commercial phenol-formaldehyde plywood glue
2003 - IRG/WP 03-30311
Liquid phenol formaldehyde (PF) glue mixes used for plywood manufacture are strongly alkaline. At this pH insecticidal additives may not be stable for long periods. In order to establish practical working life of the synthetic pyrethroid insecticide, bifenthrin, in liquid PF glues the concentration of bifenthrin in the glue mix was measured under laboratory conditions over a 24 hour period. Glu...
M J Kennedy, P A Collins, R D Vella


The effect of additives on copper losses from alkaline copper treated wood
2007 - IRG/WP 07-50246
The replacement of chromated copper arsenate (CCA) by alkaline copper compounds has heightened awareness of the potential impact of copper losses on aquatic organisms. While there remains a healthy debate concerning the actual risk of copper leaching from wood preservatives into aquatic ecosystems, it is clear that reducing these losses will be necessary to avoid continued regulatory actions aga...
J Mitsuhashi, J J Morrell, L Jin, A F Preston


Evaluation of Water Repellency of Treated Wood Using Several Alternative Methods
2009 - IRG/WP 09-20419
In this study, the results of water repellency testing using a digital swellometer method for water-borne organic-preservative systems with water repellent additives are reported. The findings suggest that the traditional method of using matched untreated controls as a reference developed from historic solvent-based treatments for determination anti-swelling efficacy (ASE) may underestimate the a...
L Jin, A F Preston


Effects of new fixative additives on leachability of boron wood preservatives
2009 - IRG/WP 09-30507
Borates are well known with their protective capacity against both fungi and insects with low mammalian toxicity and environmental acceptable. However, boron itself does not ensure the appropriate protection for wood in the exterior applications because of their easily depletion from the treated wood under wet conditions. In this study, the potential use of monoglyceride and polyvinyl alcohol prod...
A Mohareb, J Henry, E Wozniak, P Gérardin


Wettability and bonding strength of wood thermally-treated with different combinations of soy oil and chemical additives
2009 - IRG/WP 09-40454
Thermal treatment is a method which has gained wider acceptability as an alternative to the chemical treatment in wood preservation. In order to maximize the benefits of this technique several options have been adopted including the use of soy oil in transferring the heat to the wood. Available information on thermal treatment in general and the oil method in particular show that there are still n...
L Awoyemi, P A Cooper, T Ung


Effect of borax-boric acid Treatment of simul (Bombax ceiba) Veneers on Glue-Bond Quality of Plywood
2010 - IRG/WP 10-40525
The glue-bond quality of plywood made of treated simul (Bombax ceiba) veneers was investigated. The veneers were treated with cold and hot water solution of borax-boric acid (BB) of different concentrations and treatment durations. The plywoods were made at three different pressures in hot press using urea formaldehyde glue. The glue-bond strength of untreated plywood in dry shear-test was found t...
K Akhter, Md Abul Hashem, S Akhter


Silicon compounds as additives improving alkyd-based wood coatings performance
2010 - IRG/WP 10-40531
The reactivity of cellulose with solvent-born alkyd-based wood coatings supplemented with organosilanes was analyzed. Structural analysis of cellulose subjected to the reaction with organosilanes and following extraction with water was performed using Fourier-transform infrared spectroscopy (FTIR). The analyzed IR spectra comprise bands 1250 cm-1 typical for the SiC group and 800 cm-1 typical for ...
B Mazela, I Ratajczak, K Wichłacz-Szentner, P Hochmańska


Novel Approaches to the Development and Testing of Anti After-glow Additives for CCA-based Treatments of Poles
2011 - IRG/WP 11-30561
In this paper, a field fire stake testing screen method is described. This method uses stake samples from matched wood sources allowing replicates from different boards to be included. The method is easy to control and can provide quick comparative fire resistance test results. The parameters measured from the tests are percentage weight loss, minimum residual circumference and residual thicknes...
L Jin, P Walcheski, A Preston


Influence of selected additives on organic fungicides for control of bamboo mold fungi
2013 - IRG/WP 13-30626
In order to assess the long-term efficacy of supplemented organic fungicides in outdoor applications, additives - including the antioxidant butylated hydroxytoluene (BHT) and a UV absorber and free radical scavenger benzotriazole (BTA), were selected to mix with the fungicides propiconazole or tebuconazole. Freshly cut samples from four-year old bamboo stems were treated with combinations of the c...
Sun Fangli, B Goodell, Chen Anliang, Bao Binfu, Zhang Shaoyong


Glue-bond strength of simul (Bombax ceiba) plywood made of Neem (Azadiracta indica) leaves treated veneers
2013 - IRG/WP 13-40647
The glue-bond qualities of plywood made of treated simul (Bombax ceiba) veneers were investigated. The veneers were treated with cold and hot water solution of neem (Azadiracta indica, A. Juss.) leaves of different concentrations and treatment durations. The plywoods were made at three different pressures in hot press using urea formaldehyde glue. The glue-bond strength of untreated simul plywood ...
K Akhter, M A Hashem, S Akhter


Development of composite furniture using bamboo strips, bamboo mat and rubber wood veneer
2014 - IRG/WP 14-40679
Bamboo offers cost-effective component in panel form is well suited to wood substitute can be used as furniture components. In the present study, borak (Bambusa balcooa ) bamboo were used for manufacturing bamboo panel. Mitinga (B. tulda) bamboo were used for making mat and rubber wood veneers were used for manufacturing mat overlaid veneer board. Borax-boric acid (BB) treatments were given to enh...
K Akhter, M Mahabubur Rahaman, M H Chowdhury, M Zahirul Alam


Optimising wood chemical modification with lactic acid oligomers by screening of processing conditions and chemical additives
2016 - IRG/WP 16-40741
Oligomer systems based on lactic acid (OLA), were impregnated in wood and polymerised in-situ by heat treatment to improve the properties of the treated wood especially regarding anti-swelling efficiency (ASE), hygroscopicity, water leaching resistance and durability. This article relates the optimisation of the heat treatment conditions and the consideration of selected chemicals for improvement ...
C Grosse, M-F Thévenon, M Noël, P Gérardin


Effect of Furfurylation on Shear Strength of Bond Line and Screw Withdrawal Resistance of Beech and Fir Wood
2016 - IRG/WP 16-40757
The aim of this study was to investigate the effects of furfurylation on shear strength of bond line and screw withdrawal resistance of beech (Fagus orientalis) and fir (Abies alba) species. In this regard, specimens with two different values of furfurylation i.e. low (fir 14% and beech 20%) and high (fir 38% and beech 65%) levels were prepared and evaluated in comparison with untreated specimens....
A Talaei, H Abdolzadeh, M Saleh Zare


A summary of history and use of timber bridges in New Zealand
2017 - IRG/WP 17-40801
Wooden bridges have been an important part of road and rail networks in New Zealand. While wooden structures have largely been replaced by concrete and steel on major arteries they still have a place where lightweight, easily assembled structures are needed. These timber bridges may also be a cheaper alternative to other materials in roads which carry relatively low traffic loads. In the last ten ...
D Page, T Singh


Hibernation or spring awakening? – The research on wood durability and protection in marine environment
2018 - IRG/WP 18-10929
Wooden structures in marine applications are exposed to severe degradation conditions caused by mechanical loads and wood degrading organisms. The present paper presents the use of wood in marine environments in Europe from a wood protection perspective and gives an overview over relevant research topics. It compiles the most relevant literature with an emphasis on new wood protection methods and ...
A Treu, K Zimmer, C Brischke, E Larnøy, L R Gobakken, F Aloui, S M Cragg, P-O Flæte, M Humar, M Westin


In-line quality control of the film thickness in industrial coating processes for exterior cladding
2018 - IRG/WP 18-40835
The production of industrially coated wood cladding has been strongly increasing in Scandinavia during the last years. In the beginning of this development, industrial coating processes included solely the application of pigmented primers; these however provide only a short protection of the wood surface and the application of a top coat is required during the first 6 to 12 months after mounting t...
U Hundhausen, M Slabohm