In vitro sporulation of selected wood decay fungi
1978 - IRG/WP 190
Basidiospores produced axenically without laborious attention in the laboratory are useful in studies of wood decay initiation. Such spores presumably approach those collected from natural sporophores in size and germinability (Morton, 1964). Production of spores in vitro by inversion of cultures grown on 2% malt extract agar in deep glass dishes (100x80 mm²) has been the preferred method (Morton...
E L Schmidt, D W French


Moisture requirements and wood degradation of pine and spruce wood by some Basidiomycetes-fungi
1989 - IRG/WP 1406
The minimum moisture requirements for the growth of the brown rot fungi, Coniophora puteana, Gloeophyllum trabeum and Serpula lacrymans were near or above the fibre saturation point of pine and spruce, sap and heartwood, during 160 days incubation according to the standard method EN 113. The moisture of wood for the optimum growth of Coniophora puteana and Serpula lacrymans was about 35-80% and fo...
H Viitanen, A-C Ritschkoff


Improvement of wood decay resistance by tannin impregnation
1991 - IRG/WP 2380
The fungical effect of tannins is appraised after exposure of treated woods samples to wood rotting fungi. A screening-test is carried out with several solutions containing extracts of two kinds of tannins; a condensed tannin derived from Quebracho heartwood (Schinopsis sp.) and a hydrolyzable one extracted from chestnut heartwood (Castanea sativa Mill). If a fungicidal action was indeed found it ...
D Dirol, A Scalbert


Contradiction between uptake of preservative in practical situation and laboratory testing
1992 - IRG/WP 92-2392
By brush treatment water- and solvent-based products were applied on boards of Scots pine and Norway spruce to achieve an uptake of 100 and 200 g/ml. In addition the scope of work to achieve the required uptake of preservative was determined under practical conditions for both product groups. EN 113 (RAL-GZ 830) tests were carried out to test the biological efficacy of products. After 18 months ex...
R Gründlinger, O Janotta, M Melzer


A serial exposure technique for estimating probable service life of treated timber
1978 - IRG/WP 2111
This paper briefly describes part of our preliminary work aimed at developing a test procedure that culd be adopted as a standard method. A detailed version of the work has been submitted for formal publication. In both papers, the aim is to promote interest in extended laboratory testing of wood preservatives. It is believed that this work may provide the basis of a laboratory test procedure from...
J A Butcher


A chemical and mycological evaluation of fused borate rods and a borate/glycol solution for remedial treatment of window joinery
1983 - IRG/WP 3225
The possibility of using fused borate rods (Impel Borpatron) and a borate/glycol solution (Boracol-40) for depot impregnation of window joinery has been examined in a co-operative project between The Swedish Forest Products Research Laboratory, The Swedish University of Agricultural Sciences and Prolignum AB. The fused Impel rod is a glassy rod composed of disodium octaborate which readily dissolv...
M-L Edlund, B Henningsson, A Käärik, P-E Dickèr


Low polymer levels containing bioactive monomer polymerized in situ provide resistance to Gloeophyllum trabeum
1995 - IRG/WP 95-30066
Wood preservation based on in situ polymerization of potentially bioactive monomers has been studied. Tributyltin oxide acrylate (TBTOA) and pentachlorophenol acrylate (PCPA) were synthesized. Wood samples were treated at 2, 5, 10, 15 and 20% by weight solutions with varying amounts of crosslinker (trimethylolpropane trimethacrylate, TMPTM) and polymerized in situ in wood samples (2.54 x 2.54 x 0....
R E Ibach, R M Rowell


Effect of cyclic change of temperature on fungal growth and mass loss
1994 - IRG/WP 94-10065
For estimating the effect of cycling change of temparature on fungal growth, four Japanese species, sugi (Cryptomeria japonica), hinoki (Chamaecyparis obtusa), akamatsu (Pinus densiflora) and buna (Fagus crenata), four fungal species, Tyromyces palustris, Gloeophyllum trabeum, Coriolus versicolor, Pycnoporus coccineus, and five temperature conditions, 10, 20, 27, 35°C and cyclic temperature (20°...
K Suzuki, K Okada


Lethal temperature for some wood-destroying fungi with respect to eradication by heat treatment
1984 - IRG/WP 1229
The lethal heat dosis as a function of temperature and time of exposure has been tested for mycelium and for wood infested by three strains of Serpula lacrymans and by Coniophora puteana, Poria monticola, Paxillus panuoides, Gloeophyllum trabeum and Gloeophyllum sepiarium. Even for Serpula lacrymans, which is well known for its sensivity to heat treatment, 30 min at 55°C were necessary to kill th...
M Miric, H Willeitner


Natural resistance of Bamboo (Bambusa sp.) to marine wood-borers in Goa waters (India)
1993 - IRG/WP 93-10032
The paper deals with the natural durability of Bambusa sp. against the attack of marine wood-borers in Goa waters. Test specimens of this species were completely destroyed within a short period of nine months due to severe attack of borers indicating its very low natural resistance. Wood-borers involved were Martesia striata (Linnaeus), Nausitora hedleyi Schepman and Lyrodus pedicellatus (Quatrefa...
L N Santhakumaran, S G Sawant


Soft-rot control in hardwoods treated with chromated copper arsenate preservatives. Part 3: Influence of wood substrate and copper loadings
1977 - IRG/WP 2100
The hypothesis is proposed that hardwoods need more chromated copper arsenate (CCA) than softwoods to protect them from soft-rot attack mainly because hardwoods are more readily consumed by soft-rot fungi. Simple model systems, using copper-supplemented agar or groundwood pulp treated with CCA showed that fungi tolerated more toxicant (copper) as more available substrate (malt) was provided. Soft-...
M A Hulme, J A Butcher


Natural durability of 4 different Larix species tested in soil contact
2002 - IRG/WP 02-10434
Importers of Siberian Larch claimed to have a material which can replace pressure treated wood in soil contact. This gave reason to investigate the durability of 4 different Larix species (L. decidua, L. sibirica, L. decidua x sibirica, L. gmelini var ologenis) coming from 7 different origins in comparison with sapwood of Pinus sylvestris untreated as well as pressure impregnated with retentions o...
A O Rapp, H Viitanen, T Nilsson


Evaluation of bacteria for biological control of wood decay
1990 - IRG/WP 1426
Laboratory soil-block and agar-block tests were carried out to evaluate the efficacy of bacteria as biological control agents against 5 brown-rot and 3 white-rot fungi. Pretreatment of Southern pine and sweetgum with a bacterial solution prevented decay in agar-block tests. However, the bacteria were generally ineffective in preventing decay in Southern pine, Douglas-fir, sweetgum and yellow popla...
R Benko, T L Highley


Evaluation of chlorpyrifos and fungicides alone and in combination for control of insects and fungi in wood and wood composites
1998 - IRG/WP 98-30187
Wood composites are rapidly being adapted for use in exterior applications. The incorporation of a preservative system to prevent fungus and insect attack is necessary with most exterior composites. Research studies were reviewed pertaining to organic preservative systems based on Lentrek* insecticide wood treatment which contains the active ingredient chlorpyrifos alone and in combination with te...
M P Tolley, P E Laks, R Fears


Efficacy of anhydrides as wood protection chemicals
1997 - IRG/WP 97-30162
Wood samples treated with anhydrides of various compositions have been examined for their decay resistance and moisture behaviour. For this purpose two brown rot fungi (Coniophora puteana and Gloeophyllum trabeum) and two white rot fungi (Trametes versicolor and Pycnoporus sanguineus) were used in conventional and modified soil block tests. The modified soil block tests conformed to the method as ...
S C Forster, M D C Hale, G R Williams


Toxic value estimation of wood preservatives by using the probit analysis
1990 - IRG/WP 2348
As it was assumed from previous experiments, the probit analysis appears to be the most suitable method of all used to estimate the toxic value of wood preservatives. With the help of the classical agar-block method the probit analysis was tested for its suitability in: 1) fungitoxic value estimation of the WR-3 preservative (quaternary ammonium compound + borate), as compared to different test fu...
J Wazny, K J Krajewski


Non-destructive stress wave measurement of decay and termite attack in experimental wood units
1986 - IRG/WP 2256
The purpose of this study was to determine if stress wave analysis could be used to monitor the degradation of wood specimens exposed to the brown-rot decay fungi (Gloeophyllum trabeum) and of wood specimens subjected to attack by subterranean termites. One hundred fifty 3/4 by 3/4 by 12 in. Southern pine specimens were used for exposure to brown-rot decay fungi and two hundred twenty-five 3/4 by ...
R F Pellerin, R C De Groot, G R Esenther


Evaluating the potential of amine chemicals for use as wood protecting agents. Part 1: Investigation of cation components of quaternary ammonium compounds
1994 - IRG/WP 94-30049
Quaternary ammonium compounds (quats) have shown a great potential as more environmentally acceptable wood preservatives. In order to identify chemicals possessing the wood protecting potential, an evaluation was carried out of a range of commercially available 'quats', using a modified soil block test. Ponderosa pine sapwood blocks were treated with selected 'quat&a...
Hang Tang, J N R Ruddick


Laboratory tests on the natural durability of timber methods and problems
1984 - IRG/WP 2217
In literature a large variety of test methods is mentioned to examine the natural resistance of timber against fungal attack. This concerns the kind of sampling as well as the test procedure, the test fungi, the duration of test, and the classification of the resistance according to the test results. These variations, however, are of great influence on the test result. Long term exposure will lead...
H Willeitner


Differential susceptibility of living and dead timber to colonisation by sapstain and mould fungi
1998 - IRG/WP 98-10288
Field studies have revealed that when timber is irradiated (i.e. killed) it is more susceptible to colonisation by mould fungi than sapstain fungi. By comparison, freshly sawn timber shows very little mould colonisation, tending to be colonised by sapstain fungi. It appears, therefore that the physiological state of the wood may influence the pattern of colonisation. A laboratory trial was underta...
J R Williams, D J Dickinson, J F Webber


Targeted inhibition of wood decay (Using everything but the kitchen sink)
1997 - IRG/WP 97-10203
Low molecular weight oxidative decay agents have been implicated in the degradation of wood by brown-rot decay as evidenced by chemical analysis of brown-rotted wood and detection of oxalic acid and hydroxy radicals. Fenton chemistry (H2O2 / Fe++) is often proposed as the mechanism for generating hydroxy radicals. Previous authors have shown iron to enhance the brown-rot hydrolysis of wood, while ...
F Green III, T A Kuster, T L Highley


The biological effectiveness of wood modified with heptadecenylsuccinic anhydride against two brown rot fungi: Coniophora puteana and Gloeophyllum trabeum
1992 - IRG/WP 92-3705
A modified soil block test was carried out using wood samples reacted with heptadecenylsuccinic anhydride (ASA). This modification gave good resistance to decay brought about by the brown rot fungi Coniophora puteana and Gloeophyllum trabeum during the twelve week exposure period. Results indicated that there was a good correlation between increased loading of modifying reagent and an increase in ...
C Codd, W B Banks, J A Cornfield, G R Williams


Utilization of coconut timber from north Sulawesi, Indonesia. Part 1: Durability
1994 - IRG/WP 94-30044
Coconut timber from non-productive plantations is a byproduct of an agricultural crop and, by the same token, constitutes a renewable resource which may serve as a complement to or, at least in part, as a substitute for traditional timbers in local markets. Its more extensive utilization is expected to contribute to the conservation of tropical rain forests. Export of coconut timber and/or wood pr...
R-D Peek


Resistance to decay of particle boards: Presentation of a test method
1986 - IRG/WP 2260
The experimentations were undertaken on particle boards 35 and 50 mm thick. The rot resistance tests were carried out on specimens whose dimensions were 600 x 75 x 35 mm³ for particle boards 35 mm thick and 800 x 75 x 50 mm³ for particle boards 50 mm thick according to a method derived from the one described in the documents IRG/WP/2214 and IRG/WP/2243. Two exposure periods were used: 12 and 16 ...
G R Y Déon, N Trong


Chelator production and cellobiose dehydrogenase activity of wood inhabiting fungi
2000 - IRG/WP 00-10363
Multiple components have been postulated to be involved in the Fenton-based biological degradation of wood by brown rot fungi. Chelators have been implicated in essential iron reduction steps. Cellobiose dehydrogenase activity and quinone reducing activity have also been implicated in brown rot biodegradation. When biochelator production by three white rot fungi, three brown rot fungi and three wo...
Weihong Qi, J Jellison