Your search resulted in 805 documents. Displaying 25 entries per page.


Estimating the heat treatment intensity through various properties of thermally modified timber (TMT)
2009 - IRG/WP 09-40459
The suitability of different measures for prediction of the heat treatment intensity was investigated. Therefore, the resistance to impact milling (RIM), the lightness L*, the equilibrium moisture content (EMC), the anti swelling efficiency (ASE) and the total amount of soluble carbohydrates (TSC) of heat treated specimens were correlated with corresponding fungal resistance achieved by heat treat...
C R Welzbacher, C Brischke, A O Rapp


Direct estimation of the durability of high-pressure steam modified wood by ESR-spectroscopy
2010 - IRG/WP 10-40508
Heat generated persistent free radicals have been detected by electron spin resonance measurement of thermally modified wood, prepared by high pressure superheated steam treatment. The specific density of these radicals have been correlated with the durability against basidiomycetes, as measured by the European standard EN113 test. In the lower range of specific radical densities, the found correl...
W Willems, A Tausch, H Militz


Influence of heat treatment intensity on the structural integrity of 14 timber species
2012 - IRG/WP 12-40586
Thermally modified timber (TMT) is characterized by improved durability and dimensionally stability, but strength properties, especially the dynamic ones, are compromised at the same time. Because dynamic standard tests require high efforts and time, the high-energy multiple impact (HEMI) –test was developed for the fast and reliable characterisation of the structural integrity of TMT, showing a...
C R Welzbacher, C Brischke, G Maier


Effect of preservative treatment on mechanical performance of round and square poles made of small diameter Scots pine
2012 - IRG/WP 12-40612
A growing proportion of harvested Scots pine (Pinus sylvestris L.) timber originates from the first or second commercial thinning stands. There is a need to find economically viable and high quality wood products that can be manufactured from this raw material. Small log volume means not only demands of increased efficiency for material handling in logistics and manufacturing processes, but also c...
V Möttönen, R Stöd, K Heikkilä, H Heräjärvi


Experiences with an industrial system for controlled thermal wood modification in pressurized unsaturated steam
2014 - IRG/WP 14-40678
Thermal wood modification in pressurized reactors has a long history, but these processes are to date industrially scarcely used, because of the relatively complicated process equipment, compared to the more common high-temperature processes in kilns at atmospheric pressure. However, based on our practical experience with the FirmoLin® process, supported by recent scientific findings, it is foun...
W Willems


Treatability of beechwood railway sleepers with potential creosote substitutes
2017 - IRG/WP 17-40790
Maintenance of an efficient railway infrastructure still requires the use of wooden railway sleepers, particularly because wooden sleepers have more favourable properties for intensified vibrations than concrete or steel sleepers. Creosote, used for decades for the impregnation of railway sleepers, will possibly no longer be available for this application due to European legislation. This reveals ...
N Pfabigan, E Habla, R Gründlinger


Wood veneer with high flexible decorated with nanoparticles for highly efficient water treatment
2019 - IRG/WP 19-50347
Natural wood is mainly comprised of numerous long, partially aligned channels (lumens) as well as nanochannels. Wood with these quick and effective passages is suitable for a membrane/separation material. However, a suitable thickness range of wood along its growth direction is essential to effectively separate small molecular, and the wood membrane is too thick to clean easily. In this paper, woo...
S Chang, D Xu, G Liu, J Hu, X Li, Y Liu


Preliminary investigation for preservation method of CLT using non-pressure treatment
2021 - IRG/WP 21-40919
Cross-laminated Timber (CLT) is increasingly being used in residential and non-residential construction around the world, and some of these areas are at high risk of biodeterioration. Addition to moisture management of construction, preservative treatment of CLT may be needed to prevent decay and termite attack in the area. Pressure treatment being most reliable, is not feasible due to the large d...
T Miyauchi, Y Ohashi, J Miyazaki, R Takanashi, H Shibui, S Isaji, T Shigeyama, Y Sugai, A Yamamoto, T Hramiishi, T Mori, H Matsunaga


Utilization of Pressure Treated Lumber in Cross Laminated Timber Manufacture and its Impact on Bondline
2022 - IRG/WP 22-40953
Mass timber building construction is increasing dramatically across North America which presents challenges to these structures not seen in Northern Europe. Large parts of the United States harbor termites and existing mass timber building technologies that rely solely on moisture exclusion to increase durability are insufficient in these areas. The successful expansion of mass timber construction...
G Presley, C Wainscott, J Valenti, S Noble


Non-vacuum/pressure ACQ treatment
2023 - IRG/WP 23-40971
Many developing countries are located in sub-tropical or tropical regions where rapid wood deterioration results in early failure of many structures. Whilst preservative treatment would help to reduce these losses and extend the forest resource commercial vacuum pressure treatment systems are often too expensive. The use of lower technology treatment systems, while not as quick as vacuum pressure ...
J Norton


Starch modified with silanes – high hydrophobic surface treatment for wood protection
2023 - IRG/WP 23-40981
The great potential of silanes for starch modification and their utility as surface wood protection is still not sufficiently assessed. The work aimed to analyze the crosslinking process's effect on starch modification with silane and tested the hydrophobic properties of surface-treated wood. The starch treatment was modified with methyltrimethoxysilane or N-octyltriethoxysilane. SEM-EDX with a cr...
W Perdoch, M Bajstok, B Mazela, I Siemińska, B Peplińska


Danish wood preservatives approval system with special focus on assessment of the environmental risks associated with industrial wood preservatives
2001 - IRG/WP 01-50166-01
The following is a description of the procedure used by the Danish Environmental Protection Agency to assess the environmental risks associated with preservatives used in the pressure impregnation of wood. The risk assessment covers issues considered to be of significance for the environment and which are adequately documented so as to allow an assessment. Such issues are persistence and mobility ...
J Larsen


Proposal for further work on accelerated ageing
1988 - IRG/WP 2314
M-L Edlund


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 2: Report of treatment and installation in Australia
1978 - IRG/WP 440
The purpose of this test and the procedures to be followed have been fully set out in documents distributed by the International Research Group on Wood Preservation and numbered IRG/WP/414 and IRG/WP/420. The prescriptions set out in these two documents have been closely followed....
J Beesley


Field test evaluation of preservatives and treatment methods for fence posts
1985 - IRG/WP 3347
This work presents the field test results after fifteen years exposure of Eucalyptus saligna fence posts treated with six different preservatives and five treatment methods. All the combinations with oil-borne preservatives presented the best results and among the waterborne preservatives, the fence posts treated by immersion method were with the lowest performance in the field test....
G A C Lopez, E S Lepage


Problems caused by termites in buildings in the State of Sao Paulo
1976 - IRG/WP 150
Termites are the main insects attacking buildings in the State of Sao Paulo - Brazil. Their attack occurs in wood and wooden materials as well as paper, textile, leather and so on....
M S Cavalcante


Strength loss associated with steam conditioning and boron treatment of radiata pine framing
1987 - IRG/WP 3438
The combined effect of included defects and wood moisture content on the strength loss of second rotation radiata pine framing following conventional steam conditioning is investigated. The green Modulus of Elasticity (MOE) is reduced by approximately 13% after steaming. When dried after steaming, however, neither the MOE nor MOR is significantly different from unsteamed dried controls....
M J Collins, P Vinden


Soft rot penetration - Effect of groundline maintenance treatment on poles in sevice
1983 - IRG/WP 3263
R S Johnstone


Improved techniques designed for evaluation of fungicides in soil for control of dry rot fungus Serpula lacrymans
1985 - IRG/WP 2238
Improved techniques provide a laboratory method for the evaluation of chemicals in soil for control of dry rot fungus Serpula lacrymans. Results with their application to three chemicals were reported. These techniques are useful to eliminate chemicals lacking the necessary toxicity and weatherbility for dry rot control when the chemicals have been applied to the soil....
M Takahashi, K Nishimoto


How to Document the Performance of Super-Critical Treated Wood in above Ground Situations?
2005 - IRG/WP 05-20316
The paper presents practical experiences from the preparation of a new preservative treated wood product for introduction to the market. The product in question is Superwood™, which is treated with organic biocides using CO2 in a supercritical state as a solvent. The question is how to evaluate the performance of a new product such as Superwood™ in order to get an acceptance on the market a...
N Morsing, A H H Wong, F Imsgard, O Henriksen


The dry rot fungus Serpula lacrymans. Examples of attack and remedial treatment
1988 - IRG/WP 1347
The film deals with several aspects of dry rot attack and eradication in buildings. The detailed biology and morphological charasteristics of the fungus are portrayed. The various forms of mycelial growth, the role of the strands in the nourishment and spread of the fungus, as well as the many types of fruitbody formation are outlined. Environmental and nutritional requirements of the fungus as we...
G Buchwald, B M Hegarty, W Metzner, R Pospischil, H Siegmund, P Grabow


Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 3: Full penetration of the refractory sapwood of white cypress
2000 - IRG/WP 00-40167
The heartwood of white cypress, Callitris glaucophylla, is renowned for its termite resistance and durability against decay. The sapwood, which can represent up to 30% of log volume, is non-durable and refractory to conventional preservative treatment. Previous work ascribes the lack of permeability to oily deposits within tracheids and ray cells. Environmental scanning electron microscopy was use...
M J Kennedy, L M Stephens, M A Powell


Thermal treatment of wood: European Processes and their background
2002 - IRG/WP 02-40241
Recent efforts on thermal treatment of wood lead to the development of several processes introduced to the European market during the last few years. The total production capacity of heat treated wood in 2001 is estimated as approx. 165.000 m3. In the paper the different heat processes are presented. The general technology as well as scientific data on the chemical transformation of the cell wall ...
H Militz


Non-pressure treatability of plywood by CCA, CCB and boron
2005 - IRG/WP 05-40295
Study on diffusibility and absorbability of CCA, CCB and boric acid in 3 mm thick 3-ply hardwood plywood at water saturated and air-dry conditions and dipped at same concentration (5%) and same duration of time (12 hours) revealed complete diffusion of all the preservatives at water saturated condition. Only the CCA-C was found absorbed by the plywood at air-dry condition. The rate of absorption a...
A K Lahiry


Problem of the treatment of dried sawn spruce building timbers with water-borne preservatives. Interim reports for discussion at the 4th Annual Meeting in West Berlin on 27 October 1972
1972 - IRG/WP 311
One of the most difficult technical problems facing the preservation industry is how to improve the treatment of refractory species of timber such as spruce. Its resistance to penetration, even under pressure' precludes its use for more hazardous service situations, and even in less severe conditions a higher level of treatment would be desirable. The importance of this subject led us to ...
W Liese, J W W Morgan, T Hof, R O Ullevålseter