IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 90 documents. Displaying 25 entries per page.


Site characteristics impacting historic waterlogged wood: A review
2000 - IRG/WP 00-10344
Survival of waterlogged wood from hundreds and in rare cases millions of years presents scientists with a unique opportunity to examine wood specimens which, due to select properties of the wood itself and/or the depostional environment, have not been completely degraded. Although degradation patterns of various types of microbial wood decay have been studied in detail, the site parameters of the ...
B A Jordan, E L Schmidt


Health aspects concerning the use of bifluorides in wood
1981 - IRG/WP 3173
An attempt has been made to find a correlation between the quantities F¯ and HF present among other ions in an 'Improsol' solution consisting of NH4F.HF and KF.HF, the quantity absorbed by the wood from this after immersion and the toxicological effects of this treated wood when it is used in rooms destined for the residence of people or animals or for the storage of foodstuffs....
H F M Nijman


A case study on quality control on telephone poles as a cost saving tool in Tanzania
1987 - IRG/WP 3418
A sample of 28 CCA treated Eucalyptus poles from a lot of 2,000 poles awaiting delivery to the field, was studied to reveal the quality of treatment. Results showed a product of very poor quality. Average figures for penetration and retention were 8.4 mm and 2.2 kg/m³; these results are 66% and 91% below the required standards, respectively. Consequences of such results are estimated to amount to...
K K Murira


The influence of crystalline and amorphous cellulose on extracellular hydrogen peroxide production by brown-rot fungi
1991 - IRG/WP 1482
The production of hydrogen peroxide (H2O2) has been suggested to play a key role in the degradation of wood by wood-rotting fungi. The production of extracellular hydrogen peroxide was studied by a quantitative method which detects the oxidation of the 2,2-azinobis(3-ethylbenzthiazoline-6-sulphonic acid) (ABTS) by H2O2 and horseradish peroxidase (HRP) in liquid culture medium. The carbon sources u...
A-C Ritschkoff, L Viikari


Cytochemical localization of hydrogen peroxide in brown rot fungus Tyromyces palustris by cerium chloride technique
1999 - IRG/WP 99-10299
Cerium chloride (CeCl3) was used to localize H2O2 cytochemically for studying relationship between ultrastructural and functional characteristics of cellulose degradation by brown rot fungi. This technique proved very useful in localizing discrete electron-densereactionproducts at high resolution with minimal nonspecific deposition. The cytochemical localization of extracellular H2O2 by CeCl3 usin...
Yoon Soo Kim, Seung-Gon Wi


Studies on the infestation behaviour of the powder-post beetle Lyctus brunneus (Steph.) and its physical control in the wood yards of the Caspian forests of Iran
1985 - IRG/WP 1271
Lyctus brunneus (Steph.) is a pest which has not been previously thoroughly studied in Iran. It severely attacks Iranian hardwoods, especially those used in wooden houses and that have not been treated. Research work was necessary to determine the natural resistance of the most important timber species in Iran against this insect....
P Niloufari


Effect of fatty acid removal on treatability of Douglas-fir
1993 - IRG/WP 93-40008
Treatment of Douglas-fir with chromated-copper-arsenate (CCA) poses a major challenge. Several hypotheses based on the anatomical aspects as well as chemical reactivity of the preservative formulations with cell wall constituents and deposits have been proposed. Techniques to prevent pit aspiration or slow fixation reactions have, however, not significantly improved treatment. The presence of high...
S Kumar, J J Morrell


Detection of brown rot decay in wood by ion mobility spectrometry
1991 - IRG/WP 2377
A test method for the detection of brown rot decay in wood is described and involves a two-step procedure: thermal release of vapours from wood samples followed by analysis using Ion Mobility Spectrometry (IMS), with results being obtained in 5-10 seconds. The advantages, limitations as well as the detection limit of the technique are presented....
A H Lawrence, T Nilsson


The effect of temperature on the rate of fixation of an alkyl ammonium compound (AAC) wood preservative
1984 - IRG/WP 3293
The rate of fixation of an alkyl ammonium compound wood preservative was measured by soaking samples of wood wool in various preparations of the preservative for arbitrary times followed by immediate leaching in water. The wood wool was then analysed for residual preservative. The results indicated that fixation was very rapid and increased at higher temperatures....
P Vinden


Diffusion of bifluorides and borates from preservative rods in laminated beams
1991 - IRG/WP 3644
Laminated beams from spruce, pine and larch were treated with two preservative rods, based on bifluorides and octaborate respectively. After 3 and 6 months placed in different climates (65% r.h., 100% r.h., water) the diffusion of the active ingredient was measured. After the 6 months period, the diffusion of the bifluorides was, in all species, ca. 5 times larger than the diffusion from octaborat...
H Militz


Detection of trace organics by ion mobility spectrometry
1990 - IRG/WP 3635
Ion Mobility Spectrometry (IMS) is a time of flight analytical technique that is suited to detect chemicals in the low parts per billion range. Some of the advantages of IMS are: operation at atmospheric pressure, fast response time (0.1-10 sec), and the ability to characterize individual chemical species in complex matrices without any prior sample preparation. In this paper, the utility of IMS i...
A H Lawrence


Wood extractive concentration and sem examination of pretreated southern yellow pine wood chips with blue-stain fungi for mushroom production
2001 - IRG/WP 01-10407
Mushroom-producing white-rotting basidiomycetes either do not colonize or else colonize very poorly on freshly prepared southern yellow pine wood chips. This study evaluates the resinous extractive content of southern yellow pine before and after treatment with colorless mutant blue-stain fungi. The blue-stain fungi penetrate into the sapwood of southern yellow pine and utilize nonstructural resin...
S C Croan, J Haight


Involvement of hydrogen peroxide in wood decay by brown-rot and white-rot fungi
1985 - IRG/WP 1256
To gain further understanding of the role of H2O2 in wood degradation by brown- and white-rot fungi, we studied the following: (a) extracellular H2O2 production, (b) effect of various hydroxyl radical (·OH) and singlet O2 (1O2) quenching agents on wood and cellulose degradation, (c) intracellular H2O2 production and catalase activity, and (d) cytochemical localization of H2O2 with diaminobenzidin...
T L Highley, L L Murmanis


The use of bifluorides-diffusion in remedial treatments
1983 - IRG/WP 3256
A description is given about the experience to date of a 14 years' development to bring bifluorides-diffusion from laboratory evaluation to commercial service application. The described treatment is an adjunct to good design and not a replacement for it. The process is also used with an injection method for the remedial treatment of premature decayed external joinery....
H F M Nijman


CCA fixation experiments. Part 1
1989 - IRG/WP 3504
A method of squeezing solution from CCA treated wood that has not been dried at various times after treatment appears to be useful in following the fixation of CCA in wood. Experiments confirm that temperature governs the rate of fixation....
W S McNamara


Investigation of the fixation in wood of chromated zinc chloride and copperised chromated zinc chloride preservatives
1976 - IRG/WP 372
A biological method of evaluating the extent to which CZC and CCZC preparations are retained in wood in terms of the potential protection which they afford against destruction by Merulius lacrymans (dry rot) is given. CCZC is recommended for protection of wood under moderate leaching conditions, while the use of CZC under such conditions is not recommended....
V N Sozonova, D A Belenkov


Treating Eucalyptus tereticornis wood with boron: Optimizing treatment conditions
2005 - IRG/WP 05-40309
Even though Eucalyptus tereticornis wood is suitable for small timber purposes, being non-durable, it needs to be treated with preservative chemicals. As it is a heavy, hard and difficult to treat species, the possibility of using diffusible boron compounds was investigated. The present study explored the effect of impregnation conditions such as treatment schedule, concentration of treatment solu...
T K Dhamodaran, R Gnanaharan


The course of fixation of Cu-Cr-As wood preservatives
1972 - IRG/WP 307
Copper-chrome-arsenic (CCA) preservatives in contact with wood result in an instant extensive increase of pH, because of ion-exchange and adsorption reactions with the wood. During precipitation of the active elements the pH continuously increases but reaches a maximum, when all chrome is consumed. Some of the early reaction products are unstable and slowly convert via dissolution into stable comp...
S-E Dahlgren


Remedial treatment of joinery. Comparison of distribution of organic solvent preservative and ammonium bifluoride
1978 - IRG/WP 3115
It is some years since it was recognised in the United Kingdom that there was a problem of premature decay in untreated external joinery. Consequently, recommendations for preservative treatment were made by the Building Research Establishment, Princes Risborough Laboratory. In addition, the National House-Building Council has also included the preservative treatment of external joinery in its req...
J M Taylor


Iron in stone wool - one reason for the increased growth and decay capacity of Serpula lacrymans
1992 - IRG/WP 92-1537
The chemical compositions of stone wool and glass wool were analysed. There was more iron in the stone wool than in the glass wool. It was found that iron present in stone wool was easily dissolved by oxalic acid that Serpula lacrymans is able to produce. The stone wool promoted the decay of pine wood by Serpula lacrymans. The glass wool had no effect on the decay capacity of Serpula Iacrymans. Th...
L Paajanen, A-C Ritschkoff


Determination of total fluoride in preservative-treated wood by ion selective electrode, without steam distillation
1996 - IRG/WP 96-20086
An analytical method was developed to determine total fluoride in wood treated with aqueous fluoride or borate-fluoride formulations. Ground wood was mixed with 60% sodium hydroxide solution and oven-dried overnight before furnacing at 600°C. The cool fused product was dissolved in warm water before adding a powerful complexant/buffer solution containing sulphosalicylic acid and EDTA. Fluoride wa...
M J Kennedy


Health hazards and environmental aspects when using Cu-HDO-containing wood preservatives in vacuum pressure plants
1993 - IRG/WP 93-50001-11
Apart from the biological efficacy of wood preservatives, the health and environmental aspects concerning the utilisation of wood preservatives, the use of treated timber and the disposal of impregnated wood are of high significance today. Therefore, information on a possible aerial concentration of wood preservatives, on the mobility of active substances in soil leached from treated timber in ser...
W Hettler, S Breyne, M Maier


Sludge formation in timber treatment with CCA preservatives. Origin and elimination
1984 - IRG/WP 3276
The exact distributions between lignin and holocellulose and retentions on wood of copper, chromium and arsenic as a function of various sets of conditions in a factorial experiment in which combinations of three temperatures of treatment, three CCA solution concentrations, four pH's of the initial CCA solution and two timber species, namely Pinus radiata and Eucalyptus grandis, are repor...
A Pizzi, W E Conradie, A Jansen


Screening of lignin peroxidase from white-rot fungi
1998 - IRG/WP 98-10274
Since lignin peroxidase was first found in the ligninolytic culture of Phanerochaete chrysosporium, it has been regarded as an enzyme responsible for the lignin biodegradation and studied comprehensively. As the results of these studies its unique characteristics have been revealed. On the other hand, the features of lignin peroxidase produced by other white-rot fungi have not been studied so much...
I Momohara


Oxalate production and calcium oxalate accumulation by Gloeophyllum trabeum in buffered cultures
1994 - IRG/WP 94-10075
Most basidiomycetous fungi produce oxalic acid as a result of their metabolic activities and nutrient procurement. There is currently a renewed interest in the role that oxalic acid may play in the decomposition of wood by basidiomycete fungi. It has been observed that although most wood degrading fungi have the capacity to produce oxalic acid, not all of these organisms express this capacity equa...
J H Connolly, J Jellison


Next Page