IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 258 documents. Displaying 25 entries per page.


An attempt to evaluate wood resistance against fungal decay in non-sterile conditions by measuring the variation of resistance to bending test
1988 - IRG/WP 2308
The main object of this work was to determine the variation of strength on large test specimens of wood (800 x 45 x 45 mm³) when exposed to accelerated fungal attacks close to natural conditions, out of test vessels. The modulus of elasticity (MOE) and the modulus of rupture (MOR) have been assessed. Thereby, the natural resistance of the wood species to fungal decay, the efficiency of preservati...
L N Trong


A direct method for testing plywood and particle boards against fungal decay
1984 - IRG/WP 2214
A method directly inspired from the French standard testing method of the resistance of particle boards against fungal decay (AFNOR N° 51.295 May 1980) is described. But in that experimentation, the infestation is localized and realized in non sterile conditions. Small blocks of Fagus sylvatica (60 x 20 x 10 mm³) used as " inoculates " are infested with basidiomycetes, in Kolle flask for 4 to 6 ...
L N Trong


Rates of emission from CCA-treated wood in the marine environment: measurement, modelling and requirements for further research
2001 - IRG/WP 01-50166-12
Accurate estimates of rates of emission of leachate from preservative treated wood are crucial for realistic predictions of the environmental impact of its use in maritime construction. Estimates are available for some commonly used preservatives, but these vary widely. Though variable, these measurements suggest that emission generally decreases exponentially with time. Part of the variation is d...
S M Cragg, C J Brown, R A Albuquerque, R A Eaton


Dimensional stabilization of wood with dimethylol compounds
1987 - IRG/WP 3412
This study showed that a substantial degree of dimensional stability can be imparted to wood by crosslinking with low concentrations of dimethyloldihydroxyethyleneurea. It was demonstrated that by selecting the right catalyst system the cure temperature can be reduced to the point that strength loss of the treated wood is minimized....
D D Nicholas, A D Williams


Performance results of wood treated with CCA-PEG
1986 - IRG/WP 3363
The addition of polyethylene glycol (PEG) to the CCA system has been shown to reduce the surface hardness of poles and ease spur penetration during climbing. This paper addresses the results of tests dealing with preservative retention and penetration, permanence of CCA and PEG, strength, drying rate, and checking characteristics....
W P Trumble, E E Messina


Airborne algae as a wood degradation factor
1992 - IRG/WP 92-1549
The occurrence of airborne (aerophytic) algae on wood is a very frequent phenomenon. However, there is currently a lack of information concerning their effect on the wood tissue. Some important genus of algae infesting wood under natural conditions are listed, as well as the results of experimental studies in the "in vitro" culture concerning the effect of two selected algal species on some physic...
K J Krajewski, J Wazny


A summary of tests and practical experiences with the Pilodyn wood testing instrument
1980 - IRG/WP 282
This paper presents a summary of the reports, tests and practical experiences with the Pilodyn wood tester not only, however, concerning poles but also in other fields such as standing trees, sawn timber etc. The principle of the Pilodyn is a spring-loaded pin which is fired into the object and the depth to which the pin penetrates is correlated to physical and mechanical properties of the object....
H Friis-Hansen


Environmental impact of CCA poles in service
1997 - IRG/WP 97-50087
Soil samples from different depths and distances from CCA treated utility poles in Canada were analyzed for copper, chromium and arsenic content for a number of soil types, two wood species red pine (Pinus resinosa) and jack pine (P. banksiana) and different pole ages in service. A limited number of poles were equipped with water traps to collect rain water that dripped down the poles and where su...
P A Cooper, Y T Ung, J-P Aucoin


Research on the effects of wood preservatives on the physical and mechanical properties of Iranian beech (Fagus orientalis Lipsky)
1985 - IRG/WP 3351
This research work was conducted with the aim of using preservatives such as Basilit and Wolman Salts with Iranian beech and to study any physical and mechanical changes these might have on the beech species of Iran. Samples were divided into three groups; one group were used as untreated controls, the second group was treated with Basilit and the third group was treated with Wolmanit. Results obt...
P Niloufari


The performance of wood preservatives in soil-bed soft rot tests
1993 - IRG/WP 93-20007
Testing the efficacy of wood preservatives in soil is recognised as a fundamental part of the assessment of long-term wood protection in ground contact. Laboratory based tests can provide a hazardous environment in which a preservative can be challenged by a range of micro-organisms. This paper presents the results of tests carried out to investigate the performance of wood preservatives in a wet ...
G R Williams, S Caswell


Studies on the preservation of structrual plywood - Part 1: Decay resistance of structural plywood
1974 - IRG/WP 238
The weight loss and the decreases in the compression strength and in the modulus of elasticity were measured to determine the decay resistance of structural plywood (lauan). Test pieces (50x25xA mm³) were exposed to the wood destroying fungi (Coriolus versicolor and Coriolellus palustris) for 2-3 or 2-4 months. After exposure, the measurement of the compression strength was carried out on the pie...
K Minami, Y Kenjo, S Sugiyama


The performance of softwood species used as poles in Queensland
1985 - IRG/WP 1253
In Queensland, the conifer Pinus elliottii could provide material suitable for use as poles. Full size pole material has been readily treated with CCA with no significant loss in strength. Seasoning of logs prior to treatment requires particular attention in the wet tropical and sub-tropical regions of Queensland. Experimental and in service field tests have indicated excellent performance of CCA ...
L E Leightley


Bibliography: Interactions of wood preservatives with wood, metals, glues, paints and concretes
1983 - IRG/WP 3271
H Becker


The Pilodyn instrument as a non-destructive tester of the shock resistance of wood
1978 - IRG/WP 2107
A new non-destructive shock resistance tester, the PILODYN, has been developed. The instrument measures the fracture surface area created by a constant amount of energy. It operates by shooting a blunt pin into wood by an exact amount of energy. The penetration depth is read on a scale. A wide field of application is open to a non-destructive shock resistance tester such as: 1) assessment of the r...
P Hoffmeyer


Life cycle analysis: Assessing environmental impact
1994 - IRG/WP 94-50034
Environmental impact assesment is a major issue that faces every nation today. However, consistently and objectively measuring the environmental impact is difficult. During the past two decades, a process called life cycle analysis was developed that tried to make consistent and objective environmental assessments. The Society of Environmental Toxicology and Chemistry broadened the concept to not ...
S L LeVan


Heat treated timber in Finland
2000 - IRG/WP 00-40158
Heat treatment permanently changes the physical and chemical properties of wood by means of high temperatures (150 - 240°C). Heat treatment darkens the colour of the wood. Heat treatment improves the equilibrium moisture content of the wood and the shrinkage and swelling of the wood is reduced. Very high temperatures improve the resistance to rot and also reduce the susceptibility to fungal decay...
T Syrjänen, E Kangas


An experimental method to simulate incipient decay of wood by basidiomycete fungi
2000 - IRG/WP 00-20200
At very early stages of decay of wood by basidiomycete fungi, strength loss can be measured from wood before any measurable weight loss. Therefore, strength loss is a more efficient measure of incipient decay than weight loss. However, common standard decay tests (e.g. EN 113 or ASTM D2017) use weight loss as the measure of decay. A method was developed that allowed progressive removal of samples ...
S F Curling, J E Winandy, C A Clausen


A short note on the subject of pretreatment decay in wood
1984 - IRG/WP 1245
The paper reviews five national standards for wood utility poles and some literature that concerns the problems of pretreatment decay. Finally it is proposed to form a new sub-group to study that problem....
J A Taylor


Methods of assessing decay in poles in service with the Pilodyn wood tester
1978 - IRG/WP 2107 A
H Friis-Hansen


Ancillary properties of vapor boron-treated composites
2001 - IRG/WP 01-40210
This paper discusses the water absorption, thickness swelling, and internal bond strength of North American composites treated using a vapor boron treatment process. For oriented strandboard, high boron loadings led to lower internal bond strength and lower thickness swelling. Water absorption results were variable but no deleterious effect of treatment was noted. For medium density fiberboard, th...
W A Jones, H M Barnes, R J Murphy


Less environmental impact of wood preservatives by considering the risk of attack in addition to the hazard class system
1995 - IRG/WP 95-50040-10
Hazard classes, which are standardized in Europe in EN 335, are most useful to direct chemical wood preservation towards the organisms which may attack wood in the various fields of utilisation. However, hazard only signifies the fact that an attack may occur without considering the actual risk to attack. To minimize the application of chemicals with respect of less environmental impact it is nece...
H Willeitner


Dimensional stability, biological resistance, and mechanical properties of phenol-resin-treated particleboard
1990 - IRG/WP 3622
Particleboards were treated with a low molecular-weight phenol-formaldehyde (PF) resin and their enhanced properties were evaluated. Besides dipping of particles in aqeous solutions of resin, and spraying of resin solutions before spray of the conventional phenol-formaldehyde resin for adhesive binder, one step treatment by spraying of the mixture of the low molecular-weight resin and the adhesive...
Y Imamura, H Kajita


Bending properties of treated western hemlock plywood
1996 - IRG/WP 96-40064
This study investigated the mechanical properties of western hemlock plywood after treatment with waterborne preservatives and redrying. Unlike previously reported results for southern pine plywood, western hemlock plywood was more sensitive to redrying temperature than to preservative treatment. Generally, western hemlock plywood was affected by temperature and other variables. Losses in mechanic...
H M Barnes, A Khouadja, D E Lyon


Use of the Pilodyn to assess deterioration of treated aspen waferboard after 30 months of outdoor exposure
1986 - IRG/WP 2254
Samples of preservative treated aspen waferboard exposed outdoors for 30 mo. were compared using pin penetrations of the 6 Joule Pilodyn. These results correlated well with rankings of treatment performance based on more laborious standard mechanical tests, and demonstrate the potential for use of the Pilodyn as a tool to evaluate wood composites in test exposures with minimal destruction....
E L Schmidt, M G Dietz


Comparative environmental impact analysis of telecommunication utility poles: Treated wood and fibreglass
1999 - IRG/WP 99-50136
This study is aimed at providing the information necessary to assess the main environmental implications of different materials utilised in construction of utility poles. The study was performed on fibreglass and CCA treated poles timber. The work has been carried out by identifying and quantifying energy and materials used and wasted released during the entire life of the pole. The interactions w...
A Cugliandolo, M Onofrio, A Quaglino


Previous Page | Next Page