Your search resulted in 1182 documents. Displaying 25 entries per page.
Synergistic effects between 2-HPNO, Irganox 1076 and EDTA on the inhibition of wood degradation by Coriolus versicolor
2004 - IRG/WP 04-30331
The efficiency of 2-hydroxypyridine-N-oxide (2-HPNO) as wood preservative has been investigated. As shown using classical experiments as well as using response surface methodology, the efficiency of 2-HPNO as wood preservative is strongly improved in presence a chelator like EDTA and/or of Irganox 1076 an industrial antioxidant. In these conditions, wood preservative efficiency of the mixture the ...
A Mabicka, S Dumarçay, N Rouhier, M Linder, J P Jacquot, P Gérardin, E Gelhaye
Prevention of brown-rot decay by chelators
1992 - IRG/WP 92-1540
In this work the brown-rot decay was shown to be prevented by chelating the endogenous metals existing in wood by using organic or inorganic chelators or iron-binding siderophores. The fungal growth and decaying ability were significantly decreased by the chelating treatments of the solid wood-based culture medium and pine wood pieces, respectively. The transition metals existing in native wood ar...
L Viikari, A-C Ritschkoff
Changed susceptibility of the chemically and thermally degraded spruce wood to its attack by the dry rot fungus Serpula lacrymans
1999 - IRG/WP 99-10322
In buildings, some intentional or unintended situations can occur at which some wood products are exposed to aggressive chemicals and also to higher temperatures. Occasional activity of fungi on such pre-attacked wood products can be either higher or lower. This paper deals with changes in the susceptibility of spruce wood (Picea abies L. Karst.) to attack by the dry rot fungus Serpula lacrymans, ...
L Reinprecht
The effect of storage or simulated internal use on the durability of wood based panels to decay fungi
1997 - IRG/WP 97-20106
Wood based panels such as particleboard and medium density fibreboard are experiencing a steady increase in use, in areas from structural to decorative applications. Understanding the "natural" durability of these panel products against basidiomycete fungal decay is therefore of great importance. Various methods have been proposed or are under development to test the durability/susceptibility of v...
S F Curling, R J Murphy, J K Carey
Recent names for some common decay fungi
1976 - IRG/WP 143
A Käärik
Model questionnaire for preparation of monographic cards for wood-destroying fungi
1972 - IRG/WP 103
C Jacquiot
An insight into brown rot decay of timber as revealed by 13C CP/MAS NMR
1985 - IRG/WP 1259
L E Leightley
Localization of oxalate decarboxylase in the brown-rot fungus Postia placenta
1996 - IRG/WP 96-10161
Oxalate decarboxylase, the enzyme that breaks oxalic acid down into formic acid and carbon dioxide, was recently detected in mycelial extracts of the brown-rot fungus Postia placenta. Differential centrifugation was used to demonstrate that the enzyme is loosely associated with the hyphal surface. Enzyme activity can be removed by washing the hyphae with a low pH buffer. Only low levels of activit...
J A Micales
Effect of sterilization method on germination of spores of wood decay fungi observed by contact agar block method
1978 - IRG/WP 2117
Previous studies of germination of spores of wood decay fungi on wood have generally concluded that method of wood sterilization has little significant effect on germination response. This study expands the numbers of test fungi as well as number of sterilization methods employed to determine the influence of sterilization method on spore germination response of decay fungi. Germination was assess...
E L Schmidt, D W French
Characterisation of growth and stain of different groups of sapstain fungi on lodgepole pine
1999 - IRG/WP 99-10326
Canada is the world's largest exporter of softwood lumber. These softwood shipments are susceptible to a variety of wood-inhabiting fungi that can lead to sapstain discolouration, which in turn decrease the product value. Furthermore, the presence of these microorganisms may be unacceptable to the importing countries. The objective of this work is to assess the sapstaining capability and ...
C Fleet, C Breuil, A Uzunovic, A Byrne
Mold inhibition on unseasoned southern pine
2003 - IRG/WP 03-10465
Concerns about indoor air quality due to mold growth have increased dramatically in the United States. In the absence of moisture management, fungicides need to be developed for indoor use to control mold establishment. An ideal fungicide for prevention of indoor mold growth on wood-based materials needs to specifically prevent spore germination and provide long-term protection under conditions of...
C A Clausen, V W Yang
The potential of 2-deoxy-D-glucose as an active ingredient in wood preservation
1999 - IRG/WP 99-30205
2-deoxy-D-glucose (2-DOG) is a potential active ingredient against wood decaying fungi. When dissolved in water, it can be used in pressure treatment of wood. Thereby the wood is protected from attack by wood decaying fungi. A concentration of 1.5% (mean retention 9.7 kg/cubic meter sap-wood) is adequate for brown rot fungi, and 3% (mean retention 19.5 kg/cubic meter sapwood) will also provide protection against white rot fungi. 2-DOG is easily soluble in water, and is therefore easily leached from the wood upon completion of the preservation process. Different types of fixa-tion methods have been tried and evaluated. It is possible to produce 2-DOG by the hydrolysis of chitin, a constituent of the exterior skeleton of shellfish and insects. There is a potential for exploita-tion of this waste product provided by the crab and shrimp industry. The yield of 1 kg of fresh shrimp is 75 g of 2-DOG.
O V Frederiksen, A P Koch
Evaluation of the decay caused by Chaetomium globosum Kunze, in the course of time
1987 - IRG/WP 2288
The main research done on soft rot has been directed to determining, by microscopic study, the different stages of penetration into the wood of the fungi that cause it. On the basis of the information furnished by this research, in this work we have tried to quantify its effect, by evaluating the weight loss caused by Chaetomium globosum Kunce in wood of Pinus sylvestris L. and Fagus sylvatica L. ...
M T De Troya, A M Navarrete
Proposals for collaborative work on laboratory soft rot testing
1986 - IRG/WP 2265
Proposals for collaborative experiments based on soil burial are presented. It is intended to study the use of defined horticultural loams with a view to obtaining more reproducability in laboratory soft rot tests....
D J Dickinson, S M Gray
The true dry rot fungus (Serpula lacrymans) found in the wild in the forests of the Himalayas
1993 - IRG/WP 93-10002
J Bech-Andersen, S A Elborne, F Goldie, J Singh, B Walker
Detection of incipient brown rot decay in wood by fourier transform infrared spectrometry
1987 - IRG/WP 2275
Fourier transform infrared spectrometry was evaluated as a possible method for detecting different levels of brown-rot decay in pine sapwood. By using first derivative spectra and regression analysis, an equation based on 4 absorption peaks, normalized with an internal standard peak, was developed. The correlation between weight loss and absorption was highly significant indicating that this is a ...
D D Nicholas, T Schultz
Collaborative soft rot test: Amended test method
1972 - IRG/WP 208
The initial draft of a standard test method (Document IRG/WP/201) was discussed at the meeting in Brussels in 1971. It was agreed that a revised draft should be prepared and that the Princes Risborough Laboratory (formerly FPRL) should conduct a trial test using the method as a preliminary to the main collaborative test....
J G Savory
The use of C CP/MAS NMR in the chemical identification of decayed and undecayed, tropical timber species
1984 - IRG/WP 1224
13C CP/MAS NMR was found to be an extremely powerful tool for elucidating the chemical composition of Eucalyptus maculata, Pinus elliottii and Alstonia scholaris. The differences in lignin composition were different for each timber and discussed in relation to decay caused by soft-rot and white rot fungi. In particular the presence of syringyl and guaiacyl lignin types are discussed.
L E Leightley
Experimental test site to prevent maritime pine logs from bluestaining: water-spraying and water-immersion methods
2003 - IRG/WP 03-10497
Following a storm which led to windfall wood, a research project was launched to develop preservation methods with a low environmental impact for maritime pine logs. These preservation methods are intended to be suitable for large-scale storage areas of maritime pine. In addition the aim was to maintain wood quality during long term storage. An experimental field test with 1 900 m3 of maritime pin...
I Le Bayon, H Callot, D Reuling, C Brunet, P Castéra
The performance of wood preservatives in soil-bed soft rot tests
1993 - IRG/WP 93-20007
Testing the efficacy of wood preservatives in soil is recognised as a fundamental part of the assessment of long-term wood protection in ground contact. Laboratory based tests can provide a hazardous environment in which a preservative can be challenged by a range of micro-organisms. This paper presents the results of tests carried out to investigate the performance of wood preservatives in a wet ...
G R Williams, S Caswell
IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water: Final report
1987 - IRG/WP 4133
Three timbers chosen as reference species were treated with 3, 6 and 10% solutions of CCA and CCB preservatives and exposed for up to 93 months at 8 tropical and temperate marine sites. Eleven local species treated in the same way were exposed at 4 of the 8 sites. There was no apparent difference in performance between CCA and CCB treated specimens. The severest test site was Panama Canal but mari...
R A Eaton
Detection of semi-quantitative and qualitative enzymatic activities of blue-stain fungi
2000 - IRG/WP 00-10347
Blue-stain, produced in forests, continues to be a problem in countries of moderate climate. In forestry, in certain geographical areas of Spain, it has been observed that anti-sapstain products have not always been efficient, as their fungicidal effectiveness varies on occasion, depending on the species of wood and microbiota that exist in the region. It is not always easy to identify the species...
M T De Troya, F Llinares, D Muñoz-Mingarro, M J Pozuelo, N Acero, C Rodríguez-Borrajo, A M Navarrete
A summary of tests and practical experiences with the Pilodyn wood testing instrument
1980 - IRG/WP 282
This paper presents a summary of the reports, tests and practical experiences with the Pilodyn wood tester not only, however, concerning poles but also in other fields such as standing trees, sawn timber etc. The principle of the Pilodyn is a spring-loaded pin which is fired into the object and the depth to which the pin penetrates is correlated to physical and mechanical properties of the object....
H Friis-Hansen
Wood decay in Danish buildings
1985 - IRG/WP 1261
At Technological Institute identification of fungi and advisory activity concerning repair of damages has taken place since 1935. Statistical analyses based on material from 1982 and 1983 are compared to earlier investigations worked out by L. Harmsen. The material shows that building traditions influence the diversity and frequency of fungal species. Many fungal damages in the last decade have sh...
A P Koch
Copper based water-borne preservatives: The biological performance of wood treated with various formulations
1987 - IRG/WP 3451
Wood samples treated with the various components of CCA preservative singly and in combination were tested against a soft rot organism, a copper tolerant brown rot organism and in soil burial both unleached and after leaching. The results suggest that, of the elements tested, fixed copper is essential for preventing soft rot attack and fixed arsenic is essential for preventing attack by a copper t...
S M Gray, D J Dickinson