Industrial fixation systems: key factors, limitations and optimisation through the use of computer simulation modelling. Discussion paper
1994 - IRG/WP 94-40026
This paper briefly describes four fixation operative in the Netherlands, namely: circulating and non-circulating steam fixation cylinders, steam fixation chambers and controlled climate rooms. The general limitations of industrial practice are reviewed against the background of established fixation theory. The controlling variables, both material and process-related, for fixation processing are sp...
A J Pendlebury, M Riepen, M J Boonstra, W Gard


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic conditions. Part 2: Semi-industrial investigation
1995 - IRG/WP 95-50040-13
In continuation of previous leaching research on the quantification and modelling of metal elements released from CCA treated timber, a series of experiments has been carried out dealing with the influence of temperature and pH of the relative aquatic environment. The leaching method used is the Dutch prestandard for building materials, a long term static leaching test simulating practical bank-sh...
G M F Van Eetvelde, W J Homan, H Militz, M Stevens


The environment and the timber preservation in the Benelux countries
1990 - IRG/WP 3580
The environment has become a major issue in all industries. To focus on the timber preservation industry an analysis is made of the production chain. Suggestions are made for diminishing or excluding emissions of agents of pollution. After a review of the legislation in Holland, some important statements are made on the production process, the products involved and the waste materials. Finally raw...
C De Mey, R Leegwater


Industrial fixation of chromium based wood preservatives
1990 - IRG/WP 3630
Fixation is an abstract and non-defined process. Nevertheless it is a specified requirement in most impregnation standards. The impregnation industry is facing increased pressure to deliver fixed products and to increase the safety of the handling of impregnated products. Industrial fixation of impregnated wood can be obtained by using different methods. The purpose of the process is to transform ...
T Christensen


Evaluation of the efficiency of industrial kiln type CCA fixation chambers
1996 - IRG/WP 96-40063
Six commercial CCA treating plants in Canada were assessed for the fixation efficiency of their hot air fixation chambers. The wood temperature was measured with thermocouples over the fixation period at different locations in the chamber and at the end of the fixation cycle, the degree of chromium fixation was determined by a boring leaching procedure. There was a great variation in the effective...
A Taylor, P A Cooper


Laboratory Studies on Copper Availability in Wood Treated with Soluble Amine Copper and Micronized Copper Systems
2008 - IRG/WP 08-30489
A laboratory method has been employed to investigate the level of soluble copper in wood treated with various copper-based preservative systems, such as micronized copper (particulate copper) and amine copper solutions. This report describes the methodology and preliminary results on determination of the soluble copper in the treating solutions and the treated wood by these systems, as well as th...
L Jin, P Walcheski, A Preston


A theoretical-industrial correlation and perspective on copper-based wood preservatives - a review of thermodynamic and kinetic aspects on copper-wood fixation mechanism
2009 - IRG/WP 09-30499
Copper was and it will continue to remain one of the key active component in wood protection industry. Over the past decades, a significant effort from R&D teams in industry, academia and research institutes was directed toward understanding the copper-wood fixation mechanism, optimising the copper retentions in the wood and reduce leaching in order to maximized performance, prolong the lifetime o...
R Craciun, M Maier, J Habicht


Danish wood preservatives approval system with special focus on assessment of the environmental risks associated with industrial wood preservatives
2001 - IRG/WP 01-50166-01
The following is a description of the procedure used by the Danish Environmental Protection Agency to assess the environmental risks associated with preservatives used in the pressure impregnation of wood. The risk assessment covers issues considered to be of significance for the environment and which are adequately documented so as to allow an assessment. Such issues are persistence and mobility ...
J Larsen


Proposed method for out-of-ground contact trials of exterior joinery protection systems
1981 - IRG/WP 2157
Methods for testing the efficacy of preservative treatments for exterior joinery are described using the format of a European Standard. Commercially used treatments applied to jointed test units (L-joints) which are then protected by conventional finishes are exposed to normal outdoor hazards out of ground contact. Assessment is made a) by determining eventual failure through decay and b) by destr...
J K Carey, D F Purslow, J G Savory


Field performance of wood preservative systems in secondary timber species
1997 - IRG/WP 97-30152
The objective of this ongoing study is to evaluate the performance of new, potential, and standard wood preservative systems in secondary North American timber species. Eleven preservative systems were evaluated in this study - ACQ Type B, Copper Citrate 2: l, CDDC, chlorothalonil/chlorpyrifos, copper-8-quinolinolate, tebuconazole/chlorpyrifos, RH287, propiconazole/chlorpyrifos, copper naphthenate...
P E Laks, K W Gutting, R C De Groot


Influence of different fixation and ageing procedures on the leaching behaviour of copper from selected wood preservatives in laboratory trials
2003 - IRG/WP 03-20264
The paper focuses on the role of different parameters, such as fixation, sample size, wood species, and leaching in internationally standardized ageing procedures for wood preservatives from Europe, Japan and the United States. The leaching protocols used were EN 84, JIS K 1571 and AWPA E11 protocols. The wood species were Scots pine, Sugi and Southern Yellow Pine respectively. Three types of com...
J Habicht, D Häntzschel, J Wittenzellner


Modélisation sur maquette du rejet accidentel d'un gaz toxique et inflammable dans l'atmosphere - Emission de type "bouffée d'oxyde d'éthyléne [Water model simulation of toxic and flammable gases in the environment on industrial sites - Puff of ethylen oxide]
1990 - IRG/WP 3576
M Milhe


Accelerated fixation of CCA in borak bamboo (Bambusa balcooa Roxb.) of Bangladesh
2001 - IRG/WP 01-40193
CCA-C fixation study on impregnated (6% CCA solution), then boiled, oven-dried, normal, air-dried and steamed bamboo slices of air-dried borak bamboo (Bambusa balocca Roxb) of Bangladesh, revealed almost complete fixation in steamed (accelerated fixation) and air-dried (3 weeks, slow fixation) bamboo slices compared to moderate to slow fixation in boiled, oven-dried, normal and 24h air-dried slice...
A K Lahiry


A discussion of current theories concerning CCA fixation
1983 - IRG/WP 3238
The understanding of the fixation mechanism of CCA and related preservatives in wood has been greatly improved by a significant series of recent scientific papers. In view of recent concerns in New Zealand regarding the long-term efficacy of CCA in high decay-hazard situations, it was considered appropriate to review this recent work and to contrast it with theories presented by previous workers....
D V Plackett


Proposed methodology for the assessment of safety indexes
1990 - IRG/WP 3562
Safety Indexes (SI)s are developped on the same concept as Efficacy Indexes (EI)s: EIs are retentions of wood preservatives (percentages of the critical values "efficacy") which are presumed efficient for a given biological class of risk. In the same way, SIs are retentions of wood preservatives (percentages of the critical values "safety") which are taken as acceptable for human health and the ge...
G Ozanne


Physical barriers and bait toxicants: The Romeo and Juliet of future termite control
1991 - IRG/WP 1503
Soil chemical barriers are considered by some to be the most important technique for protecting buildings against subterranean termites in Australia (and elsewhere), providing a barrier against termite penetration. However, there is no such thing as a barrier that is 100 per cent +protective. And given the worldwide problems of using organochlorine termiticides, public awareness of chemical pollut...
J R J French


Application of radio frequency heating to accelerate fixation of CCA in treated round-wood
1999 - IRG/WP 99-40133
The potential of radio frequency heating to accelerate the fixation of chromated copper arsenate (CCA) in treated round-wood was assessed. Pre-dried Douglas-fir and western red cedar round-wood sections were pressure treated with CCA in a pilot plant retort, after which they were placed individually in a pilot radio frequency (RF) chamber. Based upon the color reaction of chromotropic acid with he...
Fang Fang, J N R Ruddick


Evidence supporting the use of termite baiting systems for long-term structural protection
2000 - IRG/WP 00-10377
The efficacy of the Sentricon Colony Elimination System containing Recruit II termite bait (0.5% hexaflumuron) in controlling active subterranean termite infestations has been demonstrated in numerous studies. This baiting system and other termite baiting systems are now widely used, and generally accepted, tools for remedial termite control in North America, Hawaii, and other parts of the world. ...
J K Grace, N-Y Su


A simple leaching procedure for in-plant monitoring of CCA fixation
1993 - IRG/WP 93-30023
A simple leaching test is described to quantitatively estimate the extent of fixation of chromated copper arsenate (CCA) preservative treated wood products. It is based on the reaction between diphenylcarbazide and unreacted hexavalent chromium leached from borings taken from treated wood during the fixation process. The test requires about 20 minutes to complete and can be set up in a treating pl...
P A Cooper, Y T Ung


Blue stain in timber in service. Results of co-operative tests to compare different artificial weathering systems 1981-82
1983 - IRG/WP 2193
The paper describes results of the third phase of co-operative laboratory experiments comparing the effects of different artificial weathering systems on chemicals to control blue-stain in service. Atlas, Xenotest and Marr equipments are shown to give essentially the same results for 5 of the 6 chemicals tested....
A F Bravery, D J Dickinson


Environmental issues: Messages for the wood preservation industry
1985 - IRG/WP 3353
A review of the origins and structure of environmental legislation throughout those territories of the world where wood preservation is a major industry is given. The implications of media, industry and legislation interaction is discussed and suggestions made as to the key issues the wood preservation industry should concentrate its attentions on in the immediate future....
D G Anderson, P Waldie


Problems of fixation of CCA-preservatives in palm-wood
1985 - IRG/WP 3338
Palm-wood may be used for posts and poles where it needs proper treatment for long time use. Based on observations by W. Killmann on low CCA-fixation in palm-wood, samples of Jubaea-palm grown in a Greenhouse at Hamburg, have been treated in two different series with a 4% solution of CCA-type B. After 1-16 weeks of storage the blocks were split into sticks of 1-2 mm² and leached. In all series 50...
H Willeitner, K Brandt


Radical changes in the requirements for more safe pressure impregnation in the Nordic countries in 1988
1990 - IRG/WP 3581
After introduction of quality control schemes and standards in the Nordic countries during the seventies, the first radical change of the standards and practice of work took place after pressure from the labor unions and authorities in 1988 and 1989 in Denmark and in Sweden. A new class of preservation with less retention for out of ground contact use was introduced, fixation times were prolonged ...
B Moldrup


Blue stain in service on wood surface coatings. Part 2: The ability of Aureobasidium pullulans to penetrate wood surface coatings
1992 - IRG/WP 92-1557
The ability of Aureobasidium pullulans to penetrate seven different wood surface coatings was examined. Eight isolates of Aureobasidium pullulans were used. Following penetration, light microscopy was used to examine the effect of the fungus upon the coating, and growth at the wood-film interface. The fungus showed different growth capabilities with different types of surface coatings. Some isolat...
P R Sharpe, D J Dickinson


Assessment of losses of wood preservatives from treated wood by leaching into the environment
1993 - IRG/WP 93-50001-13
Wood preservative chemicals may be lost from treated timber by leaching into water or soil. The degree to which this might occur and its effect on the environment is difficult to assess quantitatively due to the absence of appropriate test methods. This paper describes work to assess test methodology capable of allowing the rates of loss of wood preservative from treated timber to be quantified. T...
R J Orsler, G E Holland