IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 10 documents.


Behavioural and morphological adaptations to tidal inundation in the adult wood boring weevil Pselactus spadix Herbst
1999 - IRG/WP 99-10308
Pselactus spadix tunnels wood in the mid intertidal to high intertidal zones and is submersed for several hours with each tide. The submergence and subsequent recovery behaviour, together with sub elytral morphology of P. spadix was investigated and compared to a terrestrial wood borer of the same subfamily Euophryum confine. An investigation of adult activity following submersion in seawater show...
P Oevering, A J Pitman


Assessing the risk of marine borer attack of the timber trestles and decay of timber above the intertidal zone of the Barmouth Viaduct
2021 - IRG/WP 21-10974
The Barmouth Viaduct is a Grade II* listed structure which carries the single track of the Dovey Junction to Pwllheli line and footway over the Mawddach estuary. It is in a marine environment where timber below the high tide mark is at most risk in Use Class 5 and all timber above in Use Class 3.2, permanently exposed to the risk of wetting. The structure consists of a timber trestle viaduct of ...
J R Williams


Antagonistic effect of some mycorrhiza fungi as biological control of blue-stain
1987 - IRG/WP 1314
This report discussed the possibility of using some mycorrhiza fungi as biological control of blue-stain. The results show that new bio-technological possibilities are opening, because, by cultivating antibiosis fungi in fermentor, it is possible to prepare extracts which can then be used as the natural preservative to control the blue-stain in wood....
R Benko


Influence of clonal variability on the impregnability of poplar hybrids. (+ correction document of 23 April 1990)
1990 - IRG/WP 3614
The new Western European poplar clones (Populus nigra x deltoides and Populus trichocarpa x deltoides) were compared with the reference clone 'Robusta' and some old hybrids. Samples (5x5x50 cm³) with pure tangential/radial surfaces were sawn, including the transition zone between heartwood and sapwood. Treatment by a standard vacuum-pressure impregnation cycle with CCA showed a ...
J Van Acker Van, M Stevens, C De Haas


Observations on preservative penetration in poplar
1991 - IRG/WP 3662
In the course of studies on the CCA treatment and durability of poplar timber a zone of refractory wood at the sapwood/heartwood boundary was observed. Further studies were conducted to investigate the causes of this refractory behaviour. The initial results have suggested that the presence of lipid storage products in the ray tissue may lead to impermeability, either by directly blocking pits or ...
R J Murphy, S U Din, M J Stone


Social and economocal impact of an extension of service life resulting of an adequate preventive treatment. Application to wooden components used in urban areas with a high density of population
1993 - IRG/WP 93-50001-15
Le document évalue les problèmes rencontrés en zone urbaine pour le sauvetage des constructions: coordination de la lutte, délimination des chantieres et des périmètres d'investigation, nuisances causées par les interventions, risques pour la santé, risques pour l'environnement. Coûts. Comparaison socio-économique du traitement préventif et des interventions à posteri...
A T De Lelis, G A C Lopez


Inducing and Stimulating Spalting in Sugar Maple
2008 - IRG/WP 08-10652
Spalted wood has gained popularity in recent years as consumer preference has shifted towards unique and custom products. The process by which spalting is induced in clear lumber has evolved over time, and now involves much more than beer drinking and outdoor burial. Our work on the process of reliably producing spalted wood began in 2004 and involved testing a wide variety of white rot fungi on...
S C Robinson, D L Richter, P E Laks


Laboratory test of some formulations against stain and mould fungi isolated from bamboo wood
2009 - IRG/WP 09-30508
To screen the effective anti-mould formulations, fungicides such as carbendazim, tebuconazole, fludioxonil, difenoconazole, prochloraz, benomyl and 8-hydroxy-quinoline copper (copper oxine) were selected to conduct the laboratory test of fungicidal activity by method of inhibition zone against Botryodiplodia theobromae Pat., Fusarium sp., Alternaria tenuis Nees., Penicillium purpurogenum Stoll, Tr...
Xingxia Ma, Airui Sun, Mingliang Jiang, Daochun Qin


Mould resistance of bamboo timber treated with tebuconazole-loaded micells
2012 - IRG/WP 12-30586
In this paper both anti-mould test through inhibition zone and mould resistance test on bamboo samples were carried out evaluate mould resistant effect of tebuconazole (TBA) loaded micells. Results showed that TBA loaded micells prepared with a ratio of TBA to PEG113-b-PCL28 50:25 had the best mould resistance, followed by micells prepared with a ratio of TBA to PEG113-b-PCL28 50:50. PEG113-b-PCL2...
Sun Fangli, Chen Anliang, Bao Binfu, Zhou Yueying, Zhang Shaoyong, Zhang Xu


Analytical retentions of active ingredients in H2F treated framing over a 12-year period
2023 - IRG/WP 23-20702
The H2F hazard class in Australia was developed to treat internal framing timber with a surface application of an insecticide, to control mainly termites. Two of the actives approved in AS 1604.1-2010 (and subsequent revisions) for this hazard class are bifenthrin and imidacloprid. The penetration zone of both actives is 0 – 2 mm from the wood surface. Radiata pine sapwood framing timber wa...
A Siraa