Your search resulted in 3245 documents. Displaying 25 entries per page.
The evaluation of permethrin for wood preservation
1977 - IRG/WP 3107
The toxicity of the synthetic pyrethroid permethrin (NRDC 143) to a range of wood destroying insects has been investigated. In tests using Hylotrupes bajulus, Anobium punctatum, Lyctus brunneus and Reticulitermes santonensis permethrin showed a similar order of toxicity to that of gamma-BHC. Although the toxicity of permethrin to adult Anobium punctatum was of the same order as that of gamma-BHC, ...
R W Berry
Loss of preservatives from treated wood during service
1992 - IRG/WP 92-3734
During the 23rd IRG conference in Harrogate the matter of preservative losses from treated wood during service was raised. We were asked to collect information in this field and ask now for help from you. Many tests have been carried out at a laboratory scale to study fixation and leaching from wood treated with different preservatives. Very little, however, is reported on losses of preservatives ...
M-L Edlund, D Rudolph
Low temperature drying conditions of Pinus radiata wood for avoiding internal stain
1989 - IRG/WP 3507
It has been observed that, if in little sawmills, timber is dried with a low temperature schedule, it arrives at destination with internal sapstain besides of superficial mould. In this study, the lowest drying temperature at which wood should be exposed for sterilization, which results to be 52°C, is searched. It is not possible to avoid entrainment of pentachlorophenol, even though a waiting pe...
M C Rose
Report on the activities of the European Standardization Committee CEN/TC 38 'Methods of Testing wood preservatives'
1980 - IRG/WP 279 E
G Castan
Monographic cards for wood-destroying fungi. [Fiches monographiques pour les champignons lignivores]
1970 - IRG/WP I 5B
C Jacquiot
Thermal treatment of wood: European Processes and their background
2002 - IRG/WP 02-40241
Recent efforts on thermal treatment of wood lead to the development of several processes introduced to the European market during the last few years. The total production capacity of heat treated wood in 2001 is estimated as approx. 165.000 m3. In the paper the different heat processes are presented. The general technology as well as scientific data on the chemical transformation of the cell wall ...
H Militz
A practical method to evaluate the dimensional stability of wood and wood products
1990 - IRG/WP 2342
This paper presents a new simple method to evaluate wood and wood products for their resistance to swelling and to assess wood preservatives for their ability to dimensionally stabilize treated wood exposed to water. Permeable wood of various dimensions and treated with different preserving chemicals have been measured for swelling in the radial and tangential direction during immersion in liquid ...
J P Hösli
Results of chemical analyses in the field of wood preservation in the Bundesanstalt für Materialprüfung
1973 - IRG/WP 321
The results of qualitative and quantitative chemical analyses of wood preservatives are often the basis for evaluating the various works in the field of wood preservation. In the past 10 to 15 years a number of such works was carried out in the Bundesanstalt fur Materialprüfung, Berlin-Dahlem, dealing with the identification and effectiveness of wood preservatives and with methods of wood preserv...
H J Petrowitz
The decay resistance of chemically modified aspen composites to the white rot fungus Coriolus versicolor (L.) Quelet
1998 - IRG/WP 98-40122
Chemical modification of Aspen wood (Populus tremula L.) in the form of solid wood, veneers and sawdust was undertaken by a two step procedure consisting of esterification with maleic anhydride (MA) and subsequent oligoesterification with MA and glycidyl methacrylate (GMA) or allyl glycidyl ether (AGE). Modified wood was thermoplastic and was thermally formed by hot-pressing to produce veneer or s...
M C Timar, A J Pitman, M D Mihai
Wood preservation in Lithuania
2004 - IRG/WP 04-30363
This article is intended to give basic information on wood preservation activities in Lithuania and the main actors in wood preservations practice and research. Currently the main actors in practical Lithuanian wood preservation activity are enterprises of wood preservation industry united by the Lithuanian Wood Preservation Association. The most intensive activity in wood preservation practice an...
J Saladis
IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. 2nd Interim Report
1981 - IRG/WP 477
Three reference wood species - Alstonia scholaris, Fagus sylvatica and Pinus sylvestris, untreated and treated with 3%, 6% and 10% CCA and CCB solutions were supplied to all participants for submergence at local sites. Regular examination of samples is being carried out - 6 months, 12 months and then annually for 7 years....
R A Eaton
A summary of current information on actinomycetes and wood
1978 - IRG/WP 177
B King, R A Eaton, A A W Baecker
The International Resarch Group and its Sponsors
1981 - IRG/WP 5141
R Cockcroft
Improved equipment and technique for high pressure sap displacement impregnation of natural round wood
1972 - IRG/WP 309
Hitherto the main problem in the practical application of high pressure sap displacement impregnation (HPSD) has been in devising a satisfactory cap. Such a cap must be easily fitted to different size log ends to give a leak proof seal. The present contribution describes a new type of cap and sealing system designed to meet these requirements....
C G W Mason, F B Shorland
Electrodialytic remediation of creosote and CCA treated timber wastes
2002 - IRG/WP 02-50190
There is a growing concern about the environmental issue of impregnated timber waste management, since an increase in the amount of waste of treated wood is expected over the next decades. Presently, no well-documented treatment technique is yet available for this type of waste. Alternative options concerning the disposal of treated wood are becoming more attractive to study, especially the ones ...
E P Mateus, A B Ribeiro, L Ottosen
Possible regulatory status of treated wood waste and implications
1998 - IRG/WP 98-50101-07
In relation to the European Community or the French regulations, treated wood waste can get two different regulatory status: <<recycled product or fuel>> or <<waste>>. Then, into the waste status, two categories are possible for these residues: <<domestic waste and assimilated>> or <<hazardous waste>>. These different status and categories are import...
G Deroubaix
Termite resistance of pine wood treated with chromated copper arsenates
1997 - IRG/WP 97-30128
Two four-week, no-choice laboratory tests were performed with CCA-treated southern yellow pine and radiata pine against Formosan subterranean termites, Coptotermes formosanus. CCA retentions as low as 0.05 kg/m3 (0.03 pcf) provided protection from all but light termite attack (rating of 9 on a 10-point visual scale). Similar and consistent light attack on wafers containing retentions as high as 6....
J K Grace
IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 13: Report of fourth inspection (36 months) in Australia
1981 - IRG/WP 481
This report presents the results of the fourth inspection of the IRG/COIPM International Marine Test specimens installed in Sydney Harbour in December, 1977. The inspection took place on 9th December, 1980, after 36 months exposure. Full details of the treatment and installation of the specimens, as well as results of the first three inspections (after 6, 12, and 24 months exposure), have been pre...
J Beesley
The Fourteenth Report of the Internatinal Research Group on Wood Preservation 1984-1985
1985 - IRG/WP 5218
R Cockcroft
Leaching of the new boron based biocide from coated wood
2001 - IRG/WP 01-30267
We investigated leachability of the new boron based biocide - a complex of an amine and boric acid - from vacuum impregnated spruce wood samples. It was determined by the standard ENV 1250-2 procedure that the new biocide is susceptible to leaching so from the water borne as well as from the ethanol borne boron containing preservative treated wood. Leaching may be retarded by application of surfac...
M Petric, M Pavlic, F Cadez
Insects in dry wood (other than termites)
1977 - IRG/WP 153
S Cymorek
Application of radio frequency heating to accelerate fixation of CCA in treated round-wood
1999 - IRG/WP 99-40133
The potential of radio frequency heating to accelerate the fixation of chromated copper arsenate (CCA) in treated round-wood was assessed. Pre-dried Douglas-fir and western red cedar round-wood sections were pressure treated with CCA in a pilot plant retort, after which they were placed individually in a pilot radio frequency (RF) chamber. Based upon the color reaction of chromotropic acid with he...
Fang Fang, J N R Ruddick
Ultra-structural observations on the degradation of wood surfaces during weathering
1987 - IRG/WP 2280
Radiata pine (Pinus radiata D. Don) sapwood was converted into blocks with a transverse face about 5 mm square and measuring 8 mm longitudinally. Transverse (T.S.), Radial (R.L.S.) and Tangential (T.L.S.) surfaces were prepared and specimens exposed to the weather inclined at 45° facing equatorially for periods of between 20-60 days. After 30 days exposure erosion of the middle lamella was observ...
P D Evans, S Thein
Laboratory decay test of Burmese in and kanyin treated with three wood preservatives
1982 - IRG/WP 3210
Laboratory decay tests were performed on samples of In (Dipterocarpus tuberculatus Roxb.) and Kanyin (Dipterocarpus alatus Roxb. and Dipterocarpus turbinatus Gaertn f.) pressure treated with three wood preservatives - copper arsenic additive (CAA - a variation of ammoniacal copper arsenate), Arquad C-33 (a waterborne quaternary ammonium formulation), and tributyltin acetate (TBTA) dissolved in eth...
J N R Ruddick, R S Smith, A Byrne
Programme section 3, Wood protecting chemicals
1997 - IRG/WP 97-30159
IRG Secretariat