IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 168 documents. Displaying 25 entries per page.


Eco-tax - A new threat for wood preservation? The Belgian experience
1993 - IRG/WP 93-50001-32
At the end of January 1993, a bill was put for Belgian Parliament related to the introduction called "Eco-taxes" on a series of products, such as packaging for drinks (especially on PVC-bottles), non-returnable articles (shavers, small cameras), batteries, pesticides for non-agricultural use and paper....
G Van Steertegem, F De Jaeger


The influence of previous anti-blue-stain preservative treatments on the fixation of CC in spruce
1997 - IRG/WP 97-30134
Freshly cut and kiln dried spruce boards were treated with 4 different anti-blue stain preservatives (ABP). After a period of 10 days allowing the samples to dry and fixate, the samples were treated with CC (chromium, copper formulation) using a vacuum pressure cycle. After impregnation the wood was steam fixed. A submersion leaching test showed differences in the leachable quantity of copper and ...
M Van der Zee, W J Homan


Effects of the anaerobic wood decay bacterium Clostridium xylanolyticum on unbleached Pinus and Eucalyptus pulp
1991 - IRG/WP 1506
Clostridium xylanolyticum has been shown to produce extracellular enzymes capable of degrading wood. The present work was conducted to quantify growth on various lignocellulosic substrates and degradation of pulped wood fibre. In the latter tests Clostridium xylanolyticum was incubated at 35°C under anaerobic conditions in a medium containing 0.2% (w/v) peptone and 4% (w/v) unbleached Pinus and E...
G D Shelver, U Matai, W Van Wyk, A A W Baecker


Report of Section 4 2003
2003 - IRG/WP 03-40269
J Van Acker


Some experiments with hexabutylditin against fungi
1977 - IRG/WP 388
The investigation was carried out in 1972 and 1973 to collect experimental data about the poisonousness of hexabutylditin (HBDT) against the woodrotting fungi Coniophora puteana (Coniophora cerebella), strain 15, and Chaetomium globosum, strain hexabutylditin was being manufactured by the Organisch Chemisch Instituut (O.C.I.) TNO, at Utrecht....
J W P T Van der Drift


LCA applied for wooden products
1995 - IRG/WP 95-50059
This paper presents some of the international developments within ISO and SETAC to standardize and harmonize LCA methodologies. In this framework it is also important to be aware of the problems that companies have to generate and validate data for the complete product chain from cradle to grave. This concerns problems in nomenclature of substances and processes, system boundaries, allocation prob...
A Kloppenburg, A Van Dam


Fipronil - le nouvel insecticide de Rhone Poulenc pour la preservation du bois
1995 - IRG/WP 95-30078
After the 3rd International Symposium in Cannes '95. More trial results and practical information on FIPRONIL, this new insecticide from Rhone Poulenc for Wood Preservation and PCO....
M G E J Van Maanen


Decay resistance of resin treated wood
1999 - IRG/WP 99-30206
Selected natural resin systems were evaluated for their potential as wood protecting agents according to standard test procedures. As indicated by the European standard EN 599 both a Basidiomycete test according to EN 113 and a ENV 807 soil bed test were carried out. Six resin treatments were tested using 3 concentration or treatment levels. Using the biocidal activity criteria as usually applied ...
J Van Acker, A J Nurmi, S M Gray, H Militz, C Hill, H Kokko, A O Rapp


An appraisal of methods for environmental testing of leachates from salt-treated wood (2)
1998 - IRG/WP 98-50110
For wood preservatives for use in hazard class 4 information on the ecotoxicity of preservatives and ingredients as well as on the effect of losses from impregnated timber is needed for a proper environmental risk assessment. In the evaluation of a suitable test procedure the leaching behaviour of copper-based formulations was studied using analytical and ecotoxicological test methodology. These ...
H W Wegen, A Platen, G M F Van Eetvelde, M Stevens


Effect of leaching temperature and water acidity on the loss of metal elements from CCA treated timber in aquatic conditions. Part 2: Semi-industrial investigation
1995 - IRG/WP 95-50040-13
In continuation of previous leaching research on the quantification and modelling of metal elements released from CCA treated timber, a series of experiments has been carried out dealing with the influence of temperature and pH of the relative aquatic environment. The leaching method used is the Dutch prestandard for building materials, a long term static leaching test simulating practical bank-sh...
G M F Van Eetvelde, W J Homan, H Militz, M Stevens


Reporting from SPC and Working Party sessions at IRG 45
2015 - IRG/WP 14-60375
J Van Acker


Effect of double-vacuum and vacuum-pressure impregnation with water-borne preservatives on the dimensional characteristics of spruce
1990 - IRG/WP 3613
Air-dried planed spruce (Picea abies) samples were treated with a water-borne preservative (micro-emulsion) and one oil-borne type both containing azaconazole and deltamethrin. Each set of samples contained equal number of specimens with different growth ring orientation, heartwood content and density. In addition to the preservative retention and the penetration of a.i., the swelling of the sampl...
J Van Acker, M Stevens, G Rustenburg


Thermotolerant mould growth in dehumidifier kilns in New Zealand
1996 - IRG/WP 96-10169
Growth of Aspergillus fumigatus and Paecilomyces variottii is common on wood dried in dehumidifier kilns that operate within a temperature range of 35-55°C. Aspergillus fumigatus causes an unacceptable blue / grey discolouration of the woods surface and prolonged exposure to spores during handling of mouldy wood can cause health problems amongst timber workers. A survey of dehumidifier kiln opera...
R N Wakeling, J G Van der Waals


Investigation into the heterogeneous nature of the impregnability of some poplar hybrids
1995 - IRG/WP 95-40052
Retention figures of some poplar hybrids are very heterogeneous when pressure impregnated. This makes it hard to prescribe impregnation processes for fast grown poplars that make it suitable for higher hazard uses. In order to gain fundamental knowledge in their variability in impregnation properties two trees were selected for a detailed investigation. Both trees originate from the same plantatio...
J Van Acker, M Stevens


Statistically stable models for determination of PEC
1999 - IRG/WP 99-50135
In June 1998 the European Wood Preservative Manufacturer's Group prepared a document to support the Technical Guidance concerning the placing of products on the market with respect to the Directive 98/08/EC (BPD). The essentials of this document were presented at the COST E2 meeting in Cannes last year and at the following IRG conference (Baines and Davis, 1998; IRG/WP/98-50101/20). The d...
W J Homan, A L Van Oosten Van


Current models used by the European Health Authorities to evaluate the volatilization of active ingredients from treated wood used inside dwellings. A case study: Volatilization of azaconazole and propiconazole from treated wood
1990 - IRG/WP 3565
The use of wood preservatives inside houses may result in measurable aerial concentrations of active ingredients. These airborne contaminants may be inhaled by the inhabitants over periods lasting from a couple of days to several months. To assess the potential health hazard of preservative residues in the air, various risk-assessment models have been worked out. Three schemes, currently used by t...
A R Valcke, L Van Leemput


Decay resistance of high performance biocomposites based on chemically modified fibres
1998 - IRG/WP 98-40120
Different partners within the framework of a European research project produced high performance biocomposites aiming at the utilisation of board materials as durable products both in dimensional and biological degrading circumstances. This paper summarises test data, which indicate the potential of board materials produced with modified fibre material. The chemical modifications applied cover a r...
V Rijckaert, J Van Acker, M Stevens


Laboratory experiments on aerial emissions from wood treated with wood stains
1993 - IRG/WP 93-50001-06
Due to the actual environmental interest in wood preservation, a series of experiments was carried out on the emission of biocides from treated wood. The research focussed on the volatilization of 5 biocides from boards treated with wood preservative finishes containing dichlofluanide (DCF) azaconazole (AZA), pentachlorphenol (PCP), iodopropynylbuthylcarbamate (IPCB) and tributhyltinoxide (TBTO). ...
G M F Van Eetvelde, M Stevens


Criteria for basidiomycetes testing and ways of defining natural durability classes
1998 - IRG/WP 98-20144
Within the framework of a European research project several laboratories have tested a series of 17 wood species covering the total range of natural durability. Basidiomycete tests are part of the total set up. Although generally based upon standard methods some minor differences in execution of the tests were evaluated for their impact on the results. This variation was superimposed with the fac...
J Van Acker, M Stevens, J K Carey, R Sierra-Alvarez, H Militz, I Le Bayon, G Kleist, R-D Peek


Effect of wood moisture on ability of Sphaeropsis sapinea to colonise Pinus radiata
1999 - IRG/WP 99-10311
The factors influencing colonisation of unseasoned radiata pine logs by sapstaining fungi which can result in detrimental wood discolouration, are being explored. The objective of the current study was to determine the effect of wood moisture content on fungal growth and wood colouration (melanisation). Five replicate trials were set up using increment cores (10mm diameter) which were taken from ...
B Kreber, D R Eden, R N Wakeling, C M Chittenden, J G Van der Waals, B Carpenter


Highly virulent wood-rotting Basidiomycetes in cooling tower timbers
1995 - IRG/WP 95-10125
Over the past ten years most industrial cooling towers changed their water treatment systems in order to meet environmental requirements. Since this alterations wood rot attack has been reported more frequently. Several Basidiomycete fungi were isolated and determined. Amongst the most important ones are strains of Physisporinus vitreus (Pers.:Fr.) P. Karst., Phellinus contiguus (Fr.) Pat. and Don...
J Van Acker, M Stevens, V Rijckaert


The use of TCMTB in applications other than sapstain prevention: A review
1990 - IRG/WP 3606
The efficacy of TCMTB against staining fungi and surface moulds has been thoroughly investigated during the last decade. As a result, the chemical is used as an alternative to the chlorinated phenols in various parts of the world for the preservation of freshly sawn timber. Less known are the data obtained against brown rot, white rot and soft rot fungi. The termite repellent and bactericidal prop...
R Van der Eynde


Fluoride woodpill
1987 - IRG/WP 3431
Decay problems of spruce joinery in the Netherlands in the 1960's and 1970's led to the introduction of preservative treatment. Because of the known penetration difficulties with Spruce, the results of the treatments were not always successful. The fact that the decay was found only in the joints led to development of the philosophy of "local preservation" of the joints in remedi...
J W P T Van der Drift, K J M Bonsen


Evaluating the potential of modified wood for use in marine environments using a short-term laboratory bioassay
2004 - IRG/WP 04-10525
Chemically modified wood may be an alternative to preservative treated timber for marine structures. In this study a screening laboratory test using the wood-boring isopod crustacean Limnoria quadripunctata was used to assess the durability of chemically modified Pinus sylvestris, Pinus radiata and Picea sp. Most of the treatments used a combination of one of two of types of the resin dimethyloldi...
L M S Borges, S M Cragg, M van der Zee


Blue stain resistance of exterior wood coatings as a function of their typology
1998 - IRG/WP 98-20145
Paints and wood stains were evaluated on their blue stain resistance using both EN 152 method and the reverse method. The typology of these exterior coatings was varied including standard and high solid solvent-borne coatings as well as different types of waterborne coatings. For the water-borne acrylic, alkyd based and hybrid coatings both applied as opaque primer paints and as decorative wood st...
J Van Acker, M Stevens, C Brauwers, V Rijckaert, E Mol


Previous Page | Next Page