IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 174 documents. Displaying 25 entries per page.


Evaluating the potential of modified wood for use in marine environments using a short-term laboratory bioassay
2004 - IRG/WP 04-10525
Chemically modified wood may be an alternative to preservative treated timber for marine structures. In this study a screening laboratory test using the wood-boring isopod crustacean Limnoria quadripunctata was used to assess the durability of chemically modified Pinus sylvestris, Pinus radiata and Picea sp. Most of the treatments used a combination of one of two of types of the resin dimethyloldi...
L M S Borges, S M Cragg, M van der Zee


Blue stain resistance of exterior wood coatings as a function of their typology
1998 - IRG/WP 98-20145
Paints and wood stains were evaluated on their blue stain resistance using both EN 152 method and the reverse method. The typology of these exterior coatings was varied including standard and high solid solvent-borne coatings as well as different types of waterborne coatings. For the water-borne acrylic, alkyd based and hybrid coatings both applied as opaque primer paints and as decorative wood st...
J Van Acker, M Stevens, C Brauwers, V Rijckaert, E Mol


Modelling the control of decay in freshly felled pine poles
1997 - IRG/WP 97-10206
In a recent study investigating control of decay in freshly felled pine utility poles, it became apparent that the efficacy of different treatment methods was strongly related to the size of the material being treated. A topical application of 5% w/v disodium octaborate tetrahydrate (DOT), brush applied to the cut surfaces of logs with otherwise intact bark was just as effective at excluding white...
M W Schoeman, W Van der Werf, J F Webber, D J Dickinson


Xenon simulation of natural weathering of external joinery preserving - Finishing systems
1992 - IRG/WP 92-2412
Semitransparent wood stains ('lazures') for external joinery have developed by means of product combination towards complete wood finishing systems that are easy to applicate, have a good weathering resistance and low maintenance cost. The search for enhanced formulations and the possibilities to standardize these products or treatment systems are always facing long periods of we...
J Van Acker, M Stevens, M Nys


Environmental risk assessment of treated timber in service: The Environment Focus Group approach
2000 - IRG/WP 00-50162
In the context of the Biocidal Products Directive (98/8/EC), and of the OECD work on wood preservatives, the Environment Focus Group (EFG), comprising 8 institutes and the European Wood Preservative Manufacturers Group, has been working on the environmental risk assessment of treated timber in service. A literature review of emissions from treated timber has revealed that very little existing data...
G Deroubaix, G Labat, I Le Bayon, S Legay, P Marchal, C Yrieix, E Melcher, R-D Peek, S De Geyter, J Van Acker, W J Homan, D J Dickinson, R J Murphy, E D Suttie, A J Nurmi, A-C Ritschkoff, D Rudolph, I Stephan, D Aston, E F Baines, J B Simonin


The efficacy of Sentry® as a treatment for the control of sapstain in pre-infected radiata pine
2001 - IRG/WP 01-30260
Experiments were conducted to determine the efficacy of Sentry® when used to control sapstain fungi on radiata pine branch billets stored under high fungal hazard conditions. Prior to antisapstain treatment, the billets were pre-infected with a mixed inoculum of staining fungi and held from zero to 10 days at 25°C and 75% relative humidity. This was done to produce billets with different degrees...
C Chittenden, J G van der Waals, B Kreber, R N Wakeling


Probing red maple pit membrane pore size at FSP and OD using polystyrene macromolecules
2001 - IRG/WP 01-40217
A modified solute exclusion technique was used to pressure impregnate a polystyrene molecular weight (MW) series dissolved in styrene into red maple samples at approximately the fiber saturation point (FSP) and oven dry (OD). Radial penetration was less than tangential and FSP less than OD. There was a marked penetration change with MW in the tangential direction, although there appeared to be a ...
A Omidvar, M H Schneider, A R P Van Heiningen


Comparative study on leaching of CCA from treated timber: Modelling of emission data
1994 - IRG/WP 94-50027
Results of a comparative study on leaching of CCA from treated timber are reported. The study aims at investigating the applicability of prestandard leaching test methods for modelling purposes. Prestandards used are the European standard proposed by CEN/TC38/WG11 and NEN 7345 (Dutch prestandard for building materials). Parameters of study are type of fixation, wood species (pine - spruce), specim...
G M F Van Eetvelde, M Stevens, L Van der Mijnsbrugge


Sentry®, a new antisapstain formulation for protecting logs and lumber. - Part 2: protection of lumber
1999 - IRG/WP 99-30189
Recent research conducted by Forest Research, Chemcolour Industries (NZ) Ltd. and Fletcher Challenge Forest Ltd. has resulted in the development of antisapstain formulations that meet the efficacy requirements of the New Zealand Forest industry for export logs. One treatment, called Sentry®, is now poised for commercial use in New Zealand for treating export logs, having undergone an extensive su...
R N Wakeling, D R Eden, C M Chittenden, J G Van der Waals, B Carpenter, I Dorset, R Kuluz, J Wakeman


Influence of concentration, catalyst, and temperature on dimensional stability of DMDHEU modified scots pine
1998 - IRG/WP 98-40119
Dimethyloldihydroxyethyleneurea (DMDHEU) is being used in textile industry to improve wrinkle recovery. Trials on solid wood have been performed to minimise swelling of the wood. This paper focuses on the effect of various types and concentrations of catalyst and reaction temperature on the dimensional stability of Scots pine. Three different catalysts, NKS (based on magnesium chloride), 3282 (bas...
M Van der Zee, E P J Beckers, H Militz


Modified Wood – Methods, testing and applications: Outcomes of the EU-Thematic Network
2003 - IRG/WP 03-40268
In the last decade, interest in the development of wood modification systems has increased in Europe. Alongside several industrial initiatives for heat treatments, there have also been scaling up and pilot plant projects for chemical wood modification. Between 2000 and 2003, the European Commission funded the "Thematic Network on Wood Modification". This paper will feature the modification process...
D Jones, W Homan, J Van Acker


An appraisal of methods for environmental testing of leachates from salt-treated wood; part 1
1998 - IRG/WP 98-50115
The magnitude and diversity of leaching tests with salt-treated wood, performed by institutes as well as industry, strongly appeal for harmonisation towards one single method. That procedure should be well-defined, cost- and time-effective and moreover be extended with a clear detection and interpretation scheme. The paper(s) presented here tend to evaluate 2 existing leaching methods, the ENV 12...
G M F Van Eetvelde, M Stevens, F Mahieu, H-W Wegen, A Platen


Occupant re-entry times following insecticidal remedial treatments of timber in dwellings
1995 - IRG/WP 95-50055
This work was carried out principally to obtain quantitative data on the aerial concentrations of permethrin and white spirit likely to arise following the remedial treatment of timber in buildings, using insecticidal formulations. Such data are needed to allow assessments to be made of the length of time buildings should remain unoccupied following such treatments prior to re-occupation, and the ...
R J Orsler, G E Holland, G M F Van Eetvelde


Effect of treating process on efficacy of CCA in a laboratory decay test
1990 - IRG/WP 3628
Test samples of Pinus radiata sapwood measuring 40x40x500 mm³ were treated with a range of concentrations of the copper-chrome-arsenate (CCA) formulation "Tanalith C" using Rueping (empty cell), Lowry (empty cell) and Bethell (full cell) treatment processes. Samples were then reduced to 40x40x7 mm³ test blocks and exposed to the decay fungus Coniophora puteana using an agar/block technique. Repl...
M E Hedley, K Nasheri, J G Van der Waals


Environmental fate of copper-based wood preservatives in different soil substrates - Part 2: Study of the metal sorption and migration potential under simulated rainfall
1998 - IRG/WP 98-50101-21 b
In order to examine the potential environmental impact of spillages of the saltborne wood preservative CCA in treatment plants, four large scale experiments are set-up so as to follow the water transport and ion mobility in various field soils. A plastic container is filled with a sand, silt, clay and potting soil, made up at their respective bulk density and wetted to a given moisture content. U...
G M F Van Eetvelde, R Hartmann, J M Mwangi, H S Öztürk, M Stevens


FIPRONIL - une nouvelle molécule insecticide Rhône Poulenc pou le PCO et la protection du bois [FIPRONIL - A new insecticide from Rhône Poulenc for PCO and wood preservation]
1995 - IRG/WP 95-50040-16
We will explain here after the advantages and key points of the new insecticide "FIPRONIL" from Rhône Poulenc Agrochemicals. We will have a look from the physical and chemical properties to the possible uses in PCO and wood preservation, including toxicology, efficacy and the main beneficial impacts on the environment. FIPRONIL, a new solution against undesirable and damageable insects, from cock...
M G E J Van Maanen


Field performance of novel antisapstain formulations
1997 - IRG/WP 97-30125
The effectiveness as antisapstain formulations of combinations of oxine copper (Cu-8), carbendazim, hexaconazole, cyproconazole, flusilazole, didecyldimethyl ammonium chloride (DDAC), an alkanolamine borate (SB), benzalkonium chloride (BAC), 2-n-octylisothiazolin -3-one (isothiazoline) and p-chlorophenyl-3-iodopropagilformal (CPIPF) was determined for freshly sawn, block-stacked radiata pine in th...
D R Eden, R N Wakeling, C M Chittenden, J G Van der Waals


Influence of clonal variability on the impregnability of poplar hybrids. (+ correction document of 23 April 1990)
1990 - IRG/WP 3614
The new Western European poplar clones (Populus nigra x deltoides and Populus trichocarpa x deltoides) were compared with the reference clone 'Robusta' and some old hybrids. Samples (5x5x50 cm³) with pure tangential/radial surfaces were sawn, including the transition zone between heartwood and sapwood. Treatment by a standard vacuum-pressure impregnation cycle with CCA showed a ...
J Van Acker Van, M Stevens, C De Haas


Qualifying ecotoxicity research on tropical hardwood leachates
1997 - IRG/WP 97-50096
Almost as a rule, quantification and identification of various types of environmental contamination is grounded on chemical evaluation principles. Yet for monitoring surface water pollution, aquatic bio-assays may provide a more direct way to assess the potential hazard of environmental samples. A battery of such tests is experienced onto leachates of tropical hardwoods used in ground and water co...
G M F Van Eetvelde, P Marchal, M Stevens


Evaluation of the european standard ENV 12038 for durability testing of plywood
2001 - IRG/WP 01-20237
The latest improved version of the standard ENV 12038 drafted as document N44 by CEN Technical Committee 38 (WG 7 - WG 23) is used to evaluate the effect of wood composition and structure on plywood durability. The method described is based on the agar-block test of the EN 113 standard used for the determination of the efficacy of wood preservatives and the assessment of the natural durability of ...
J Van Acker, M Stevens, E De Clercq


The WOODCARE project: Development of detection methods for Death watch beetle larvae and fungal decay
1999 - IRG/WP 99-20172
Woodcare was a European project coordinated by English Heritage. The aim of the research was to develop more targeted and more environmentally friendly treatment methods for Death watch beetle infections in Oak constructions of historical buildings. TNO has developed two new methods for fast and reliable detection of Death watch beetle larvae and related fungal decay in Oak. The problem with Death...
P Esser, P Van Staalduinen, A C Tas


Treatment of poplar plywood with solvent and water-borne preservatives
1989 - IRG/WP 3538
Poplar as a light hardwood is appropriate for plywood production. Owing to its low natural durability it is generally recommended to preserve it in all conditions where risks of fungal attack may be present. A research project has been carried out on preservative treatments of plywood commodities. Parameters studied were various treatment cycles, three types of plywood, and a number of solvent and...
J Van Acker, M Stevens


Laboratory testing of wood natural durability - In soil-bed assays
1998 - IRG/WP 98-20141
Laboratory methods for assessing wood decay resistance are being investigated in the framework of an ongoing European research project. This paper summarizes the main results obtained for soil-bed tests based on the European prestandard ENV 807-Test 2. The data suggest that this testing methodology is suitable for evaluating the natural durability of timber species in soil-contact under conditions...
R Sierra-Alvarez, I Le Bayon, J K Carey, I Stephan, J Van Acker, M Grinda, G Kleist, H Militz, R-D Peek


Is laboratory testing of decay resistance questionable as a single criterion for natural durability?
1996 - IRG/WP 96-20096
In a laboratory test set up over 20 hardwood species were evaluated according to the European Standard EN 350-1 including Basidiomycete and soft rot testing. Half of the species used were of a known natural durability. The Basidiomycete testing was carried out using Coriolus versicolor, Gloeophyllum trabeum and Coniophora puteana in a malt agar test similar to EN 113. From this test it was not pos...
J Van Acker, M Stevens, T Van Cauwenberghe, T Seynaeve


The effect of pretreatments on the impregnation of air-dried sawn Belgian spruce
1988 - IRG/WP 3490
In general the impregnation of airdried spruce results in a variable treatment and limited penetration. This is the result of pit aspiration that occurs during drying of the spruce sapwood and heartwood. Spruce timber is becoming of greater importance in Belgium and hence research for better treatment of this vulnerable wood species is needed. Squared airdried timber of different dimensions were e...
J Van Acker, M Stevens


Previous Page | Next Page