IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 474 documents. Displaying 25 entries per page.


Analysis of degradation observed on ancient wooden objects buried underground
2001 - IRG/WP 01-10403
Ancient wooden objects were sometimes excavated from the moat of mounded tombs in Japan. Such wooden objects were in the shape of a sunshade, bird, shield, pole, yugi(a bag that holds arrows) among others. Archaeologists discussed the usage of such shaped objects, but no one could clearly explain their use. Some objects were observed using an ordinary microscope. Deterioration by bacteria was foun...
H Sakai


Termite-tunnels formation on the surface of termite-resistant wood species in field sites
2001 - IRG/WP 01-10400
In this report, termite-tunnels formation by the subterranean termite, Coptotermes formosanus Shiraki on the surface of termite-resistant wood species, namely, Hinoki (Chamaecyparis abtsu), Yoshino Hinoki (Chamaecyparis abtsu), Miyazaki Hinoki (Chamaecyparis abtsu), Hiba (Chamaecyparis abtsu) and Japanese cedar (Cryptomeria japonica) was conducted in field sites. Westernhemlock (Tsuga heterophylla...
Y Kadekaru, K Kinjo, S Yaga


Efficacies of an insecticide and a fungicide for preventing blue-stain of Japanese red pine logs
2006 - IRG/WP 06-20329
We examined blue-stain fungi on Japanese red pine at 3 forests and 2 saw mills in Iwate Prefecture, Japan. The isolated ophiostomatoid fungi were Leptographium sp and Ophiostoma sp. There were 3 routes of the blue-stain; fungal growth from the spore or hypha stuck on the cross cut surfaces, fungal spread through the inner bark by bark beetles and fungal invasion around whorled knot. The larger ext...
H Taniuchi, T Koiwa, H Masuya, S Doi


Efficacies of physical barriers for preventing blue-stain of Japanese red pine logs
2007 - IRG/WP 07-20359
This paper deals with field trials on physical barriers to prevent blue stain on Japanese red pine logs using a fly screen, bark and leaves of Japanese cedar as covering materials. These barriers arrested blue stain and bark beetle attacks to low levels than control for 1 month except covering with a small amount of bark. Covering with the fly screen and a large amount of bark permissibly suppress...
H Taniuchi, T Koiwa, H Masuya, S Doi


Confocal laser scanning microscopy of a novel decay in preservative treated radiata pine in wet acidic soils
1997 - IRG/WP 97-10215
Light microscopy of radiata pine (Pinus radiata D. Don) field test stakes (20x20x500mm3) exposed in wet acidic (pH 3-4) soil for 12 - 24 months showed predominance of an unusual type of decay characte-rised by tunnelling attack of wood cell walls. After two years decay was moderate to severe in wood treated to ground contact CCA specifications and also equivalent retentions of creosote, and a numb...
R N Wakeling, Ying Xiao, A P Singh


Field trial with poles of Scots pine treated with six different creosotes
1996 - IRG/WP 96-30115
In the middle of the 50's field trials with creosote-treated poles were started in France, Germany and Sweden. The trials were initiated by WEI (Western-European Institute for Wood Preservation). Six different creosotes were used and 40 poles per creosote were installed at each test field. Results after 39 years of exposure in Simlangsdalen, Sweden are reported. Poles treated with a heavy...
Ö Bergman


Screening potential preservatives against stain and mould fungi on pine timber in Zimbabwe
1995 - IRG/WP 95-30063
The search for environmentally and toxicologically safer chemicals for use in the timber preservative industry against stain and mould fungi has been intensified during the past few years. Results of field tests with two chemicals previously evaluated in the laboratory are presented. The conventional sodium pentachlorophenate was the more efficacious chemical against stain and mould fungi, providi...
A J Masuka


Moisture content levels and decay of hemlock
1986 - IRG/WP 1287
As a model of decay conditions of wooden members in wooden houses, a decay test was set up in which samples of western hemlock (Tsuga heterophylla) under 4 moisture levels were examined. Each week the samples were weighed and if the weights indicated that their moisture contents were lower than the expected levels, distilled water was added. Every 8 weeks 3 samples from each condition were oven dr...
K Suzuki


Strength loss associated with steam conditioning and boron treatment of radiata pine framing
1987 - IRG/WP 3438
The combined effect of included defects and wood moisture content on the strength loss of second rotation radiata pine framing following conventional steam conditioning is investigated. The green Modulus of Elasticity (MOE) is reduced by approximately 13% after steaming. When dried after steaming, however, neither the MOE nor MOR is significantly different from unsteamed dried controls....
M J Collins, P Vinden


Soil virulence tests using Scots pine sapwood
1973 - IRG/WP 222
Following the tests reported in Document No: IRG/WP/210, in which soils from different laboratories were investigated for virulence, supplementary tests have been carried out using Scots pine sapwood and an extended incubation period....
J K Carey, J G Savory


Types of decay observed in CCA-treated pine posts in horticultural situations in New Zealand
1984 - IRG/WP 1226
The few reported failures of 11-12-year-old horticultural posts in New Zealand in 1982 were caused by brown-rot. A subsequent survey of CCA-treated posts in all the major horticultural areas has revealed decay of many posts. A microscopic examination of these posts has shown decay by brown-rot, white-rot, soft-rot and bacteria. Several types of bacterial decay have been observed....
J A Drysdale, M E Hedley


Light organic solvent preservative treatment schedules for New Zealand-grown radiata pine
1986 - IRG/WP 3379
The influence of pressure differential and treatment time on preservative uptake and distribution in radiata pine heartwood and sapwood is investigated. Treatment schedules are defined which minimise solvent usage but ensure complete sapwood penetration and optimise heartwood penetration....
P Vinden


Dimensional stability and decay resistance of hot-melt self-bonded particleboard by surface benzylated pine chips
1991 - IRG/WP 3652
Akamatsu (Pinus densiflora Sieb. et Zucc: Japanese red pine) particles were pretreated with 40% NaOH solution and benzylated with benzyl chloride, and the surface of particle was converted into meltable materials. Hot-melt self bonded particleboard having smooth and high glossiness surface was prepared by hot pressing at 150°C and 1.96 MPa without using any conventional adhesives. Dimensional sta...
M Kiguchi, K Yamamoto


Termite resistance of pine wood treated with chromated copper arsenates
1997 - IRG/WP 97-30128
Two four-week, no-choice laboratory tests were performed with CCA-treated southern yellow pine and radiata pine against Formosan subterranean termites, Coptotermes formosanus. CCA retentions as low as 0.05 kg/m3 (0.03 pcf) provided protection from all but light termite attack (rating of 9 on a 10-point visual scale). Similar and consistent light attack on wafers containing retentions as high as 6....
J K Grace


Durability of pine modified by 9 different methods
2004 - IRG/WP 04-40288
The decay resistance was studied for pine modified by nine methods of wood modification: 1) Acetylation, 2) Treatment with methylated melamine resin (MMF), 3) Acetylation followed by post-treatment with MMF-resin, 4) Thermal modification, 5) Furfurylation, 6) Maleoylation (using water solution of MG or ethanol solution of maleic anhydride), 7) Succinylation, 8) NMA-modification and 9) modification...
M Westin, A O Rapp, T Nilsson


Performance of Tebbacop in laboratory, fungus cellar and field tests
2000 - IRG/WP 00-30222
A novel organo-copper wood preservative ("Tebbacop") has been exposed to 12 years fungus cellar testing and 6 years above ground field testing. In the fungus cellar, Tebbacop at a retention of 0.053% Cu m/m oven dry wood out-performed CCA at a retention of 0.55% m/m oven dry wood. In above ground tests, L-joints treated to a Tebbacop retention of 0.012% Cu are performing as well as joints treated ...
M E Hedley, D R Page, B E Patterson


Creosoted radiata pine by non-pressure methods
1988 - IRG/WP 3486
Posts of Pinus radiata have been impregnated with creosote by immersion for 1, 3, and 7 days, and by hot-and-cold open tank with hot bath temperatures at 40°C and 60°C. On the basis of the retention rates obtained, suitable procedures are described for wood elements that are going to be in ground contact, and an analysis is made of the way in which the variables tested affect the results....
M V Baonza Merino, C De Arana Moncada


Light organic solvent preservative treatment of glue-laminated radiata pine
1986 - IRG/WP 3380
The high permeability of radiata pine (Pinus radiata D. Don) is associated with ray-tissue and in particular the cross-field pits linking ray-tissue to tracheids. This pathway is absent in the tangential grain direction, leading to poor preservative penetration when treatment is restricted to the radial face - for example, timber fabricated into glue-laminated beams....
P Vinden


Dimensional stabilization of wood with dimethylol compounds
1987 - IRG/WP 3412
This study showed that a substantial degree of dimensional stability can be imparted to wood by crosslinking with low concentrations of dimethyloldihydroxyethyleneurea. It was demonstrated that by selecting the right catalyst system the cure temperature can be reduced to the point that strength loss of the treated wood is minimized....
D D Nicholas, A D Williams


Steam conditioning of partially dried radiata and Corsican pine roundwood
1988 - IRG/WP 3499
The effect of partial air drying prior to steam conditioning and its effect on subsequent preservative treatment by the Bethell treatment process was investigated. A high standard of preservative treatment was obtained in both radiata and Corsican pine, irrespective of whether a period of partial drying was imposed before or after steam conditioning....
P Vinden, D R Page, K Nasheri


Japanese wood preserving industry
1990 - IRG/WP 3596
Although a great amount of wood is in use in Japan, a little attention has been paid to the significance and importance of wood preservation. The fact reflects that only less than 0.5% of the total wood consumption is treated with wood preservatives today in the country. Over the 20 years before 1970, the annual volume of preservative treated (pressure treatment) wood was relatively at a stable le...
K Tsunoda


Leaching of copper, chromium and arsenic from CCA-treated Scots pine exposed in sea water
2000 - IRG/WP 00-50149
A laboratory leaching trial combining a static and a flowing seawater system was carried out to measure the leaching rates of copper, chromium and arsenic from the surface of Scots pine panels vacuum-pressure treated to 3, 6, 12, 24, and 48 kgm-3 CCA. Untreated and treated panels were exposed in flowing seawater for up to 8 weeks followed by 2 weeks submersion in static seawater which was taken fo...
C J Brown, R A Eaton


The effect of treatment method on CCA efficacy in Corsican pine
1992 - IRG/WP 92-3723
As part of a study into the influence of application method on preservative efficacy Corsican pine (Pinus nigra) samples (50 x 50 x 400 mm³) were treated with a CCA formulation using Bethel, Steam/Bethel or Lowry processes. Full penetration of the preservative at a gross level was confirmed using a copper disclosing reagent. The preservative was allowed to fix and then samples were converted into...
P R Newman, R J Murphy


Movement of boron from fused boron rods implanted in Southern pine, Douglas fir, red oak, and white oak timbers
1995 - IRG/WP 95-30061
This paper reports the distribution of boron from fused boron rods installed into six-inch (15.2 cm) square timbers of Douglas-fir, Southern Pine, red oak and white oak exposed aboveground. The composition and size of rods was: sodium borate and sodium borate-copper oxide (8.5 x 100 mm²); sodium borate-copper, sodium borate and boric oxide-copper oxide (12 x 76 mm²). The boric acid equivalent wa...
T L Highley, L Ferge


Study of the natural durability and impregnability of a metropolitan species of tree
1986 - IRG/WP 2261
The current and predictable evolution of construction timber supply conditions is motivating research for a more efficient utilization of native woods. It is now important to determine statistically reliable impregnability values on a national scale, and to evaluate the natural durability of woods recently introduced in France, or economically important native woods....
M E Mathieu


Next Page