IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 692 documents. Displaying 25 entries per page.


Application of roller-pressing method to the novel liquid impregnation treatment of green timber
2001 - IRG/WP 01-40198
A transverse compression technique enabled us to impregnate liquid into green timber through replacement of the free water in the timber with a treatment liquid without any critical physical damage to the timber by the roller-pressing method. The roller-pressing is supposed to remove free water the cell cavities and to concurrently introduce the treatment solution into green timber in the treatmen...
M Inoue, K Adachi, K Tsunoda, Y Imamura, S Kawai


Environmental characterisation of retification process by-products (liquid and gaseous wastes)
2005 - IRG/WP 05-50224-10
In order to reduce environmental risks during the service life of the treated wood and to find new alternative developments on the durability of wood, some research and technology development have been made on thermal treatment. The retification process is one of these processes. The retification process induces chemical modification of the lignin and cellulosic components and modifies the intrins...
G Labat, E Bucket, S Legay, C Yriex, P Marchal, E Raphalen, M Vernois, R Guyonnet, H Besset, E Fredon), G Vilarem, L Rigal, C Raynaud


"XYLOPHENE ANTI-TERMITES" :A complete range of treatment products against termites
2000 - IRG/WP 00-30230
Dyrup-Xylochimie purpose for several years efficient treatment products for timber and wood materials, with its trade mark : "Xylophèn". As everybody know, termites become an important problem for construction in France. So important that, a national law was voted in May 1999, to define areas where termites are present, in order to protect future landowner. To prevent efficiently termites damages...
L Cubizolles, E Wozniak


The effect of an ionic liquid of imidazolium tetrafluoroborates series on Scots pine wood properties
2007 - IRG/WP 07-40357
Ionic liquids (ILs) of imidazolium tetrafluoroborates series penetrate Scots pine wood very well and are active against wood destroying fungi. The requirement to use ILs as wood preservatives is determined by the liquid influence on the functional properties of wood. Investigations were undertaken to clarify the influence of an ionic liquid, 3-heptyloxymethyl-1-methylimidazolium tetrafluoroborate ...
A Fojutowski, R Szukala, J Pernak


Superhydrophobic treatment of Norway spruce wood for improvement of its resistance against brown rot and moulds
2016 - IRG/WP 16-40734
Water repellence of wood can be increased and its some other properties influenced by introduction of hydrophobic chemicals into and on cell walls without affecting the wood’s bulk density due to lumen filling. Herein, a simple dipping method to insert octadecyltrichlorosilane (OTS) into cell walls and to deposit the self-assembled hydrophobic monolayers (SAMs) of OTS is reported. It was found o...
A Kumar, P Ryparová, P Hajek, B Kričej, M Pavlič, A S Škapin, M Šernek, J Tywoniak, J Žigon, M Petrič


Proposal for further work on accelerated ageing
1988 - IRG/WP 2314
M-L Edlund


Status of the research and development of a new preservative system (EFPL) for pressure treatment of spruce in Canada
1975 - IRG/WP 348
Our work has been to develop a system which would have the stability of the ACA system and the formulation flexibility of the CCA system enabling properties such as fixation of arsenic, water repellency, appearance and cost to be controlled. Our permeability studies of spruce using a method previously developed indicated that an ammoniacal solution of copper arsenate is an excellent candidate for ...
J Rak, M R Clarke


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 2: Report of treatment and installation in Australia
1978 - IRG/WP 440
The purpose of this test and the procedures to be followed have been fully set out in documents distributed by the International Research Group on Wood Preservation and numbered IRG/WP/414 and IRG/WP/420. The prescriptions set out in these two documents have been closely followed....
J Beesley


Field test evaluation of preservatives and treatment methods for fence posts
1985 - IRG/WP 3347
This work presents the field test results after fifteen years exposure of Eucalyptus saligna fence posts treated with six different preservatives and five treatment methods. All the combinations with oil-borne preservatives presented the best results and among the waterborne preservatives, the fence posts treated by immersion method were with the lowest performance in the field test....
G A C Lopez, E S Lepage


Manual of a mini treating plant for waterborne preservative treatment of timber and bamboo
1999 - IRG/WP 99-40130
This contributional article includes machinaries and equipments necessary for a small wood treating plant for the pressure treatment of tim bers with waterborne preservatives along with the cost and design. The preservative treatment limitations, treatment schedules and specifications for different products have been described. The cost of a mini treating plant will be 6,00,000 Tk. (13,000 US$), s...
A K Lahiry


Blue stain in service on wood surface coatings. Part 3: The nutritional capability of Aureobasidium pullulans compared to other fungi commonly isolated from wood surface coatings
1993 - IRG/WP 93-10035
The nutritional capability of Aureobasidium pullulans was previously examined, using agar plate tests, with regard to nutrient sources that are potentially available in fresh and weathered wood (Sharpe and Dickinson, 1992). This study compared these findings with the nutritional capability of four other fungi (Alternaria sp., Cladosporium cladosporoides, Stemphylium sp. and Trichoderma sp.) common...
P R Sharpe, D J Dickinson


Strength loss associated with steam conditioning and boron treatment of radiata pine framing
1987 - IRG/WP 3438
The combined effect of included defects and wood moisture content on the strength loss of second rotation radiata pine framing following conventional steam conditioning is investigated. The green Modulus of Elasticity (MOE) is reduced by approximately 13% after steaming. When dried after steaming, however, neither the MOE nor MOR is significantly different from unsteamed dried controls....
M J Collins, P Vinden


Soft rot penetration - Effect of groundline maintenance treatment on poles in sevice
1983 - IRG/WP 3263
R S Johnstone


Improved techniques designed for evaluation of fungicides in soil for control of dry rot fungus Serpula lacrymans
1985 - IRG/WP 2238
Improved techniques provide a laboratory method for the evaluation of chemicals in soil for control of dry rot fungus Serpula lacrymans. Results with their application to three chemicals were reported. These techniques are useful to eliminate chemicals lacking the necessary toxicity and weatherbility for dry rot control when the chemicals have been applied to the soil....
M Takahashi, K Nishimoto


Thermal treatment of wood: European Processes and their background
2002 - IRG/WP 02-40241
Recent efforts on thermal treatment of wood lead to the development of several processes introduced to the European market during the last few years. The total production capacity of heat treated wood in 2001 is estimated as approx. 165.000 m3. In the paper the different heat processes are presented. The general technology as well as scientific data on the chemical transformation of the cell wall ...
H Militz


How to Document the Performance of Super-Critical Treated Wood in above Ground Situations?
2005 - IRG/WP 05-20316
The paper presents practical experiences from the preparation of a new preservative treated wood product for introduction to the market. The product in question is Superwood™, which is treated with organic biocides using CO2 in a supercritical state as a solvent. The question is how to evaluate the performance of a new product such as Superwood™ in order to get an acceptance on the market a...
N Morsing, A H H Wong, F Imsgard, O Henriksen


Comparison of cubic and plug samples for preparation and data assembly in permeability study
2000 - IRG/WP 00-20197
In order to determine if plug experimental samples (PES: 30 x 15 mm2 diameter) could be used for inspection of wood permeability characteristics, radial and longitudinal flow directions were prepared according to either PES or cubic experimental samples (CES: 100 x 20 x 20 mm3) from the sapwood zone of Sitka spruce and treated by tanalith-C according to full-cell process. Results from the two prep...
I Usta


The dry rot fungus Serpula lacrymans. Examples of attack and remedial treatment
1988 - IRG/WP 1347
The film deals with several aspects of dry rot attack and eradication in buildings. The detailed biology and morphological charasteristics of the fungus are portrayed. The various forms of mycelial growth, the role of the strands in the nourishment and spread of the fungus, as well as the many types of fruitbody formation are outlined. Environmental and nutritional requirements of the fungus as we...
G Buchwald, B M Hegarty, W Metzner, R Pospischil, H Siegmund, P Grabow


Improved equipment and technique for high pressure sap displacement impregnation of natural round wood
1972 - IRG/WP 309
Hitherto the main problem in the practical application of high pressure sap displacement impregnation (HPSD) has been in devising a satisfactory cap. Such a cap must be easily fitted to different size log ends to give a leak proof seal. The present contribution describes a new type of cap and sealing system designed to meet these requirements....
C G W Mason, F B Shorland


Treatment of fresh green round bamboos culms (Dendrocalamus strictus) by sap-displacement (wick) method
2005 - IRG/WP 05-40311
Sap displacement method has great potential for treating short length bamboos as it does not require any technical equipment. The process is simple and large nos. of bamboos can be simultaneously treated in relatively short period. There is no wastage of chemicals as the remnant solution reused. Bottom ends and middle portion had better treatment in compared to lop end portion. With increasing len...
R Lal, C N Vani


An investigation of the effects of pre-steaming on the treatment of sawn spruce timber with Celcure A, a copper-chrome-arsenic preservative
1981 - IRG/WP 3150
Difficulties in the treatment of spruce using standard vacuum/pressure techniques with both water-borne and organic solvent preservatives are well known. We have evaluated the influence of steaming on treatability with a waterborne CCA preservative....
C R Coggins


The utilisation and preservation of Eucalyptus globulus agricultural stakes from Portugal
1989 - IRG/WP 3520
This paper reviews the development and utilisation of Tanalith C treated Eucalyptus globulus stakes: particular reference is made to their use in vineyards. The treatment characteristics of commercially available stakes will be described and penetration patterns evaluated....
A Milne e Carmo, D A Lewis, A Lyman


Natural durability transfer from sawmill residues of white cypress (Callitris glaucophylla). - Part 3: Full penetration of the refractory sapwood of white cypress
2000 - IRG/WP 00-40167
The heartwood of white cypress, Callitris glaucophylla, is renowned for its termite resistance and durability against decay. The sapwood, which can represent up to 30% of log volume, is non-durable and refractory to conventional preservative treatment. Previous work ascribes the lack of permeability to oily deposits within tracheids and ray cells. Environmental scanning electron microscopy was use...
M J Kennedy, L M Stephens, M A Powell


Problem of the treatment of dried sawn spruce building timbers with water-borne preservatives. Interim reports for discussion at the 4th Annual Meeting in West Berlin on 27 October 1972
1972 - IRG/WP 311
One of the most difficult technical problems facing the preservation industry is how to improve the treatment of refractory species of timber such as spruce. Its resistance to penetration, even under pressure' precludes its use for more hazardous service situations, and even in less severe conditions a higher level of treatment would be desirable. The importance of this subject led us to ...
W Liese, J W W Morgan, T Hof, R O Ullevålseter


Durability of pine modified by 9 different methods
2004 - IRG/WP 04-40288
The decay resistance was studied for pine modified by nine methods of wood modification: 1) Acetylation, 2) Treatment with methylated melamine resin (MMF), 3) Acetylation followed by post-treatment with MMF-resin, 4) Thermal modification, 5) Furfurylation, 6) Maleoylation (using water solution of MG or ethanol solution of maleic anhydride), 7) Succinylation, 8) NMA-modification and 9) modification...
M Westin, A O Rapp, T Nilsson