Your search resulted in 663 documents. Displaying 25 entries per page.
Microscopic characteristics of microbial attacks of CCA-treated radiata pine wood
1993 - IRG/WP 93-10011
Light and electron microscopic observations were made of CCA-treated radiata timbers, which had been placed in service in a vineyard soil as supporting poles and as part of a house pile, to determine the cause of their deterioration. The house pile had failed in service after between 9 and 13 years and was of particular interest because decay was more severe in deeper regions than at the surface a...
A P Singh, R N Wakeling
Observations on the performance of copper-based wood preservatives in fungal cellar (soil-bed) tests
1994 - IRG/WP 94-20047
Fungal cellar (soil-bed) tests are considered to be an important tool for the evaluation of the performance of ground contact wood preservatives. Facilities of this type have been established world wide although caution has been exercised in their introduction into standard testing methods for the approval of wood preservatives. This is the result of concerns over the variability in the biological...
G R Williams, D Rudolph, M E Hedley, J A Drysdale, R F Fox
The probable mechanism of action of boric acid and borates as wood preservatives
1990 - IRG/WP 1450
The tetrahydroxyborate ion [B(OH)4-] acts by complexation with poly-ols and probably attacks decay fungi through extracellular substrate sequestration; intracellular substrate sequestration; enzyme inhibition; and change in membrane function. Work was carried out to investigate this further and to try to explain certain phenomena observed in the area of boron preservation. The effect of Na borate ...
J D Lloyd, D J Dickinson, R J Murphy
Hardwood field experiment - 10 year report
1989 - IRG/WP 3560
The international hardwood field experiment was planned in 1976 and set up in some 34 different sites around the world. The test stakes include 4 reference species common to each site and in most cases at least 2 species of local importance (supplementary species). It was hoped that a picture of performance of a range of economically important timber species would be built up and at the same time ...
D J Dickinson, S M Gray
Biodegradation of wood in wet environments: A review
1997 - IRG/WP 97-10217
Wood in wet environments is attacked and degraded by soft rot fungi and erosion and tunnelling bacteria, which are more tolerant to high moisture and reduced oxygen conditions than basidiomycetes, such as white and brown rot fungi. Since basidiomycetes are normally more aggressive and can degrade wood faster than soft rot fungi and bacteria wood in wet environments can survive longer. In fact, arc...
A P Singh, Yoon Soo Kim
Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 1: Laboratory screening tests using a filter paper technique
1977 - IRG/WP 290
Thirty-one miscellaneous formulations have been screened using a filter paper assay technique, for their efficacy in controlling the growth of Chaetomium globosum, Cephalosporium acremonium, and a mixed inoculum of finely ground soft-rotted wood obtained from preservative treated transmission poles. The formulations consisted of various organic compounds and inorganic preparations made from differ...
H Greaves
Remedial ground-line treatment of CCA poles in service. Results of chemical and microbiological analyses 6 months after treatment
1986 - IRG/WP 3388
CCA-treated poles in service with incipient internal soft rot were remedially treated by inserting borate rods, brushing with a boron/glycol solution and injecting boric acid paste, copper/creosote paste or a commercial product (DFCK paste). The spread of active chemicals in the treated zone as well as the change in microflora have been studied with time. After six months chemicals had spread to m...
B Henningsson, H Friis-Hansen, A Käärik, M-L Edlund
Localized induction of hemlock brownstain by Ophiostoma piceae
1995 - IRG/WP 95-10106
Hemlock brownstain, a coloration disfiguring western hemlock and amabilis fir, causes economic loss in the high-value Canadian export lumber market. Recent work by the author has suggested that wood-sapstaining fungi can induce the formation of brownstain. Ophiostoma piceae, the most frequent staining fungus on western hemlock lumber in B.C., was chosen as a model to investigate fungal participati...
B Kreber
Effect of microfibril orientation of bamboo cell wall on soft rot penetration hyphae
1994 - IRG/WP 94-10087
The effect of microfibrillar orientation of bamboo (Phyllostachys virideglaucescence) cell wall on the development of soft rot (Chaetomium globosum) penetration hyphae was investigated. It was found that the soft rot penetration hyphae normally followed the microfibril angle of the cell wall. Bamboo cell walls have alternating broad and narrow lamellae with different microfibrillar angles. The mic...
O Sulaiman, R J Murphy
The mechanism of leaching of copper-chrome-arsenic preservatives from treated timber in saline waters
1976 - IRG/WP 374
A mechanism for the leaching of copper-chrome-arsenic preservatives is proposed on the basis of theoretical calculations and experimental studies using timber subjected to a range of water types of different ionic compositions. Complex formation by copper (II) and chromium (III) with chloride and hydroxide ions is shown to affect the leaching rate. Of even greater importance is the salt effect on ...
J Irvine, S-E Dahlgren
Chlorothalonil: A new ground contact wood preservative
1992 - IRG/WP 92-3712
Extensive investigations have been conducted in recent years on the performance of chlorothalonil (tetrachloroisophthalonitrile) as a ground contact wood preservative. Efficacy information is presented on a soil block test with 11 Basidiomycetes, a fungus cellar evaluation, above-ground field testing against termites in Australia and Hawaii, and ground-contact field stakes installed in Florida (9 ...
P E Laks, T L Woods
Evidence for the participation of the osmiophilic particles in the enzymatic demethylation of lignin
1984 - IRG/WP 1239
Transmission electron microscopic observations of the white-rot fungi Trametes hirsuta and Phanerochaete chrysosporium grown on a series of wood pulp with a graded lignin content and mycelium from the clarified centre of an agar-medium containing lignin (E1-effluent from the bleaching process) showed that osmiophilic particles are only induced by native lignin. Taking into account that the osmioph...
K Messner, H Stachelberger
A study of the colonization of wood blocks in a laboratory unsterile soil test
1988 - IRG/WP 2318
CCA treated and untreated beech blocks were exposed to a defined horticultural loam using the method proposed for the collaborative soft rot test in the soft rot sub-group of Working Group Two. At intervals during the incubation wood samples were removed and fungal isolations were made using selective media. Fungi were identified and tested for their cellulolytic ability and their decay capacity i...
M T De Troya, S M Gray, D J Dickinson
Degradation of lignin model compounds with coordinated copper in the presence of peroxide
1998 - IRG/WP 98-10282
A novel diffusible system capable of decomposing lignin model compounds with copper, coordinators and peroxides has been proposed. When pyridine was used as a copper coordinator, two synthetic dyes, Poly-R and RBBR were intensively decolorized with Cu(II) and H2O2 in aqueous solutions at room temperature. Although reactions with Cu(II) and H2O2 produce a strong oxidant, hydroxyl radical, via a Fen...
K Koller, K Messner, T Watanabe
Soft-rot control in hardwoods treated with chromated copper arsenate preservatives. Part 3: Influence of wood substrate and copper loadings
1977 - IRG/WP 2100
The hypothesis is proposed that hardwoods need more chromated copper arsenate (CCA) than softwoods to protect them from soft-rot attack mainly because hardwoods are more readily consumed by soft-rot fungi. Simple model systems, using copper-supplemented agar or groundwood pulp treated with CCA showed that fungi tolerated more toxicant (copper) as more available substrate (malt) was provided. Soft-...
M A Hulme, J A Butcher
A laboratory technique to measure the performance of preservative treated hardwoods in ground contact
1982 - IRG/WP 2172
A laboratory technique to measure the performance of preservative treated timber in ground contact is described. It uses partially sealed blocks of timber which are treated, leached and sawn into small stakelets for soil exposure in a fungal cellar. Performance is monitored by the loss of static bending strength with time, and a simple apparatus for measuring the deflection of a stakelet under a l...
E F Baines
An evaluation of chemical pre-treatments for controlling kiln brown stain in radiata pine
1997 - IRG/WP 97-30124
Clear radiata pine (Pinus radiata D. Don) is widely used for fine millwork owing to its attractive light colour. However, kiln drying of radiata pine sapwood often results in the development of a brown stain causing substantial loss in revenues in New Zealand's high-value export markets. In this study chemical pre-treatments were evaluated for their ability to control the formation of kil...
B Kreber, A McDonald
Bacterial brown stain on sawn timber cut from water-stored logs
1992 - IRG/WP 92-1532
Brown stains which appear on the surface of sawn radiata pine cut from water-stored logs were identified as tannin-like compounds. They are derived from bacterial breakdown of flavanoid-glucosides. When timber is sawn from infected logs, the free flavanoids migrate to the wood surface as the timber dries. There, they condense and oxidise to form permanent brown discolourations. Stains occurred on ...
M E Hedley, R Meder
Application of a novel strength evaluation technique during screening of wood preservatives
1986 - IRG/WP 2262
The effectiveness of CCA and ACA in treated aspen mini stakes tested using a novel bag procedure, with unsterile soil fortified with Chaetomium globosum and Ceratocystis albida, is reported. Good agreement between toxic limits determined using the standard weight loss procedure, and those determined by the strength technique were found, with some indication that the strength loss method is more se...
J N R Ruddick
Enhanced biodegradation of cocopeat by soft rot fungi
1998 - IRG/WP 98-10276
Biodegradation of cocopeat (coir dust) was enhanced by the addition of nitrogen (N) fertilizer and inoculation with the soft rot fungus Chaetomium globosum. The N and fungally treated cocopeats had a greater percentage weight loss (27%) after 3 months compared with 7% weight loss without the added fungi and N fertilizer. In addition, their hemicellulose, cellulose and lignin contents were greatly ...
P Y Yau, R J Murphy
Protection of southern pine using N,N-Napthaloylhydroxylamine: Field tests, soft-rot cellars and aquatic bioassay leach testing
1999 - IRG/WP 99-30204
Recent environmental restrictions are limiting the use of broad-spectrum biocides for wood preservation. There is an urgent need for new, sharply targeted, environmentally benign wood preservatives. N'N-Napthaloylhydroxylamine (NHA), a water-soluble calcium-precipitating agent, has been shown to inhibit decay by brown-rot and white-rot fungi in soil-block tests and prevent damage by Easte...
D M Crawford, F Green III
Hardwood field experiment: Progress report 1977-82
1982 - IRG/WP 3200
The international hardwood field experiment was planned in 1976 and set up in some 30 different sites around the world. The test stakes include 4 reference species common to each site and in most cases at least 2 species of local importance. It was hoped that a picture of performance of a range of economically important species would be built up and at the same time provide vital background inform...
D J Dickinson, J F Levy
Soft rot
1978 - IRG/WP 179
Soft rot decay of treated wood is examined with special reference to hardwoods treated with CCA. Factors which adversely affect the chances of protection of hardwoods against soft rot are discussed. The ratio of the volume of the fibre cell wall to the volume of the fibre lumen is presented as a major factor influencing final preservative concentration in the fibre cell wall, the major strength co...
C R Levy
Molecular studies on house rot fungi by RAPD-PCR
1997 - IRG/WP 97-10195
For genetic information and in view as a possible diagnosis method various isolates of the dry rot fungus, Serpula lacrymans, the wild merulius, S. himantioides, and the cellar fungus, Coniophora puteana, from Asia, Europe and USA were investigated by the polymerase chain reaction (PCR) based technique of randomly amplified polymorphic DNA (RAPD). The banding patterns obtained revealed for S. lacr...
O Schmidt, U Moreth
Diffuse cavity formation in soft rot of pine
1992 - IRG/WP 92-1541
A new type of soft rot of southern pine longitudinal tracheids is described. In this type, soft rot cavities form by diffuse degradation of the S2 cell wall layer by hyphae growing within the cell wall. Erosion is diffuse and irregular as opposed to the restricted, periodic erosion typical of type 1 soft rot cavity formation. Proboscis hyphae remain small (diameter 0.6 to 0.8 µm) and rapidly auto...
S E Anagnost, J J Worrall, C J K Wang