A deflection test for monitoring decay in miniature beams
1986 - IRG/WP 2269
A laboratory apparatus for assessing decay in small stakes is described. It involves the measurement of deflection in a static bending apparatus using a displacement transducer linked to a microcomputer. Measurements are non-destructive, rapid, accurate and automatic and decay can be assessed repeatedly over long time periods....
S M Gray


The effect of certain wood extractives on the growth of marine micro-organisms
1977 - IRG/WP 438
S E J Furtado, E B G Jones, J D Bultman


Decay resistance of wood removed from poles treated with Trichoderma
1989 - IRG/WP 1386
Wood blocks removed from a distribution pole previously treated with a biological control product (Binab FYT pellets) were exposed in soil block tests to selected basidiomycetes. The blocks were removed from regions of poles where Trichoderma colonization had been confirmed by extensive sampling and computer mapping of microbial inhabitants. The results indicate that material from pole interiors c...
A Bruce, B King, T L Highley


Comparative studies on the distribution of lignin and CCA elements in birch using electron microscopic X-ray microanalysis
1987 - IRG/WP 1328
The microdistribution of metal preservatives in treated wood has received considerable research over the last two decades. Despite this, little effort seems to have been made to try and correlate the distribution of CCA elements with respect to naturally occurring wood cell wall components in wood. In the present preliminary study an attempt is made to relate the distribution of lignin in-situ wit...
G F Daniel, T Nilsson


Ultrastructural and TEM-EDAX studies on the degradation of CCA treated radiata pine by tunnelling bacteria
1985 - IRG/WP 1260
An ultrastructural study was carried out on bacterial attacked Pinus radiata stakes treated with a high level (24.7 kg/m³) of Tanalith NCA preservative. The purpose of the investigation was to determine whether the organism possessed intracellular and/or extracellular detoxification mechanisms in order to overcome the high levels of copper, chrome and arsenic present within the wood fibre walls. ...
G F Daniel, T Nilsson


Soil-bed studies (Part 3): A cause of failure of multisalt preservatives following soil-bed exposure
1983 - IRG/WP 3261
P Vinden, J F Levy, D J Dickinson


Waterborne silicones as wood preservatives
1995 - IRG/WP 95-30062
For more than thirty years silicones are used as water repellents for masonry. Their excellent properties make them also attractive for non-mineral substrates like wood. Although it was always thought that silicones are not able to perform on wood, a new type of aqueous silicone materials proofed the opposite: Excellent water repellency and astonishing durability were achieved. This paper describe...
R Hager


The interaction of polyflavonoid tannins with CCA in Pinus radiata
1987 - IRG/WP 3422
Polyflavonoid tannins complex easily and rapidly with metal ions such as copper, chromium, and arsenic. such complexes in high-tannin-containing CCA treated hardwoods might result in essentially under-treated timber. Four aspects of this interaction were investigated: 1) The relationship between tannin contents of seven hardwoods (Betula pendula, Alstonia scholaris, Fagus sylvatica, Liquidambar st...
K G Ryan, D V Plackett


Practical testing of wood preservatives to prevent weathering damage and infection by micro-organisms on spruce and pine
1989 - IRG/WP 3530
Brush application, is generally used to prevent wooden window frames from decay caused by influence of weathering and fungi. Accordingly 10 boards of pine (Pinus sylvestris) and spruce (Picea abies) were treated with 10 commercially used wood preservatives. The efficiency of fungicides by using chiptest and blue stain test (EN 152), the effectiveness against weathering as well as the course of col...
R Gründlinger, O Janotta, H Melzer, K Messner


Computer-assisted numerical clustering analysis of various strains of Serpula lacrymans (Wulfen:Fr.) Schroeter apud Cohn
1992 - IRG/WP 92-2396
Eight strains of Serpula lacrymans were compared in relation to their previously determined factors (5 physiological and 10 toxicometrical). A numerical clustering analysis was used along with, as coefficient of similarity, "cos Q" after standardization of all results. Results with respect to the combined factors showed a mutual similarity within four groups of strains. The first of these groups c...
J Wazny, J D Thornton, P Stenzel


Penetration of deltamethrin in micro-emulsion formulation after injection in wood
1996 - IRG/WP 96-40068
In the Netherlands (and some other European Countries) the remedial treatment of death watch beetle is still a problem. This is because the larvae of this insect penetrate the central heartwood of mainly large oak beams. The heartwood is difficult to treat. The preventive treatment of wood boring insects has only recently been permitted in the Netherlands. Since 1989 injection of insecticides is r...
P Esser, W L D Suitela


Three dimensional computer representations of growth of microbial populations in wood
1984 - IRG/WP 1243
Creosoted distribution poles inoculated with either Lentinus lepideus, biological control organisms including Triochoderma or combinations of both were extensively sampled to monitor the spread of organisms. A computer program which enabled the results to be portrayed in a three dimensional graphic form was developed and is illustrated. Results showed that computer mapping of this type usefully en...
A Bruce, B King, C Bruce, G M Smith


The attack of naturally durable and creosote treated timbers by Limnoria tripunctata Menzies
1995 - IRG/WP 95-10132
Limnoria tripunctata was found tunnelling in creosote treated Douglas fir (Pseudotsuga menziesii) pilings and naturally durable greenheart (Ocotea rodiaei) gate seals at two sites on the south coast of the United Kingdom. Examination of thc creosote-treated wood showed that Limnoria tunnels were concentrated at a depth of 2-3 cm from the timber surface, where creosote loading was lower. Fewer tunn...
A J Pitman, G S Sawyer, G F Daniel


Polyflavonoid tannins - From a cause of CCA soft-rot failure to the "missing link" between lignin and microdistribution theories
1986 - IRG/WP 3359
Polyflavonoid tannins are proven to be fast-reacting with CCA solutions and hence, to be strong competitors of the structural wood constituents for fixation of CCA preservatives. The consequence of this effect is that even relatively small amounts of tannin cause severe undertreatment of the structural wood constituents which in turn badly affects the long term durability of CCA-treated timber. Th...
A Pizzi, W E Conradie, M Bariska


Detection of termite attack in wood using AE monitoring
1990 - IRG/WP 2355
An acoustic emission (AE) monitoring method for detecting termite activity in wood was applied to lumber of 3 by 3 cm to 10 by 10 cm square, 1 m long. Furthermore, the propagation of AEs due to the feeding activities of termites in the specimens and the locations of AE sources were analyzed. Also discussed was the feasibility of the method applied to posts out in the field of subterranean termites...
Y Fujii, M Owada, M Noguchi, Y Imamura, M Tokoro


High CCA retentions and the protection of eucalypt power poles
1983 - IRG/WP 3226
Tasmanian power pole material treated to high retentions, was analysed to accurately determine the amount of CCA preservative in the timber. Material from the same disc was subsequently exposed in unsterile soil in order to determine the effectiveness of treatment. Results showed that even at high retention levels, soft-rot attack was not prevented. Fourteen further poles were sampled, but this ti...
L E Leightley, J Norton


Anatomical Characteristics to the Distribution of Water-borne Copper Wood Preservatives in Wood
2004 - IRG/WP 04-40277
The objective of this study was to understand the micro-distribution of a copper-based preservative in wood in connection with anatomical morphology and to consider the fixation of copper in wood. Bulk specimens and semi-ultra thin sections (0.5µm) obtained from Japanese cedar were treated with a CuAz preservative solution. After fixation, SEM-EDXA was used to investigate the micro-distribution...
H Matsunaga, J Matsumura, K Oda


Co-operative work on the performance of treated timber in ground contact
1975 - IRG/WP 344
At the 6th meeting of The International Research Group on Wood Preservation in Vienna, it was decided to approach all interested parties in order to: collate available information, set up collaborative work and to stimulate research on the performance of treated timber, especially hardwoods, in ground contact. In recent years, considerable concern has been expressed about the performance of preser...
D J Dickinson, J F Levy


Penetration of surface applied deltamethrin micro-emulsion formulations in four European timber species
1994 - IRG/WP 94-20030
The Netherland's Government, in line with many other European Governments initiated a programme (KWS2000) aimed at significantly reducing the emission of volatile organic compounds by the year 2000. As part of this programme a research project is currently underway to evaluate the potential for replacing organic solvent based remedial treatments with micro-emulsion formulations of the sam...
P Esser, W L D Suitela, A J Pendlebury


Behaviour of some selective Indian species towards treatment with solvent based water repellent preservative
1984 - IRG/WP 3309
This paper discusses a solvent based preservative using PCP and a water repellent for preserving three species of timber commonly used in India for the manufacture of doors and windows. It examines the method of treatment to achieve desired levels of penetration and retention of the preservative-cum-water repellent, and tests made on these timbers to examine the success of the processing methods a...
V R Sonti, B Chatterjee


Statistical evaluation of 'micro-bending' samples for classification of wood attacking fungi
1992 - IRG/WP 92-1544
Micro-specimens from both hardwood and softwood were exposed to selected species of field isolated fungi. The strength reduction and weight loss caused by these fungi were determined. A statistical procedure was then developed to classify the fungi into brown-, white-rot, or non-decay fungal categories based on these data. The procedure reveals the extent of hazard a fungus poses to wood members. ...
B Goodell, Jing Liu, A Homola, J Jellison, J Shottafer


An Australian test of wood preservatives. Part 1: Preservatives, principles and practices
1978 - IRG/WP 2123
Between November, 1963, and July, 1964, a graveyard test of some 6000 preservative-treated stakes was installed at 8 sites equally distributed between Papua New Guinea in the tropics, through Queensland and New South Wales to Victoria. More than 40 different preservatives and preservative mixtures, mostly at several different levels of retention, were used to impregnate sawn specimens of Pinus rad...
J Beesley


Field test design for service life prediction of wooden components
2005 - IRG/WP 05-20308
Wood is predominantly degraded by organisms. Thus, compared to other building materials, service life of wooden material is influenced by many more factors, which are divided into direct and indirect factors. Climate, geographical position, and construction criteria count to the indirect decay factors. Besides material inherent properties (natural durability, wood preservatives), wood temperature...
A O Rapp, C Brischke


New conception for shortering the duration of fungitoxic test of wood preservatives. Part 2: Computer-assisted miniaturisation of wood specimens
1994 - IRG/WP 94-20052
The mass loss of wood used as a criterion in the standarised agar-block method of evaluation of toxic value of preservatives depends upon the relationship between volume of specimens, their outspread planes and ratio of areas of particular anatomic sections. Upon the computer-assisted mathematical basis the dimensions of miniaturized specimens which make 1/2, 1/4, and 1/8 part of standarized ones ...
J Wazny, K J Krajewski


Aspects of leaching
1976 - IRG/WP 267
With respect to Document No: IRG/WP/246, and the recommendation that an economic leaching test can be based on a non-changing volume of water (500 ml/block), I would like to relate our experiences with this suggestion. Following 14 days of continuous immersion in de-ionized water it was found that blocks treated with moderate and above concentrations of a preservative gave no problems, but those b...
R S Smith


Next Page