IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 762 documents. Displaying 25 entries per page.


Slice - Cut and Analyze Laser Microdissection (LMD): A method to produce sample material from modified wood for chemical quality analysis
2011 - IRG/WP 11-20478
Wood modification with its various systems is an established way to enhance a wood products’ service life in outdoor applications. Per definition, selected material properties are enhanced by means of modification without producing toxic substances or residues during service life and combustion afterwards. The systems of impregnation modification include a physical and often chemical alteration ...
K Zimmer, E Larnøy, A Treu, M Fongen


Non-destructive evaluation of wood decay
2011 - IRG/WP 11-20479
Evaluation of wood decay is often prone to subjective assessment. Standard rating scales are based on human perception of decay, often in addition to weight loss measurements. Especially the assessment of graveyard specimens or other long term testing material that has to be monitored regularly on a non-destructive basis, is challenging. In this paper two techniques are presented that can deliver ...
J Van den Bulcke, I De Windt, N Defoirdt, J Van Acker


LOSP for glulam, when should the treatment be applied?
2011 - IRG/WP 11-30555
Treatment options for outdoor above-ground (H3) exposed glulam of Pinus radiata and P. elliottii were examined. Beams were treated with azole LOSP (containing a zinc tracer) aiming for retentions of 35-40 l/m3 or 70-80 l/m3. Treatment was conducted either before or after gluing. TBTN LOSP and CCA were included as comparative treatments. Test specimens for exposure were cut after treatment, while w...
L J Cookson


Ten Year Field Tests of Borate-Treated Wood Against Subterranean Termites
2011 - IRG/WP 11-30557
In the mid 1990s, Forintek Canada Corp. initiated a study of the termite resistance of borate-treated lumber above ground, protected from rain in Canada, Japan and Hawaii. Predominant termite species at three test were Reticulitermes flavipes in Canada, and Coptotermes formosanus in both Japan and Hawaii. The material included hemlock and amabilis fir lumber treated with disodium octaborate tetrah...
P I Morris, J K Grace, K Tsunoda


Copper Nanoparticles in Southern Pine Wood Treated with a Micronised Preservative: Nanodistribution of Copper in the Pit Membrane and Border of an Earlywood Bordered Pit
2011 - IRG/WP 11-30566
Copper nanoparticles can penetrate the cell walls of unlignified parenchyma cells in southern pine wood treated with a micronised wood preservative, but they are excluded from lignified tracheid walls. This paper extends these observations to include the cell wall layers of the bordered pit. Focused ion beam and ion milling were used to make an ultra-thin section of the cell wall layers of an earl...
H Matsunaga, Y Kataoka, M Kiguchi, P Evans


Biological and mechanical performances of particleboard panels made from maritime pine (Pinus pinaster) and glued with cornstarch-mimosa tannin-urea formaldehyde adhesive
2011 - IRG/WP 11-40542
The objective of this work was to demonstrate the utility of cornstarch-mimosa tannin-based resins designed for application as an adhesive in the particleboard production. Bond qualities of cornstarch-mimosa tannin- urea formaldehyde (UF) (10:4:86, weight ratios) resins and commercial UF resin were assessed by using an automatic bonding evaluation system, prior to production of particleboard panel...
A Moubarik, F Charrier, A Pizzi, A Allal, B Charrier


Decay resistance of a commercial pistachio twig-plastic composite
2011 - IRG/WP 11-40553
In this research, the decay resistance of commercial extruded pistachio twig flour-plastic composite was investigated against the white-rot fungi Trametes versicolor and the brown-rot fungus Coniophora puteana. The composite specimens containing 60% pistachio twig flour were exposed to a decay test according to modified ASTM standard for 3 months. The results showed that the composite could be d...
M R M Farahani, M Safarzadeh


Challenges and new developments in testing electro osmotic pulsing technology (PLEOT) by means of conventional laboratory methods
2011 - IRG/WP 11-40555
A new wood protection system, electro-osmotic pulsing technology, called PLEOT, is tested in lab trials using different test setup. The technology is tested on Scots pine sapwood and beech wood samples exposed to brown- and white rot fungi. Mass loss and moisture content is calculated after testing and a chitin analysis are performed on the sample powder. Two different electrodes are used in ord...
A Treu, E Larnøy


Evaluation effect of kiln schedule on Warp, Twist, Bow and surface checks in Poplar Wood
2011 - IRG/WP 11-40565
In this research, to establish a kiln-drying schedule for poplar (Populus nigra) lumber with 75 mm thickness that cut down from North Khorasan province in Iran, with three schedules T5-D2 (Forest Product Laboratory), T5-D3 and T8-D5 were adapted for drying the lumbers down to the final moisture content of 8±2%. primary dry bulb temperature each three schedules was adjusted at 49,49 and 54°C and ...
M. Akhtari, M.Arefkhani


Decrease of stiffness properties of degraded wood predicted by means of micromechanical modeling
2011 - IRG/WP 11-40570
Wood exhibits a highly anisotropic mechanical behavior due to its heterogeneous microscopic structure and composition. Its microstructure is organized in a strictly hierarchical manner from a length scale of some nanometers, where the elementary constituents cellulose, hemicelluloses, lignin, and extractives are found, up to a length scale of some millimeters, where growth rings composed of earlyw...
T K Bader, K Hofstetter, G Alfredsen, S Bollmus


Effects of nano-silver on brittleness of heat-treated solid woods
2011 - IRG/WP 11-40572
The present study is aimed at the effect of heat-treatment of normal as well as nano-silver-impregnated Populus nigra, Populus deltoides, and Fagus orientalis on brittleness. Specimens were impregnated with 200 ppm water-based solution of nano-silver particles under 3 bars in a pressure vessel using empty-cell process. For heat treatment, both nano-silver-impregnated and normal specimens were kept...
H Reza Taghiyari, B Moradi Malek, A Karimi


Characterizing long term leaching behaviour of copper from preservative treated wood in a practical exposure scenario
2011 - IRG/WP 11-50278
To investigate the prediction of the long term emission of copper from preservative treated wood in a Use Class Class 3 scenario, treated boards were exposed vertically above ground to natural weather conditions. The study included two products; an amine copper ACQ-type formulation, air-dried after treatment to a 22 kg/m3 retention, and the same formulation which was hot oil vacuum dried after tre...
T Mark Venås, M Klamer


A genomic sequencing approach to study wood decay and copper tolerance in the brown rot fungus, Antrodia radiculosa
2010 - IRG/WP 10-10720
We used Illumina paired-end short read sequencing (76 nt, 300 bp insert size) to produce a de novo assembly of the genome of Antrodia radiculosa, a copper-tolerant brown rot fungus that is capable of aggressive wood decay. Quality analysis of the base calls in the dataset (8.95 Gb) showed that the majority of the nucleotide sequence was of the highest quality with 5% in the lowest quality group. ...
J D Tang, T Sonstegard, S Burgess, S V Diehl


Effect of Heavy Metals on the Expression of Manganese Dependent Peroxidases of Phanerochaete chrysosporium
2010 - IRG/WP 10-10722
This work is part of an ongoing investigation that studies the application of a solution rich in Zn and Mn, obtained from a recycling process, as a preservative for wood. The effects of Zn2+ and Mn2+ on the enzyme-expression level of manganese-dependent peroxidase (MnP) from Phanerochaete chrysosporium was studied by real-time PCR. The glyceraldehyde 3-phosphate dehydrogenase gene (gpd) was used a...
C Ibáñez, M Rabinovich, M Barraco, G Gecchetto, M Cerdeiras


Natural Durability of Fence Poles from Fourteen Semi-Arid Land Species after Six-Month Exposition
2010 - IRG/WP 10-10724
...
A Carrillo, F Garza, V Bustamante, S Sandoval, H Villalón


Frequency of fungal decay in softwood windows in Germany
2010 - IRG/WP 10-10725
Knowing how often fungal decay occurs is a fundamental basis for general recommendations of preservative measures. To optimize the German recommendations for chemical wood preservation of windows made out of pine or spruce more than 2000 windows have been inspected. All windows had an opaque coating and were between 2 and 17 years old. The selection of the inspected windows was kept as randomly as...
D Lukowsky, O Moarcas, A Luette


Qualitative - Quantitative Analysis of Wood-Inhabiting Fungi in External Wooden Structures of the Latvian Cultural Heritage
2010 - IRG/WP 10-10728
The frequency and diversity of wood inhabiting fungi in the exterior wood were established in the Araishi lake fortress, the Lielvarde wooden castle, the Latvian Ethnographic Open-Air Museum, Riga, and twelve wooden heritage objects in the Eastern part of Latvia (Latgale). The inspected wooden structures of the external woodwork included windows, stairs, walls, floorings, roofs, fences, and benche...
I Irbe, M Karadelev, B Andersons


Glutathione transferases as functional biomarkers of wood degradation?
2010 - IRG/WP 10-10735
The recent release of several fungal genome sequences allows the report of an overview of fungal glutathione transferases (GSTs) focused on their function in the wood-degrading basidiomycete Phanerochaete chrysosporium. A genomic and phylogenetic analysis of GST classes in various sequenced fungi –zygomycetes, ascomycetes and basidiomycetes- revealed some specificity in GSTs distribution, in com...
E Gelhaye, M Morel


Towards Understanding the Biology of Wood Decay
2010 - IRG/WP 10-10739
Our previous research has focused primarily on ways to identify the wood decay fungi and microbial community. We continue to explore this complex and dynamic community and its interactions through microbial community ecology studies, gene expression interactions and proteomics. However, in order to better understand the mechanisms of fungal decay, we have sequenced the genome of a copper tolerant...
J Tang, K Jenkins, L Parker, S V Diehl


Stained wood: The identification of natural dyes and mordants in wooden works of art
2010 - IRG/WP 10-20434
On the basis of current knowledge only natural-colored wood species crafted to veneers were used for the decorative design of furniture and wooden interior in classical antiquity.First applications of artificially stained wood can be dated to the late Middle Ages. In the Renaissance wooden works of art were manufactured by using intarsia of natural-colored, fungus-stained and artificially stained ...
A Unger, W Unger


Detection of Wood Destroying Fungi Using DNA Microarray Technology
2010 - IRG/WP 10-20435
Wood decay fungi of the phylum Basidiomycota cause serious damage to wooden constructions and building elements. The elimination and the appraisement of fungal decay require an assured species identification. Conventional fungal diagnostics are mainly based on morphological characteristics by macro- and microscopy analysis. For some years, standardised and highly sensitive molecular methods focuss...
K Jacobs, N Rangno, W Scheiding, B Weiss, D Müller, C Hiller, W Brabetz


Onset of mould growth – the effect of climate variability and different geographic locations
2010 - IRG/WP 10-20446
This paper presents a study on how climate conditions at numerous locations in Sweden affect the risk of onset of mould on wood sheltered outdoors. The results indicate that the risk is clearly higher in the south compared to the north of Sweden. These differences are mainly explained by colder and dryer winter periods in the north which is unfavorable for development of mould. The results also sh...
M Häglund, T Isaksson, S Thelandersson


Stress wave and visual analysis of treated and non treated fence posts after 15 years in field test
2010 - IRG/WP 10-20449
Wood preservation may play an important role in protecting tropical rain forest. Basically, it can reduce pressure on natural resources by increasing wood durability. Field tests are conducted to simulate final use of woods under different environmental conditions. Visual analysis, non destructive testing, and non destructive evaluation techniques were applied to assess wood resistance and chemica...
A Florian da Costa, R Faustino Teles, J Costa Gonçalves


Improved analysis of field test data related to service life prediction of tropical wood species
2010 - IRG/WP 10-20458
Long field trials of wood in ground contact give valuable data on the natural durability of the material. The European Standard EN 350 gives guidance on how to perform these durability classification, but is limited to the use of averages of in-service life of a set of specimens compared to a reference set. Starting from a database of visual assessment of field stake testing, it is possible to obt...
J Van den Bulcke, A Wong, Ling Wang Choon, Yoon Soo Kim, J Van Acker


Effects of polyvinyl alcohol on leachability and efficacy of boron wood preservatives against fungal decay and termites attack
2010 - IRG/WP 10-30526
In this study, the use of polyvinyl alcohol (PVA) as boron fixative agent was investigated. Two levels of PVA (2.5 and 4%) were evaluated with disodium octaborate tetrahydrate (DOT) at three concentrations (1, 2 and 4% boric acid equivalent (BAE) using a double vacuum impregnation processes on Scots pine sapwood specimens. Leaching was performed according to a laboratory leaching procedure. Boron ...