IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 653 documents. Displaying 25 entries per page.


A laboratory method for assessing the effectiveness of fungicides in preventing the spread of decay fungi within packages of unseasoned lumber
1983 - IRG/WP 2202
To study the deterioration caused by decay fungi in the laboratory, a method for testing fungicides for their effectiveness in preventing spread of decay was devised. Some experiments using this method are reported here....
A J Cserjesi, E L Johnson, A Byrne


Wood extractives as carbon sources for staining fungi in the sapwood of lodgepole pine and trembling aspen
1995 - IRG/WP 95-10098
Wood discoloration by sapstaining fungi reduces lumber value. In Canada, the most commonly recorded sapstaining fungi belong to the genera Ophiostoma. This work evaluated the effect that Ophiostoma piceae, Ophiostoma ainoae, and Ophiostoma piliferum used the lipids present in the sapwood of lodgepole pine (Pinus contorta Dougl.) and trembling aspen (Populus tremuloides Michx.). Wood lipids, common...
Yong Gao, C Breuil


Comparison of methods for monitoring CCA fixation
1994 - IRG/WP 94-40023
The CCA fixation status in the outer 12.5 mm of pole sections of southern pine (Pinus sp.), red pine (Pinus resinosa) and lodgepole pine (Pinus contorta var. latifolia) were followed during fixation at 21°C under non-drying conditions by the following procedures: - Qualitative CrVI indication by the chromotropic acid spot test. - Quantitative CrVI in the expressate by the diphenylcarbazide method...
P A Cooper, Y T Ung, G Zanjani


Application of non-destructive techniques (durometric and ultrasonic) to evaluate the degradation of woods in service by Gloeophyllum trabeum
2001 - IRG/WP 01-20220
In order to establish the degree of degradation of wood used in construction, it is necessary to employ non-destructive methods (ultrasonic, durometric, densitometric). In this study, ultrasonic and Pilodyn durometric techniques have been applied to try to establish parameters of relationship between the values obtained by both, for their immediate application to wood in service. As a method of re...
M T De Troya, L Palaia, A Navarrete, V Galvañ, R Molina, A Guijarro, J Camacho


"Refractory" is a relative term. Incised alpine fir is treatable
1991 - IRG/WP 3670
While certain wood species carry a reputation for being 'treatable' this normally refers to the sapwood. For most Canadian species, heartwood penetration is the major determinant of whether treatment meets Canadian, USA and Japanese standards and in this respect alpine fir turns out to be a treatable species. Alpine fir is the fir component of the Western Canadian spruce-pine-fir...
P I Morris


Run-off quality from sprinkled debarked logs and logs with bark from Picea abies and Pinus contorta
2007 - IRG/WP 07-50248
Storage of roundwood is necessary for efficient industrial production at sawmills and pulpmills. The need for wood storage becomes even more critical when large storm fellings create huge volumes of wood that is at risk for deterioration. In Scandinavia, the technique of sprinkling of water on roundwood is used to protect stored wood from fungal and insect infestation and drying during the summer....
M Jonsson


A comparison of soft rot, white rot and brown rot in CCA, CCP, CCF, CCB, TCMTB and benzalkonium chloride treated Pinus radiata IUFRO stakes, after 9-15 years exposure at five test sites in New Zealand
1991 - IRG/WP 1485
The aim of this study was to determine if decay type varies significantly between five field trial test sites of different soil type, aspect and climate in 9-15 year old, replicate CCA, CCF, CCP. CCB, TCMTB and AAC treated IUFRO stakes. A visual on-site assessment of decay type on every test stake was made and observations confirmed by microscopical examination. Regression analyses were used to de...
R N Wakeling


JWPA method for testing effectiveness of surface coatings with preservatives against decay fungi
1981 - IRG/WP 2164
In 1979 JWPA established a new method for testing effectiveness of surface coatings in accordance with practical use of preservative-treated lumber. Comparing the new testing method with JIS A 9302, a few new trials - size of wood specimen, weathering procedure, and decay-test procedure - are incorporated....
K Tsunoda


Screening potential preservatives against stain and mould fungi on pine timber in Zimbabwe
1995 - IRG/WP 95-30063
The search for environmentally and toxicologically safer chemicals for use in the timber preservative industry against stain and mould fungi has been intensified during the past few years. Results of field tests with two chemicals previously evaluated in the laboratory are presented. The conventional sodium pentachlorophenate was the more efficacious chemical against stain and mould fungi, providi...
A J Masuka


Marine testing of selected waterborne preservatives
1987 - IRG/WP 4137
In 1978 a marine test was established at West Vancouver, B C. to determine the performance of selected waterborne preservatives. The preservatives in test were chromated-copper-arsenate (CCA-C), ammoniacal copper arsenate (ACA), a modified formulation of ACA which contained a higher copper content (modified ACA), ammoniacal copper zinc arsenate (ACZA) and ammoniacal zinc arsenate (AZA). The wood s...
J N R Ruddick


Dimensional stability and decay resistance of hot-melt self-bonded particleboard by surface benzylated pine chips
1991 - IRG/WP 3652
Akamatsu (Pinus densiflora Sieb. et Zucc: Japanese red pine) particles were pretreated with 40% NaOH solution and benzylated with benzyl chloride, and the surface of particle was converted into meltable materials. Hot-melt self bonded particleboard having smooth and high glossiness surface was prepared by hot pressing at 150°C and 1.96 MPa without using any conventional adhesives. Dimensional sta...
M Kiguchi, K Yamamoto


Utilization of curcumin for detection of presence of boron in wood
1982 - IRG/WP 3191
It has been shown that curcumin is not a reliable reagent for detecting boron in wood that has been attacked by fungi...
M-L Edlund


Pinus and Eucalyptus fenceposts treated with creosote and solvex tar by hot and cold open-tank process
1987 - IRG/WP 3455
A comparative study of the behaviour of two different wood preservatives, creosote and solvex-tar, was made, using two wood species, Pinus pinaster Ait and Eucalyptus globulus Labill, by the hot and cold open-tank process. Results showed that the creosote behaved better in relation with the uniformity of its distribution in wood. On the other hand, better results were obtained on Pinus for both pr...
M V Baonza Merino


Fire resistance of preservative treated fence posts
1994 - IRG/WP 94-30033
Pine fence posts were pressure treated separately with CCA-C, CCA-wax, CCA-oil and creosote. Treated posts and untreated controls were planted in the ground in a randomised block design, weathered for six months and then subjected to a controlled burning test using two fuel loads. Creosote treatment increased the time that posts were alight whereas CCA treatment had no such effect. However, CCA tr...
P D Evans, P J Beutel, C F Donnelly, R B Cunningham


Soft rot in CCA-treated utility poles in Sweden
1989 - IRG/WP 1398
Soft rot investigations of CCA-treated utility poles (Pinus sylvestris L.) have been conducted throughout large parts of Sweden during 1974-1985. The investigation included 179 utility poles of the State Power Board which had been used for 10-18 years in the different administrative regions from northern to southern Sweden. In addition, 193 telephone poles from the Östersund area and 218 from the...
H Friis-Hansen, H Lundström


Low temperature drying conditions of Pinus radiata wood for avoiding internal stain
1989 - IRG/WP 3507
It has been observed that, if in little sawmills, timber is dried with a low temperature schedule, it arrives at destination with internal sapstain besides of superficial mould. In this study, the lowest drying temperature at which wood should be exposed for sterilization, which results to be 52°C, is searched. It is not possible to avoid entrainment of pentachlorophenol, even though a waiting pe...
M C Rose


Fungal and bacterial attack of CCA-treated Pinus radiata timbers from a water-cooling tower
1991 - IRG/WP 1488
Transmission electron microscopy of decaying CCA-treated Pinus radiata timbers from an industrial water cooling tower showed presence of a thick biofilm covering some areas of the wood. The biofilm contained various morphologically distinct forms of microorganisms embedded in a slime. The study provided evidence of the activity of soft rot fungi and tunnelling and erosion bacteria in wood cells. T...
A P Singh, M E Hedley, D R Page, C S Han, K Atisongkroh


Strength loss associated with steam conditioning and boron treatment of radiata pine framing
1987 - IRG/WP 3438
The combined effect of included defects and wood moisture content on the strength loss of second rotation radiata pine framing following conventional steam conditioning is investigated. The green Modulus of Elasticity (MOE) is reduced by approximately 13% after steaming. When dried after steaming, however, neither the MOE nor MOR is significantly different from unsteamed dried controls....
M J Collins, P Vinden


The use of pressure cycling to improve heartwood penetration in Pinus radiata (D. Don)
1995 - IRG/WP 95-40050
This study investigates the effect of cycling pressure on the treatability of radiata pine heartwood. The results indicate that liquid penetration into the heartwood is affected by the preconditioning method used and pressure treatment time. There is no significant improvement in the penetration of Pinus radiata (D. Don) heartwood when a cycling or pulsation process is used....
P R S Cobham, P Vinden


Collaborative soft rot tests: PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1973 - IRG/WP 223
These tests were undertaken as a preliminary to the next series of collaborative soft rot tests. An interim report has already been presented at Berlin in 1972 as Document No: IRG/WP/211...
J K Carey, J G Savory


International collaborative laboratory comparison of two wood preservatives against subterranean termites: Third update and first report
1996 - IRG/WP 96-10174
At the 24th annual meeting of IRG in Orlando, USA, in May 1993 an international subterranean termite laboratory bioassay to compare the various preferred termite protocols used by IRG termitologists was initiated. The author was nominated to co-ordinate this comparative laboratory evaluation of two wood preservatives, copper-chrome-arsenic (CCA) and copper naphthenate (Cu-Na) against the subterran...
J R J French


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 13: Report of fourth inspection (36 months) in Australia
1981 - IRG/WP 481
This report presents the results of the fourth inspection of the IRG/COIPM International Marine Test specimens installed in Sydney Harbour in December, 1977. The inspection took place on 9th December, 1980, after 36 months exposure. Full details of the treatment and installation of the specimens, as well as results of the first three inspections (after 6, 12, and 24 months exposure), have been pre...
J Beesley


Ultra-structural observations on the degradation of wood surfaces during weathering
1987 - IRG/WP 2280
Radiata pine (Pinus radiata D. Don) sapwood was converted into blocks with a transverse face about 5 mm square and measuring 8 mm longitudinally. Transverse (T.S.), Radial (R.L.S.) and Tangential (T.L.S.) surfaces were prepared and specimens exposed to the weather inclined at 45° facing equatorially for periods of between 20-60 days. After 30 days exposure erosion of the middle lamella was observ...
P D Evans, S Thein


Performance of preservative-treated hardwoods with particular reference to soft rot. Report of condition of specimens installed in Victoria, Australia
1980 - IRG/WP 3155
J Beesley, R McCarthy


Soil virulence tests using Scots pine sapwood
1973 - IRG/WP 222
Following the tests reported in Document No: IRG/WP/210, in which soils from different laboratories were investigated for virulence, supplementary tests have been carried out using Scots pine sapwood and an extended incubation period....
J K Carey, J G Savory


Next Page