Your search resulted in 1792 documents. Displaying 25 entries per page.
Surface morphology and short-term water uptake of charred and coated wood
2021 - IRG/WP 21-40916
Charring of the wood surface represents a traditional alternative surface treatment technique with the purpose of aesthetics and protection. By the treatment with flame the surface of wood becomes carbonized and a few millimetres thick charred layer is formed on the top of the wooden element. Further, the charred layer can be removed by brushing, which accentuates the structure of the surface. Add...
J Zigon
Marine borer resistance of various wood materials in Japan
2021 - IRG/WP 21-10983
Wood resistance against marine borer was intensively studied in the 1940s in Japan, but the research activities on the subject diminished afterward, as the use of wooden marine structures and ships decreased. Today, however, use of wood as a construction material is officially promoted for its environmental benefits. The author started to immerse some wood materials in the seawater pool at PARI ...
M Yamada
Mechanical and biological durability properties against soft-rot and subterranean termite in the field (grave-yard test) of beech wood impregnated with different derivatives of glycerol or polyglycerol and maleic anhydride followed by thermal modification in an opened or in a closed system
2021 - IRG/WP 21-40917
This paper presents mechanical and biological durability properties in soil beg test (soft-rot test) and field test (grave-yard test) against subterranean termite of the wood modified with an aqueous vinylic derivative of glycerol/polyglycerol or maleic anhydride cured in an opened or in a closed system. Wood modification was performed through impregnation of European beech (Fagus sylvatica) with ...
M Mubarok, H Militz, S Dumarcay, I W Darmawan, Y S Hadi, P Gerardin
Preliminary investigation for preservation method of CLT using non-pressure treatment
2021 - IRG/WP 21-40919
Cross-laminated Timber (CLT) is increasingly being used in residential and non-residential construction around the world, and some of these areas are at high risk of biodeterioration. Addition to moisture management of construction, preservative treatment of CLT may be needed to prevent decay and termite attack in the area. Pressure treatment being most reliable, is not feasible due to the large d...
T Miyauchi, Y Ohashi, J Miyazaki, R Takanashi, H Shibui, S Isaji, T Shigeyama, Y Sugai, A Yamamoto, T Hramiishi, T Mori, H Matsunaga
Treatability of South African-grown Eucalyptus grandis with water-borne copper azole and disodium octaborate tetrahydrate wood preservatives
2021 - IRG/WP 21-40920
This study investigated the treatability of the sapwood and heartwood of sawn Eucalyptus grandis with copper-azole (CuAz) and disodium octaborate tetrahydrate (DOT) water-borne preservatives towards improving its durability for enhanced use in structural solid wood applications. The results obtained showed that, at a moisture content of 12 ± 1%, sawn E. grandis sapwood can be impregnated to a mea...
A A Alade, Z Naghizadeh, C B Wessels
Effect of a Water Repellent Treatment on Moisture Behavior of Three Australian Hardwoods: A Preliminary Report
2021 - IRG/WP 21-40921
Wood is inherently hygroscopic and will sorb moisture either directly from the atmosphere or via capillary action. Moisture can have marked effects on wood properties and repeated wetting and drying creates dimensional changes that lead to physical damage. Exposure to elevated moisture levels also increases the risk of fungal attack.
Wood preservatives have long been used to minimize the risk of ...
B Hassan, J J Morrell, K Wood
Effect of Heat Treatment on Physical and Mechanical Properties of Oriental Beech Wood (Fagus orientalis L.)
2021 - IRG/WP 21-40923
The present study aims to investigate the influence of heat treatment on physical and mechanical properties of Oriental beech wood (Fagus orientalis Lipsky.). Samples were exposed to temperature levels of 130˚C, 160˚C, and 190˚C for 3, 6, and 9 h. Selected physical and mechanical properties including compression strength parallel to grain, compression strength perpendicular to grain, bending st...
M D Ghalehno, D Chu, B N Sheshkal, M Humar, M Bahmani
Leaching of copper, chromium and arsenic from CCA-treated slash pine heartwood
1994 - IRG/WP 94-50020
Drying green slash pine with any of three high temperature drying schedules produced a product in which both the sapwood and the heartwood could be penetrated with CCA using a modified Bethell treatment schedule. Required H3 retentions were achieved in both sapwood and heartwood, from 200 litres per m³ charge uptake. Post-treatment fixation/drying was accomplished by three different regimes, incl...
M J Kennedy, G Palmer
Durability of Eucalyptus globulus floating structures mussels trough in marine environment against marine borers in the Atlantic coast of Spain
2020 - IRG/WP 20-10965
In Spain, since forever damages caused by marine borers are frequent in wood elements and wood structures located in sea water conditions. Galicia is a region located in the North West of Spanish, above Portugal, characterized by their typical estuaries, where since ancient times, the natural production of mussels from floating structures mussels trough. Since ever, wood species selected to build ...
D Lorenzo, M Touza, J Fernández-Golfin, A Lozano, J Benito
Monitoring of wood preservatives exposed to weathering: Extraction and analysis methods of organic biocides from treated wood and collected rain runoff
2020 - IRG/WP 20-30753
Weathering is the cause of numerous damages for outdoor joineries. Protection of wood using a preservative treatment covered with a coating is a process widely used to limit these damages. However, biocides from preservative treated wood are prone to degradation and leaching, having a direct influence on the joinery service life. This document deals with extraction and analytical methods for bioci...
O Ouali, K Le Ménach, E Raphalen, L Podgorski, S Legay, H Budzinski
Investigations into the use of Maleic Anhydride/Sodium Hypophosphite as a Wood Modification Process
2020 - IRG/WP 20-40891
The formation of crosslinked bonds between wood constituents is believed to be an effective way to stabilize wood against wet conditions. The possibility to use maleic anhydride (MA) combined with sodium hypophosphite (SHP) as crosslinking agents was studied, using Scots pine sapwood and a model compound. The modified wood showed weight gain and bulking effect after treatment and subsequent Soxhle...
I Kim, D Jones, O Karlsson, D Sandberg, O N Antzutkin, F Ullah Shah
Elucidation of reactive sites of wood modified with acetic anhydride: Insights from density functional theory calculations
2020 - IRG/WP 20-40892
Density functional theory (DFT) was employed to investigate the interaction of cellulose and lignin with acetic anhydride for explaining the wood modification process. Atoms in molecules (AIM) and reduced density gradient (RDG) along with non-covalent interaction (NCI) plots were used to analyse the intermolecular bonding characteristics. Cellulose was modelled with a cellobiose unit (dimer of glu...
V Ponnuchamy, A Sandak, J Sandak, R Herrera Diaz
Self-regulating heating cables for conductive heat transfer in pest control
2020 - IRG/WP 20-40895
Pest control by means of conductive heating of wooden elements requires considerable measuring and control efforts in order to avoid overheating of wooden surfaces, damage of structural elements and risk of fire. The usage of self-regulating heating cables might overcome such problems. In laboratory tests and under real conditions the applicability of self-regulating heating cables is tested with ...
J Müller, E Melcher, J Welling
Impregnation of railway sleepers - Investigation of a system-sleeper as an alternative for creosote treated sleepers
2020 - IRG/WP 20-40896
For nearly 200 years wooden railway sleepers are impregnated with creosote. After initially using vacuum pressure processes for impregnation, empty-cell processes have been developed quickly and are used until today. Because of political developments, creosote will probably be banned on the European market in the near future. The Fürstenberg-System-Sleeper, which combines for Europe innovative as...
M Starck, A Heidel, C Brischke, H Militz
Performance of a water-borne stain on beech, spruce, MDF and OSB improved by plasma pre-treatment
2020 - IRG/WP 20-40897
Coatings are an important part of wood protection, especially for outdoor applications. In order to provide a good protection, protective coatings need to exhibit good adhesion, mechanical resistance, and weathering resistance. Plasma pre-treatments are an established method to increase the performance of existing coatings including those on wood and wood-based substrates. Moreover, plasma deposit...
S Dahle, J Žigon, I Uranjek, M Petrič
Future development of durability assessment of wood, according to typical usage of preservative-treated wood and naturally durable wood in Japan
2020 - IRG/WP 20-20675
A market of preserved wood products in Japan has two unique histories. First is the market shift to residential ground sills from utility poles and sleepers; the other is the stop of CCA treatment caused by the new effluent standard. In 2018, around 85% of preserved wood products used for residential ground sills were treated with non-CCA such as Cu-based agents. Since the market of treated wood h...
T Osawa, W Ohmura, H Kurisaki
Macro biological degradation of wood treated with sorbitol and citric acid – first results from marine environment and termite exposure
2020 - IRG/WP 20-40901
Most European wood species are rapidly and severely degraded in termite-infested areas and the marine environment. There is a need for new solutions, especially in the marine environment, since we lack wood preservatives approved for marine applications in Europe. Several wood modification systems show high resistance against both marine borers and subterranean termites. However, the existing comm...
A Treu, L Nunes, E Larnøy
Biofinish: A Functional Wood Surface Treatment based on Aureobasidium
2020 - IRG/WP 20-40903
Xyhlo Biofinish is a natural and environmentally friendly wood protection concept based on linseed oil impregnation and a fungal-based coating. It emerged in the late 1990s and has been developed over the past 15 years into an industrially applicable process in the Netherlands. The combination of linseed oil impregnation and a surface treatment with the living fungus Aureobasidium extends the serv...
S Rensink, M Sailer, S Roukens, J Gerber, H van der Mel, K Potgieter, J Spit, R Bulthuis, C Struck, M Bennink
PlasmaSolution – Curing of coating formulations using non-thermal plasmas
2020 - IRG/WP 20-40904
Coatings are an important part of wood protection, especially for outdoor applications. In order to provide a good protection, protective coatings need to exhibit good adhesion, mechanical resistance, and weathering resistance. Plasma pre-treatments are an established method to increase the performance of existing coatings including those on wood and wood-based substrates. Moreover, plasma deposit...
S Dahle, J Žigon, M Petrič
Thermal spray coatings to protect wood from termites
2020 - IRG/WP 20-40905
Protecting buildings and construction materials against subterranean termites in Europe relies on combined physical and chemical approaches. Buildings can be protected by physical or physico-chemical barriers such as gravel aggregates, steel mesh or plastic films impregnated with insecticides. Wood and wood-based materials are traditionally protected by insecticides applied on the surface or deepl...
L Podgorski, H Myalska, A Dinoirjean, M Kutnik
Hydrophilization of wood using a FE-DBD air plasma
2020 - IRG/WP 20-40907
One of the goals of surface protection of wood with coatings is to prevent the evolution of moisture in wood, which accelerates its degradation by abiotic and biotic factors. Good wettability of wood is a necessary pre-condition for sufficient protection with water-based coatings. Treatment of wood surface with atmospheric dielectric barrier discharge in configuration with a floating electrode was...
J Žigon, M Petrič, S Dahle
The influence of chemical compounds on wood cell wall to surface cracks
2020 - IRG/WP 20-40908
Degradation due to cracking and dimensional changes caused by drying, have a significantly negative impact on the preservation and durability of wood. Therefore, the prevention of surface cracking, which tends to occur during the drying process, is vital. High temperature set drying is one of the most effective methods for preventing wood surface cracking. It begins with softening the wood at a hi...
R Suzuki, Y Mori, K Yoshihiro, K Yamashita, M Kiguchi
NewSiest-Enhancement of UV stability of thermally modified wood through envelope impregnation with nanobased stabilisers
2020 - IRG/WP 20-40909
Thermal modification is a process which improves the properties of wood, resulting in a material that can be disposed at the end of the product life cycle without presenting an environmental hazard. Thermally modified wood retains as a natural product and the grain, original colour variances and characteristics of wood are still present. However, exposure to daylight causes brightening or greying ...
K Srinivasa, M Petrič
Enhancing the durability of low durability Eucalyptus plantation species: a review of strategies
2020 - IRG/WP 20-40910
Eucalyptus species native to Australia have shown excellent growth rates, good physical properties and resistance to diseases. As a result, they are widely planted globally for a variety of uses. One negative aspect of many of these faster growing species is that they have a high percentage of low durability heartwood that resists preservative treatment. In Australia, large plantations of these sp...
K C Wood, J J Morrell, W Leggate
Thirty-four year test of on-site preservative treatments to control decay in wood above ground
1993 - IRG/WP 93-30015
This research was initiated in 1958 to investigate efficacy of various preservatives and treating methods for new lumber going into exterior structures of buildings. Post-rail units (2x4 inches) constructed of Southern Pine sapwood, Douglas-fir heartwood, and mill run western hemlock were dip- or brush-treated before or after assembly. Units were trested with pentachlorophenol in various petroleum...