Window test. Direct testing of wood resistance to decay: A study of its fitness, its reliability and its accelerating factor
1984 - IRG/WP 2219
This is the results of an experiment using the window-test specimens, exposing the specimens to three different types of testing procedure: 1. Natural infestation in the open air; 2. Artificial infestation and exposure in the open air; 3. Artificial infestation in a green-house. The results show good similiraties of the three parallel tests in term of decay, and assess the reliability of the windo...
G R Y Déon, L N Trong


Improved preservative penetration of spruce after pre-treatment with selected fungi. II. Creosote treatment, analysis and strength testing
1998 - IRG/WP 98-40106
This paper describes the creosote treatment and analysis of logs pre-treated with selected fungal agents as a method of increasing the porosity of the wood prior to preservative treatment. The paper also reports the subsequent strength testing of the timber to evaluate the effects of the fungal pre-treatment on the structural integrity of the wood. European spruce logs were pre-treated with eithe...
E J Tucker, A Bruce, H J Staines, B Rosner, K Messner


Improved preservative penetration of spruce after pre-treatment with selected fungi. I. Fungal pre-treatment of pole sections
1998 - IRG/WP 98-40117
European spruce logs were pre-treated with either Phanaerochete chrysosporium, Dichomitus squalens, Trichoderma viride and Trichoderma aureoviride for incubation periods of between 1-4 weeks prior to pressure treatment with creosote in a commercial treatment plant and analysed for strength and creosote uptake (see part II Tucker et al.). A method to pre-treat logs was optimised. The pole sections ...
B Rosner, K Messner, E J B Tucker, A Bruce


Research studies on infecting behaviour of Fomes fomentarius (L. ex FR) Fr. and its physical control in the wood yards of the Hyrcanian (Caspian) forests of Ira
1996 - IRG/WP 96-10179
Due to illegal cutting, girdling and ringbarking many damages of tinder fungus (Fomes fomentarius (L. ex Fr) Fr.) are seen on beech, poplar, oak and birch at Hyrcanian (Caspian) forests of Iran. The beeches (Fagus orientalis Lipsky) are damaged highly and the beech community of Fagetum are infected from 800 meter altitudes at Gorgan (East of Caspian forests) to 600 meters altitudes at Gilan (West ...
P Niloufari


The effect of soil pre-exposure on the results of laboratory Basidiomycete testing
1991 - IRG/WP 2385
Scots pine sapwood blocks were treated with several concentrations of copper chrome arsenic (CCA), copper chrome boron (CCB) and a copper modified quaternary ammonium compound (CMAAC). Leached and unleached samples were exposed in a basidiomycete monoculture test using Coniophora puteana, a copper tolerant brown rot. Prior to testing half of the blocks were buried in unsterile soil for 4 weeks. Th...
S M Gray


Variation in biological performance of CCA caised by preservative application method
1996 - IRG/WP 96-40072
A series of laboratory studies to investigate the influence of treatment application method on CCA performance in Cosican pine has been completed. Biological decay tests, such as serial exposures, were used to induce decay in wood at preservative retentions of up to 10 kg/m³ CCA salts. Significant differences in performance of the preservative against either brown, white or soft rot decay fungi w...
P R Newman, R J Murphy


Shorter-term biological control of wood decay in pre-seasoning pine roundwood as an alternative to chemical methods
1992 - IRG/WP 92-1555
Previous studies on the long-term control of decay in creosoted transmission poles, using Trichoderma and other antagonistic moulds, have met with limited success. However, it is possible biological control is more suited to control of decay on shorter time scales. An earlier study, focusing on pre-seasoning treatment of transmission poles showed that favourable porosity increases could be brought...
M W Schoeman, D J Dickinson


Effects of pre-harvest girdling on selected properties of red pine, red maple and Eastern larch
1999 - IRG/WP 99-40137
Trees of three species - tamarack (Larix laricina), soft maple (Acer rubrum) and red pine (Pinus resinosa) - were girdled immediately below the crown,one to two years before felling. The wood from these trees was compared with wood taken from un-girdled control trees felled at the same. Sapwood and heartwood, from the controls, and from above and below the girdle of treated trees, were examined fo...
A Taylor, P A Cooper


Enhancing the Performance of Transparent Coatings by UV Protective Pre-treatments
2006 - IRG/WP 06-30399
Most industry observers anticipate a change from copper-based preservatives to metal-free combinations of organics for residential treated wood products in North America within the next one to five years. While the chromium copper provide considerable protection against UV, metal-free formulations will need UV protection in the form of additives or coatings. While transparent coatings can be made ...
P I Morris, S McFarling


Effects of acetic acid and nitric acid pre-treatment on copper content of spruce wood treated with CBA-A and CCA
2008 - IRG/WP 08-40406
This work investigates the effects of nitric acid and acetic acid on compression strength values and copper retention contents of refractory spruce wood (Picea oriental L.) treated with the waterborne preservative Copper azole, (CBA-A, Tanalith-E 3492) and copper / chrom / arsenic (CCA). Before the CBA-A and CCA treatment, the samples were immersed in 500 ml of nitric and acetic acid solutions for...
S Yildiz, E Dizman, Ü C Yildiz


Use of biological and low toxicity products against subterranean termites
2009 - IRG/WP 09-20410
The climatology of Mediterranean countries is favourable to the development of termites that cause important damage to wood structures in both furniture and buildings. Until a few years ago the treatment for this type of insect was based on the impregnation of the wood with chemical products. The use of these chemicals is now being restricted in Europe since the publication and harmonization of n...
M T Troya, M J Prieto, F Rubio


Assessment of Boracol 200RH (FrameSaver) as a remedial treatment to control decay in pre-decayed model timber frame units
2010 - IRG/WP 10-30529
Model timber frame units constructed from untreated radiata pine were pre-wetted to approximately 40% moisture content and inoculated with Coniophora puteana and Oligoporus placenta. Units were transferred to a controlled environment room maintained at 25°C and 95% RH for 7 and 10 weeks to allow two levels of decay to become established in units. Following pre-decay, units were disassembled, clea...
Mick Hedley, Dave Page, Jackie van der Waals


Determination of the natural durability of solid wood against wood-destroying fungi - a European round-robin test
2013 - IRG/WP 13-20511
In Europe the durability of wood against wood-destroying basidiomycetes is tested according to CEN/TS 15083-1 (2005). Hitherto existing experience with this standard is quite heterogeneous and results from previous round-robin tests have stayed unreported or have been reported incompletely. In particular the need for natural pre-weathering of the test specimens to allow potential detoxification of...
C Brischke, C R Welzbacher, A Gellerich, S Bollmus, M Humar, K Plaschkies, W Scheiding, G Alfredsen, J Van Acker, I De Windt


Pre-treatment decay and strength loss of railroad ties, and their prevention
2013 - IRG/WP 13-30610
Evidence of fungal decay in air-drying, untreated railway crossties is referred to as ‘stack burn’ in the industry. The deleterious consequences of stack burn on tie mechanical properties was confirmed by evaluating the impact bending toughness of wood samples taken from untreated tie stock air dried in the southern United States. These results suggest that careful consideration should be give...
A M Taylor, B Jordan, J D Lloyd


Characterization of wood modification prepared by in situ polymerization with pre-polymer and the mechanism of modification
2013 - IRG/WP 13-40633
Chemical modification of wood is a potential way to obtain high quality wood. In this study, the fast-growing poplar was impregnated with modifier using a pulse-dipping machine by in situ polymerization. Fungal decay analysis, mechanical properties and dimension stability of the natural and modified woods were investigated. The wood samples were also characterized by X-ray diffraction (XRD) Therma...
Qian Lang, Zeng Bi, Junwen Pu


Relevance of natural pre-weathering for laboratory decay tests with native, modified, and preservative-treated wood
2013 - IRG/WP 13-20522
The on-going development of new wood protection systems is hampered by the long term field tests currently in use. New accelerated test methods and novel methods for faster and more accurate evaluation of wood protection methods are requested. For both field decay tests and accelerated laboratory decay tests, limitations are imposed. This study is part of the research program ‘WoodBuild’, whic...
A Pilgård, C Brischke, L Meyer


Prevention of fungal damage of oil and date palm wood by organic acids
2017 - IRG/WP 17-10877
Felled palm trunks are susceptible to fungi as long as their moisture content is above fibre saturation. During this period, palm wood has to be protected against mould and rot fungi. Environmental-friendly organic acids are suitable. Small samples of oil palm (Elaeis guineensis) and date palm (Phoenix dactylifera) wood were treated with 1 to 10% solutions of acetic acid and propionic acid, respec...
M Bahmani, O Schmidt


The Effects of Pre-Microwave Treatment on Retention Levels And Some Mechanical Properties of Spruce Wood Treated with CCA
2017 - IRG/WP 17-40800
Microwave (MW) treatment of wood has been evaluated in recent years for different purposes by several scientists. Microwave conditioning improves permeability, reduces density and heat conductivity and changes dimensional stability. Furthermore, it could even improve the permeability of refractory wood species such as spruce and Douglas fir. In this study, MW pre-treatment was applied to spruce wo...
E D Gezer, S Kuştaş, S Durmaz


Suggestive remarks for designing of experimental samples and trial devices to treat wood by pre-vacuumed immersion method
2019 - IRG/WP 19-40862
This study was conducted to test the impregnability of wood material according to the pre-vacuumed immersion process and to reveal the usability of cylindrical (plug) samples in impregnation experiments in addition to the cuboid or cubic samples. In this context, cuboids were prepared 30 mm in length, 20 mm in width and 20 mm in thickness, whereas plugs were prepared radially and longitudinally wi...
I Usta


Performance of a water-borne stain on beech, spruce, MDF and OSB improved by plasma pre-treatment
2020 - IRG/WP 20-40897
Coatings are an important part of wood protection, especially for outdoor applications. In order to provide a good protection, protective coatings need to exhibit good adhesion, mechanical resistance, and weathering resistance. Plasma pre-treatments are an established method to increase the performance of existing coatings including those on wood and wood-based substrates. Moreover, plasma deposit...
S Dahle, J Žigon, I Uranjek, M Petrič


Steam Pre-conditioning Treatment Prior to Acetylation: Impact on Dimensional Stability, Moisture Response Behaviour, and White-Rot Fungal Resistance of Hevea brasiliensis and Mitragyna ciliata Wood
2022 - IRG/WP 22-40930
The effect of steam pre-conditioning treatment on the dimensional stability, moisture response behaviour, and durability against white-rot fungus P. chrysosporium of acetylated Hevea brasiliensis and Mitragyna ciliata wood species were assessed. Defect-free specimens of both species from the top, middle, and base positions were selected, prepared according to ASTM D143-09 & ASTM D-2017 standards a...
E Uchechukwu Opara, J Mayowa Owoyemi, J Adeola Fuwape


The impact of pre-drying on treatment level variations of esterified solid wood analysed by X-ray densitometry
2023 - IRG/WP 23-40977
Wood modification requires homogenous treatment levels within the wood matrix to prevent insufficiently treated areas being subject to biodeterioration. Esterification of wood by citric acid and sorbitol can show differences in density caused by uneven chemical distribution during the curing phase and can be detected by x-ray densitometry. This study used density profiling to investigate the influ...
A Treu, S O Amiandamhem, E Larnoy