Your search resulted in 1047 documents. Displaying 25 entries per page.
Isolation and evaluation of Lactobacillus brevis from chilli waste for potential use as a wood preservative
2011 - IRG/WP 11-10749
Lactic acid bacteria were isolated from chilli waste and evaluated for their ability to arrest wood rotting basidiomycetes. In previous work a quick screening method using 96 well plates and measuring absorbance to determine fungal growth was developed specifically to investigate the efficacy of isolated bacteria against wood decay fungi. Using this method, one bacterium (isolate C11) was identif...
D O’Callahan, T Singh, I R McDonald
Basidiomycete colonization of Scots pine sapwood quantified by qPCR and TGA
2011 - IRG/WP 11-10750
Scots pine (Pinus sylvestris L.) is an important softwood species in Northern Europe and is frequently used as material for various wood protection systems. In Europe, EN 113 is the standard basidiomycete laboratory durability test method, using mass loss as evaluation criteria. In this paper quantitative real-time PCR (qPCR) and thermogravimetric analysis (TGA) was used to characterize coloniza...
G Alfredsen, S Bollmus, T K Bader, K Hofstetter
Molecular investigation of Postia placenta growing in modified wood
2011 - IRG/WP 11-10756
Brown rot is the most common and destructive type of fungal decay for wood in service. These fungi depolymerize preferentially the structural carbohydrates, cellulose and hemicellulose in the cell wall leaving oxidized lignin behind. Modified wood can provide protection against a variety of wood deteriorating organisms, including decay fungi. However, there is still little known about the mode of ...
B Schmöllerl, G Alfredsen, C G Fossdal, M Westin, A Steitz
Sample Origin Influencing the Leachability of Wood Preservatives
2011 - IRG/WP 11-20474
The aim of this study is to see if the raw material influences fixation and leachability of wood preservatives. Moving towards more eco-friendly and –concious society, the wood industries must adjust itself to new rules and regulations. Greener solutions in wood protection are being tested and introduced, older systems are being improved, but questions still arise concerning some elements curren...
K Kängsepp. E Larnøy, P Meier
Slice - Cut and Analyze Laser Microdissection (LMD): A method to produce sample material from modified wood for chemical quality analysis
2011 - IRG/WP 11-20478
Wood modification with its various systems is an established way to enhance a wood products’ service life in outdoor applications. Per definition, selected material properties are enhanced by means of modification without producing toxic substances or residues during service life and combustion afterwards. The systems of impregnation modification include a physical and often chemical alteration ...
K Zimmer, E Larnøy, A Treu, M Fongen
LOSP for glulam, when should the treatment be applied?
2011 - IRG/WP 11-30555
Treatment options for outdoor above-ground (H3) exposed glulam of Pinus radiata and P. elliottii were examined. Beams were treated with azole LOSP (containing a zinc tracer) aiming for retentions of 35-40 l/m3 or 70-80 l/m3. Treatment was conducted either before or after gluing. TBTN LOSP and CCA were included as comparative treatments. Test specimens for exposure were cut after treatment, while w...
L J Cookson
Comparison of rates of wood decay from four different field test protocols following 4-5 years exposure at a site in New Zealand
2011 - IRG/WP 11-30565
The rate of decay of Pinus radiata was evaluated using four different field test protocols at a site near New Plymouth, New Zealand. The average Scheffer index was 86 over the five year period of testing. The field tests were an in-ground stake test (AWPA Std E7-01) and three above ground tests – lap-joint (AWPA Std E16-98), decking (AWPC protocol) and ground proximity tests (AWPA Std E18-06) T...
P Lobb, K Day, A Siraa
Termite resistance of timber envelope treated with imidacloprid then modified by typical building site operations
2011 - IRG/WP 11-30570
Imidacloprid is a new envelope insecticide approved by Australian regulatory authorities for framing timber. It is a non repellent insecticide. Results are reported for timber envelope treated with imidacloprid and altered post treatment with typical building site operations to expose untreated surfaces. These modifications included, cutting, notching and drilling. Pinus radiata timber samples w...
K Day, A Siraa, P Lobb
The potential of silicone-based formulations to enhance wood properties through industrial treatment for outdoor use
2011 - IRG/WP 11-30578
High hygroscopicity is one of the main weaknesses of wood as far as its susceptibility to biodegradation, and specifically to fungal decay. New wood preservation technologies are constantly entering the wood protection market, competing with traditional, biocide-based preservation. Silicones are commercially used as hydrophobic agents on stones and concrete. They belong to the restricted number of...
F Simon, F Marchal, F Pochon, M Kutnik, I Le Bayon
The Effectiveness of Machined Profiles at Reducing the Checking of Wooden Decking
2011 - IRG/WP 11-40541
This study tests the hypothesis that ‘the ability of surface profiling to reduce checking of deck boards exposed to weathering will vary with wood species and profile type’. Southern pine (Pinus sp.) and Pacific silver fir (Abies amabilis) deck boards were machined to produce three different types of surface profiles: flat (control), ribbed (V-shaped grooves), and rippled (U-shaped grooves). B...
P Evans, I Cullis, P Morris
Study of the durability of the Maderon® against wood decay fungi and insects
2011 - IRG/WP 11-40548
Many industries produce residues that are not easily degradable. One of these is nut husks which, due to their high level of resistance to biological and environmental degradation, have become an ecological problem. Maderón® is a material invented and patented in Spain employed as an ecological substitute and a modern alternative to certain uses of wood. At present, Maderón® is commercialized ...
M T Troya, F Llinares, P Jiménez, J I Fernández-Golfín, M Conde, R Díaz
Treatability variation of scots pine heartwood from Northern Europe
2011 - IRG/WP 11-40563
Scots pine (Pinus sylvestris L.) is one of the most common construction materials for general exterior applications in northern Europe. It has a wide natural geographical distribution, a good availability and it is low-priced compared to other materials. According to EN 350-2 Scots pine heartwood is considered being “untreatable” and having durability class 3. This means that its durability co...
G Behr, E Larnøy, C-T Bues
Decrease of stiffness properties of degraded wood predicted by means of micromechanical modeling
2011 - IRG/WP 11-40570
Wood exhibits a highly anisotropic mechanical behavior due to its heterogeneous microscopic structure and composition. Its microstructure is organized in a strictly hierarchical manner from a length scale of some nanometers, where the elementary constituents cellulose, hemicelluloses, lignin, and extractives are found, up to a length scale of some millimeters, where growth rings composed of earlyw...
T K Bader, K Hofstetter, G Alfredsen, S Bollmus
Microscopy evaluation of microbial decay patterns in wood stakes after 6 years in soil contact
2010 - IRG/WP 10-10715
Most studies on wood modification have so far been concerned with service life predictions rather than investigating the decay protection mechanism. Very little is known about the mode of action of these new treatments and about the strategies used by wood degraders in order to utilize the wood material despite a treatment. Access to such knowledge would allow further modification and improvement ...
A Pilgård, C G Björdal
Seasonal shifts of fungal community structure at the interface of treated or untreated wood and soil
2010 - IRG/WP 10-10721
Many wood species are degraded rapidly in soil by the fungal community. In order to preserve wood and structures in which it is used, chemical preservatives are used. Little is known about the interaction of treated wood and the surrounding soil fungal community. For this work, presented at IRG 41, wooden specimens (Pinus sylvestris sapwood, sizes 25 mm x 50 mm x 500 mm (longitudinal)) were treate...
M Noll, I Stephan
Qualitative - Quantitative Analysis of Wood-Inhabiting Fungi in External Wooden Structures of the Latvian Cultural Heritage
2010 - IRG/WP 10-10728
The frequency and diversity of wood inhabiting fungi in the exterior wood were established in the Araishi lake fortress, the Lielvarde wooden castle, the Latvian Ethnographic Open-Air Museum, Riga, and twelve wooden heritage objects in the Eastern part of Latvia (Latgale). The inspected wooden structures of the external woodwork included windows, stairs, walls, floorings, roofs, fences, and benche...
I Irbe, M Karadelev, B Andersons
Postia placenta gene expression during growth in furfurylated wood
2010 - IRG/WP 10-10734
Modified wood can provide protection against a range of wood deteriorating organisms. But we still lack information about why the modified wood is protected from microbial attack. Several hypotheses have been put forward for the mode of action against wood decaying fungi, including inhibition of action of specific enzymes, but they still need further testing. In this study gene expression of the b...
G Alfredsen, C G Fossdal
The Use of Micro-Tensile Testing to Assess Weathering Decay and Oxidative Degradation of Wooden Items
2010 - IRG/WP 10-20433
This paper presents a method to study the weathering performance of wooden items and to assess the oxidative degradation of wood via the Fenton reaction. Weathering resistance and photo-stability of wood was tested using pine wood (Pinus sylvestris) veneer strips measuring approximately 60 µm in thickness. The veneer strips were treated using a reactive chemical to impart surface protection. The ...
C Mai, Yanjun Xie, Zefang Xiao, P D Evans, H Militz
Service life prediction of wooden components – Part 1: Determination of dose-response functions for above ground decay
2010 - IRG/WP 10-20439
Scots pine sapwood (Pinus sylvestris L.) and Douglas fir heartwood (Pseudotsuga menziesii Franco) specimens were exposed in double layer field trials at 24 different European test sites under different exposure conditions (in total 28 test sets). The material climate in terms of wood moisture content (MC) and wood temperature was automatically recorded over a period of up to eight years and compar...
C Brischke, A O Rapp
Stress wave and visual analysis of treated and non treated fence posts after 15 years in field test
2010 - IRG/WP 10-20449
Wood preservation may play an important role in protecting tropical rain forest. Basically, it can reduce pressure on natural resources by increasing wood durability. Field tests are conducted to simulate final use of woods under different environmental conditions. Visual analysis, non destructive testing, and non destructive evaluation techniques were applied to assess wood resistance and chemica...
A Florian da Costa, R Faustino Teles, J Costa Gonçalves
Synthesis of novelty borate compounds for wood preservatives: Laboratory test of leachability and decay resistance
2010 - IRG/WP 10-30520
A novel series of ammonium tetraphenylborate (ATB) and borate chemical compounds (BBC) were synthesized as wood preservatives. The leaching rates and decay resistance of boron formulations containing ATB and BBC were conducted. The laboratory leaching results showed that boron leaching rate of treated wood by ATB formulations was from 2.1% - 6.7%, while that of BBC formulations from 23.3% -59.0%. ...
Zhiqiang Li, Mingliang Jiang, Xingxia Ma
Adsorption of ACQ components in wood
2010 - IRG/WP 10-30522
To investigate the chemical adsorption capacity of copper-monoethanolamine (Cu-Mea) components on wood, the Na+ cation exchange capacity (CEC) of red pine (Pinus resinosa Ait.) was determined and compared to the adsorption capacity of free Mea and Cu-Mea complexes. The CEC increased with increasing pH. Free Mea adsorption as a function of pH followed the sodium adsorption curve except at pH over 9...
Myung Jae Lee, P Cooper
Evaluation of ACQ-D treated Chinese fir and Mongolian Scots pine with different post-treatments after 20 months of exposure
2010 - IRG/WP 10-30530
The performance of alkaline copper quat-type D (ACQ-D) treated Chinese fir (Cunninghamia lanceolata Hook.) and Mongolian Scots pine (Pinus sylvestris Linn. var. mongolica Litv.) stakes after 20 months exposure in Chengdu and Guangzhou of southern China were evaluated according to AWPA standard E07-07. The ACQ-D treatments used two concentration levels (0.5 and 1.0%) and four different post-treatme...
Lili Yu, Jinzhen Cao, Wei Gao, Haitao Su
Chemical protection of historic timber structures: Results and future needs
2010 - IRG/WP 10-40487
The paper concentrates on the analysis of the effectiveness of chemical protection for timber structures in the Russian State Museums “Kizhi” (Karelia) and “Vitoslavlitsy” (Novgorod).
The condition of historic timber was tested at the monuments treated with PCP, borax, potassium carbonate, boric acid, Pinotex chemicals in the 1970-80. Long-term analysis revealed that in many cases the...
M Kisternaya, V Kozlov
Decay and termite resistance of particleboard and MDF panels made from pinecones
2010 - IRG/WP 10-40493
Particleboard and medium density fiberboard (MDF) panels were produced by using pinecone from stone pine (Pinus pinea L.) tress and wood particles from pine and beech wood at various ratios. Specimens from the panels were subjected to slightly modified soil-block tests according to AWPA E10-06 standard method by using two brown-rot fungi, Gloeophyllum trabeum and Postia placenta and two white rot ...
C Köse, E Terzi, Ü Büyüksar, Erkan Avcı, Nadir Ayrılmış, S Nami Kartal, Y Imamura