Eucalyptus globulus. Impregnability in relation with plantation and crop
1992 - IRG/WP 92-2402
Eucalyptus globulus Lasill is currently classified in Pr EN 350 on the basis of the characteristics of the first log. In practice, there are usually several following crops of branches developped on each stump in plantations. Up to a diameter of 8 cm, round wood of 2nd crop and further crops present a maximum of sapwood and characteristics which differ significantly from the basic classification a...
D Dirol


Incomplete fixation of chromium in the pre-treated wood with a solution of copper and arsenic compounds
1995 - IRG/WP 95-50052
Ponderosa pine wood thin sections were treated with a combination of chromium, copper, and arsenic chemicals. The wood sections was analyzed by electron spin resonance spectrometry (ESR) and X-ray photoelectron spectrometry (XPS) to elucidate the mechanism of fixation of the chromated-copper preservatives. The wood subjected to the two-step treatment with copper and arsenic followed by chromium ex...
J N R Ruddick, K Yamamoto, F G Herring, P C Wong, K A R Mitchell


Evaluation of the european standard ENV 12038 for durability testing of plywood
2001 - IRG/WP 01-20237
The latest improved version of the standard ENV 12038 drafted as document N44 by CEN Technical Committee 38 (WG 7 - WG 23) is used to evaluate the effect of wood composition and structure on plywood durability. The method described is based on the agar-block test of the EN 113 standard used for the determination of the efficacy of wood preservatives and the assessment of the natural durability of ...
J Van Acker, M Stevens, E De Clercq


Kiln drying of poles as a means of solving the problems of pre-treatment decay in poles
1985 - IRG/WP 1263
The concept that pre-treatment decay can cause wide variation in the treatability of wood and especially wood poles has caused much discussion and debate in wood preservation circles. Yet it seem only logical that if decay has effected the strength characteristics of the wood and caused a differential moisture content in the wood the treatment of the end product will be highly variable and the lon...
J A Taylor


Laboratory trial to identify potential in-forest treatments to control fungal pre-infections of radiata pine logs
2000 - IRG/WP 00-30220
Development of fungal infections of radiata pine logs by wood degrading fungi commences immediately after tree felling. In general, subsequent antisapstain treatments are unable to control fungal degrade on logs where the pre-treatment log storage time exceeds 2-5 days. However, use of an in-forest treatment of logs may be advantageous to log exporters to control fungal pre-infections during the p...
D R Eden, B Kreber, R N Wakeling, J G Van der Waals, C M Chittenden


The effect of alternative pre-conditioning procedures on the durability of wood based board materials to decay fungi
1997 - IRG/WP 97-20105
In the biological testing of wood based board materials it has been shown that exposure of boards in a closed vessel system may lead to inaccurate results due to the build up of volatile substances that inhibit the test fungi. It is thought that this is a transitory effect of freshly manufactured boards. In the European standard for testing fungal durability of board materials which is currently u...
S F Curling, R J Murphy, J K Carey


Status of Work on OECD Test Guidelines for Emissions of Wood Preservatives to the Environment
2005 - IRG/WP 05-50224-3
In April, 2003, OECD published an ESD on wood preservatives that provides guidance on how to estimate emissions: 1) during the wood preservative application processes and storage of treated wood prior to shipment; and 2) from treated wood-in-service. The ad hoc Expert Group that developed the wood preservatives ESD identified the need to develop Test Guidelines to estimate the amount of biocides ...
W Jakob


Some studies on fungal deterioration of rubber wood (Hevea brasiliensis)
1980 - IRG/WP 2140
For the sreening of anti-stain chemicals trials with selected agricultural fungicides and new chemicals were carried out. Botryodiplodia theobromae, Aspergillus sp. and Penicillium sp. were used at test organisms. For testing the durability of rubber wood (Hevea brasiliensis) suitable local rotting fungi (Basidiomycetes), based on high degrading power, which may later be employed in standard tests...
A Sujan, A G Tan, M Stevens


Accelerated diffusion treatment of sawn Sitka spruce grown in the UK
1986 - IRG/WP 3395
The treatment of 'green' sapwood and heartwood of Sitka spruce by diffusion methods was investigated. Steam/dip treatment processes gave increased solution uptakes and depths of penetration of copper in comparison with a simple dip treatment. Further investigation is required to reduce diffusion gradients with copper based formulations and to improve the penetration of '...
R J Murphy, D J Dickinson


Improved preservative penetration of spruce after pre-treatment with selected fungi. II. Creosote treatment, analysis and strength testing
1998 - IRG/WP 98-40106
This paper describes the creosote treatment and analysis of logs pre-treated with selected fungal agents as a method of increasing the porosity of the wood prior to preservative treatment. The paper also reports the subsequent strength testing of the timber to evaluate the effects of the fungal pre-treatment on the structural integrity of the wood. European spruce logs were pre-treated with eithe...
E J Tucker, A Bruce, H J Staines, B Rosner, K Messner


Improved preservative penetration of spruce after pre-treatment with selected fungi. I. Fungal pre-treatment of pole sections
1998 - IRG/WP 98-40117
European spruce logs were pre-treated with either Phanaerochete chrysosporium, Dichomitus squalens, Trichoderma viride and Trichoderma aureoviride for incubation periods of between 1-4 weeks prior to pressure treatment with creosote in a commercial treatment plant and analysed for strength and creosote uptake (see part II Tucker et al.). A method to pre-treat logs was optimised. The pole sections ...
B Rosner, K Messner, E J B Tucker, A Bruce


Artificial weathering exposure as an alternative for standard ageing according to EN 84 (leaching) and EN 73 (evaporation)
2002 - IRG/WP 02-20254
In order to verify potential weaknesses of wood preservatives fungal tests are carried out after ageing of wood preservative treated test blocks. The European standard EN 599 as a framework for efficacy assessment of wood preservatives includes the use of two ageing methods prior to fungal testing, namely a leaching method (EN 84) and an evaporation method (EN 73). The European research project "F...
J Van Acker, M Grinda, D J Dickinson


Standard principles of testing termiticides: A discussion paper
1991 - IRG/WP 1502
Recent restrictions and banning of termiticides such as organochlorines in some countries has focussed attention on the need for new and novel compounds as termiticides. However, this poses problems for both wood preservative manufacturers and termitologists. Test procedures have to be devised to evaluate the new termiticides so that the tests are practical, encourage vigorous termite activity, an...
J R J French


Characterization of Poria indoor brown-rot fungi
1995 - IRG/WP 95-10094
The heterogeneous group of "Poria" fungi causing brown rot in buildings and also of wood in ground contact comprises Antrodia vaillantii, Antrodia serialis, Antrodia sinuosa, Antrodia xantha and Tyromyces placenta. These fungi have similar morphological appearance and biology. Their nomenclature has a confusing history and is still not uniform. As a consequence, misinterpretations may occur. SDS p...
O Schmidt


Experiences with supervision schemes for treated timber in Denmark
1984 - IRG/WP 3315
Since 1967 a voluntary supervision scheme for vacuum-pressure treatment was established in Denmark. In 1976 the Nordic Wood Preservation Council - NWPC - established a scheme based on wood preservation classes for treated timber as a joint technical standard valid in Denmark, Finland, Norway and Sweden. This paper deals with inspection results over 17 years for CCA treatment within our organizatio...
J Sabroe


Determination of corrosive effect of liquid wood preservatives to metals – First experiences with a National Standard which is in revision
2006 - IRG/WP 06-20321
The development of standards is an essential tool to characterise different kind of materials and products. An important aspect during the development of a new product is to check the corrosion behaviour with other materials. Corrosion can cause several problems like pitting corrosion. Consequently the knowledge concerning the corrosive effect of liquid wood preservatives is important due to the s...
E Melcher


Reappraisal of some fungicides by the amended JWPA method
1992 - IRG/WP 92-3689
Organoiodine compounds which have been commercialized these years in Japan poorly performed as fungicides in the amended JWPA decay test (Standard 1, 1989) when applied to superficial treatment of timber. Because some parts of active ingredients seemed to disappear from the treated timber surface mainly due to the severe leaching cycles. This was prominently true for beech (Fagus crenata Blume) sa...
K Tsunoda


Standard and accelerated testing of boron-additive wood protection systems
2005 - IRG/WP 05-30381
The main objective of this research was to determine the effectiveness of boron-additive protection systems for above ground applications by means of field testing. The two field test procedures used are based on the L-joint test described in the European standard EN 330. For the first set up the boron treated timber was coated in accordance with the standard EN 330 system. The second set up is ba...
A Mohareb, J Van Acker, M Stevens


The effect of soil pre-exposure on the results of laboratory Basidiomycete testing
1991 - IRG/WP 2385
Scots pine sapwood blocks were treated with several concentrations of copper chrome arsenic (CCA), copper chrome boron (CCB) and a copper modified quaternary ammonium compound (CMAAC). Leached and unleached samples were exposed in a basidiomycete monoculture test using Coniophora puteana, a copper tolerant brown rot. Prior to testing half of the blocks were buried in unsterile soil for 4 weeks. Th...
S M Gray


Determination of fungitoxic value of preservatives in laboratory wood-block tests. Part 1: Standard procedures
1989 - IRG/WP 2326
By applying a modified agar-block method, a comparative analysis was made on the toxic value of the wood preservative CCA against the test fungus Serpula lacrymans. The procedure applied to determine the results accounted for different standards: EN (Toxic limit), ASTM (threshold retention), GOST (threshold retention and protection probability), PN (toxic doses) and JIS (value of efficiency). Desp...
J Wazny, J D Thornton


Variation in biological performance of CCA caised by preservative application method
1996 - IRG/WP 96-40072
A series of laboratory studies to investigate the influence of treatment application method on CCA performance in Cosican pine has been completed. Biological decay tests, such as serial exposures, were used to induce decay in wood at preservative retentions of up to 10 kg/m³ CCA salts. Significant differences in performance of the preservative against either brown, white or soft rot decay fungi w...
P R Newman, R J Murphy


Physiological properties of fungal test strains according to the European Standard EN 113
1986 - IRG/WP 2258
For the discussion of the European standard EN 113 the EMPA's procedure of culturing the test fungi and the corresponding virulence of the test fungi as well as the wood moisture content at the end of the test are shown. It is mainly shown that within the standard the choice of the solvent may not be left at the test lab if reproducible results shall be obtained. The different solvents in...
E Graf, B Zgraggen, P Manser


Japanese standardized method for evaluating effectiveness of anti-sapstain and anti-mould chemicals
1988 - IRG/WP 2299
Japan Wood Preserving Association established a method for testing effectiveness of chemicals against sapstain and mold fungi on wood in 1979. The method is concerned with a laboratory technique using small timber specimens (20 x 50 x 3 mm³), petri dish and 5 test fungi. Effectiveness of each candidate chemical is evaluated on the basis of the relative resistance to sapstain and mold fungi which ...
K Tsunoda, K Nishimoto


Methodologies for termiticide testing and standardization
1993 - IRG/WP 93-10043
Standardization of testing methodologies for termiticides has been one of the main topics of discussion for Working Group 1b in recent IRG meetings. While it is agreed that there is a need to provide a standardized testing procedure for industry and regulatory agencies, concerns remain that such a standardized procedure may become an obstacle for developing better testing methods or innovations in...
N-Y Su


Towards a unified international hazard class system
1996 - IRG/WP 96-20081
Working party 2.5 on International Standardisation has set the development of a unified hazard class system as a short-term objective. This document is intended to stimulate the discussion required to work towards such a system. Two possible approaches are discussed, the compromise approach and the development of a basic system from first principles. For the second approach, the factors impacting ...
P I Morris