Rapid analysis - chances and limitations
1999 - IRG/WP 99-50130
The reuse of wood out of service in the particle board industry demands a proper handling and separation of assortments with differing content and nature of preservative. A pre-selection based on visual and olfactorial characteristics can be carried out for certain assortments like sleepers, poles, etc. Problems arise from diffuse and less intensive treated wood which is regularly dip-treated or b...
A Peylo, R-D Peek


A case study on quality control on telephone poles as a cost saving tool in Tanzania
1987 - IRG/WP 3418
A sample of 28 CCA treated Eucalyptus poles from a lot of 2,000 poles awaiting delivery to the field, was studied to reveal the quality of treatment. Results showed a product of very poor quality. Average figures for penetration and retention were 8.4 mm and 2.2 kg/m³; these results are 66% and 91% below the required standards, respectively. Consequences of such results are estimated to amount to...
K K Murira


Wood preservation in France. "Bois plus" chain of quality. Description of the scheme early 1989
1989 - IRG/WP 3519
1989 - description of the French "CTB-BOIS PLUS" homologation scheme
G Ozanne


Treatment of dried sawn spruce and redwood building timbers with water-borne preservatives under a scheme for the quality control of the preservation and preserved wood in the Netherlands
1978 - IRG/WP 3123
Treatment of dried sawn spruce and redwood Building Timbers with water-borne preservatives under a scheme for the quality control of the preservation and preserved wood in the Netherlands. The aim of this article is to give the reader a modest description of the evaluation of fundamental research in wood preservation into a practical application....
H F M Nijman, N Burgers


Wood Preservation in France. A statement of quality control early 1986
1986 - IRG/WP 3389
A statement of quality control in France early 1986 - Summary of new - Standards criteria for preservatives and treated wood - Aptitude of treated wood for use per class of biological hazard...
M Romeis, G Ozanne


A simple leaching procedure for in-plant monitoring of CCA fixation
1993 - IRG/WP 93-30023
A simple leaching test is described to quantitatively estimate the extent of fixation of chromated copper arsenate (CCA) preservative treated wood products. It is based on the reaction between diphenylcarbazide and unreacted hexavalent chromium leached from borings taken from treated wood during the fixation process. The test requires about 20 minutes to complete and can be set up in a treating pl...
P A Cooper, Y T Ung


Quality control of microwave treatment of timber after dry rot attack
2001 - IRG/WP 01-40205
In Denmark microwave treatment of timber has been used during the last 15 years for eradication of dry rot (Serpula lacrymans). About 1500 microwave treatments have been employed in coorporation with Hussvamp Laboratoriet. Previously all the infected timber was removed plus an extra metre as a safety zone. This meant that all casting boards and plaster had to be removed as well and joists replaced...
J Bech-Andersen, J Andreasson, S A Elborne


The role of third party independent inspection agency for wood preservation industry in China
2009 - IRG/WP 09-20425
This presentation attempts to provide a brief historical background and a current status report on the wood preservation industry in China. In addition, it will briefly introduce the need for building the quality control procedures and China wood protection Quality Supervision and Testing Center, a third-party inspection agency. Besides, some suggestions of this industry are proposed for its furth...
Zhenzhong Tang, Changsheng Shen, Yujie Han, Changming Song


Quality assurance approach of the German TMT manufacturers
2010 - IRG/WP 10-40513
Due to an increasing number of TMT manufacturers in central Europe, an organisation of TMT manufacturers was founded in Germany in the beginning of 2010. Since the current level of product testing and property declaration is not satisfying, one of the first activities is the establishment of a quality assurance system. In this paper a concept for quality assurance (QA) will be outlined....
W Scheiding, C R Welzbacher, A O Rapp


Measurement of VOC emissions from curative treated wood: A new emission test chamber
2001 - IRG/WP 01-50166-13
A poor indoor air quality (IAQ) is now recognized as a potential factor affecting occupants health. There are three basic strategies to improve IAQ: source control, improvement of the ventilation and use of air cleaners. Usually, the most efficient way to improve IAQ is to eliminate the different pollutant sources or to reduce their emissions. In order to precisely measure emissions from building ...
F Maupetit, O Ramalho, C Yrieix


A study of wood quality of Juglans nigra and hybrid walnut (MJ 209xRA) : durability against Coriolus versicolor, density and MOR
2004 - IRG/WP 04-10522
The study investigated possible effects of harvesting season on some wood properties of Juglan nigra (JN) and a hybrid walnut (MJ209xRA). The samples were taken from trees which were harvested in June July, August, November of the same year, and March in the year after to determine whether there were any significant differences in wood properties as regards the harvesting seasons. In order to test...
B Charrier, F Charrier, D P Kamdem, J B Aurel, G Janin


The effect of felling time of year on CCA fixation rate and quality of selected hardwoods
1998 - IRG/WP 98-40116
White birch (Betula papyrifera), poplar (Populus sp.) and red maple (Acer rubrum) trees were harvested in winter, in spring, before the leaves flushed, after leaf flush and later in the summer. Sapwood discs were cut from the freshly felled trees, dried and cut into 25 mm and 19 mm cubes. The cubes were pressure impregnated with CCA-C and fixed under high relative humidity and at 50°C or at room ...
Y T Ung, A Taylor, P A Cooper, D P Kamdem


Work programme of CEN/TC 38 (April 1999) and European publications
1999 - IRG/WP 99-20165
Scope of the CEN/TC38: Standardization of the characteristics of natural or conferred durability of wood and its derived materials against biological agents, including the characteristics of protection products and associated processes to obtain this durability. This applies in particular to: - the identification of hazard classes-, - the test methods (wood preservatives and treated wood and wood ...
R Hüe


The dip diffusion treatment of tropical building timbers in Papua New Guinea
1972 - IRG/WP 310
In Papua New Guinea a dip diffusion process using a multi salt preservative developed by C.S.I.R.0. has been in commercial use for 8 years. Over 200 million super feet (236,000 m³ ) of timber has been treated during this period and current rate of treatment is 34 million super feet (80,400 m³ ) of timber per year in 70 licenced treatment plants. The process has been found to be simple to apply, ...
C R Levy, S J Colwell, K A Garbutt


The effect of mortality diseases on wood quality of sissoo (Dalbergia sissoo Roxb)
2006 - IRG/WP 06-10569
Sissoo (Dalbergia sissoo Roxb.) is a lagre deciduos, fast growing, strong light demanding and leguminous tree specie. It is an important multipurpose specie widely being planted in the agro forestry and and social forestry pratices in Bangladesh, particularly in the north and south-western parts of the country. On account of its better quality, sissoo is valued as good as construction and utility ...
M M Islam, M O Hannan, G N M Ilias


Sampling rates and the probability of detecting defective treatment in the sampling of preservative treated timber
1987 - IRG/WP 2277
When attempting to enforce standards of penetration and retention set for treated timber, the regulating authority must establish a sampling or inspection scheme which will prevent large quantities of substandard product entering the market. On the other hand, the scheme should not penalise treaters for the small quantities of such material which are inevitably produced by any industrial process. ...
M J Kennedy, L E Leightley


Experiences with penetration of copper-based wood preservatives
2001 - IRG/WP 01-20233
In the Nordic countries there is a long tradition of result type based specifications for preservative-treated wood. A common Nordic standard for treated pine (Pinus sylvestris) wood was published in 1976. After a revision in 1989 this standard, then named INSTA 140, defined four classes of treated wood: M, A, AB and B. Treaters producing according to this standard had to be affiliated to a qualit...
J Jermer, F G Evans, I Johansson


Natural Durability of Tropical Species – Variations and Prospects
2005 - IRG/WP 05-10568
The tropical timber resources of the world play an unequivocal role in economic development of both the tropical timber producing and importing regions. This paper describes natural durability as an important and preferred wood quality of tropical species of the world with emphasis on Malaysian hardwoods, the link between various aspects of tropical hardwood durability, hardwood utilization and bi...
A H H Wong, Yoon Soo Kim, A P Singh, Wang Choon Ling


Quality of timber impregnated with preservatives of class AB after three years in service
2002 - IRG/WP 02-20241
Quality of impregnated timber is most often expressed by penetration and retention of the preservative used. Relatively less information is available about the performance of the final product, e.g. decks, panels etc. regarding product’s surface checks, deformations and overall appearance. Together with the timber durability, the above mention features are of esthetical importance in the above g...
N Terziev


A field test with anti-sapstain chemicals on sawn pine timber stored and seasoned under different conditions
1984 - IRG/WP 3245
Newly sawn timber of European redwood (Pinus sylvestris L.) was dip treated in four different anti-sapstain chemicals. The protectife effect against sapstain, mould and decay was examined after 10 weeks' and 10 months' storage in open and closed stacks. The results showed that the performance of individual chemicals was different in open and close stacks, although the wood as wel...
D J Dickinson, B Henningsson


Efficacy of Didecyl Dimethyl Ammonium Chloride (DDAC), Disodium Octaborate Tetrahydrate (DOT), and Chlorothalonil (CTL) against Common Mold Fungi
2004 - IRG/WP 04-30338
The fungitoxic properties of four fungicides, alone and in combination, against four different mold fungi commonly associated with indoor air quality problems were evaluated on two different wood species and sheetrock. The fungicides were chlorothalonil (2,4,5,6-tetrachloroisophthalonitrile) (CTL) in a 40.4% aqueous dispersion, disodium octaborate tetrahydrate (DOT) in two different forms - a ...
J A Micales-Glaeser, J D Lloyd, T L Woods


Quality assured wooden sidings - Criteria, performance evaluations and current status
2000 - IRG/WP 00-20216
Quality assured wooden sidings were brought to the Swedish market in 1998. The system was worked out during a six year period in a close cooperation between the sawmill industry and several research institutes. Centuries of use have given a wealth of experience of spruce boards as a siding material, showing that it works well in most cases but also that its longevity is highly variable, depending ...
F Englund, I Johansson, J Ekstedt, R Nussbaum


Failure of overhead power transmission and telecommunication poles in Tanzania: Causes, preventive and remedial measures
1988 - IRG/WP 3465
Unless measures are considered urgently to combat massive pole failures occuring in service, it is likely that wooden poles may soon become unpopular. Consequently, pole users may be forced to use costlier alternatives such as underground cables and concrete or steel poles. In trying to countercheck this trend, this paper names the main agents of pole failure, discusses different models of pole fa...
K K Murira


Microwave digestion of preserved wood for the determination of Cu, Cr, As, B and P in quality control
1991 - IRG/WP 2364
A microwave digestion method for the determination of copper, chromium, arsenic, boron and phosphorus in preserved woods is described. Samples were digested with nitric acid in pressure-relief type teflon PFA vessels by microwave heating in a commercial laboratory microwave oven. Fast, efficient and complete digestion was achieved within 29 min for 12 samples. The digestion time compared favourabl...
N Bernth, L B Sheard


Screening of modified linseed oils on their applicability in wood protection
2004 - IRG/WP 04-30346
In this study modified linseed oils, rape oil and three waxes were screened on their efficacy as wood protecting agents. By testing all products when impregnated with high retentions in Scots Pine sapwood on water repellence qualities, additionally an accelerated weathering test, drying quality, accelerated brown rot and blue stain test, an indication is formed of the capability of these products ...