Results of field tests on the natural durability of timber (1932-1975)
1976 - IRG/WP 3105
This paper describes a continuing field stake trial to determine the natural resistance of different species of timber to decay. Data are presented for about 180 timbers, covering over 6000 stakes, and the results are discussed in terms of a natural durability classification....
D W Purslow


An appraisal of methods for environmental testing of leachates from salt-treated wood (2)
1998 - IRG/WP 98-50110
For wood preservatives for use in hazard class 4 information on the ecotoxicity of preservatives and ingredients as well as on the effect of losses from impregnated timber is needed for a proper environmental risk assessment. In the evaluation of a suitable test procedure the leaching behaviour of copper-based formulations was studied using analytical and ecotoxicological test methodology. These ...
H W Wegen, A Platen, G M F Van Eetvelde, M Stevens


A fixation model, based on the temperature dependence of CCA-C fixation
2000 - IRG/WP 00-40163
A model was prepared for the fixation of 1% CCA-C in red pine that allows the prediction of extent of fixation based on the temperature history of the treated wood following pressure treatment. The reaction kinetics of the rapid initial reaction and the slower main reaction were characterized using the Van t'Hoff equation. The initial reaction could be represented by a 10th order chemical...
P A Cooper, K M F Kazi, Jianbin Chen, Y T Ung


Copper based water-borne preservatives: The biological performance of wood treated with various formulations
1987 - IRG/WP 3451
Wood samples treated with the various components of CCA preservative singly and in combination were tested against a soft rot organism, a copper tolerant brown rot organism and in soil burial both unleached and after leaching. The results suggest that, of the elements tested, fixed copper is essential for preventing soft rot attack and fixed arsenic is essential for preventing attack by a copper t...
S M Gray, D J Dickinson


In ground contact field trial results of preservative treated incised and unincised spruce
1996 - IRG/WP 96-40076
Field trials of treated spruce stakes have been demonstrated that incising the stake before treatment improves the preservative uptake both for CCA and creosote. This results in a substantially extended service life for the incised stakes over the unincised stakes for preservative concentrations at commercial levels. After 24 years in ground contact the majority of incised spruce samples are sound...
E D Suttie


Termite field test results of preservative treated and modified woods in Kumamoto, Japan
2001 - IRG/WP 01-30275
Various preservative treated or modified wood stakes other than CCA, were buried in the soil, maximum for six years in Kumamoto, south west side of Japan. In this area, two main termite species, Coptotermes formosanus and Reticulitermes speratus, are distributed. After two years in field, untreated sapwood of sugi (Cryptomeria japonica) were observed severe attacks by termites, but the preservativ...
K Suzuki


Virulence tests with fungal strains used in EN 113 CEN ring test. Results with Coniophora puteana (Schum.ex Fr.) Karst
1986 - IRG/WP 2249
D Dirol


Status of the Working Group on Preservation of Wood in the Marine Environment - Questionnaire results
1977 - IRG/WP 434
At the joint meeting of the IRG and COIPM dealing with preservation of wood in the marine environment, it was suggested that a Marine Group should be formally recognised within IRG. It was agreed that a questionnaire (Document No: IRG/WP/424) should be circulated to determine the views of the membership on the future status of this group. The results of this questionnaire are presented....
R A Eaton


Copper based water-borne preservatives: The use of a thin section technique to compare the protection of wood by copper based preservatives against soft-rot and bacterial decay
1987 - IRG/WP 2286
This paper describes the techniques developed and gives examples of results obtained for the performance of copper based wood preservatives against both the bacterial and fungal hazards....
A M Wyles, D J Dickinson


Field Test Results after Nine Years for CCA and ACQ Preservative-treated Wood Fixed in Different Climates
2003 - IRG/WP 03-30303
During assessment of the ground contact stakes in the Norwegian test field, we have frequently found that the first visual rot attack is in the zone of the stakes, where the stakes have been in contact with each other during the fixation. These parts are usually light green, caused by the lack of light during fixation, compared to the rest of the stake surface, which has a darker colour. To inves...
F G Evans


Fungal degradation of wood treated with metal-based preservatives. Part 2: Redox states of chromium
1996 - IRG/WP 96-10164
Concerns have arisen about the leaching of heavy metals from wood treated with metal-based preservatives, such as chromated copper arsenate (CCA). Of particular concern is the toxic redox state of chromium and arsenic in aging and decayed CCA-treated wood. Generally, hexavalent chromium is more toxic than trivalent chromium and trivalent arsenic is more toxic than pentavalent arsenic. The desired ...
B Illman, S Bajt, T L Highley


The effective control of moulds on freshly impregnated wood
2004 - IRG/WP 04-30352
Beside natural timber it is known, that moulds can also groth at the surface of impregnated wood. This material shows “defects” like resistant dark spots or color changes and causes complaints. During the last years, the problem by moulds seems to increase. Laboratory studies were carried out to show the effect of impregnations against moulds. Wood samples (Pinus sylvestris L.) were impregn...
G Cofta, K Lutomski, P Jüngel


Results of survey conducted at Orlando to solicit attendee feedback on program design
1994 - IRG/WP 94-60026
J N R Ruddick


A bibliography of organic solvent-based wood preservatives
1973 - IRG/WP 313 E
H Alliot


Co-operative research project on L-joint testing. Progress report to May 1989
1989 - IRG/WP 2338
Further sets of data received from STU (Sweden) after 36 months exposure and Sipad-IRC (Yugoslavia) after 45 months exposure are presented and discussed in conjunction with data reported previously. The new data are generally in agreement with those presented previously and the major difference between institutes continues to be one of rate of colonisation rather than any relative difference in pe...
J K Carey, A F Bravery


Report on questionnaire: Facility for accelerated stake tests in unsterile soil
1983 - IRG/WP 2169
In October 1981 a questionnaire (IRG Doc. No. IRG/WP/2166) on the so-called fungus cellar tests in unsterile soil was prepared and despatched to 56 individuals representing various institutes, organisations, or companies. In addition a further 68 letters describing the purpose of the questionnaire were sent to additional IRG members who could request the full questionnaire if appropriate. This rep...
J A Butcher


Fungicidal properties of boron containing preservative Borosol 9
2004 - IRG/WP 04-30348
The fungicidal properties of new boron containing wood preservative Borosol 9 is described in this paper. These properties were of particular interest as this new boron containing preservative, exhibit very good performance against wood damaging insects. But because the tested boron formulation contain also nitrogen compounds, we wanted to verify if nitrogen as a nutrient could promote...
G Babuder, M Petric, F Cadež, M Humar, F Pohleven


Decay resistance of high performance biocomposites based on chemically modified fibres
1998 - IRG/WP 98-40120
Different partners within the framework of a European research project produced high performance biocomposites aiming at the utilisation of board materials as durable products both in dimensional and biological degrading circumstances. This paper summarises test data, which indicate the potential of board materials produced with modified fibre material. The chemical modifications applied cover a r...
V Rijckaert, J Van Acker, M Stevens


Tebuconazole - a new triazole fungicide for wood preservation
1991 - IRG/WP 3680
The great potential of Tebuconazole for wood preservation is demonstrated. Test carried out by official institutes shown that Tebuconazole is particularly effective against wood-rotting basidiomycetes strains. The efficacy of Tebuconazole against the brown rot Gloeophyllum trabeum is outstanding: the toxic value measured in accordane with EN 113, without·ageing, after leaching (EN 84) and after e...
O Exner


Collaborative soft rot experiments 1974. Preliminary analysis of results
1975 - IRG/WP 251
J K Carey, J G Savory


Water-borne wood preservatives against marine borers. Results from NWPC marine trials started in 1972 and 1976
1990 - IRG/WP 4162
The paper presents the results from NWPC (Nordic Wood Preservation Council) marine trials started in 1972 and 1976. The trials are carried out according to the NWPC Standard No. 1.4.2.2./73 "Marine test - a test against marine wood boring organisms in sea water". The test site is Kristineberg Marine Biology Station on the west coast of Sweden. The wood blocks used in the trials were made from sapw...
Ö Bergman, C Lundberg


Vapour boron treatment of wood based panels: Further studies on mechanical properties
1993 - IRG/WP 93-30028
Samples of medium density fibreboard, chipboard and oriented strandboard were treated to two retentions of boric acid by vapour phase methods. The results of short term mechanical tests on this material were discussed by Hashim et al. (1992). The present paper discusses results with long term studies on bending and impact resistance with panel types. Long term tests of impact resistance showed no ...
R Hashim, R J Murphy, D J Dickinson, J Dinwoodie


Test Methods – Performance Based Requirements
2004 - IRG/WP 04-20297
In this paper is briefly described the present approach to service life prediction as an essential part of the architectural engineering process. The system of testing the durability of wood is described more in detail including laboratory tests as well as field trials. It is concluded that the system has a lot of weaknesses which makes it less well suited for practical building applications. A le...
M-L Edlund, F Englund, J Jermer, T Nilsson, M Westin, K Ödeen


Comparison of decay rates of preservative-treated stakes in field and fungus cellar tests. Results after 40 months fungal cellar exposure
1983 - IRG/WP 2200
Decay rates of preservative-treated Pinus radiata stakes during 40 months exposure in the FRI fungus cellar were compared with those of similarly treated material in a field test. Decay rates in the fungus cellar were from 4 to 100 times higher than in the field, although for the majority of preservatives the rate was between 7 and 12 times higher. The lag phase before onset of decay, noticeable w...
M E Hedley


Chemical Analysis of Southern Pine Pole Stubs Thirty-Nine Months Following Treatment with Three Methylisothiocyanate-Based Fumigants
2004 - IRG/WP 04-30349
Agricultural fumigants have been commercially used in the United States for over 20 years to control internal decay in utility poles and other wooden structures. Of the four fumigants which are currently used in the remedial treatment of utility poles, three are based on methylisothiocyanate (MITC) as being the principal fungitoxic component. Two of these MITC-based fumigants, liquid metham sodi...
R J Ziobro, J Fomenko, D J Herdman, J Guzzetta, T Pope