Influence of sampling on the composition of test solutions
1985 - IRG/WP 2235
For four commercial products of CCB-salts the influence of the kind of sampling on the composition of test solutions has been tested. For each product several 5 g samples have been taken at random, after careful mixing the content of each bottle, and after grinding the whole content. With each sample a 5% test solution was made and analyzed on the content of chromium, copper and boron. Altogether ...
H Willeitner, K Brandt


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 2: Report of treatment and installation in Australia
1978 - IRG/WP 440
The purpose of this test and the procedures to be followed have been fully set out in documents distributed by the International Research Group on Wood Preservation and numbered IRG/WP/414 and IRG/WP/420. The prescriptions set out in these two documents have been closely followed....
J Beesley


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 13: Report of fourth inspection (36 months) in Australia
1981 - IRG/WP 481
This report presents the results of the fourth inspection of the IRG/COIPM International Marine Test specimens installed in Sydney Harbour in December, 1977. The inspection took place on 9th December, 1980, after 36 months exposure. Full details of the treatment and installation of the specimens, as well as results of the first three inspections (after 6, 12, and 24 months exposure), have been pre...
J Beesley


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. 2nd Interim Report
1981 - IRG/WP 477
Three reference wood species - Alstonia scholaris, Fagus sylvatica and Pinus sylvestris, untreated and treated with 3%, 6% and 10% CCA and CCB solutions were supplied to all participants for submergence at local sites. Regular examination of samples is being carried out - 6 months, 12 months and then annually for 7 years....
R A Eaton


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 10 from Naos Island, Panama
1980 - IRG/WP 462
Blocks of 3 wood species, Beech (Fagus sylvatica), Scots pine (Pinus sylvestris) and Alstonia (Alstonia scholaris) were exposed at site number 12 at Naos Island, Panama on March 8, 1978 by John R. DePalma. The arrangement of the panels in the exposure site is as shown in Figure 1....
D W French


Factors affecting leaching of preservatives in practice
1978 - IRG/WP 3113
At the 7th Meeting of the IRG in Poland in May 1975, the findings of collaborative laboratory leaching techniques were discussed, and the dangers inherent in using such results to predict the behaviour of preservative-treated components in service were emphasised. In order to improve our understanding of the factors governing leaching of preservatives in practice, and to identify areas where furth...
R Cockcroft, R A Laidlaw


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 8: Panama test results
1980 - IRG/WP 458
Summary of damage to ITRG test stakes by pholadidae and teredinidae at the Panama test site - 8 Mar. '78 to 11 Oct. '79...
J R De Palma


Resistance to soft rot of hardwood plywood treated with CCA salt
1983 - IRG/WP 3258
Plywood made from indigenous hardwoods was treated at an average loading of 34 kg Celcure A per m³ and was installed in a field test. After 20 years the samples were only slightly attacked by soft rot and the glue bonds were still intact....
R S Johnstone


Contribution to study of the degradation caused in Pinus spp. poles used in field test
1989 - IRG/WP 1417
The study of the degradation produced by soil natural microflora on wood in contact with it in the field, has been going on for several years now. Our contribution to this aim in the present work has dealt with the possible relationship of the microorganisms in the soil. The microscopic visualization of wood colonization by the microorganisms, and the chemical analysis of the degraded wood compare...
M T De Troya, A Garcia, M J Pozuelo, A M Navarrete, A Cabanas


The internal-external diffusion process: Table salt treated poles
2005 - IRG/WP 05-50224-25
This new technique of preservation of wooden poles consists of keeping preservative in stock, in a reservoir drilled inside the pole, in its whole length. This permits the use of non toxic, common products such as table salt, grease, etc, in the preservation of utility poles, building columns, or the like. Some major obstacles to a good implementation of a good preservation with the classical pr...
L Nitunga


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water: Final report
1987 - IRG/WP 4133
Three timbers chosen as reference species were treated with 3, 6 and 10% solutions of CCA and CCB preservatives and exposed for up to 93 months at 8 tropical and temperate marine sites. Eleven local species treated in the same way were exposed at 4 of the 8 sites. There was no apparent difference in performance between CCA and CCB treated specimens. The severest test site was Panama Canal but mari...
R A Eaton


An appraisal of methods for environmental testing of leachates from salt-treated wood (2)
1998 - IRG/WP 98-50110
For wood preservatives for use in hazard class 4 information on the ecotoxicity of preservatives and ingredients as well as on the effect of losses from impregnated timber is needed for a proper environmental risk assessment. In the evaluation of a suitable test procedure the leaching behaviour of copper-based formulations was studied using analytical and ecotoxicological test methodology. These ...
H W Wegen, A Platen, G M F Van Eetvelde, M Stevens


Literature survey on the permanence and distribution of salt-type wood preservatives
1969 - IRG/WP III 1B
The objective of this survey is generally to review some of the more important published work dealing with the distribution and permanence of salt-type waterborne wood preservatives in treated timber. The survey is limited to the major chrome-containing formulations and the classification system proposed by Becker (1964) has been adopted throughout. CK - chromium, copper (copper, chrome); CKA - c...
Anonymous


Absorption of inorganic salts solutions. Retentions of inorganic salts. Fire retardants
1990 - IRG/WP 3625
The study aims evaluated the impregnation capacity using fire retardants on woods with differents densities. At the same time, impregnation with several fire retardant salts were carried out in order to obtain their absortion and retention in wood....
A Garcia, J Navarro


The benefits to New Zealand of boron salt treatment of Pinus radiata
1992 - IRG/WP 92-3692
The historical reasons for New Zealand adopting boric salt diffusion of Pinus radiata are summarised, and present day processes and their associated costs are given. The biological hazards of using Pinus radiata untreated are then argued, using endemic fungal and insect species as examples, as well as a discussion of the risks from species that may yet be accidentally introduced into the country....
D J Cross


A study of salt imbalances observed in recycled copper/chrome/arsenic preservative solutions in commercial practice
1987 - IRG/WP 3461
The study reported monitored tank solutions, sludge and other by-products using a standard CCA solution, when recycled. This recycling of the CCA solution is quite usual in between any commercial treatment schedules. Salt imbalances were observed and the possible reasons for such phenomena were studied. The paper discusses the procedure followed, the method of sampling the liquid after the charge ...
V R Sonti, S Sonti, B Chatterjee


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. 3rd Interim Report
1983 - IRG/WP 4101
This paper updates the results of microbiological examination and marine borer assessment of untreated wood samples (15 x 2 x 2 cm³) and samples treated with 3, 6 and 10% CCA and CCB preservatives. Three reference species - Alstonia scholaris, Fagus sylvatica, Pinus sylvestris were used at all the test sites in addition to local species chosen by participants in the test....
R A Eaton


An experimental method to simulate incipient decay of wood by basidiomycete fungi
2000 - IRG/WP 00-20200
At very early stages of decay of wood by basidiomycete fungi, strength loss can be measured from wood before any measurable weight loss. Therefore, strength loss is a more efficient measure of incipient decay than weight loss. However, common standard decay tests (e.g. EN 113 or ASTM D2017) use weight loss as the measure of decay. A method was developed that allowed progressive removal of samples ...
S F Curling, J E Winandy, C A Clausen


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 9: Report of third inspection (2 years) in Italy
1980 - IRG/WP 461
The wood samples were submerged in the sea at Follonica, Italy, in April 1977. Follonica, latitudine 42°55' North and longitude 10°45' East, is situated on the Tyrrhenian sea. The recorded temperature varies between 13°C to 25°C, salinity 37-38% and pH about 8. The inspections were carried out after 6 months (10/1977), 1 year (4/1978) and 2 years (4/1979)....
A Gambetta, E Orlandi


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 7: Second report on the samples in Papua New Guinea
1980 - IRG/WP 459
This report presents the findings to date regarding specimens installed in Papua New Guinea, as part of a world-wide marine trial of certain timbers treated with CCA or CCB preservatives. The details of the trial are set out in document number IRG/WP/414. The report discusses the findings in the context of the conditions prevailing at the trial site and of the properties of the trial timbers. The ...
S M Cragg, C R Levy


Conditions and possibility of nanobiocides formulation for wood protection
2008 - IRG/WP 08-30467
During development of nanobiocides for wood protection the need to identify mineral composition of wood in respect of trace elements and nourishing conditions of wood destroying fungi in relation to these elements was discussed....
J Wazny, A Kundzewicz


A rapid colorimetric assay for mold spore germination using XTT tetrazolium salt
2011 - IRG/WP 11-20462
A rapid colorimetric assay was developed to quantitate metabolic activity in mold spores during germination using 2,3-Bis(2-methoxy-4-nitro-5-sulfophenyl)-5-[9phenyl-amino)carbonyl]-2H-tetrazolium hydroxide (XTT). The assay was used to demonstrate inhibition of spore germination following exposure to different biocides and variability in the inhibition of spore germination of different mold specie...
C A Clausen, V W Yang


Treating Eucalyptus tereticornis wood with boron: Optimizing treatment conditions
2005 - IRG/WP 05-40309
Even though Eucalyptus tereticornis wood is suitable for small timber purposes, being non-durable, it needs to be treated with preservative chemicals. As it is a heavy, hard and difficult to treat species, the possibility of using diffusible boron compounds was investigated. The present study explored the effect of impregnation conditions such as treatment schedule, concentration of treatment solu...
T K Dhamodaran, R Gnanaharan


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 20: Report on the inspection of specimens at Sekondi, Ghana after 48 months
1985 - IRG/WP 4116
The results of the second inspection of CCA- and CCB-treated test panels exposed at Sekondi, Ghana, in June 1980, are presented. The panels of Pinus sylvestris treated with 3% CCA are stil unattacked after 48 months. Panels treated with 10% CCA and still in test (Fagus sylvatica, Pinus sylvestris and Alstonia scholaris) are still free of attack. Locol species treated with 3% CCB have all been dest...
F F K Ampong, N Asare-Nyadu


Biodegradation of acetylated southern pine and aspen composition boards
1994 - IRG/WP 94-40020
This objective of this study was to investigate the influence of the acetylation treated wood fiber, Phenol-formaldehyde resin content level, two wood fiber species, three fungi species on the dimensional stability and decay resistence of high density composition boards. A standard ASTM method was used to evaluate weight loss and thickness change. The linear shrinkage and expansion of each species...
P Chow, T Harp, R Meimban, J A Youngquist, R M Powell