IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 11 documents.


Properties of plywood and Oriented Strand Board manufactured with an organic insecticide incorporated in the adhesive formulation
2000 - IRG/WP 00-40174
The efficacy of Fipronil as an insecticide has been established by laboratory and field experiments and commercial use against a broad range of insect pests for various crops. It can be used by either foliar or soil application. Development is underway for the non-agricultural uses of fipronil. Research is ongoing for the control of ants, cockroaches, fleas, ticks, houseflies, mosquitoes, termites...
D P Kamdem, J H Hope, A Jermannaud


Treatment of lumber with preservative/water repellent emulsions - The significance of shear stability on penetration
1997 - IRG/WP 97-20124
Currently, the treatment of lumber with a water repellent emulsion and a wood preservative formulation in combination is the most cost effective way to prevent decay and to maintain the appearance of uncoated lumber in service. Water repellents influence the movement of moisture into and out of wood and, by so doing, can decrease checking and splitting significantly. Adequate penetration of the em...
F Cui, K J Archer


The effect of oil-borne preservative treatments on the shear strength of FRP/wood composite adhesive bonds
2003 - IRG/WP 03-40265
Reinforcement of structural wood components with Fiber Reinforced Polymer (FRP) will enhance the beam’s strength, but actual data on long-term durability is sparse, not well documented or not readily accessible. In this study, bond properties of FRP-wood composite materials were investigated following treatment with creosote or copper naphthenate preservatives. The properties investigated inclu...
B Herzog, B Goodell, R Lopez-Anido


Influence addition of boron compounds to adhesives on the bonding quality and fungicidal properties of glued wood
2010 - IRG/WP 10-40497
Wood is one of the most important construction materials. However, users of wood face two issues: limited dimensions and insufficient durability. These issues have been overcome with the development of bonding and wood preservation. The preservation of glued wood is elucidated in this paper. Through the addition of boric acid to adhesives, we tried to improve the fungicidal properties of glued woo...
M Humar, B Lesar, A Ugovsek, M Kariz, P Kralj, M Šernek


Effect of borax-boric acid Treatment of simul (Bombax ceiba) Veneers on Glue-Bond Quality of Plywood
2010 - IRG/WP 10-40525
The glue-bond quality of plywood made of treated simul (Bombax ceiba) veneers was investigated. The veneers were treated with cold and hot water solution of borax-boric acid (BB) of different concentrations and treatment durations. The plywoods were made at three different pressures in hot press using urea formaldehyde glue. The glue-bond strength of untreated plywood in dry shear-test was found t...
K Akhter, Md Abul Hashem, S Akhter


Effect of Furfurylation on Shear Strength of Bond Line and Screw Withdrawal Resistance of Beech and Fir Wood
2016 - IRG/WP 16-40757
The aim of this study was to investigate the effects of furfurylation on shear strength of bond line and screw withdrawal resistance of beech (Fagus orientalis) and fir (Abies alba) species. In this regard, specimens with two different values of furfurylation i.e. low (fir 14% and beech 20%) and high (fir 38% and beech 65%) levels were prepared and evaluated in comparison with untreated specimens....
A Talaei, H Abdolzadeh, M Saleh Zare


Influence of Drying Condition of Wood on Rusting of Nail
2019 - IRG/WP 19-40887
Recently in Japan, the durability of metal joint in wooden structures become important. Revised Building Standard Law was enacted in 2000 and Act on the Promotion of Popularization of Long-life Quality Housing was enacted in 2008 in Japan. Since then, the durability of the metal joints in the wooden houses becomes important. But there are not any detailed regulation for the durability of the metal...
H Ishiyama, N Wada, T Nishimura, T Mori


Study on Nailed Joint with Iron Contamination. Part1: Shear Performance of Nailed Joint with Iron Contamination
2019 - IRG/WP 19-50349
In Japan, The building standard law was amended in 2000.1) The use of metal joint was obligated by this law. Since then, metal joints have been largely used for wooden buildings. Also, Act on the Promotion of Popularization of Long-life Quality Housing was enacted in 2009 and leaving Long-life Quality Housing has been focused on2). However, leaving houses to posterity for a long time causes severa...
R Nakano, D Nakano, H Ishiyama


Longitudinal tensile shear properties of polyurethane-bonded preservative-impregnated Eucalyptus grandis laminates subjected to varied simulated climatic conditions
2023 - IRG/WP 23-40967
Bonding process adaptations have yielded improvements in the adhesive bonding of Eucalyptus grandis wood for manufacturing hardwood laminates. However, there are still concerns over the adhesive-bond performance, particularly preservative-impregnated E. grandis laminates, under exposure to varying climatic conditions. These concerns could limit the implementation of E. grandis laminates, especiall...
A A Alade, C B Wessels


Estimation of single shear strength performance of screw joints with decayed wood
2023 - IRG/WP 23-40968
In order to use existing wooden structures for a long term, it is necessary to evaluate appropriately the damage degree of bio-deterioration of the structural performance including the members and joint systems. As one for them, it is necessary to estimate more accurate the single shear strength performance of screw joints with decay. Therefore, we proposed the model considering the yield strength...
R Inoue, K Tanaka, T Mori


Relationships between deterioration part and structural performance in wooden houses
2023 - IRG/WP 23-50376
Based on the survey examples, there are four patterns of deterioration that tend to occur in plywood bearing walls of wooden houses in Japan. The first is a pattern in which wall is in a whole deterioration. It is a no damage wall or test specimen. The second is a pattern in which only the sill is deteriorating. It is caused by moisture or termites from ground to the base. In addition, there is a ...
Y Ota, H Ishiyama, S Okamoto