Effect of acetylation on decay resistance of wood against brown-rot, white-rot and soft-rot fungi
1989 - IRG/WP 3540
Effect of acetylation on decay resistance of wood was investigated using wood blocks of Cryptomeria japonica, Pinus densiflora, Albizia falcata and Fagus crenata. Blocks were treated with uncatalyzed acetic anhydride for different lengths of time and exposed to Tyromyces palustris, Serpula lacrymans, Coriolus versicolor and unsterilized soil. The action of OH-radical on acetylated wood was also ex...
M Takahashi, Y Imamura, M Tanahashi


Resistance to soft rot of hardwood plywood treated with CCA salt
1983 - IRG/WP 3258
Plywood made from indigenous hardwoods was treated at an average loading of 34 kg Celcure A per m³ and was installed in a field test. After 20 years the samples were only slightly attacked by soft rot and the glue bonds were still intact....
R S Johnstone


Efficacy of anhydrides as wood protection chemicals - II. Performance against soft rot fungi
1998 - IRG/WP 98-30174
Pine sapwood modified with various anhydrides and with butyl isocyanate was tested for its resistance to soft rot decay. Small stakes were exposed for 20 months in unsterile soil in a fungal cellar test. Wood modified with butyl isocyanate performed better than any of the anhydrides tested, with a threshold level of protection (less than 3% weight loss) at 12% weight percent gain (WPG). Stakes ac...
S C Forster, M D C Hale, G R Williams


A summary of tests and practical experiences with the Pilodyn wood testing instrument
1980 - IRG/WP 282
This paper presents a summary of the reports, tests and practical experiences with the Pilodyn wood tester not only, however, concerning poles but also in other fields such as standing trees, sawn timber etc. The principle of the Pilodyn is a spring-loaded pin which is fired into the object and the depth to which the pin penetrates is correlated to physical and mechanical properties of the object....
H Friis-Hansen


Practical consequences of the clarification of the chemical mechanism of CCA fixation to wood
1983 - IRG/WP 3220
Practical consequences derived from the chemical investigation of the mechanism of fixation of CCA to the wood constituents are discussed. Among these, formulas for the calculation of the time of hexavalent chrome fixation are presented. Furthermore, three parameters are shown to be important to the long-term effectiveness of CCA-treated timber: (i) the temperature of treatment, (ii) the initial p...
A Pizzi


Laboratory tests on light organic solvent preservatives for use in Australia. - Part 6: Soft rot resistance of three fully formulated preservatives on different timber substrates
2000 - IRG/WP 00-30245
The above-ground soft rot resistance of substrates treated with three fully formulated light organic solvent preservatives (Cuprivac Green WR, Impresol WR 205 and Vacsol) was studied using a modified vermiculite burial method. The substrates were sapwood of Pinus elliottii and P. radiata and heartwood of Eucalyptus regnans, Pseudotsuga menziesii, Shorea sp. (a lower and a higher density source) an...
G C Johnson, M A Tighe, J D Thornton


Evaluation of the pulsed-current resistance meter (Shigometer®) for determination of the internal condition of utility poles
1979 - IRG/WP 2128
A number of Telecom poles, which had been removed from service to be replaced by a radio link, were inspected using an electrical resistance meter (Shigometer®). These poles were creosoted, non-durable Victorian species in service in New South Wales. Six of these poles, chosen to represent various internal conditions typical of the range of the population tested, are discussed here. Data, from tr...
J D Thornton, W G Seaman, M McKiterick


Resistance of acetylated wood to basidiomycetes, soft rot and blue stain
1994 - IRG/WP 94-40021
Poplar (Populus spp.), beech (Fagus sylvatica) and pine sapwood (Pinus sylvestris) samples were acetylated in a semi-industrial acetylation plant and tested for durability according to European standards. Resistance to Gloeophyllum trabeum, Coniophora puteana and Coriolus versicolor could be reached at a weight percent gain (WPG) of 12%. Susceptibility of acetylated pine to Poria placenta was high...
E P J Beckers, H Militz, M Stevens


Is laboratory testing of decay resistance questionable as a single criterion for natural durability?
1996 - IRG/WP 96-20096
In a laboratory test set up over 20 hardwood species were evaluated according to the European Standard EN 350-1 including Basidiomycete and soft rot testing. Half of the species used were of a known natural durability. The Basidiomycete testing was carried out using Coriolus versicolor, Gloeophyllum trabeum and Coniophora puteana in a malt agar test similar to EN 113. From this test it was not pos...
J Van Acker, M Stevens, T Van Cauwenberghe, T Seynaeve


The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...
A A H Wong, A P Singh


Efficacy of waterborne copper naphthenate as preservative for northern hardwood species
1995 - IRG/WP 95-30091
Northern red oak (Quercus rubra) and red maple (Acer rubrum) cubes pressure treated with waterborne formulation of copper naphthenate were evaluated for resistance to attack by brown fungi Gloeophyllum trabeum (Pers. ex Fr.) Murr. (Madison 617 ATCC 11539) and Poria placenta (Fr.) Cooke (Madison 698, ATCC 11538), white rot fungi Trametes versicolor (L. ex Fr.) Pilat (R-105 from Jeff Morrell), Irpex...
D P Kamdem, R Fair, M H Freeman


Influence of the content of organic matter of soil on the degradation of wood by soft rot fungi
1970 - IRG/WP 27
The degradation of wood specimen burried in the soil by soft rot fungi is influenced by a number of factors. These are in particular the water holding capacity, water content, content of organic matter, pH, content of mineral nutritive substances etc. The results of the interlaboratory tests, carried out within the IRG/WP let presume that the intensity of wood degradation occurs proportionally inv...
O Wälchli


Laboratory Evaluation of Soft Rot Resistance of Non-Durable Lesser-Known Malaysian Hardwoods
2006 - IRG/WP 06-10582
Resistance of six non-durable lesser-known Malaysian hardwoods, Pulai (Alstonia spp.), Rubberwood (Hevea brasiliensis), Ludai (Sapium spp.), Jelutong (Dyera costulata), Gaham Badak (Blumeodendron tokbrai) and Kayu arang (Diospyros spp.) compared with temperate Scots pine sapwood (Pinus sylvestris), were evaluated using the unsterile soil burial (mixed with Chaetomium globosum) versus vermiculite-b...
A H H Wong


Biological resistance of didecyl dimethyl ammonium tetrafluoroborate (DBF)-treated wood in soil-bed and Basidiomycetes tests
2006 - IRG/WP 06-30393
This study evaluated the decay resistance of treated wood with a new quaternary ammonia compound, didecyl dimethyl ammonium tetrafluoroborate (DBF) in laboratory soil bed and Basidiomycetes tests. Treated sugi sapwood specimens with DBF at various concentration levels were first subjected to soil bed tests using two types of soil. The specimens subjected to soil bed tests were then used for Basidi...
S N Kartal, C Brischke, A O Rapp, Y Imamura


Feasibility study on three furfurylated non-durable tropical wood species evaluated for resistance to brown, white and soft rot fungi
2008 - IRG/WP 08-40395
Furfurylation can protect non-durable wood species against biological degradation, but the method used today cannot fully protect the heartwood of Scots pine due to insufficient penetration. In order to test alternative wood substrates for furfurylation, three Malaysian grown wood species (Kelempayan, Rubberwood and Sena) were furfurylated and subjected to soil block decay testing. Their performan...
T Mark Venås, A H H Wong


Testing of decay resistance of sapwood and heartwood of thermally modified Scots pine and Norway spruce
2010 - IRG/WP 10-40523
Thermal modification at elevated temperatures changes the chemical, biological and physical properties of wood. One of the main targets of thermal modification is to increase the biological durability and decay resistance of wood. Although the effects of thermal modification on wood have been widely studied, the significance of sapwood and heartwood on the resistance of thermally modified wood has...
H Viitanen, S Metsä-Kortelainen


Influence of soil moisture, Sarawak soil types and decay types on decay susceptibility of rubberwood and kelempayan
2012 - IRG/WP 12-10780
Wood and soils are important natural resources of the land, the former widely used as structural supports in contact with the latter. Many low durability wood species exposed to soil contact has reportedly high incidence of decay failures in poorly treated and untreated materials depending on soil types, properties and soil microbial virulence. This paper probes the relationship of the main soil t...
A H.H. Wong, P K.F. Chong, J Sabang


Mechanical and biological durability properties against soft-rot and subterranean termite in the field (grave-yard test) of beech wood impregnated with different derivatives of glycerol or polyglycerol and maleic anhydride followed by thermal modification in an opened or in a closed system
2021 - IRG/WP 21-40917
This paper presents mechanical and biological durability properties in soil beg test (soft-rot test) and field test (grave-yard test) against subterranean termite of the wood modified with an aqueous vinylic derivative of glycerol/polyglycerol or maleic anhydride cured in an opened or in a closed system. Wood modification was performed through impregnation of European beech (Fagus sylvatica) with ...
M Mubarok, H Militz, S Dumarcay, I W Darmawan, Y S Hadi, P Gerardin


Microbiological degradation of wooden piles in building foundations
1988 - IRG/WP 1370
White rot, soft rot and bacterial attack have been detected in softwood piles under buildings. In some cases bacteria were found to be the main degradation organisms in the studied piles. The water content of degraded piles was very high. The compression strength was quite low also in the piles deteriorated by bacteria. The density of wood was very variable, and the degree of degradation could not...
L Paajanen, H Viitanen


A comparison of soft rot, white rot and brown rot in CCA, CCP, CCF, CCB, TCMTB and benzalkonium chloride treated Pinus radiata IUFRO stakes, after 9-15 years exposure at five test sites in New Zealand
1991 - IRG/WP 1485
The aim of this study was to determine if decay type varies significantly between five field trial test sites of different soil type, aspect and climate in 9-15 year old, replicate CCA, CCF, CCP. CCB, TCMTB and AAC treated IUFRO stakes. A visual on-site assessment of decay type on every test stake was made and observations confirmed by microscopical examination. Regression analyses were used to de...
R N Wakeling


Questionnaire - Fungal decay types
1985 - IRG/WP 1265
T Nilsson


Collaborative soft rot tests. Names and addresses of collaborators
1973 - IRG/WP 231
IRG Secretariat


Soft rot penetration - Effect of groundline maintenance treatment on poles in sevice
1983 - IRG/WP 3263
R S Johnstone


Soft rot in CCA-treated utility poles in Sweden
1989 - IRG/WP 1398
Soft rot investigations of CCA-treated utility poles (Pinus sylvestris L.) have been conducted throughout large parts of Sweden during 1974-1985. The investigation included 179 utility poles of the State Power Board which had been used for 10-18 years in the different administrative regions from northern to southern Sweden. In addition, 193 telephone poles from the Östersund area and 218 from the...
H Friis-Hansen, H Lundström


Collaborative soft rot tests: PRL tests of Cu/Cr/As preservative using method of Document No: IRG/WP/208
1973 - IRG/WP 223
These tests were undertaken as a preliminary to the next series of collaborative soft rot tests. An interim report has already been presented at Berlin in 1972 as Document No: IRG/WP/211...
J K Carey, J G Savory


Next Page