IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 65 documents. Displaying 25 entries per page.


Trend in entomology of wood in use and in storage in Nigeria
1978 - IRG/WP 180
The current and potential impact of biotic agents of wood deterioration in Nigeria is reviewed, with emphasis on the insects and marine borers, their recognition and mode of damage. Some essential areas have no doubt been neglected and these are highlighted, while future lines of approach are outlined....
M O Akanbi


Reticulitermes lucifugus Rossi, and its damages in Turkey
1982 - IRG/WP 1152
The moist-wood termite, Reticulitermes lucifugus Rossi, is generally observed on the wood material which has a direct contact with the soil as trunks and fence stakes. It was reported to be found in some provinces in Turkey. The termite has been seen in these areas so far at the endemic level, but any considerable damage or epidemy has not yet been reported. Considerable damages were observed on t...
O A Sekendiz


Fungal defacement of water-stored softwoods
1993 - IRG/WP 93-10009
Sapstain, mould and basidiomycete defacement of untreated sawn boards of Scots and Corsican pine was recorded during a 14 week field trial. Boards were cut from freshly felled logs and from logs previously maintained under water sprinklers for 6 months and ca. 4 years. The incidence of sapstain defacement or the freshly felled wood was very servere aftcr 2 weeks and remained so throughout the boar...
M A Powell, R A Eaton


Tentative method of testing wood preservatives against blue staining
1977 - IRG/WP 259
The blue stain of sawn wood is still a real problem in Poland. Although a preservative based on sodium orthophenylphenoxide has been introduced into sawmill practice, and the technology of wood protection developed with it, new information has been obtained concerning blue stain in wood material destined for export. In order to select new chemicals or to improve the effectiveness of the ones in cu...
E Tarocinski, O Lewandowski, M H Zielinski


The leaching of copper, chrome and arsenate from CCA-impregnated poles stored for ten years in running water
1978 - IRG/WP 3122
There is no evidence to indicate that the chromium and copper components are leached from the outermost 5 mm of sapwood in poles impregnated with Boliden K33 and Tanalith C and stored in running water for ten years. The arsenic component, however, seems to be leached out during the first few months to an extent of about 20% of the initial amount. The leaching time is dependent on the preservative ...
F G Evans


The effect of storage or simulated internal use on the durability of wood based panels to decay fungi
1997 - IRG/WP 97-20106
Wood based panels such as particleboard and medium density fibreboard are experiencing a steady increase in use, in areas from structural to decorative applications. Understanding the "natural" durability of these panel products against basidiomycete fungal decay is therefore of great importance. Various methods have been proposed or are under development to test the durability/susceptibility of v...
S F Curling, R J Murphy, J K Carey


Working Group II: Sub-group: Methods of testing anti-stain chemicals for protecting sawn lumber during storage, transit
1978 - IRG/WP 2121
R Smith


Influence of storage on mould susceptibility of wood at relative humidity values lower than 100%
1989 - IRG/WP 1413
It is well known that wood material changes with time because of different environmental influences. The effects of such changes on the subsequent mould susceptibility are less known. In this paper we report on increased mould susceptibility of pine wood after storage. Mould growth was detected by indirect methods....
J Bjurman


Bacteria and wood. A review of the literature relating to the presence, action and interaction of bacteria in wood
1971 - IRG/WP 101
S E Rossell, E G M Abbot, J F Levy


Studies on the biological improvement of permeability in New Zealand grown Douglas fir
1983 - IRG/WP 3231
This report outlines progress towards optimizing conditions for water storage of New Zealand grown Douglas fir with the aim of improving permeability to water-borne preservatives, in particular CCA. Small scale laboratory tests are in progress but the need to scale up to potential commercial applications is being considered. Mixed populations of bacteria isolated from 10 week water sprinkled Dougl...
K J Archer


Examination of timbers from the Mary Rose in storage
1988 - IRG/WP 4149
Timbers from the Tudor ship, Mary Rose, have been examined for the presence of fungal fruiting structures. Wood specimens were also examined for the presence of microbial decay patterns using light and scanning electron microscopy. Structural timbers were surveyed using the Pilodyn for an overall picture of the extent of decay. Mary Rose timbers were predominantly inhabited by marine fungi. Fourte...
R Mouzouras


CCA fixation experiments. Part 1
1989 - IRG/WP 3504
A method of squeezing solution from CCA treated wood that has not been dried at various times after treatment appears to be useful in following the fixation of CCA in wood. Experiments confirm that temperature governs the rate of fixation....
W S McNamara


Chromium on the surface of CCA-treated wood
1978 - IRG/WP 386
Chromium in solutions of CCA preservatives is predominantly in the hexavalent state (Cr VI). It is well known that Cr VI is associated with dermatitis and skin ulceration in workers handling chromium containing products and processes. When reduced to the trivalent state, however, chromium is considerably safer. An essential part, therefore, of safety procedures in any chromium - using industry is ...
C R Coggins, P Hiscocks


The shower test method. A leaching test for assessing preservative losses from treated timber under simulated open storage conditions
1993 - IRG/WP 93-50001-04
In the late 1980's against the background of increasing environmental concern a laboratory based accelerated leaching test method for assessing preservative losses-from stored, treated timber was developed by the Dutch organisation for applied Scientific Research (TNO). This test method quantifies the amount of specific preservative components which leach from treated timber under simulat...
J B G A Havermans, W J Homan, M J Boonstra


Evaluation of an alkyl ammonium compound as a fungicide to control sapstain and mould during diffusion storage
1984 - IRG/WP 3282
An alkyl ammonium compound ('Akzo' ES 255) was evaluated for its effectiveness against mould and sapstain during diffusion storage of boron-treated rubber wood. Though ES 255 at 1.0% concentration was effective against mould (71%) and sapstain (89%) it is less satisfactory compared to 0.5% sodium pentachlorophenoxide against mould (92%) and sapstain (98%)....
R Gnanaharan


The rate of losses of creosote from power transmission poles during storage
1998 - IRG/WP 98-50101-24
The purpose of this work was to study the rate of losses of creosote from power transmission poles and its consequences on the expected life of the poles stored for a long period in horizontal position. Apart from this main target of the study, the results could allow a rough estimate of the load of creosote substances on the soil especially when the poles are stored and this load accumulates over...
Z Vassou, A Satanakis, C Koutsikopoulus, J Petinarakis


Fungal Stain Development in Canadian Hardwood Logs
2004 - IRG/WP 04-10505
In most sawmills around the world, trees are harvested into logs and stored in the forest or in a log yard for a period of time before being sawn into lumber. These logs may be attacked by various pigmented fungi, which results in staining of the wood. Since hardwood species are used to a great extent in furniture manufacturing and in the making of other valuable wood products, the reduction of wo...
Dian-Qing Yang, M-C Bisson


The new National Directive on wood preservation in the Netherlands
1998 - IRG/WP 98-50101-03
In the Netherlands the major part of treated timber is sold under the KOMO-certificate. The National Directive for vacuum pressure treated timber on which certification is based, is currently being revised. The new National Directive will contain a code of good practice including maximum leaching figures. It incorporates quality requirements for treated timber, existing legislative requirements an...
W J Homan, J K B Kwisthout, J Dubelaar


Evaluating possibilities of leaching of deltamethrin and TCMTB (insecticides and fungicide for protecting wood) by rain water or by soaking in water
1988 - IRG/WP 3464
Deltamethrin and TCMTB have been subjected to several field leaching tests on freshly fallen trees and in the laboratory, using standard EN 84. All the trials gave the same results and confirm that Deltamethrin and TCMTB are not washed out after they have been allowed to penetrate the trunk surface properly. According to the EN 84 standard, less than 1% Deltamethrin and less than 1.7% TCMTB were r...
J S Duguet, V Dartigues


Selective chromate elimination from the storage-drainage-water of a wood impregnation plant
1980 - IRG/WP 3153
With the Enviro-Chrom-Ex process it is possible to eliminate ecologically and economically hexavalent chromium (chromate) from water selectively. The process which is based on the principle of selective ion exchange works with different chromate concentrations and under the presence of other ions, irrespective of the water hardness. The values of water-offtake reach 0.1 mg CrVI at maximum, causing...
O Wälchli, R Ott, R Hugener, E Graf, B Lieberherr


Check development on jack pine logs in Eastern Canada
2001 - IRG/WP 01-10387
Logs in storage are subject to check damage. The severity of the problem may vary with various environmental and storage conditions. In this study, an investigation was conducted on the development of checks in debarked and bark-on jack pine (Pinus banksiana) logs in Eastern Canada. In the summer of 1999, jack pine trees were felled, logs were debarked and stored in a sawmill yard. The logs were i...
Dian-Qing Yang, R Beauregard


Treatability of waterstored poles of Norway spruce by sap-displacement and pressure treatment with Boliden K33 and creosote
1973 - IRG/WP 328
Poles of windthrown Norway spruce were stored in bark under water sprinklers for 11-20 months or fully submerged in a lake for 3 years (tab. 1 and 2). Water content after storage is shown in fig. 1 and 8. Treatment with Boliden K33 by sap-displacement (open tank suction) gave a poor result. The Danish requirements of delivery claim a penetration of 20 mm and a net retention of 12 kg/m³ in outer 2...
P Moltesen, E Borsholt, B Bang


Copper storage in the digestive caecae of Limnoria tripunctata and Limnoria quadripunctata (Crustacea: Isopoda) tunnelling in CCA treated and untreated wood in laboratory cultures
1998 - IRG/WP 98-10257
Digestive tract tissues of Limnoria quadripunctata Holthuis and Limnoria tripunctata Menzies, tunnelling untreated and CCA treated Scot's pine sapwood under laboratory conditions were examined using X-ray microanalysis and transmission electron microscopy. Populations of both Limnoria species tunnelling treated and untreated wood stored copper within their digestive caecae in the form of ...
C Wykes, A J Pitman, S M Cragg


A field test with anti-sapstain chemicals on sawn pine timber stored and seasoned under different conditions
1984 - IRG/WP 3245
Newly sawn timber of European redwood (Pinus sylvestris L.) was dip treated in four different anti-sapstain chemicals. The protectife effect against sapstain, mould and decay was examined after 10 weeks' and 10 months' storage in open and closed stacks. The results showed that the performance of individual chemicals was different in open and close stacks, although the wood as wel...
D J Dickinson, B Henningsson


The use of propionic acid to prevent Pinus patula biodeterioration during outside chip storage in Zululand
1989 - IRG/WP 3531
Pinus patula SCHIEDE ET DEPPE IN SCHLD. ET CHAM. is susceptible to biodeterioration during outside chip storage (OCS), reducing pulp quality and tear and burst indices of resulting paper. Accelerated laboratory trials showed that chips treated with 2% (w/v) propionic acid and stored for 17 weeks, produced pulp of quality indistinguishable from fresh untreated chips. Pulp tests during field trials ...
S Ismail, E J Smith, A A W Baecker


Next Page